Oxidation of High-temperature Alloy Wires in Dry Oxygen and Water Vapor

Small diameter wires (150 to 250 microns) of the high temperature alloys Haynes 188, Haynes 230, Haynes 230, Haynes 214, Kanthal Al and PM2000 were oxidized at 1204 C in dry oxygen or 50% H2O /50% O2 for 70 Hours. The oxidation kinetics were monitored using a thermogravimetric technique. Oxide phase composition and morphology of the oxidized wires were determined by X-ray diffraction,field emission scanning electron microscopy, and energy dispersive spectroscopy. The alumina-forming alloys, Kanthal Al and PM2000, out-performed the chromia-forming alloys under this conditions. PM2000 was recommended as the most promising candidate for advanced hybrid seal applications for space reentry control surface seals or hypersonic propulsion system seals. This study also demonstrated that thermogravimetric analysis of small diameter wires is a powerful technique for the study of oxide volatility, oxide adherence, and breakaway oxidation.

Opila, Elizabeth J.↗

Creep/Rupture Behavior of Melt-Infiltrated SiC/SiC Composites Being Investigated

The failure behavior of melt-infiltrated SiC/SiC ceramic matrix composites is under investigation at the NASA Glenn Research Center as part of NASA's Ultra-Efficient Engine Technology Program. This material was originally developed under the High Speed Research Office's Enabling Propulsion Materials Program. Creep and rupture data provide accelerated testing information to predict material behavior under engine use situations (1500 to 2400 F). This information gives insights into various material development paths to improve composites as well as improve understanding of failure mechanisms. The left figure shows the fracture surface of a CMC material following over 200 hr of testing at 2400 F. This surface demonstrates the kind of fibrous pullout desirable for maximum crack deflection, hence non-brittle failure. Microscopy suggests that creep and rupture of these materials can best be considered as a probabilistic property, rather than a material property. Fiber failure occurs first in isolated regions, while stronger adjacent fibers remain intact. The right figure shows a region where oxide deposits blur and round the fiber images. Because the oxidation kinetics of SiC are well understood, this oxide scale can be used as a measure of the length of time various regions of the composites have been exposed to the environment, hence providing vital information regarding the sequence of failure. The oxide scale in the right figure indicates an early failure of this tow of fibers, whereas adjacent tows remain oxide free, suggesting failure much later in time. The path of various cracks can be followed throughout the composite in this manner, suggesting failure mechanisms.

Hurst, Janet B.↗

Oxidation Protection of Porous Reaction-Bonded Silicon Nitride

Oxidation kinetics of both as-fabricated and coated reaction-bonded silicon nitride (RBSN) were studied at 900 and 1000 C with thermogravimetry. Uncoated RBSN exhibited internal oxidation and parabolic kinetics. An amorphous Si-C-O coating provided the greatest degree of protection to oxygen, with a small linear weight loss observed. Linear weight gains were measured on samples with an amorphous Si-N-C coating. Chemically vapor deposited (CVD) Si3N4 coated RBSN exhibited parabolic kinetics, and the coating cracked severely. A continuous-SiC-fiber-reinforced RBSN composite was also coated with the Si-C-O material, but no substantial oxidation protection was observed.

Fox, D. S.↗

Study of the effects of gaseous environments on sulfidation attack of superalloys

Studies were conducted to examine the effect of the gaseous corrodents NaCl, HCl, and NaOH on the high temperature oxidation and Na2SO4-induced corrosion behavior of the alumina former NiAl, the chromia former Ni-25 wt.% Cr, elemental Cr, and the superalloy B-1900. Experiments were conducted at 900 and 1050 C in air in the presence and absence of the gaseous corrodents. Effects involving both reaction rates and microstructural changes in oxide morphology were observed due to the presence of these corrodents at levels anticipated to be present in operating industrial and marine gas turbines. The effect of gaseous NaCl, HCl, and possibly NaOH on NiAl in simple oxidation was to remove aluminum from below the protective alumina layer and to simultaneously weaken the adherence of the protective alumina oxide scale to the substrate. The aluminum removed from below the oxide scale was redeposited on its surface as alpha-Al2O3 whiskers. With respect to the chromia formers, gaseous NaCl and HCl promoted breakaway oxidation kinetics and changes in the microstructures of the oxide scales.

Smeggil, J. G.↗

Grain boundary oxidation and fatigue crack growth at elevated temperatures

Fatigue crack growth rate at elevated temperatures can be accelerated by grain boundary oxidation. Grain boundary oxidation kinetics and the statistical distribution of grain boundary oxide penetration depth were studied. At a constant delta K-level and at a constant test temperature, fatigue crack growth rate, da/dN, is a function of cyclic frequency, nu. A fatigue crack growth model of intermittent micro-ruptures of grain boundary oxide is constructed. The model is consistent with the experimental observations that, in the low frequency region, da/dN is inversely proportional to nu, and fatigue crack growth is intergranular.

Liu, H. W.↗

Grain boundary oxidation and fatigue crack growth at elevated temperatures

Fatigue crack growth rate at elevated temperatures can be accelerated by grain boundary oxidation. Grain boundary oxidation kinetics and the statistical distribution of grain boundary oxide penetration depth were studied. At a constant delta K-level and at a constant test temperature, fatigue crack growth rate, da/dN, is a function of cyclic frequency, nu. A fatigue crack growth model of intermittent micro-ruptures of grain boundary oxide is constructed. The model is consistent with the experimental observations that, in the low frequency region, da/dN is inversely proportional to nu, and fatigue crack growth is intergranular.

Liu, H. W.↗

Characterization of Iridium Coated Rhenium Used in High-Temperature, Radiation-Cooled Rocket Thrusters

Materials used for radiation-cooled rocket thrusters must be capable of surviving under extreme conditions of high-temperatures and oxidizing environments. While combustion efficiency is optimized at high temperatures, many refractory metals are unsuitable for thruster applications due to rapid material loss from the formation of volatile oxides. This process occurs during thruster operation by reaction of the combustion products with the material surface. Aerojet Technical Systems has developed a thruster cone chamber constructed of Re coated with Ir on the inside surface where exposure to the rocket exhaust occurs. Re maintains its structural integrity at high temperature and the Ir coating is applied as an oxidation barrier. Ir also forms volatile oxide species (IrO2 and IrO3) but at a considerably slower rate than Re. In order to understand the performance limits of Ir-coated Re thrusters, we are investigating the interdiffusion and oxidation kinetics of Ir/Re. The formation of iridium and rhenium oxides has been monitored in situ by Raman spectroscopy during high temperature exposure to oxygen. For pure Ir, the growth of oxide films as thin as approximately 200 A could be easily detected and the formation of IrO2 was observed at temperatures as low as 600 C. Ir/Re diffusion test specimens were prepared by magnetron sputtering of Ir on Re substrates. Concentration profiles were determined by sputter Auger depth profiles of the heat treated specimens. Significant interdiffusion was observed at temperatures as low as 1000 C. Measurements of the activation energy suggest that below 1350 C, the dominant diffusion path is along defects, most likely grain boundaries, rather than bulk diffusion through the grains. The phases that form during interdiffusion have been examined by x ray diffraction. Analysis of heated test specimens indicates that the Ir-Re reaction produces a solid solution phase of Ir dissolved in the HCP structure of Re.

Stulen, R. H.↗

10 000-hr Cyclic Oxidation Behavior of 68 High-Temperature Co-, Fe-, and Ni- Base Alloys Evaluated at 982 deg. C (1800 deg. F)

Power systems with operating temperatures in the range of 815 to 982 C (1500 to 1800 F) frequently require alloys that can operate for long times at these temperatures. A critical requirement is that these alloys have adequate oxidation resistance. The alloys used in these power systems require thousands of hours of operating life with intermittent shutdown to room temperature. Intermittent power plant shutdowns, however, offer the possibility that the protective scale will tend to spall (i.e., crack and flake off) upon cooling, increasing the rate of oxidative attack in subsequent heating cycles. Thus, it is critical that candidate alloys be evaluated for cyclic oxidation behavior. It was determined that exposing test alloys to ten 1000-hr cycles in static air at 982 10 000-hr Cyclic Oxidation Behavior of 68 High-Temperature Co-, Fe-, and Ni-Base Alloys Evaluated at 982 C (1800 F) could give a reasonable simulation of long-time power plant operation. Iron- (Fe-), nickel- (Ni-), and cobalt- (Co-) based high-temperature alloys with sufficient chromium (Cr) and/or aluminum (Al) content can exhibit excellent oxidation resistance. The protective oxides formed by these classes of alloys are typically Cr2O3 and/or Al2O3, and are usually influenced by their Cr, or Cr and Al, content. Sixty-eight Co-, Fe-, and Ni-base high-temperature alloys, typical of those used at this temperature or higher, were used in this study. At the NASA Lewis Research Center, the alloys were tested and compared on the basis of their weight change as a function of time, x-ray diffraction of the protective scale composition, and the physical appearance of the exposed samples. Although final appearance and x-ray diffraction of the final scale products were two factors used to evaluate the oxidation resistance of each alloy, the main criterion was the oxidation kinetics inferred from the specific weight change versus time data. These data indicated a range of oxidation behavior including parabolic (typical of isothermal oxidation), paralinear, linear, and mixed-linear kinetics.

Barrett, Charles A.↗

The effect of yttrium and thorium on the oxidation behavior of Ni-Cr-Al alloys

The effect of quaternary additions of 0.5% Y, 0.5 and 1.0% Th to a base alloy of Ni-10CR-5Al on the oxidation behavior and mechanism was studied during oxidation in air over the range of 1000 to 1200 C. The presence of yttrium decreased the oxidation kinetics slightly, whereas, the addition of thorium caused a slight increase. Oxide scale adherence was markedly improved by the addition of the quaternary elements. Although a number of oxides formed on yttrium containing alloys, quantitative X-ray diffraction clearly showed that the rate-controlling step was the diffusion of aluminum through short circuit paths in a thin layer of alumina that formed parabolically with time. Although the scale adherence of the yttrium containing alloy was considerably better than the base alloys, spalling did occur that was attributed to the formation of the voluminous YAG particles which grew in a mushroom-like manner, lifting the protective scale off the subrate locally. The YAG particles formed primarily at grain boundaries in the substrate in which the yttrium originally existed as YNi9.

Kumar, A.↗

Brazing of Stainless Steel to Yttria-Stabilized Zirconia Using Gold-Based Brazes for Solid Oxide Fuel Cell Applications

Two gold-base active metal brazes (gold-ABA and gold-ABA-V) were evaluated for oxidation resistance to 850 C, and used to join yttria-stabilized zirconia (YSZ) to a corrosion-resistant ferritic stainless steel for possible use in solid oxide fuel cells. Thermogravimetric analysis and optical microscopy and scanning electron microscopy coupled with energy-dispersive spectroscopy were used to evaluate the braze oxidation behavior, and microstructure and composition of the YSZ/braze/steel joints. Both gold-ABA and gold-ABA-V exhibited nearly linear oxidation kinetics at 850 C, with gold-ABA-V showing faster oxidation than gold-ABA. Both brazes produced metallurgically sound YSZ/steel joints due to chemical interactions of Ti and V with the YSZ and steel substrates.

Singh, M.↗

Silicon Carbide Nanotube Oxidation at High Temperatures

Silicon Carbide Nanotubes (SiCNTs) have high mechanical strength and also have many potential functional applications. In this study, SiCNTs were investigated for use in strengthening high temperature silicate and oxide materials for high performance ceramic nanocomposites and environmental barrier coating bond coats. The high · temperature oxidation behavior of the nanotubes was of particular interest. The SiCNTs were synthesized by a direct reactive conversion process of multiwall carbon nanotubes and silicon at high temperature. Thermogravimetric analysis (TGA) was used to study the oxidation kinetics of SiCNTs at temperatures ranging from 800degC to1300degC. The specific oxidation mechanisms were also investigated.

Ahlborg, Nadia↗

Durability of YSZ coated Ti2AlC in 1300°C high velocity burner rig tests

A thermal barrier coating system survived 500 h in cyclic burner rig tests at 1300°C, exceeding the life of all previous systems. An yttria stabilized zirconia (7YSZ) thermal barrier coating (TBC) was plasma sprayed on the oxidation resistant Ti2AlC MAX phase and tested in a jet fuel burner. No coating spallation or recession was observed, only a 2.4 mg/sq.cm mass gain due to typical cubic Al2O3 oxidation kinetics. The modest weight gain contrasted with large TBC spallation or oxide volatility losses that might occur under cyclic, high velocity (~100 m/s) burner conditions. The coating surface exhibited colonies of [111]flourite fiber-textured columns separated by craze crack patterns, but with no visible moisture attack. The thickness of the alumina scale under the YSZ face was >20 μm, more than twice that formed on TBC/superalloy systems at failure. TiO2 nodules, initially formed on the uncoated backside, were then removed as volatile hydroxides formed in high temperature, high velocity water vapor (~10%). Overall, the test indicated the exceptional stability of the YSZ/Ti2AlC system under turbine conditions, due in large part to good thermal expansion matching.

alumina, MAX phases, thermal barrier coatings (TBC↗

Oxidation characteristics of Ti-14Al-21Nb ingot alloy

Static oxidation kinetics of Ti14Al21Nb (wt pct) ingot alloy were studied in air over the temperature interval of 649 to 1093 C in a thermogravimetric apparatus. The oxidation products were characterized by x ray diffraction, electron microprobe analysis, energy dispersive x ray analysis, and Auger electron spectroscopy. Cross-sections of the oxidized samples were also examined using light and scanning electron microscopy. The oxidation rate was substantially lower than the conventional alloys of titanium, but the kinetics displayed a complex behavior involving two or more oxidation rates depending on the temperature and duration of exposure. The primary oxide formed was TiO2, but this oxide was doped with Nb. Small amounts of Al2O3 and TiN were also present in the scale. Diffusion of oxygen into the alloy was observed and the diffusivity seemed to be dependent on the microstructure of the metal. A model was presented to explain the oxidation behavior of the alloy in terms of the reduction in the oxygen diffusivity in the oxide caused by the modification of the defect structure of TiO2 by Nb ions.

Sankaran, Sankara N.↗

Fundamentals of Passive Oxidation In SiC and Si3N4

The very slow oxidation kinetics of silicon carbide and silicon nitride, which derive from their adherent and passivating oxide films, has been explored at length in a broad series of studies utilizing thermogravimetric analysis, electron and optical micrography, energy dispersive spectrometry, x-ray diffractometry, micro-analytical depth profiling, etc. Some interesting microstructural phenomena accompanying the process of oxidation in the two materials will be presented. In Si3N4 the oxide is stratified, with an SiO2 topscale (which is relatively impervious to O2)underlain by a coherent subscale of silicon oxynitride which is even less permeable to O2- Such "defence in depth" endows Si3N4 with what is perhaps the highest oxidation resistance of any material, and results in a unique set of oxidation processes. In SiC the oxidation reactions are much simpler, yet new issues still emerge; for instance, studies involving controlled devitrification of the amorphous silica scale confirmed that the oxidation rate of SiC drops by more than an order of magnitude when the oxide scale fully crystallizes.

Thomas-Ogbuji, Linus U.↗

A Theoretical Investigation of Oxidation Efficiency of a Volatile Removal Assembly Reactor Under Microgravity Conditions

Volatile Removal Assembly (VRA) is a subsystem of the Closed Environment Life Support System (CELSS) installed in the International Space Station. It is used for removing contaminants (volatile organics) in the wastewater produced by the space station crews. The major contaminants are formic acid, ethanol, and propylene glycol. The VRA contains a slim packbed reactor (3.5 cm diameter and four 28 cm long tubes in series) to perform catalyst oxidation of wastewater at elevated pressure and temperature under microgravity conditions. In the reactor, the contaminants are burned with oxygen gas (O2) to form water and carbon dioxide (CO2) that dissolves in the water stream. Optimal design of the reactor requires a thorough understanding about how the reactor performs under microgravity conditions. The objective of this study was to develop a mathematical model to interpret experimental data obtained from normal and microgravity conditions, and to predict the performance of VRA reactor under microgravity conditions. Catalyst oxidation kinetics and the total oxygen-water contact area control the efficiency of catalyst oxidation for mass transfer, which depends on oxygen gas holdup and distribution in the reactor. The process involves bubbly flow in porous media with chemical reactions in microgravity environment. This presents a unique problem in fluid dynamics that has not been studied. Guo et al. (2004) developed a mathematical model that predicts oxygen holdup in the VRA reactor. No mathematical model has been found in the literature that can be used to predict the efficiency of catalyst oxidation under microgravity conditions.

Guo, Boyun↗

Optical and Probe Diagnostics Applied to Reacting Flows

The general theme of the research my NASA colleague and I have planned is "Optical and probe diagnostics applied to reacting flows". We plan to explore three major threads during the fellowship period. The first interrogates the flame synthesis of carbon nanotubes using aerosol catalysts. Having demonstrated the viability of the technique for nanotube synthesis, we seek to understand the details of this reacting system which are important to its practical application. Laser light scattering will reveal changes in particle size at various heights above the burner. Analysis of the flame gas by mass spectroscopy will reveal the chemical composition of the mixture. Finally, absorption measurements will map the nanotube concentration within the flow. The second thread explores soot oxidation kinetics. Despite the impact of soot on engine performance, fire safety and pollution, models for its oxidation are inhibited by uncertainty in the values of the oxidation rate. We plan to employ both optical and microscopic measurements to refine this rate. Cavity ring-down absorption measurements of the carbonaceous aerosol can provide a measure of the mass concentration with time and, hence, an oxidation rate. Spectroscopic and direct probe measurements will provide the temperature of the system needed for subsequent modeling. These data will be benchmarked against changes in soot nanostructures as revealed by transmission electron microscopic images from directly sampled material.

Ticich, Thomas M.↗

Short-time oxidation of zirconium.

Study of zirconium oxidation kinetics for maximum exposure times of 3 min and in the temperature range 440 to 850 C. 'Discontinuous' oxidation runs were employed whereby a specimen was inserted into the gas stream for a predetermined time, removed and weighed, and reinserted into the oxidation atmosphere. It is considered that the increase in the observed activation energy for the early stage parabolic oxidation is a manifestation of a change from an n-type oxide to a predominantly p-type oxide, in agreement with the authors' earlier conclusion (1971) based on pressure effects.

Srivastava, L. P.↗

Effect of oxidation on the mechanical properties of a NbAl3 alloy at intermediate temperatures

The effect of environment on the mechanical properties of an Nb-67Al-7Cr-0.25W-0.5Y alloy was investigated experimentally in the temperature range 800-1200 K. It is found that the severity of environmental attack in the alloy is determined by both matrix plasticity and oxidation kinetics. The former determines the ability of the matrix to accommodate the localized stresses generated during deformation and oxidation, while the latter governs the rate of formation of a protective oxide scale. The environmental degradation of the alloy can thus be reduced or eliminated by increasing atomic mobility.

Raj, S. V.↗