At least 73 records · Page 4

The effect of environment on mechanical properties of coated and uncoated alloys

Combined creep and corrosion testing, as well as creep testing of pre-oxidized specimens has been used to assess the effect of oxidation on alloy creep strength. Exposure in wet air for up to 1500 h at 650 C for alloy T92 resulted in the formation of a 80 m thick oxide scale that did not affect the alloy creep resistance. Alloy 230 creep properties were also only slightly affected by pre oxidation for 2000 h in steam at 800 C. Application of an aluminide coating protected the alloy from oxidation but decreased the substrate mechanical properties because of the weak coating mechanical properties. Stress was found to have an effect on the Fe-rich oxide grown on alloy T92 during oxidation in wet air by promoting cracking of the scale. However, no effect of the creep deformation was observed on the aluminide coating integrity. In-situ steam testing is necessary to provide relevant data for lifetime models of in-service components.

36 MATERIALS SCIENCE↗

Comparison of Heparin-Coated and Conventional Split-Tip Hemodialysis Catheters

Catheter coatings have the potential to decrease infection and thrombosis in patients with chronic dialysis catheters. We report our midterm experience with a heparin-coated dialysis catheter. This retrospective, case-control study was approved by our Institutional Review Board. A total of 88 tunneled dialysis catheters were inserted over a 13-month period via the internal jugular vein. Thirty-eight uncoated split-tip catheters and 50 heparin-coated catheters were inserted. Primary catheter patency was compared between the two groups using the log rank test, with infection and/or thrombosis considered as catheter failures. Dialysis parameters during the first and last dialysis sessions, including pump speed, actual blood flow, and arterial port pressures, were compared using unpaired t-tests. Primary patency of the uncoated catheters was 86.0 {+-} 6.5% at 30 days and 76.1 {+-} 8.9% at 90 days. Primary patency of heparin-coated catheters was 92.0 {+-} 6.2% at 30 days and 81.6 {+-} 8.0% at 90 days (p = 0.87, log rank test). Infection requiring catheter removal occurred in four patients with uncoated catheters and two patients with heparin-coated catheters (p = 0.23). Catheter thrombosis requiring catheter replacement or thrombolysis occurred in one patient with an uncoated catheter and two patients with heparin-coated catheters (p = 0.9). No differences in catheter function during hemodialysis were seen between the two groups. In conclusion, the heparin-coated catheter did not show a significantly longer patency compared to the uncoated catheter. The flow characteristics of this device were comparable to those of the conventional uncoated catheter. A demonstrable benefit of the heparin-coated catheter in randomized trials is needed before a recommendation for routine implementation can be made.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Effects of Interface Modification on Mechanical Behavior of Hi-Nicalon Fiber-Reinforced Celsian Matrix Composites

Unidirectional celsian matrix composites having approx. 42 volume percent of uncoated or BN/SiC-coated Hi-Nicalon fibers were tested in three-point bend at room temperature. The uncoated fiber-reinforced composites showed catastrophic failure with strength of 210 +/- 35 MPa and a flat fracture surface. In contrast, composites reinforced with BN/SiC-coated fibers exhibited graceful failure with extensive fiber pullout. Values of first matrix cracking stress and strain were 435 +/- 35 MPa and 0.27 +/- 0.01 %, respectively, with ultimate strength as high as 960 MPa. The elastic Young's modulus of the uncoated and BN/SiC-coated fiber-reinforced composites were measured as 184 q 4 GPa and 165 +/- 5 GPa, respectively. Fiber push-through tests and microscopic examination indicated no chemical reaction at the uncoated or coated fiber-matrix interface. The low strength of the uncoated fiber-reinforced composite is probably due to degradation of the fibers from mechanical surface damage during processing. Because both the coated and uncoated fiber reinforced composites exhibited weak interfaces, the beneficial effect of the BN-SiC dual layer is primarily the protection of fibers from mechanical damage during processing.

Bansal, Narottam P.↗

Hi-Nicalon Fiber-Reinforced Celsian Matrix Composites: Influence of Interface Modification

Unidirectional celsian matrix composites having 42-45 vol % of uncoated or BN-SIC coated Hi-Nicalon fibers were tested in three-point bend at room temperature. The uncoated fiber-reinforced composites showed catastrophic failure with strength of 210 35 MPa and a flat fracture surface. In contrast, composites reinforced with coated fibers exhibited graceful failure with extensive fiber pullout. Values of first matrix cracking stress and strain were 435 +/- 35 MPa and 0.27 +/- 0.01%, respectively, with ultimate strength as high as 960 MPa. The elastic Young modulus of the uncoated and coated fiber-reinforced composites were 184 +/- 4 GPa and 165 +/- 5 GPa, respectively. Fiber push-through tests and microscopic examination indicated no chemical reaction at the uncoated or coated fiber-matrix interface. The low strength of composite with uncoated fibers is due to degradation of the fiber strength from mechanical damage during processing. Because both the coated- and uncoated-fiber-reinforced composites exhibited weak interfaces, the beneficial effect of the BN-SIC dual layer is primarily the protection of fibers from mechanical damage during processing.

Bansal, Narottam P.↗

Oversizing and Restenosis with Self-Expanding Stents in Iliofemoral Arteries

Purpose: Uncoated self-expanding nitinol stents (NS) are commonly oversized in peripheral arteries. In current practice, 1-mm oversizing is recommended. Yet, oversizing of NS may be associated with increased restenosis. To provide further evidence, NS were implanted in porcine iliofemoral arteries with a stent-to-artery-ratio between 1.0 and 2.3. Besides conventional uncoated NS, a novel self-expanding NS with an antiproliferative titanium-nitride-oxide (TiNOX) coating was tested for safety and efficacy. Methods: Ten uncoated NS and six TiNOX-coated NS (5-6 mm) were implanted randomly in the iliofemoral artery of six mini-pigs. After implantation, quantitative angiography (QA) was performed for calculation of artery and minimal luminal diameter. Follow-up was performed by QA and histomorphometry after 5 months. Results: Stent migration, stent fracture, or thrombus formation were not observed. All stents were patent at follow-up. Based on the location of the stent (iliac/femoral) and the stent-to-artery-ratio, stent segments were divided into 'normal-sized' (stent-to-artery-ratio < 1.4, n = 12) and 'oversized' (stent-to-artery-ratio {>=} 1.4, n = 9). All stent segments expanded to their near nominal diameter during follow-up. Normal-sized stent segments increased their diameter by 6% and oversized segments by 29%. A significant correlation between oversizing and restenosis by both angiography and histomorphometry was observed. Restenosis rates were similar for uncoated NS and TiNOX-coated NS. Conclusions: TiNOX-coated NS are as safe and effective as uncoated NS in the porcine iliofemoral artery. All stents further expand to near their nominal diameter during follow-up. Oversizing is linearly and positively correlated with neointimal proliferation and restenosis, which may not be reduced by TiNOX-coating.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Effects of Fiber Coatings on Tensile Properties of Hi-Nicalon SiC/RBSN Tow Composites

Uncoated Hi-Nicalon silicon carbide (SiC) fiber tows and those coated with a single surface layer of pyrolytic boron nitride (PBN), double layers of PBN/Si-rich PBN, and boron nitride (BN)/SiC coatings deposited by chemical vapor deposition (CVD) method were infiltrated with silicon slurry and then exposed to N2, for 4 hr at 1200 and 1400 C. Room temperature ultimate tensile fracture loads and microstructural characterization of uncoated and CVD coated Hi-Nicalon SiC fiber reinforced reaction-bonded silicon nitride (RBSN) tow composites were measured to select suitable interface coating(s) stable under RBSN processing conditions. Results indicate that room temperature ultimate fracture loads of the uncoated Hi-Nicalon SiC/RBSN tow composites nitrided at both temperatures were significantly lower than those of the uncoated Hi-Nicalon tows without slurry infiltration. In contrast, all CVD coated Hi-Nicalon SiC/RBSN tow composites retained a greater fraction of the dry tow fracture load after nitridation at 1200 C, but degraded significantly after nitridation at 1400 C. Reaction between metal impurities (Fe and Ni) present in the attrition milled silicon powder and uncoated regions of SiC fibers appears to be the probable cause for fiber degradation.

Bhatt, Ramakrishna T.↗

Effects of HF Treatments on Tensile Strength of Hi-Nicalon Fibers

Tensile strengths of as-received Hi-Nicalon fibers and those having a dual BN/SiC surface coating, deposited by chemical vapor deposition, have been measured at room temperature. These fibers were also treated with HF for 24 h followed by tensile strength measurements. Strengths of uncoated and BN/SiC coated Hi-Nicalon fibers extracted from celsian matrix composites, by dissolving away the matrix in HF for 24 h, were also determined. The average tensile strength of uncoated Hi-Nicalon was 3.19 +/- 0.73 GPa with a Weibull modulus of 5.41. The Hi-Nicalon/BN/SiC fibers showed an average strength of 3.04 q 0.53 GPa and Weibull modulus of 6.66. After HF treatments, the average strengths of the uncoated and BN/SiC coated Hi-Nicalon fibers were 2.69 +/- 0.67 GPa and 2.80 +/- 0.53 GPa and the Weibull moduli were 4.93 and 5.96, respectively. The BN/SiC coated fibers extracted from the celsian matrix composite exhibited a strength of 2.38 +/- 0.40 GPa and a Weibull modulus of 7.15. The strength of the uncoated Hi-Nicalon fibers in the composite was so severely degraded that they disintegrated into small fragments during extraction with HF. The uncoated fibers probably undergo mechanical surface damage during hot pressing of the composites. Also, the BN layer on the coated fibers acts as a compliant layer which protects the fibers from mechanical damage during composite processing. The elemental composition and thickness of the fiber coatings were deten-nined using scanning Auger analysis. Microstructural analyses of the fibers and the coatings were done by scanning electron microscopy and transmission electron microscopy. Strengths of fibers calculated using average and measured fiber diameters were in good agreement. Thus, the strength of fibers can be evaluated using an average fiber diameter instead of the measured diameter of each filament.

Bansal, Narottam P.↗

Gear Performance Improved by Coating

Gears, bearings, and other mechanical elements transmit loads through contacting surfaces. Even if properly designed, manufactured, installed, and maintained, gears and bearings will eventually fail because of the fatigue of the working surfaces. Economical means for extending the fatigue lives of gears and bearings are highly desired, and coatings offer the opportunity to engineer surfaces to extend the fatigue lives of mechanical components. A tungsten-containing diamondlike-carbon coating exhibiting high hardness, low friction, and good toughness was evaluated for application to spur gears. Fatigue testing was done at the NASA Glenn Research Center on both uncoated and coated spur gears. The results showed that the coating extended the surface fatigue lives of the gears by a factor of about 5 relative to the uncoated gears. For the experiments, a lot of spur test gears made from AISI 9310 gear steel were case-carburized and ground to aerospace specifications. The geometries of the 28-tooth, 8-pitch gears were verified as meeting American Gear Manufacturing Association (AGMA) quality class 12. One-half of the gears were randomly selected for coating. The method of coating was selected to achieve desired adherence, toughness, hardness, and low-friction characteristics. First the gears to be coated were prepared by blasting (vapor honing) with Al2O3 particles and cleaning. Then, the gears were provided with a thin adhesion layer of elemental chromium followed by magnetron sputtering of the outer coating consisting of carbon (70 at.%), hydrogen (15 at.%), tungsten (12 at.%), and nickel (3 at.%) (atomic percent at the surface). In total, the coating thickness was about 2.5 to 3 microns. As compared with the steel substrate, the coated surface was harder by a factor of about 2 and had a smaller elastic modulus. All gears were tested using a 5-centistoke synthetic oil, a 10,000-rpm rotation speed, and a hertzian contact stress of at least 1.7 GPa (250 ksi). Tests were run until either surface fatigue occurred or 300 million stress cycles were completed. Tests were run using either a pair of uncoated gears or a pair of coated gears (coated gears mated with uncoated gears were not evaluated). The fatigue test results, shown on Weibull coordinates in the graph, demonstrate that the coating provided substantially longer fatigue lives even though some of the coated gears endured larger stresses. The increase in fatigue life was a factor of about 5 and the statistical confidence for the improvement is high (greater than 99 percent). Examination of the tested gears revealed substantial reductions of total wear for coated gears in comparison to uncoated gears. The coated gear surface topography changed with running, with localized areas of the tooth surface becoming smoother with running. Theories explaining how coatings can extend gear fatigue lives are research topics for coating, tribology, and fatigue specialists. This work was done as a partnership between NASA, the U.S. Army Research Laboratory, United Technologies Research Corporation, and Sikorsky Aircraft.

Krantz, Timothy L.↗

Hydrothermal Corrosion of SiC Materials for Accident Tolerant Fuel Cladding with and Without Mitigation Coatings

As a candidate material for accident-tolerant fuel cladding for light water reactors (LWR), SiCf–SiC composite materials possess many attractive properties. However, prior work has shown that SiC is susceptible to aqueous dissolution in LWR coolant environments. To address this issue, candidate coatings have been developed to inhibit dissolution. For this study, CVD SiC samples were prepared with Cr, CrN, TiN, ZrN, NiCr, and Ni coatings. Uncoated SiC and SiCf–SiC samples were also prepared. The samples were exposed for 400 h in 288 °C water with 2 wppm DO in a constantly-refreshing autoclave to simulate BWR–NWC. Cr and Ni coated samples lost less mass than the uncoated SiC sample, indicating an improvement in performance. The CrN coating resisted oxidation, but some of the coating was lost due to poor adhesion. The TiN coated sample gained significant mass due to oxidation of the coating. ZrN and NiCr coatings showed significant corrosion attack. SiCf–SiC ceramic matrix composite materials dissolved much faster than the CVD SiC sample, demonstrating the need for mitigation coatings if CMCs are to be used in LWRs. This work demonstrates the promise of Cr, Ni and CrN coatings for corrosion mitigation in LWRs, and shows that NiCr and ZrN are not promising coating materials.

Raiman, Stephen S.↗

Biocompatibility and Recanalization Characteristics of Hydrogel Microspheres with Polyzene-F as Polymer Coating

The objective of this study was to evaluate inflammatory response and recanalization after embolization with a new spherical embolic agent based on a core and shell design with a hydrogel core of polymethylmethacrylate (PMMA) and a Polyzene-F nanoscale coating in a porcine kidney model. Thirty-six minipigs were enrolled for superselective renal embolization. Polyzene-F-coated PMMA particles and uncoated PMMA particles with a diameter of 300-600 {mu}m were used. Either 4 or 12 weeks post-embolization, arteriography of the embolized kidneys was performed and then compared with pre- and immediate post-embolization arteriograms using a specific recanalization score to determine the extent of recanalization. Using a microscopic inflammation score (Banff classification), the embolized organs were examined for local inflammatory effects which occurred in response to the embolic agent. In Polyzene-F-coated particles, the Banff classification showed an average inflammation score of 0.26 {+-} 0.58 at 4 weeks and of 0.08 {+-} 0.28 at 12 weeks. In uncoated particles, the Banff score measured 0.37 {+-} 0.6 at 4 weeks, which was higher, but without a statistically significant difference. According to the recanalization score used in this study, mild angiographic recanalization was evident in all groups, without statistically significant differences (3.0 {+-} 0.71 in coated particles, 3.09 {+-} 0.81 in uncoated particles; p = 0.74). We conclude that both uncoated hydrogel particles and Polyzene-F-coated embolic agents triggered virtually no inflammatory response and effectively occluded target arteries. This study demonstrates good biocompatibility of the new embolic material. As in other spherical embolic agents, recanalization can occur to some degree.

62 RADIOLOGY AND NUCLEAR MEDICINE↗

Influence of MAO Treatment on the Galvanic Corrosion Between Aluminum Alloy and 316L Steel

To slow down the galvanic corrosion of aluminum alloy and 316L stainless steel in subsea water, a micro-arc oxidation (MAO) coating was prepared on the surface of the Al alloy, and no treatment was performed on the surface of the 316L. The surface morphology of MAO-coated Al alloy was evaluated using a scanning electron microscope (SEM) before and after corrosion. A micro-hardness tester was used to measure the micro-hardness. Corrosion behaviors were evaluated by open-circuit potential (OCP), potentiodynamic polarization (PDP) and electrode impedance spectroscopy (EIS) tests in a 3.5 g/L NaCl solution. The results of PDP testing show that the corrosion potential of the MAO-coated galvanic pair was more positive than that of the uncoated galvanic pair and that the corrosion current density was smaller than that of the uncoated galvanic pair. EIS results show that the impedance of the galvanic pair increased after MAO coating. SEM images show that the corrosion damage of the uncoated Al alloy was more severe than that of the MAO-coated one, and the post-corrosion images of the surface of the 316L connected with MAO-coated Al alloy were more compact than those of the 316L connected with uncoated Al alloy. A physical model was developed to discuss the influence of MAO treatment on the galvanic corrosion process and corrosion mechanism.

36 MATERIALS SCIENCE↗

Impacts of PTL coating gaps on cell performance for PEM water electrolyzer

The anode porous transport layer (PTL) is a critical component of polymer electrolyte membrane (PEM) water electrolyzers, providing electrical conduction and water/oxygen transport to the anode catalyst layer. Platinum group metal (PGM) coatings are applied to titanium PTLs to prevent oxidation and preserve conductivity. To implement PEM water electrolysis on a large scale, it is essential to minimize the cost of mass-manufactured cell components while ensuring that defects in materials and components do not adversely affect the performance of the cell. In this study, we created gaps in the Pt coatings that are typically applied to PTLs to understand their effects on cell performance and inform on fabrication tolerances. The PTL coatings were fabricated by sputter deposition of Pt, intentionally leaving uncoated regions in either large patches or thin strips. For either geometry, the cell performance decreased with the increasing fraction of the uncoated regions. However, PTLs containing multiple thin uncoated strips caused a less severe performance effect than PTLs with continuous uncoated regions of the same relative total area. Through analysis of cell performance, impedance, and 3D charge transport modelling, here we demonstrate that both the anode catalyst layer and membrane play a role in distributing current to mitigate the impact of coating defects at a short length scale. These results allow to draw conclusions about the tolerance requirements with regards to PTL coating uniformity in terms of both the size and total area of defects.

08 HYDROGEN↗

Electrochemical and Interfacial Behavior of All Solid State Batteries Using Li10SnP2S12 Solid Electrolyte

Thio-Lithium Superionic Conductor (Thio-LISICON) Li10GeP2S12 equivalent Li10SnP2S12 (LSPS) is comparable in ionic conductivity yet with a lower cost as an electrolyte for all solid-state batteries (ASSBs). ASSBs with LSPS solid electrolyte (SE), lithium-indium alloy anode, and LiCoO2 (LCO) cathode were successfully fabricated and their electrochemical performance at 60 °C was examined. Atomic layer deposition of Li3NbO4 on LCO was conducted to improve the interfacial stability. The Li3NbO4 coating significantly improves the cycle stability of the ASSB, which retains about 85% of the initial capacity after 70 cycles at a current density of 0.13 mA/cm2, while the ASSB with uncoated LCO retains ~ 60% of the initial capacity after 70 cycles. Electrochemical impedance spectroscopy tests indicate a rapid growth of charge transfer resistance upon cycling for the cell with the uncoated LCO, primarily due to the surface instability and build-up of a space charge layer between LSPS and LCO. However, the ASSBs with Li3NbO4 coated LCO show a more stable interface with a negligible impedance increase upon cycling, attributable to the buffering and passivating roles of the Li3NbO4 coating. The interfacial microstructure was analyzed to elucidate at the underlying reasons for the impedance increase and the pivotal role of the Li3NbO4 coating. Our study indicates that the surface coating significantly improves the cycle stability of the ASSBs with LSPS as the electrolyte, mostly due to an improvement of the charge transfer mechanism. The coating reduced the interphase thickness and the interfacial resistance to about a third of the uncoated one after 10 cycles.

Vinado, Carolina↗

Minimizing Oxygen Permeability in Chitin/Cellulose Nanomaterial Coatings by Tuning Chitin Deacetylation

The demand for packaging materials with low gas permeabilities is increasing, but commonly used petroleum-derived single-use plastics are not renewable, biodegradable, or easy to recycle. Nanomaterials composed of chitin and cellulose, which are abundant in nature, have high crystallinities and low oxygen permeabilities (OP), providing a viable alternative. In this work, we explore how deacetylation conditions of crab shell chitin can be used to tune the charge and size of resulting chitin nanowhiskers (ChNWs) and the resulting OP of layered film structures. Three deacetylation factors, the concentration of sodium hydroxide (%NaOH), temperature (T), and reaction time, were explored using a three-factor three-level Taguchi design with an orthogonal array. Furthermore, the resulting ChNW suspensions were sequentially spray-coated with suspensions of cellulose nanocrystals (CNCs) onto cellulose acetate (CA) films to form a multilayer structure. We show that ChNWs prepared under more aggressive deacetylation conditions inside the original orthogonal array (higher %NaOH, T, and time) had shorter lengths but the surface charge was significantly influenced only by more aggressive deacetylation outside of the original design conditions. With only ~10% decrease in the ultimate tensile strength and no significant loss in failure strain, the ChNW-CNC coating resulted in ~20% decrease in WVTR in comparison to uncoated CA films. The optimization of process conditions resulted in CA-ChNW-CNC films with a 91-99% decrease in OP (132-16.7 cm 3 ∙μm/m 2 /day/kPa versus 1553 cm3∙μm/m2/day/kPa for uncoated CA).

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ice Nucleation and Droplet Formation by Bare and Coated Black Carbon Particles

We have studied the ice formation at heterogeneous and homogeneous temperatures, as well as droplet activation and hygroscopicity of soot particles of variable size and composition. Coatings of adipic, malic, and oleic acid were applied to span a relevant range of solubility, and both uncoated and oleic acid coated soot particles were exposed to ozone to simulate atmospheric oxidation. The results are interpreted in terms of onset ice nucleation with a comparison to a well characterized mineral dust particle that acts as an efficient ice nucleus, as well as particle hygroscopicity. At 253K and 243K, we found no evidence of heterogeneous ice nucleation occurring above the level of detection for our experimental conditions. Above water saturation, droplet formation was observed. At 233K, we observe the occurrence of homogeneous ice nucleation for all particles studied. Coatings also did not significantly alter the ice nucleation behavior of soot particles, but aided in the uptake of water. Hygroscopicity studies confirmed that pure soot particles were hydrophobic, and coated soot particles activated as droplets at high water supersaturations. A small amount of heterogeneous ice nucleation either below the detection limit of our instrument or concurrent with droplet formation and/or homogeneous freezing cannot be precluded, but we are able to set limits for its frequency. We conclude from our studies that both uncoated and coated soot particles are unlikely to contribute to the global budget of heterogeneous ice nuclei at temperatures between 233K and 253K.

58 GEOSCIENCES↗

Effect of sputtered lanthanum hexaboride film thickness on field emission from metallic knife edge cathodes

We report experiments and analysis of field emission from metallic knife-edge cathodes, which are sputter-coated with thin films of lanthanum hexaboride (LaB{sub 6}), a low-work function material. The emission current is found to depend sensitively on the thickness of the LaB{sub 6} layer. We find that films thinner than 10 nm greatly enhance the emitted current. However, cathodes coated with a thicker layer of LaB{sub 6} are observed to emit less current than the uncoated metallic cathode. This result is unexpected due to the higher work function of the bare metal cathode. We show, based on numerical calculation of the electrostatic potential throughout the structure, that the external (LaB{sub 6}/vacuum) barrier is reduced with respect to uncoated samples for both thin and thick coatings. However, this behavior is not exhibited at the internal (metal/LaB{sub 6}) barrier. In thinly coated samples, electrons tunnel efficiently through both the internal and external barrier, resulting in current enhancement with respect to the uncoated case. In contrast, the thick internal barrier in thickly coated samples suppresses current below the value for uncoated samples in spite of the lowered external barrier. We argue that this coating thickness variation stems from a relatively low (no higher than 10{sup 18} cm{sup -3}) free carrier density in the sputtered polycrystalline LaB{sub 6}.

36 MATERIALS SCIENCE↗

Thermal conductivity prediction of magnetic composite sheet for near-field electromagnetic absorption

The magnetic composite sheets were designed by using core-shell structured magnetic fillers instead of uncoated magnetic fillers to resolve concurrently the electromagnetic interference and thermal radiation problems. To predict the thermal conductivity of composite sheet, we calculated the thermal conductivity of the uncoated magnetic fillers and core-shell structured fillers. And then, the thermal conductivity of the magnetic composites sheet filled with core-shell structured magnetic fillers was calculated and compared with that of the uncoated magnetic fillers filled in composite sheet. The magnetic core and shell material are employed the typical Fe-Al-Si flake (60 μm × 60 μm × 1 μm) and 250 nm-thick AlN with high thermal conductivity, respectively. The longitudinal thermal conductivity of the core-shell structured magnetic composite sheet (2.45 W/m·K) enhanced about 33.4% in comparison with that of uncoated magnetic fillers (1.83 W/m·K) for the 50 vol. % magnetic filler in polymer matrix.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Observation of radio frequency ring-shaped hollow cathode discharge plasma with MgO and Al electrodes for plasma processing

Various high-density plasma sources have been proposed for plasma processing. Especially, the hollow cathode discharge is one of the powerful ones. In this work, radio-frequency (RF) driven ring-shaped hollow cathode discharges with high secondary-electron emission have been investigated, using an aluminum (Al) cathode, coated or not with magnesium oxide (MgO). The thickness of MgO thin film is approximately 200 nm. The RF discharge voltage for the coated cathode is almost the same as that for the uncoated one, in a wide range of Ar gas pressure, from 5.3 to 53.2 Pa. The results reveal that the plasma density has a peak at an Ar gas pressure of 10.6 Pa for both cathodes. The plasma density for the coated cathode is about 1.5–3 times higher than that for the uncoated one, at various gas pressures. To the contrary, the electron temperature for the coated cathode is lower than temperature obtained with the uncoated cathode, at various gas pressures. Radial profiles of electron saturation current, which is proportional to plasma flux, are also examined for a wide range of gas pressure. Radial profiles of electron temperature at various axial positions are almost uniform for both cathodes so that the diffusion process due to density gradient is dominant for plasma transport. The secondary electrons emitted from the coated cathode contribute to the improvement of the plasma flux radial profile obtained using the uncoated cathode.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗