Mechanisms and kinetics of nickel chromite and cobalt chromite spinel formation Final report
Reaction kinetics and mechanisms of nickel chromite and cobalt chromite spinel formation
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Reaction kinetics and mechanisms of nickel chromite and cobalt chromite spinel formation
Oxide spinel formation kinetics and reaction mechanisms with emphasis on Ni and Co chromites, discussing cation diffusion
Homogeneous static deformation method crystals in NaCl and spinel structures using homogeneous static deformation method
Spinel lithium ferrite magnetic and crystallographic properties, considering effects of Li and oxygen losses, sintering temperature and cooling rate
Thermal expansion of nickel and cobalt spinels and their solid solutions
Cobalt and copper ferrite spinels as catalysts in oxidative dehydrogenation of butenes
Lunar 12 spinel compositional variation and textures as petrogenetic indicators, showing magma differentiation by crystal settling after lunar surface extrusion
The opaque mineralogy of the Luna 16 soil sample is studied, with an emphasis on a detailed survey of the compositional variations of the Fe-Ti-Cr-Al-Mg spinels. Analytical data are also presented for ilmenite. Textural characteristics and shock-metamorphic effects on the opaque minerals are briefly described and comparisons are made throughout between the Luna 16 samples and published and unpublished data on the Apollo samples.
Review of some of the results of a reflection microscopy and electron microprobe study performed on a part of the Luna 20 soil sample designated as the East Coast Consortium aliquot. The study is restricted to analyses of the oxides of Fe, Ti, Mg, Mn, Cr, and Al in this sample. The spinel mineral group, ilmenite and rutile only are discussed.
An X-ray structural study was made of a lunar spinel sample from the Sea of Fertility. The chemical composition and distribution of cations in the structure were characterized. Interpretation of the experimental data by the least squares method yielded the oxygen parameter u = 0.261 and the isotropic temperature factor 1.09 AU squared.
The partitioning of chromium between olivines, spinels and silicate liquids was studied as a function of temperature, oxygen fugacity, and cooling rate between 1175 and 1300 C and redox states near the Fe-FeO buffer. It is found that the weight ratio of Cr2O3 in olivine to that in the liquid increases slightly as oxygen fugacity decreases, but the effect is very small. The cooling experiments showed that the Cr2O3 content does not re-equilibrate with cooling.
Several objects have been found in sections of lunar igneous spinel troctolite 62295 that resemble certain meteoritic barred olivine chondrules. Each consists of an apparently spherical single crystal of Fo90 olivine, approximately 0.6-0.8 mm in diameter, containing a set of approximately 30-40 subparallel stringers of An95 plagioclase, whereas the stringers in ordinary meteoritic chondrules consist of glass. The olivine of the 62295 chondrules is also more magnesian, and is radially zoned, having a relatively iron-rich core and rim and an iron-poor intermediate zone. Several possible origins are proposed: impact-generated melt globules solidified in flight, spherical phenocrysts, and meteoritic chondrules, but none of these seems adequate to explain the detailed observations.
A two-layer lunar crust model is proposed in light of geochemical relationships between spinel cataclasites and anorthosites, discussing the relative abundances of these rocks. The uppermost stratigraphic unit of this model consists of members of the anorthositic series, and is estimated to be 12-20 km thick. The lower, Mg-rich unit consists of rocks with cotectic mineralogical proportions, and may constitute the greatest volume of the crust.
Magnesium aluminate spinel was tested in a water environment at room temperature to establish its slow crack-growth behavior. Ring specimens with artificial flaws on the outside surface were loaded hydraulically on the inside surface. The time to failure was measured. Various precracking techniques were evaluated and multiple precracks were used to minimize the scatter in the static fatigue tests. Statistical analysis techniques were developed to determine the strength and crack velocities for a single flaw. Slow crack-growth rupture was observed at stress intensities as low as 70 percent of K sub c. A strengthening effect was observed in specimens that had survived long-time static fatigue tests.
A significant increase in energy density may be possible if a two-unit alkaline regenerative H2-O2 fuel cell is replaced with a single-unit system that uses passive means for H2O transfer and thermal control. For this single-unit system, new electrocatalysts for the O2 electrode will be required which are not only bifunctionally active but also chemically and electrochemically stable between the voltage range of about 0.7 and 1.5 V. NiCo2O4 spinel is reported to have certain characteristics that make it useful for a study of electrode fabrication techniques. High surface area NiCo2O4 powder was fabricated into unsupported, bifunctional, PTFE-bonded, porous gas fuel cell electrodes by commercial sources using varying PTFE contents and sintering temperatures. The object of this study is to measure the bifunctional activities of these electrodes and to observe what performance differences might result from different commercial electrode fabricators. O2 evolution and O2 reduction data were obtained at 80 C (31 percent KOH). An irreversible reaction (i.e., aging) occurred during O2 evolution at potentials greater than about 1.5 V. Anodic Tafel slopes of 0.06 and 0.12 V/decade were obtained for the aged electrodes. Within the range of 15 to 25 percent, the PTFE content was not a critical parameter for optimizing the electrode for O2 evolution activity. Sintering temperatures between 300 and 340 C may be adequate but heating at 275 C may not be sufficient to properly sinter the PTFE-NiCo2O4 mixture. Electrode disintegration was observed during O2 reduction. Transport of O2 to the NiCo2O4 surface became prohibitive at greater than about -0.02 A/sq cm. Cathodic Tafel slopes of -0.6 and -0.12 V/decade were assumed for the O2 reduction process. A PTFE content of 25 percent (or greater) appears to be preferable for sintering the PTFE-NiCo2O4 mixture.
The solubility and partitioning of Ar in natural anorthite, diopside, forsterite, spinel, and synthetic iron-free basaltic melts was investigated using a new technique that obviates the postquenching phase separation. It was found that the solubility of Ar in the minerals was surprisingly high. Moreover, the solubility of Ar in different samples of a particular mineral run in the same experiment varied more than the solubility in the same sample run in different experiments, suggesting that noble gases are held in lattice vacancy defects. Moreover, the results of TEM imaging revealed no anomalous microstructures, while EXAFS studies of some samples showed that Kr has no preferred site in the lattices, supporting the defect siting conclusion.
The kinetics of the olivine-spinel transformation in Ni2SiO4 were investigated in an in situ X-ray diffraction experiments in which synchrotron radiation was used as an X-ray source. The starting material was Ni2SO4 olivine which was hot-pressed in situ at 980 C and 2.5 GPa; during the transformation, X-ray diffraction patterns were collected at intervals of 30 or 120 sec. The kinetic data were analyzed using Cahn's (1956) model. The activation energy for growth at 3.6-3.7 GPa was estimated as 438 + or - 199 kJ/mol. It is shown that, in order to make significant extrapolations of the kinetic data to a geological scale, the dependence of the rates of both nucleation and growth on temperature and pressure must be evaluated separately.
Most Ca-Al-rich inclusions (CAls) from Allende are surrounded by a series of mineralogically distinct rim layers. Proposed modes of formation for these layers include flash heating, evaporation, and condensation. The innermost of these rim layers is generally spinel (SP), in some cases intergrown with perovskite (PV), and commonly containing varying amounts of secondary iron increasing towards the edge of the CAI. The SP or SP+PV rim is not always contiguous with the other rim layers, indicating that it is probably the result of a separate event. We have produced continuous SP rims on synthetic analogs representing Type A/B1, average Type B, and Type B2 bulk compositions by reheating a solid glass experimental charge to subliquidus crystallization temperatures. This experimental result is consistent with the formation of chondrules; and CAIs by more than one sequence of heating and cooling. Previous work indicated that prior crystallization events produced observable effects in the texture and chemistry of the final run product. Information on the nature of the heating/cooling cycles experienced by CAls and chondrules is important in modeling the environment of their formation. Additional information is contained in the original extended abstract.