Search NASA⌕ Search

SEARCH · Search NASA

Results for “polysiloxane”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

High-Speed Fabrication of Lithium-Ion Battery Electrodes by UV-Curing

In this study, UV-curing was investigated as an alternative method to provide fast production of composite cathodes and significantly reduce the time and energy required for solvent removal in lithium-ion battery fabrication. To serve our purpose, low-molecular-weight polysiloxane acrylate (PSA) was designed and synthesized from a polysiloxane epoxide precursor. In the presence of the acrylic acid additive LiNi1/ 3Mn1/3Co1/3O2 (NMC), electrode laminates containing 10 wt% PSA binder were successfully fabricated by UVcuring. The cured electrode exhibited good mechanical and electrochemical properties. At current rates up to C/3, the cell performance of the UV-cured NMC electrode was comparable to that of conventional polyvinylidene fluoride (PVDF)-bound NMC electrode. Our initial success in applying high-speed UV-curing in composite electrode fabrication has proved that it is a promising route to substantially reducing the capital and operation costs of lithium-ion battery electrode manufacturing and additionally bringing about important environmental benefits.

binder↗

Controlled In Situ Foaming for Mechanical Responsiveness of Architected Foams

Addition of chemical blowing agents to polysiloxane resins produces foams with closed–cell morphology. Combining this chemistry with the 3D–printing technique direct ink writing (DIW) permits the creation of architected foams with controllable, hierarchical tiers of porosity. Here, using a two–component foaming ink, the extent of foaming can be controlled by incorporating an active mixing printhead as part of the fabrication process. Changes in the mixing speed allows for in situ control of the foaming reaction where the mixing speed is directly correlated with the resulting foaming that occurs upon extrusion. These architected foams display tunable mechanical responses, porosities, and open–to–closed cell ratios. While chemically blown polysiloxane foam is a well–established material, utilizing DIW as fabrication technique presents a novel approach for creating tailored, architected foams that require minimal post–processing.

36 MATERIALS SCIENCE↗

3D Printing of Transparent Silicone Elastomers

Here in this paper, inks for transparent elastomers that are formulated by matching the refractive index of silica and polysiloxanes are described. The transparent inks transmit up to ≈90% of 700 nm light through 1 cm and remain transparent when solidified. The inks and solidified materials exhibit a thermochromic effect. This thermochromic effect can be controlled by the refractive index mismatch. Transparency may increase or decrease as temperature increases, depending on the refractive index mismatch of the base polysiloxane and silica. It is found that the rheological properties of the ink depend on the distribution of silica particles, which is dictated by silica functionality, weight content, and processing. Siloxane precursors that vary in chemical functionality are introduced to tailor the mechanical properties of the printed elastomers, which obtain stretchability >65% along with a tensile modulus of 1.9 MPa. After optimizing siloxane chemistry and ink processing, the authors are able to print transparent elastomers. Potential applications are demonstrated for printed structures by printing encapsulation structures for light-emitting diodes, semitransparent dye-filled structures, a microfluidic mixing device, and a multimaterial structure that exhibits temperature-dependent camouflage.

36 MATERIALS SCIENCE↗

Siloxane-modified polycarbosilane flexible Prepregs for fabrication of ceramic matrix composites via compression molding and PIP densification

For this work, the development of ceramic matrix composites (CMCs) using 5 harness satin carbon fiber fabric impregnated with commercial polycarbosilane precursor plasticized by siloxane copolymer was investigated aiming to improve wetting behavior and shape conformability. The polycarbosilane precursor and polysiloxane plasticizer were mixed at varying weight ratios to obtain flexible preceramic resin prepreg cloths. 13 plies of preceramic polymer prepreg cloths were stacked in 0/90° layup and cured by compression molding, followed by densified via PIP process. The CMCs were densified with eight PIP cycles followed by final crystallization at 1600 °C. The CMCs made with 10 wt% polysiloxane loading showed lower viscosity of the prepreg resin as well as higher strength and displacement to failure compared to those fabricated from unplasticized polycarbosilane prepolymer. In contrast, at higher concentration of plasticizer, viscosity of the prepreg resin increased, and the CMC became more brittle; however, it exhibited considerably higher thermal conductivity.

Carbosilane↗

Spectroscopic Signatures of MQ-Resins in Silicone Elastomers

Polysiloxane elastomers have a large application space due to their versatile cross-linking chemistry and highly tunable physical and mechanical properties. One approach for improving the mechanical integrity of commercial polysiloxane “silicone” elastomers while maintaining their optical transparency is the addition of small, silicone-resin molecules to the network. However, both the poly(dimethylsiloxane) (PDMS) network and the silicone-resin particles have an amorphous structure and complex chemistry, which makes the characterization of their structural properties and segmental network dynamics difficult. Here, we report the synthesis and characterization of a series of model silicone networks modified with a specific class of silicone-resin known as MQ-resin using Raman and advanced nuclear magnetic resonance (NMR) spectroscopy methods. Raman spectroscopy was successfully used to quantify the contribution of the MQ-resin to the network, to determine the type of MQ-resin present in the network, and to investigate the completeness of the network cross-linking reaction. Furthermore, solid-state and 1H double-quantum (DQ) NMR spectroscopies were used not only as a detection method for the MQ-resins but also to quantify changes in the segmental dynamics of the network as a function of MQ-resin concentration. The combination of Raman and NMR spectroscopies describes a series of samples where the MQ-resin particles and PDMS chains maintain their independent segmental dynamics up to high concentrations of MQ-resins (40–50% MQ), where the physical properties of the resin dominate the physical properties of the overall network. The results from our spectroscopic analyses are consistent with the results from macroscopic characterization techniques such as solvent uptake and mechanical testing. The spectroscopic insights into the structure–property relationships of PDMS-MQ composites presented in this study are a valuable tool not only for the synthesis and reverse engineering of future generations of commercial silicone elastomers but also for understanding the mechanisms of aging and degradation over the material lifetime.

36 MATERIALS SCIENCE↗

Effect of Diphenyl Content on Viscoelasticity of Poly(dimethyl- co -diphenyl)siloxane Melt and Network

Polydimethylsiloxane (PDMS) is one of the most widely used polymeric materials for sealants, adhesives, lubricants, and thermal as well as electrical insulation. At low temperatures, however, PDMS is subject to crystallization that can cause deterioration in mechanical function. A common way to suppress such crystallization is through the incorporation of phenylsiloxane into the backbone of polysiloxane. Nevertheless, the introduction of phenyl components, even in small quantities, could potentially change the properties of the siloxane in a significant way. In this work, a series of mechanical tests and finite element simulations were performed to study the macroscale viscoelasticity of two poly(dimethyl-co-diphenyl)siloxane formulations in order to understand the effects of a few percent diphenyl contents on the viscoelasticity of the polysiloxane material. Here, we utilized the small-angle X-ray scattering to investigate the microscopic structures of the copolymers and broadband dielectric spectroscopy and rheology to probe the chain dynamics at the microscale. The results of these characterizations were used to inform the finite element simulations. We found that the degree of cross-linking does not significantly alter the microstructure but can profoundly affect the viscoelastic response of the copolymer networks. The corresponding hysteretic behavior is interpreted in terms of reptation-like motion and relaxation of the effective free chains in the cured polymer network. The relaxation of the copolymer chains is slowed significantly by even a small increase in the molar ratio of the diphenyl component.

36 MATERIALS SCIENCE↗

Investigating structure and dynamics of unentangled poly(dimethyl- co -diphenyl)siloxane via molecular dynamics simulation

Polysiloxane is one of the most important polymeric materials in technological use. Polydimethylsiloxane displays glass-like mechanical properties at low temperatures. Incorporation of phenyl siloxane, via copolymerization for example, improves not only the low-temperature elasticity but also enhances its performance over a wide range of temperatures. Copolymerization with the phenyl component can significantly change the microscopic properties of polysiloxanes, such as chain dynamics and relaxation. However, despite much work in the literature, the influence of such changes is still not clearly understood. In this work, we systematically study the structure and dynamics of random poly(dimethyl- co -diphenyl)siloxane via atomistic molecular dynamics simulations. As the molar ratio Φ of the diphenyl component increases, we find that the size of the linear copolymer chain expands. At the same time, the chain-diffusivity slows down by over an order of magnitudes. In conclusion, the reduced diffusivity appears to be a result of a complex interplay between the structural and dynamic changes induced by phenyl substitution.

36 MATERIALS SCIENCE↗

Outgassing of casted and 3D printed silicones

Outgassing of 3D printed and casted silica-filled silicones was studied using a standard ASTM E-595 procedure and a modified Soreq’s method that allows very sensitive measurements of the outgassing kinetics even at low temperatures, 20 – 50 °C. We studied three different silica-filled silicones, non-porous cased M9787, and 3D printed LL50 and 40P materials. The present report shows that vacuum outgassing products of polysiloxane-based materials include multiple species. In addition to chemisorbed and physisorbed water outgassing, previously studied by TPD, polymer fragments of varying sizes evaporate as well. The chemical composition of the condensable volatile species collected on a Germanium substrate, was analyzed by FTIR. It was shown that all studied materials produce mostly PDMS-based outgassing products that form stable droplet-like structure on the Ge substrate. The highest amount of the condensable volatile species was measured for LL50. Isothermal TGA in nitrogen atmosphere of the LL50 material was compared to the standard vacuum outgassing. The results of TGA showed lower mass loss and higher water regain. The kinetics of the outgassing at relatively low temperatures of 20, 30 and 50 °C was studied using Thermoelectric Quartz Crystal Microbalance (TQCM). The TQCM surface was held at -10 °C to enhance condensation of the outgassed moisture. The analysis presented here, when combined with the extensive previous work on moisture outgassing, provides a better understanding of the aging mechanism of polysiloxane-based materials. In this work we show that outgassing techniques, usually applied for qualification of polymers for space-related applications, may be used as a complementary method to study thermal degradation and aging of silica-based silicones. Our results indicate that the long-term degradation mechanics and thermal degradation products depend primarily on the chemical composition of silicone-based material and only slightly affected by the manufacturing process. Surprisingly, the surface-to-volume ratio of the 3D printed vs. casted/molded materials showed only minor effect on the outgassing kinetic parameters.

36 MATERIALS SCIENCE↗

Toxicity of pyrolysis gases from some cellular polymers

Various samples of cellular polymers were evaluated for toxicity of pyrolysis gases, using the screening test method developed at the University of San Francisco. The cellular polymer samples included polyimide, polymethacrylimide, polybismaleimide, polyurethane, polyisocyanurate, polyethylene, polychloroprene, polyvinyl chloride, polystyrene, polysiloxane, and polyphosphazene. The cellular polymers exhibited varying levels of toxicity under these test conditions. Among the rigid cellular polymers, times to death were shortest with the imide type foams and longest with polyvinyl chloride and polystyrene. Among the flexible cellular polymers, times to death were shortest with polyimide and polyester, and longest with polychloroprene and polysiloxane. Increased char yield was not necessarily associated with reduced toxicity.

Hilado, C. J.↗

Surface characterization of LDEF materials

The NASA Long Duration Exposure Facility (LDEF), a passive experimental satellite, was placed into low-Earth orbit by the Shuttle Challenger in Apr. 1984. The LDEF spent an unprecedented 69 months in space. The flight and recovery of the LDEF provided a wealth of information on the longterm space environmental effects of a variety of materials exposed to the low-Earth orbit environment. Surface characterization of LDEF materials included polymers, composites, thermal control paints, and aluminum. X-ray photoelectron spectroscopy (XPS), Auger electron spectroscopy (AES), scanning electron microscopy (SEM), and contact angle analysis were used to document changes in both the surface composition and surface chemistry of these materials. Detailed XPS analysis of the polymer systems, such as Kapton, polyimide polysiloxane copolymers, and fluorinated ethylene propylene thermal blankets on the backside of the LDEF revealed significant changes in both the surface composition and surface chemistry as a result of exposure to the low-Earth orbit environment. Polymer systems such as Kapton, polyimide polysiloxane copolymers, and polysulfone showed a common trend of decreasing carbon content and increasing oxygen content with respect to the control sample. Carbon 1s curve fit XPS analysis of the composite samples, in conjunction with SEM photomicrographs, revealed significant ablation of the polymer matrix resin to expose the carbon fibers of the composite during exposure to the space environment. Surface characterization of anodized aluminum tray clamps, which were located at regular intervals over the entire LDEF frame, provided the first results to evaluate the extent of contamination with respect to position on the LDEF. The XPS results clearly showed that the amount and state of both silicon and fluorine contamination were directly dependent upon the position of the tray clamp on the LDEF.

Wightman, J. P.↗

Reaction and Protection of Electrical Wire Insulators in Atomic-oxygen Environments

Atomic-oxygen erosion on spacecraft in low Earth orbit is an issue which is becoming increasingly important because of the growing number of spacecraft that will fly in the orbits which have high concentrations of atomic oxygen. In this investigation, the atomic-oxygen durability of three types of electrical wire insulation (carbon-based, fluoropolymer, and polysiloxane elastomer) were evaluated. These insulation materials were exposed to thermal-energy atomic oxygen, which was obtained by RF excitation of air at a pressure of 11-20 Pa. The effects of atomic-oxygen exposure on insulation materials indicate that all carbon-based materials erode at about the same rate as polyamide Kapton and, therefore, are not atomic-oxygen durable. However, the durability of fluoropolymers needs to be evaluated on a case by case basis because the erosion rates of fluoropolymers vary widely. For example, experimental data suggest the formation of atomic fluorine during atomic-oxygen amorphous-fluorocarbon reactions. Dimethyl polysiloxanes (silicone) do not lose mass during atomic-oxygen exposure, but develop silica surfaces which are under tension and frequently crack as a result of loss of methyl groups. However, if the silicone sample surfaces were properly pretreated to provide a certain roughness, atomic oxygen exposure resulted in a sturdy, non-cracked atomic-oxygen durable SiO2 layer. Since the surface does not crack during such silicone-atomic oxygen reaction, the crack-induced contamination by silicone can be reduced or completely stopped. Therefore, with proper pretreatment, silicone can be either a wire insulation material or a coating on wire insulation materials to provide atomic-oxygen durability.

Hung, Ching-Cheh↗

Development of Highly-Conductive Polyelectrolytes for Lithium Batteries

Future NASA and Air Force missions require reliable and safe sources of energy with high specific energy and energy density that can provide thousands of charge-discharge cycles at more than 40% depth- of-discharge and that can operate at low temperatures. All solid-state batteries have substantial advantages with respect to stability, energy density, storage fife and cyclability. Among all solid-state batteries, those with flexible polymer electrolytes offer substantial advantages in cell dimensionality and commensurability, low temperature operation and thin film design. The above considerations suggest that lithium-polymer electrolyte systems are promising for high energy density batteries and should be the systems of choice for NASA and US Air Force applications. Polyelectrolytes (single ion conductors) are among most promising avenues for achieving a major breakthrough 'in the applicability of polymer- based electrolyte systems. Their major advantages include unit transference number for the cation, reduced cell polarization, minimal salt precipitation, and favorable electrolyte stability at interfaces. Our research is focused on synthesis, modeling and cell testing of single ion carriers, polyelectrolytes. During the first year of this project we attempted the synthesis of two polyelectrolytes. The synthesis of the first one, the poly(ethyleneoxide methoxy acrylateco-lithium 1,1,2-trifluorobutanesulfonate acrylate, was attempted few times and it was unsuccessful. We followed the synthetic route described by Cowie and Spence. The yield was extremely low and the final product could not be separated from the impurities. The synthesis of this polyelectrolyte is not described in this report. The second polyelectrolyte, comb polysiloxane polyelectrolyte containing oligoether and perfluoroether sidechains, was synthesized in sufficient quantity to study the range of properties such as thermal stability, Li- ion- conductivity and stability toward lithium metal. Also, the batteries containing this polyelectrolyte were assembled and tested. The results are detailed below. The synthesis of another polyelectrolyte similar to polysiloxane polyelectrolyte has been started, however, the synthesis was not completed due to termination of the project.

Shriver, D. F.↗

Processing and Characterization of Basalt Fiber Reinforced Ceramic Composites for High Temperature Applications Using Polymer Precursors

The development of high temperature structural composite materials has been very limited due to the high cost of the materials and the processing needed. Ceramics can take much higher temperatures, but they are difficult to produce and form in bulk volumes. Polymer Derived Ceramics (PDCs) begin as a polymer matrix, allowing a shape to be formed, to be cured, and be pyrolized in order to obtain a ceramic with the associated thermal and mechanical properties. The two PDCs used in this development are polysiloxane and polycarbosilane. Polysiloxanes contain a silicon oxycarbide backbone when pyrolized up to 1000degC. Polycarbosilane, an organosilicon polymer, contain a silicon-carbon backbone; around 1200degC, -SiC begins to crystallize. The use of basalt in structural and high temperature applications has been under development for over 50 years, yet there has been little published research on the incorporation of basalt fibers as a reinforcement in composites. Basalt is a naturally occurring material found in volcanic rock. Continuous basalt fiber reinforced PDCs have been fabricated and tested for the applicability of this composite system as a high temperature structural composite material. Testing for this included thermal and mechanical testing per ASTM standard tests.

High Temperature Composites↗

Processing and Characterization of Basalt Fiber Reinforced Ceramic Composites for High Temperature Applications Using Polymer Precursors

The development of high temperature structural composite materials has been very limited due to the high cost of the materials and the processing needed. Ceramics can take much higher temperatures, but they are difficult to produce and form in bulk volumes. Polymer Derived Ceramics (PDCs) begin as a polymer matrix, allowing a shape to be formed and cured and then to be pyrolized in order to obtain a ceramic with the associated thermal and mechanical properties. The two PDCs used in this development are polysiloxane and polycarbosilane. Polysiloxanes contain a silicon oxycarbide backbone when pyrolized up to 1000C. Polycarbosilane, an organosilicon polymer, contain a silicon-carbon backbone; around 1200C, beta-SiC begins to crystallize. The use of basalt in structural and high temperature applications has been under development for over 50 years, yet there has been little published research on the incorporation of basalt fibers as a reinforcement in composites. Basalt is a naturally occurring material found in volcanic rock. Continuous basalt fiber reinforced PDCs have been fabricated and tested for the applicability of this composite system as a high temperature structural composite material. Thermal and mechanical testing includes oxyacetylene torch testing and three point bend testing.

Ceramic Matrix Composites↗

Processing and Characterization of Basalt Fiber Reinforced Ceramic Composites for High Temperature Applications Using Polymer Precursors

The development of high temperature structural composite materials has been very limited due to the high cost of the materials and the processing needed. Ceramics can take much higher temperatures, but they are difficult to produce and form in bulk volumes. Polymer Derived Ceramics (PDCs) begin as a polymer matrix, allowing a shape to be formed and cured and then to be pyrolized in order to obtain a ceramic with the associated thermal and mechanical properties. The two PDCs used in this development are polysiloxane and polycarbosilane. Polysiloxanes contain a silicon oxycarbide backbone when pyrolized up to 1000 deg C. Polycarbosilane, an organosilicon polymer, contain a silicon-carbon backbone; around 1200 deg C, Beta-SiC begins to crystallize. The use of basalt in structural and high temperature applications has been under development for over 50 years, yet there has been little published research on the incorporation of basalt fibers as a reinforcement in composites. Basalt is a naturally occurring material found in volcanic rock. Continuous basalt fiber reinforced PDCs have been fabricated and tested for the applicability of this composite system as a high temperature structural composite material. Thermal and mechanical testing includes oxyacetylene torch testing and three point bend testing.

Polymer Derived Ceramics↗

Silicone-containing composition

A silicone-containing composition comprises the reaction product of a first component and an excess of an isocyanate component relative to the first component to form an isocyanated intermediary. The first component is selected from one of a polysiloxane and a silicone resin. The first component includes a carbon-bonded functional group selected from one of a hydroxyl group and an amine group. The isocyanate component is reactive with the carbon-bonded functional group of the first component. The isocyanated intermediary includes a plurality of isocyanate functional groups. The silicone-containing composition comprises the further reaction product of a second component, which is selected from the other of the polysiloxane and the silicone resin. The second component includes a plurality of carbon-bonded functional groups reactive with the isocyanate functional groups of the isocyanated intermediary for preparing the silicone-containing composition.

36 MATERIALS SCIENCE↗

Cross-linked polymeric membranes for carbon dioxide separation

A membrane useful in gas separation, the membrane comprising a cross-linked polysiloxane structure having a cross-link density of about 0.1.times.10.sup.-5 mol/cm.sup.3 to about 6.times.10.sup.-5 mol/cm.sup.3, where, in particular embodiments, the cross-linked polysiloxane structure has the following general structure: ##STR00001## wherein R.sup.1, R.sup.2, R.sup.3, R.sup.4, R.sup.5, and R.sup.6 are independently selected from hydrocarbon groups having at least 1 and up to 6 carbon atoms; A.sup.1 and A.sup.2 are independently selected from cyclic hydrocarbon groups; L.sup.1 and L.sup.2 are linking groups or covalent bonds; n is an integer of at least 1; r and s are independently selected from integers of at least 1; and p is an integer of at least 10. The invention also includes methods for making and using the above-described membranes for gas separation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrolyte for electrochemical cell

The electrolyte includes a cyclic polysiloxane having one or more side chains that each includes a poly(alkylene oxide) moiety and a spacer. Each spacer is positioned between the poly(alkylene oxide) moiety and a silicon on the main chain of the polysiloxane.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗