At least 73 records · Page 4

Deep learning approaches to semantic segmentation of fatigue cracking within cyclically loaded nickel superalloy

Improvements to synchrotron-based micro-computed tomography scanning capabilities have gifted researchers the ability to characterize 4D material thermomechanical responses more thoroughly than ever before. These advancements, however, have brought about new challenges in analyzing the resulting deluge of data. We report on a nickel-based superalloy specimen imaged 26 times in-situ during cyclic loading at Argonne National Laboratory Advanced Photon Source beamline 1ID, in order to monitor crack growth within the microstructure. Therefore, several deep learning approaches which utilize convolutional neural networks are implemented to segment crack features from reconstructed tomography scans. U-Net architecture implementations are found to be especially effective, achieving IoU = 0.995 +/- 0.004 and Matthews correlation coefficient scores of Φ = 0.826 +/- 0.085. These advancements broaden possibilities for scientists seeking to automate segmentation analyses of similar large datasets.

36 MATERIALS SCIENCE↗

High Temperature Oxidation Behavior of Ni-based High Entropy Superalloys

A new class of polycrystalline gamma-prime strengthened superalloys with alloy compositions of (wt%) Ni-20Co-13Cr-6Fe-4Al-3W-2Mo-(4-x)Nb-(x)Ti (x = 0,1,2) were subjected to cyclic oxidation exposures in dry air at 800 °C for 3600 h. The alloys were borderline chromia/alumina formers, showing good oxidation resistance relative to commercially available materials of similar composition. While all alloys formed alumina scales initially, only the alloy with the lowest Ti/Nb ratio retained an alumina scale for the duration of the exposure. Formation of a continuous layer of rutile TiO 2 at the alumina/alloy interface is proposed to cause eventual alumina failure for the alloys containing Ti.

36 MATERIALS SCIENCE↗

Creep anisotropy modeling and uncertainty quantification of an additively manufactured Ni-based superalloy

The advantages offered by additive manufacturing over traditional processes has driven a great deal of industrial and academic interest in recent years. However, the process is relatively new and requires additional investigation to become sufficiently mature for wide scale industrial adoption. Electron beam melting powder bed fusion is one technology that has shown promise for fabricating high temperature resistant materials such as nickel based superalloys. The resulting microstructures typically exhibit a strong fiber texture in the build direction giving rise to anisotropic time-dependent deformation behavior. In order to accelerate the qualification of these materials for industrial adoption accurate numerical models are needed for simulating their behavior. In this work a crystal plasticity model including non-Schmid effects is presented for capturing creep anisotropy observed in additively manufactured IN738LC. The model is calibrated via a probabilistic framework where model parameters are treated as random variables. An iterative sequential design strategy is utilized to efficiently identify the probability density of the unknown model parameters. As a case study the model is utilized to investigate the behavior of randomly oriented equiaxed grain clusters sometimes observed embedded in the additively manufactured columnar structure. A synthetic realization is simulated and uncertainty is propagated through to the full-field response. Results indicate that these features are the source of significant creep relaxation and strain accumulation which partially explains observed grain boundary decohesion at these locations.

36 MATERIALS SCIENCE↗

Characterization of γ′/γ″ compact and sandwich type precipitates during long-term high-temperature exposure in Ni-based superalloys

Here, the formation of γ′/γ″ co-precipitates is investigated in Ni-based superalloys with a varying Ti/Al ratio and Ta content and their stability is studied using long-term high-temperature exposure. Transmission electron microscopy and atom probe tomography analyses demonstrate that both higher Ti/Al ratios and increased Ta promote γ″ phase formation, leading to sandwich and compact structures. The compact co-precipitation significantly reduces γ′ precipitate coarsening during 10,000 h exposure at 700°C by restricting elemental diffusion, particularly of aluminum, from the γ matrix to the γ′ phase. For the alloy without a compact structure, and only γʹ precipitates, at the beginning of the exposure, the coarsening rate over 10,000 h was 3.5 times faster than for the alloy with compact γʹ/γʺ precipitates. Evidence of destabilization of the compact morphology was found to occur between 5,000 and 10,000 h exposure and originated from the extensive formation and growth of δ platelets that extended throughout the grains. Thus, the outer layer of the compact, which consists of γʺ, was subjected to the γ″ to δ phase transformation.

gamma double prime↗

Microstructural evolution and hardness changes in ion irradiated nickel-based Haynes 282 superalloy

This study investigated the crucial aspects of thermal and irradiation stability in precipitation hardened Haynes 282 Ni-based superalloy. The Haynes 282 Ni-based alloy was irradiated by 8 MeV Ni 3+ ions to assess its resistance to phase instabilities and mechanical property alterations. The mid-range doses (at a depth of ∼1 µm) were 1 and 10 displacements per atom (dpa) at temperatures of 600°C and 750°C. Nanoindentation tests provided insights into bulk equivalent hardness of the irradiated and pristine regions, while scanning transmission electron microscopy (STEM) and energy dispersive X-ray spectroscopy (EDS) were used to examine the microstructural evolution of irradiation-induced defects and γ′ -Ni 3 (Al, Ti) precipitates and defect structure under irradiation. These precipitates, with an average diameter of 29 nm and a number density of 5 x 10 21 /m 3 , acted as robust dispersion strengthening agents with high radiation point defect sink strength. Remarkably, irradiation did not significantly alter the size or number density of the γ′ precipitates, indicating exceptional thermal stability and radiation resistance of these precipitates at the examined conditions. Radiation-induced dislocation loops were observed at 600°C, albeit without a substantial impact on mechanical properties due to the dominance of γ′ precipitates on the overall alloy strength. The superior stability of γ′ precipitates observed in this study contrasts with several previous research findings on Ni-based alloys that reported poor precipitate stability. Plausible reasons for this difference are discussed. Moreover, this work explicitly outlines a physically grounded approach to ensure accurate microstructure-hardness correlations and clarifies the hardening model by addressing common misapplications of superposition in prior studies.

36 MATERIALS SCIENCE↗

On the effect of elemental partitioning to secondary phases after solution and aging heat treatments in a Co-Ni-based superalloy

Here, this paper presents the phase stability and elemental partitioning in a Co-40Ni-10Al-7.5W-10Cr-3Nb-0.06B-0.6C (at.%) superalloy (referred to as 3Nb) after a two-step heat treatment. The resulting microstructure consisted of γ, γ', MC carbides and µ-Co 7 W 6 phase decorating the regions near and at the grain boundaries. Nb preferentially partitioned to the γ'-phase and other elements such as Ni, Cr and W were responsible for the μ-phase formation.

36 MATERIALS SCIENCE↗

Elevated temperature nanoscratch of Inconel 617 Superalloy

Inconel 617 superalloy is a main candidate to be used for mechanical and tribo-components in high temperature helium-cooled reactors. Recent findings show that it grows a unique surface oxide, especially under high temperature helium with distinct wear, friction, and contact properties. Here, this study reports the elevated temperature nanoscratch behavior of Inconel 617 and further utilizes it to understand the effect of temperature on contact friction constituent contributors, adhesion and plowing at small scales. Inconel 617 is aged in high temperature helium, and consequently, the total kinetic friction coefficient of the alloy surface oxide is obtained in temperatures ranging from 25 °C to 400 °C. A finite element model is developed and validated based on the experimental results. The model is then utilized along with previously established techniques to determine the adhesion and plowing components of the friction coefficient. At small scale, the experimental results show that with increasing temperature the friction coefficient increases. It was inferred that this increase is mainly due to the increased contribution of plowing friction at high levels of deformation.

36 MATERIALS SCIENCE↗

Implications of carbon content for the processing, stability, and mechanical properties of cast and wrought Ni-based superalloy Nimonic 105

As the temperature and pressure requirements in land-based turbines for power generation increase, the shift towards more advanced alloys, e.g., Ni-based superalloys, requires improved understanding of their long-term stability and mechanical properties. Additionally, the larger size of the components also presents fabrication and cost-reduction problems. In this study, we investigated Nimonic 105 as a potential rotor material at two carbon content levels – the commonly used maximum of the alloy specification and a lower carbon content variant. Reducing the carbon content presented fabrication challenges, resulting in surface crack formation during hot working. Additionally, a lower M 6 C carbide fraction was present after fabrication/solutioning, leading to a significantly larger grain size. After the standard aging treatment, similar γ' populations formed in the two variants, however the M 6 C carbides in the high-carbon variant already started transforming to intergranular M 23 C 6 . Although we did not observe a noticeable effect on the tensile properties of the two variants, the lower carbon content alloy possessed a superior creep property – mainly due to the larger grain size as the microstructural stability was inferior. Further, upon prolonged thermal exposure, the M 6 C carbides in the low-carbon variant further decomposed to intergranular and intragranular σ and μ precipitates, as opposed to mainly M 23 C 6 as in the high-carbon variant.

36 MATERIALS SCIENCE↗

Directed energy deposition of Haynes 282 nickel superalloy

Laser powder directed energy deposition was employed to fabricate Haynes® 282 Ni-based superalloy for high temperature creep testing. Material was heat treated using a single-step aging heat treatment of 800 °C for 4 h. Microstructural analysis was conducted in the as-deposited, solution-annealed, and age-hardened conditions. γ′ precipitates were absent in the as-deposited and annealed condition but formed during aging with an average size of 48.5 ± 12 nm. γ’ denuded zones ranging in thickness from 73 to 469 nm were observed adjacent to an effectively continuous grain boundary carbide film that covered 72.5% of the measured boundary length. The heat-treated material contained a high-volume fraction of TiC carbides ranging in size from 38 to 457 nm. Electron backscatter diffraction showed partial recrystallization, with 77-83% recrystallized area and a heterogeneous grain-size distribution. Creep testing at 750 °C at 300, 320, and 350 MPa revealed significantly inferior performance compared to wrought material, with higher strain rates, earlier tertiary onset, and shorter rupture lives. Fractography shows that failure was dominated by intergranular rupture. Post rupture microstructural analysis results suggest that the creep behavior was primarily governed by the non-equilibrium interface network rather than the bulk γ/γ’ matrix. In conclusion, the findings indicate that achieving wrought-like creep performance necessitates substantial improvements in the additive process, specifically focusing on enhanced homogenization, full recrystallization, and precise control over the morphology and distribution of carbides.

36 - MATERIALS SCIENCE↗

Partitioning of tramp elements Cu and Si in a Ni-based superalloy and their effect on creep properties

An alloy's processing history, including melting, remelting or the choice of stock material, affects its purity and eventually involves tramp element pickup or retention. Herein, variants of a novel Ni-based superalloy were manufactured with different levels of purity. The so-called low purity alloys contained 0.138 wt. % Cu and 0.019 wt. % Si while the Cu and Si levels were below x-ray fluorescence (XRF) detection limits of 0.003 and 0.010 wt. %, respectively, in the high purity ingots. Atom-probe tomography (APT) was carried out and revealed Si partitioning at the following interfaces: grain boundaries, MC carbide/γ, M 3 B 2 boride/$γ$ and M 3 B 2 boride/$γ$'. Copper was found to primarily segregate to the $γ$' precipitates. An average of 2.4 × decrease in creep life and 4.3 × decrease in creep ductility was measured in the low purity alloys, which was attributed to the embrittlement caused by Si segregation to grain boundaries. Furthermore, the positive effect of B on the creep properties was mitigated by the presence of Si. Thermodynamic predictions for the matrix and γ' precipitate compositions represented the trends observed experimentally although the extent of preferential partitioning lacks accuracy. Monte Carlo simulations were performed to describe the partitioning of Cu and Si atoms to either $γ$ or $γ$' phases.

36 MATERIALS SCIENCE↗

The detrimental effect of elemental contaminants when using B additions to improve the creep properties of a Ni-based superalloy

The effect of Si contamination when using B to improve the creep properties of a Ni-based superalloy was investigated using advanced characterization techniques and first-principles simulations on alloys with high and low B levels with varying Si contents. The positive effect of B segregation along grain boundaries on the creep properties was mitigated by the presence of Si which showed a similar segregation preference. Density functional theory calculations were used for validation by calculating grain boundary cleavage energies. Silicon was shown to decrease grain boundary cohesion which offsets the positive effect of B.

36 MATERIALS SCIENCE↗

Characterization of Build Parameters and Microstructure in Low Heat Input WAAM of Ni-Based Superalloy Haynes 282

Ni-based superalloy Haynes® 282® is being targeted for various applications in advanced power generation systems for its superior fabricability, weldability, and excellent high temperature creep and corrosion performance. This process optimization study aims to use a low heat-input, high deposition rate, controlled Gas Metal Arc Welding (GMAW) process, Cold Metal Transfer (CMT) by Fronius, attempting to achieve fully dense fabrication and possibly avoid the need for HIP. Twenty-one multilayer blocks (~25x100x40 mm3) were deposited to explore a large set of build parameters variations that focused on varying the travel speed from 14 to 42 inches per minute (ipm) and wire feed speed from 150 to 450 ipm. A strong correlation has been observed between arc energy – controlled primarily by travel and wire feed speed. Initial visual inspection, internal microstructural examination, and computed tomography (CT) have been used to determine the effects of built parameters on evolution of internal porosity and defects. Scanning electron microscopy techniques enabled structural and compositional imaging of heterogeneity and changes in microstructural properties.

additive manufacturing↗

Machine Learning Vacancy Formation Energy in Nickel-Based Superalloys

Thermal vacancies play a critical role in high-temperature Ni-based superalloys and influence various properties such as creep resistance, oxidation, etc. This study systematically investigates the impact of commonly used transition metals (Cr, Co, Fe), refractory metals (Nb, Ta, Mo, W) and other elements (Al, Cu, Ti, Mn) on the thermodynamic stability of 36 binary, 20 ternary, 11 quaternary, 9 quinary, and 3 senary FCC Ni-based alloys covering various elemental combinations. Density functional theory-based studies on Ni-X binary alloys show that higher concentrations of Cr, Nb, Ta, Al, and Ti introduce significant lattice distortions and broaden the distribution of vacancy formation energies (standard deviation up to 0.15 eV). These elements partially donate electrons, reducing their self-consistent chemical potentials relative to single-element reference values and lowering vacancy formation energies, while Co, Fe, Mo, and W show lower charge localization. These trends extend from 3-6 element alloys, where Cr, Nb, and Ta-rich compositions have low-energy states (~0.5 eV) that increase vacancy concentrations. Finally, graph neural network models are developed to screen over 5000 virtual alloys. Eleven leading compositions are identified with mean vacancy formation energy higher than 1.75 eV and vacancy concentration ~2 orders of magnitude lower than pure Ni at 1000 K. These results provide valuable guidelines to achieve controlled defect engineering in structural alloys.

DFT↗

Strength in Rotary Friction Welding of Five Dissimilar Nickel-Based Superalloys

Advanced manufacturing processes improve the cost and quality of goods. Rotary friction welding is a fast, energy-efficient, and reliable joining process for metals, but new applications are hindered by large development costs for each new alloy. Each alloy set has different welding characteristics; therefore, lessons learned from a single alloy are not always broadly applicable. To establish knowledge that is applicable across multiple alloys, a family of different superalloys were welded to discover process trends that were applicable beyond a single alloy set. In this study, weld symmetry did not correlate to weld strength across alloy systems. Some alloys’ strongest welds occurred at maximum symmetry, whereas high asymmetry was associated with different alloys’ maximum strength. High feed rates, high welding forces, low energy, and low temperatures all resulted in high-strength welds across all alloy and geometry combinations. Tensile strengths greater than 95% of base-metal strength were recorded for most alloy systems.

36 MATERIALS SCIENCE↗

Residual stress and microstructure in IN718-René41 graded superalloy fabricated by laser blown directed energy deposition

Additively printed Ni-based superalloy with a compositionally graded transition from IN718 to René41 was fabricated by laser blown-powder directed energy deposition (DED/LB-M), with the goals of meeting location-specific temperature capability and reducing component cost for hot gas path turbine components. Residual stress distribution in thin wall specimens with three sets of DED build parameters in the as-built and stress-relieved states was measured by neutron diffraction. For calculating residual stress, the calculated d0 method was found to be more appropriate as stress-free reference than using the lattice spacing measured from the stress-relief heat treated specimens. Longer dwell time (lower interpass temperature), higher energy input, smaller layer thickness resulted in a higher magnitude of tensile residual stresses at edges and compressive residual stresses at center of the specimens. The residual stress results did not show a strong dependence on graded compositions, indicating that the residual stress build-up was more geometry and process dependent. Non-destructive neutron imaging based on the attenuation coefficient qualitatively visualized the compositional variation in the bulk and showed good agreement with quantitative Electron Probe Micro-Analysis (EPMA) measurement. Grain structure, texture, and residual plastic strain along the build direction were characterized by Electron Backscatter Diffraction (EBSD). Long columnar grains with (001) preferred grain orientation were dominant along the build direction. Compositional change did not show an obvious effect on the epitaxial growth of dendrites and the continuation of the columnar grains. Residual plastic strain was relatively low in the as-built specimens.

36 MATERIALS SCIENCE↗

Ab Initio Simulation of Structure and Properties in Ni-Based Superalloys: Haynes282 and Inconel740

The electronic structure, interatomic bonding, and mechanical properties of two supercell models of Ni-based superalloys are calculated using ab initio density functional theory methods. The alloys, Haynes282 and Inconel740, are face-centered cubic lattices with 864 atoms and eleven elements. These multi-component alloys have very complex electronic structure, bonding and partial-charge distributions depending on the composition and strength of the local bonding environment. We employ the novel concept of total bond order density (TBOD) and its partial components (PBOD) to ascertain the internal cohesion that controls the intricate balance between the propensity of metallic bonding between Ni, Cr and Co, and the strong bonds with C and Al. We find Inconel740 has slightly stronger mechanical properties than Haynes282. Both Inconel740 and Haynes282 show ductile natures based on Poisson’s ratio. Poisson’s ratio shows marginal correlation with the TBOD. Comparison with more conventional high entropy alloys with equal components are discussed.

36 MATERIALS SCIENCE↗

Enabling Multi-Material Structures of Co-Based Superalloy Using Laser Directed Energy Deposition Additive Manufacturing

Cobalt superalloys such as Tribaloys are widely used in environments that involve high temperatures, corrosion, and wear degradation. Additive manufacturing (AM) processes have been investigated for fabricating Co-based alloys due to design flexibility and efficient materials usage. AM processes are suitable for reducing the manufacturing steps and subsequently reducing manufacturing costs by incorporating multi-materials. Laser directed energy deposition (laser DED) is a suitable AM process for fabricating Co-based alloys. T800 is one of the commercially available Tribaloys that is strengthened through Laves phases and of interest to diverse engineering fields. However, the high content of the Laves phase makes the alloy prone to brittle fracture. In this study, a Ni-20%Cr alloy was used to improve the fabricability of the T800 alloy via laser DED. Different mixture compositions (20%, 30%, 40% NiCr by weight) were investigated. The multi-material T800 + NiCr alloys were heat treated at two different temperatures. These alloy chemistries were characterized for their microstructural, phase, and mechanical properties in the as-fabricated and heat-treated conditions. SEM and XRD characterization indicated the stabilization of ductile phases and homogenization of the Laves phases after laser DED fabrication and heat treatment. In conclusion, the NiCr addition improved the fabricability and structural integrity of the T800 alloy.

36 MATERIALS SCIENCE↗