Search NASA⌕ Search

SEARCH · Search NASA

Results for “yttria stabilized”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 73 records · Page 4

Formulations for Stronger Solid Oxide Fuel-Cell Electrolytes

Tests have shown that modification of chemical compositions can increase the strengths and fracture toughnesses of solid oxide fuel-cell (SOFC) electrolytes. Heretofore, these solid electrolytes have been made of yttria-stabilized zirconia, which is highly conductive for oxygen ions at high temperatures, as needed for operation of fuel cells. Unfortunately yttria-stabilized zirconia has a high coefficient of thermal expansion, low resistance to thermal shock, low fracture toughness, and low mechanical strength. The lack of strength and toughness are especially problematic for fabrication of thin SOFC electrolyte membranes needed for contemplated aeronautical, automotive, and stationary power-generation applications. The modifications of chemical composition that lead to increased strength and fracture toughness consist in addition of alumina to the basic yttria-stabilized zirconia formulations. Techniques for processing of yttria-stabilized zirconia/alumina composites containing as much as 30 mole percent of alumina have been developed. The composite panels fabricated by these techniques have been found to be dense and free of cracks. The only material phases detected in these composites has been cubic zirconia and a alumina: this finding signifies that no undesired chemical reactions between the constituents occurred during processing at elevated temperatures. The flexural strengths and fracture toughnesses of the various zirconia-alumina composites were measured in air at room temperature as well as at a temperature of 1,000 C (a typical SOFC operating temperature). The measurements showed that both flexural strength and fracture toughness increased with increasing alumina content at both temperatures. In addition, the modulus of elasticity and the thermal conductivity were found to increase and the density to decrease with increasing alumina content. The oxygen-ion conductivity at 1,000 C was found to be unchanged by the addition of alumina.

Bansal, Narottam P.↗

Microstructure and mechanical properties of bulk yttria-partially-stabilized zirconia

A commercially available bulk 4.5 mole percent yttria-Y2O3)-partially-stabilized zirconia (PSZ) was studied by light microscopy, X-ray analysis, microhardness measurement, and fracture toughness testing. The growth of the precipitates and the phase transformations were studied as a function of aging in air at 1500 C. Aging cuves were constructed for both the as-received and the solution-annealed-and-quenched materials; the curves showed hardness peaks at 1397 and 1517 kg/sq mm, respectively. A total of twelve different types of tetragonal precipitates were found. The rectangular plate-shaped tetragonal precipitates were found to have a (110) habit plane. Grinding of the Y2O3 PSZ into powder did not cause a significant amount of metastable tetragonal precipitates to transform into the monoclinic phase, thus indicating that transformation toughening is not a significant mechanism for the material. The fracture toughness of the aged and of the unaged solution-annealed-and-quenched PSZ was found to be between 2 and 3 MN/cu m/2.

Valentine, P. G.↗

Multilayer Thermal Barrier Coating (TBC) Architectures Utilizing Rare Earth Doped YSZ and Rare Earth Pyrochlores

To allow for increased gas turbine efficiencies, new insulating thermal barrier coatings (TBCs) must be developed to protect the underlying metallic components from higher operating temperatures. This work focused on using rare earth doped (Yb and Gd) yttria stabilized zirconia (t' Low-k) and Gd2Zr2O7 pyrochlores (GZO) combined with novel nanolayered and thick layered microstructures to enable operation beyond the 1200 C stability limit of current 7 wt% yttria stabilized zirconia (7YSZ) coatings. It was observed that the layered system can reduce the thermal conductivity by approximately 45 percent with respect to YSZ after 20 hr of testing at 1316 C. The erosion rate of GZO is shown to be an order to magnitude higher than YSZ and t' Low-k, but this can be reduced by almost 57 percent when utilizing a nanolayered structure. Lastly, the thermal instability of the layered system is investigated and thought is given to optimization of layer thickness.

Thermal Barrier Coating↗

Microwave Photoelasticity: Exploiting Multiple Resonances to Measure Stress Changes within Yttria-Partially-Stabilized-Zirconia

The NASA Glenn Research Center is developing non-destructive-testing (NDT) methods to enable the measurement of stresses embedded in optically opaque materials using microwave radiation in a free-space quasi-optical system. This methodology tracks microwave resonances observed in reflected scattering parameters extracted from materials under load. In this paper, we report the successful measurement of the stress-optic-coefficient of bulk yttria-partially stabilized zirconia (YTZP) ceramic of C = 1.42 x 10-4 ± 6.65 x 10-6 (1/GPa), across W-Band (80-100 GHz), and determined that this result is independent of sample thickness. The primary goal of this research is to establish a methodology to quantify and assess the life expectancy of ceramic thermal and environmental barrier coating (TBCs/EBCs). Bulk YTZP samples can undergo multiple resonances within a contiguous measurement bandwidth, each corresponding to an integer multiple wave number ∝. This allows for the acquisition and analysis of multiple stress measurement points within a single sample. As an additional benefit, one can approximate the refractive index of YTZP across a wide bandwidth by observing multiple resonances produced by a set of samples with varying thicknesses. Using this approach, the refractive index of bulk YTZP was found to be n = 5.80 ± 0.043 across the 85-115 GHz frequency band.

Seth W. Waldstein↗

Lower-Conductivity Thermal-Barrier Coatings

Thermal-barrier coatings (TBCs) that have both initial and post-exposure thermal conductivities lower than those of yttria-stabilized zirconia TBCs have been developed. TBCs are thin ceramic layers, generally applied by plasma spraying or physical vapor deposition, that are used to insulate air-cooled metallic components from hot gases in gas turbine and other heat engines. Heretofore, yttria-stabilized zirconia (nominally comprising 95.4 atomic percent ZrO2 + 4.6 atomic percent Y2O3) has been the TBC material of choice. The lower-thermal-conductivity TBCs are modified versions of yttria-stabilized zirconia, the modifications consisting primarily in the addition of other oxides that impart microstructural and defect properties that favor lower thermal conductivity.

Miller, Robert A.↗

Nanoscale chemistry and ion segregation in zirconia-based ceramic at grain boundaries by atom probe tomography

In this work nanoscale features that are of importance in the stability of yttria-stabilized tetragonal zirconia (Y-TZP) are quantified through atom probe tomography. In-depth analysis of grain boundary chemistry revealed preferential segregation of lighter and smaller ions towards specific grain boundaries. The relationship between elemental segregation and the local atomistic structure is investigated at the sub-nanometer level to gain insights on nanoscale features associated with the tetragonal-monoclinic phase transformation in Y-TZP through grain boundary characterization. Furthermore, principal component analysis was implemented to reveal any potential biases from varied field evaporation across stabilizer-rich grain boundaries. The observed variations in ion density across different grains suggested a variation in field which was attributed to potential variations in grain crystal orientation. In order to reveal the subtle depletion of oxygen atoms within grain boundaries a new methodology to map oxygen vacancies is proposed, utilizing the relative neighborhood chemistry of individual yttrium atoms.

36 MATERIALS SCIENCE↗

Ceramic thermal-barrier coatings for cooled turbines

Coating systems consisting of a plasma sprayed layer of zirconia stabilized with either yttria, magnesia or calcia over a thin alloy bond coat have been developed, their potential was analyzed and their durability and benefits evaluated in a turbojet engine. The coatings on air cooled rotating blades were in good condition after completing as many as 500 two-minute cycles of engine operation between full power at a gas temperature of 1644 K and flameout, or as much as 150 hours of steady state operation on cooled vanes and blades at gas temperatures as high as 1644 K with 35 start and stop cycles. On the basis of durability and processing cost, the yttria stabilized zirconia was considered the best of the three coatings investigated.

Liebert, C. H.↗

Durability of zirconia thermal-barrier ceramic coatings on air-cooled turbine blades in cyclic jet engine operation

Thermal barrier ceramic coatings of stabilized zirconia over a bond coat of Ni Cr Al Y were tested for durability on air cooled turbine rotor blades in a research turbojet engine. Zirconia stabilized with either yttria, magnesia, or calcia was investigated. On the basis of durability and processing cost, the yttria stabilized zirconia was considered the best of the three coatings investigated.

Liebert, C. H.↗

Ceramic thermal-barrier coatings for cooled turbines

Ceramic thermal-barrier coatings on hot engine parts have the potential to reduce metal temperatures, coolant requirements, cost, and complexity of the cooling configuration, and to increase life, turbine efficiency and gas temperature. Coating systems consisting of a plasma-sprayed layer of zirconia stabilized with either yttria, magnesia or calcia over a thin alloy bond coat have been developed, their potential analyzed and their durability and benefits evaluated in a turbojet engine. The coatings on air-cooled rotating blades were in good condition after completing as many as 500 two-minute cycles of engine operation between full power at a gas temperature of 1644 K and flameout, or as much as 150 hours of steady-state operation on cooled vanes and blades at gas temperatures as high as 1644 K witn 35 start and stop cycles. On the basis of durability and processing cost, the yttria-stabilized zirconia was considered the best of the three coatings investigated.

Liebert, C. H.↗

Thermal-Mechanical Stability of Single Crystal Oxide Refractive Concentrators for High-Temperature Solar Thermal Propulsion

Single crystal oxides such as yttria-stabilized zirconia (Y2O3-ZrO2), yttrium aluminum garnet (Y3Al5O12, or YAG), magnesium oxide (MgO) and sapphire (Al2O3) are candidate refractive secondary concentrator materials for high temperature solar propulsion applications. However, thermo-mechanical reliability of these components in severe thermal environments during the space mission sun/shade transition is of great concern. Simulated mission tests are important for evaluating these candidate oxide materials under a variety of transient and steady-state heat flux conditions, and thus provide vital information for the component design. In this paper, a controlled heat flux thermal shock test approach is established for the single crystal oxide materials using a 3.0 kW continuous wave CO2 laser, with a wavelength 10.6 micron. Thermal fracture behavior and failure mechanisms of these oxide materials are investigated and critical temperature gradients are determined under various temperature and heating conditions. The test results show that single crystal sapphire is able to sustain the highest temperature gradient and heating-cooling rate, and thus exhibit the best thermal shock resistance, as compared to the yttria-stabilized zirconia, yttrium aluminum garnet, and magnesium oxide.

Zhu, Dongming↗

Thermal-Mechanical Stability of Single Crystal Oxide Refractive Concentrators for High-Temperature Solar Thermal Propulsion

Single crystal oxides such as yttria-stabilized zirconia (Y2O3-ZrO2), yttrium aluminum garnet (Y3Al5O12, or YAG), magnesium oxide (MgO) and sapphire (Al2O3) are candidate refractive secondary concentrator materials for high temperature solar propulsion applications. However, thermo-mechanical reliability of these components in severe thermal environments during the space mission sun/shade transition is of great concern. Simulated mission tests are important for evaluating these candidate oxide materials under a variety of transient and steady-state heat flux conditions, and thus provide vital information for the component design. In this paper, a controlled heat flux thermal shock test approach is established for the single crystal oxide materials using a 3.0 kW continuous wave CO2 laser, with a wavelength 10.6 micron. Thermal fracture behavior and failure mechanisms of these oxide materials are investigated and critical temperature gradients are determined under various temperature and heating conditions. The test results show that single crystal sapphire is able to sustain the highest temperature gradient and heating-cooling rate, and thus exhibit the best thermal shock resistance, as compared to the yttria-stabilized zirconia, yttrium aluminum garnet and magnesium oxide.

Zhu, Dongming↗

Enhancing the efficiency benefit of thermal barrier coatings for homogeneous charge compression ignition engines through application of a low-k oxide

Prior experiments reported by the authors have proven the hypothesis that achieving a dynamic temperature swing on the combustion chamber surface will lead to improved thermal and combustion efficiencies of the homogeneous charge compression ignition engine. A thin layer of yttria-stabilized zirconia, roughly 150 μm, was plasma sprayed on the piston top. It led to markedly advanced ignition and heat release in the gasoline homogeneous charge compression ignition engine, accompanied with reduced unburnt hydrocarbon and carbon monoxide emissions, improved combustion efficiency, and a higher thermal efficiency. A related computational study highlighted the critical role of coating thermal conductivity in achieving a desired dynamic response; hence, the second phase of experimental investigations focused on introducing structured porosity in the yttria-stabilized zirconia coating, as a means of reducing effective conductivity. Indeed, additional incremental improvements were observed, as well as limitations related to adverse effects of the surface roughness and the fuel interactions with the surface roughness and open pores. Erosion can also be a problem in a direct injection engine. Therefore, the third round of investigations focused on a material with a natively low conductivity (low-k), sprayed on the top of an Al piston in a relatively dense form, and in a way that yields a smooth surface. The objective was to capitalize on the low conductivity, while avoiding the pitfalls accompanying high-porosity formulations. The heat-storage capacity was limited by keeping the thickness relatively low. The results verify the paramount importance of thermal conductivity in the context of high “temperature swing” behavior and indicate a potential to improve the homogeneous charge compression ignition engine’s combustion efficiency roughly 1.5%, with the overall indicated efficiency improvement on the order of 5%, on a relative basis. In addition, the low-k oxide thermal barrier applied to the piston extended significantly the low-load homogeneous charge compression ignition operability limit.

42 ENGINEERING↗

Environmental Barrier Coatings for Silicon-Based Ceramics

Silicon-based ceramics, such as SiC fiber-reinforced SiC (SiC/SiC ceramic matrix composites (CMC) and monolithic silicon nitride (Si3N4), are prime candidates for hot section structural components of next generation gas turbine engines. Silicon-based ceramics, however, suffer from rapid surface recession in combustion environments due to volatilization of the silica scale via reaction with water vapor, a major product of combustion. Therefore, application of silicon-based ceramic components in the hot section of advanced gas turbine engines requires development of a reliable method to protect the ceramic from environmental attack. An external environmental barrier coating (EBC) is considered a logical approach to achieve protection and CP long-term stability. The first generation EBC consisted of two layers, mullite (3Al2O3-2SiO2) bond coat and yttria-stabilized zirconia (YSZ, ZrO2-8 Wt.% Y2O3) top coat. Second generation EBCs, with substantially improved performance compared with the first generation EBC, were developed in the NASA High Speed Research-Enabling Propulsion Materials (HSR-EPM) Program. The first generation EBC consisted of two layers, mullite (3Al2O3-2SiO2) bond coat and yttria-stabilized zirconia (YSZ, ZrO2-8 wt.% Y2O3) top coat. Second generation EBCs, with substantially improved performance compared with the first generation EBC, were developed in the NASA High Speed Research-Enabling Propulsion Materials (HSR-EPM) Program (5). They consist of three layers, a silicon first bond coat, a mullite or a mullite + BSAS (BaO(1-x)-SrO(x)-Al2O3-2SiO2) second bond coat, and a BSAS top coat. The EPM EBCs were applied on SiC/SiC CMC combustor liners in three Solar Turbines (San Diego, CA) Centaur 50s gas turbine engines. The combined operation of the three engines has accumulated over 24,000 hours without failure (approximately 1,250 C maximum combustor liner temperature), with the engine in Texaco, Bakersfield, CA, accumulating about 14,000 hours. As the commercialization of Si-based ceramic components in gas turbines is on the horizon, a major emphasis is placed on EBCs for two reasons. First, they are absolute necessity for the protection of Si-based ceramics from water vapor. Second, they can enable a major enhancement in the performance of gas turbines by creating temperature gradients with the incorporation of a low thermal conductivity layer. Thorough understanding of current state-of-the-art EBCs will provide the foundation upon which development of future EBCs will be based. Phase stability and thermal conductivity of EPM EBCs are published elsewhere. This paper will discuss the chemical/environmental durability and silica volatility of EPM EBCs and their impact on the coating's upper temperature limit.

Lee, Kang N.↗

Thermal barrier coatings for thermal insulation and corrosion resistance in industrial gas turbine engines

Four thermal barrier coatings were subjected to a 500-hour gas turbine engine test. The coatings were two yttria stabilized zirconias, calcium ortho silicate and calcium meta titanate. The calcium silicate coating exhibited significant spalling. Yttria stabilized zirconia and calcium titanate coatings showed little degradation except in blade leading edge areas. Post-test examination showed variations in the coating due to manual application techniques. Improved process control is required if engineering quality coatings are to be developed. The results indicate that some leading edge loss of the coating can be expected near the tip.

Vogan, J. W.↗

Long-term stability and properties of zirconia ceramics for heavy duty diesel engine components

Physical, mechanical, and thermal properties of commercially available transformation-toughened zirconia are measured. Behavior is related to the material microstructure and phase assemblage. The stability of the materials is assessed after long-term exposure appropriate for diesel engine application. Properties measured included flexure strength, elastic modulus, fracture toughness, creep, thermal shock, thermal expansion, internal friction, and thermal diffusivity. Stability is assessed by measuring the residual property after 1000 hr/1000C static exposure. Additionally static fatigue and thermal fatigue testing is performed. Both yttria-stabilized and magnesia-stabilized materials are compared and contrasted. The major limitations of these materials are short term loss of properties with increasing temperature as the metastable tetragonal phase becomes more stable. Fine grain yttria-stabilized material (TZP) is higher strength and has a more stable microstructure with respect to overaging phenomena. The long-term limitation of Y-TZP is excessive creep deformation. Magnesia-stabilized PSZ has relatively poor stability at elevated temperature. Overaging, decomposition, and/or destabilization effects are observed. The major limitation of Mg-PSZ is controlling unwanted phase changes at elevated temperature.

Larsen, D. C.↗

An Investigation of the Electrochemical Activity of (Ba/Sr)FeO 3-y Anodes

FeO x , SrFeO 3-y (SF), and Ba 0.5 Sr 0.5 FeO 3–y (BSF) were studied for application as fuel oxidation catalysts in solid oxide fuel cells (SOFC) anodes. Electrodes were prepared by impregnation into porous yttria-stabilized zirconia (YSZ), with La 0.3 Sr 0.7 TiO 3–y (LST) added for electronic conductivity. The electrode impedances decreased dramatically upon addition of SF and BSF and much less when only SrO or FeO x were added. Temperature Programmed Desorption (TPD) of O 2 from oxidized BSF showed O 2 desorbing between 200 °C and 700 °C, while no O 2 desorbed from Fe 2 O 3 below 900 °C. The results, together with thermodynamic analysis, suggest that stabilization of Fe +4 in the perovskite lattice plays an important role in enhancing the catalytic activity of SF and BSF by providing access to a Fe 3+ /Fe 4+ redox couple that can accept oxygen anions from the yttria-stabilized zirconia (YSZ) electrolyte. Oxygen is weakly bound to these sites facilitating its reaction with adsorbed H 2 .

Electrochemistry↗

Siloxane Deposition on the Ni-YSZ Solid Oxide Fuel Cell Anode Exposed to Bio-Syngas

Siloxane, a common contaminant present in biogas, is known for adverse effects on cogeneration prime movers. In this study, the siloxane deposition products and mechanism in the solid oxide fuel cell nickel-yttria stabilized zirconia (Ni-YSZ) anode are investigated analytically and experimentally. An SOFC with Ni-YSZ anode and pure Ni/YSZ pellets were exposed to a simulated biogas-reformate fuel with octamethylcyclotetrasiloxane (D4) contamination at 750 °C. The electrochemical characterization results show that the SOFCs performance degradation caused by D4 contamination is irreversible. Morphology and XRD results illustrate that silicon and carbon deposition can both be detected in the anode and pellets. Graphite, SiC and SiO2 are all possible products based on the results of XRD test. Here, according to the formation of graphite and SiC, the new mechanism suggests that carbon is also an essential factor in siloxane contamination of Ni-YSZ anodes besides silicon, which can be explained by the catalytic and electrochemical analysis.

25 ENERGY STORAGE↗

Dispersal of high-burnup fuel fragment surrogate particles during and after loss-of-coolant accident tests

The issue of fuel fragmentation, relocation, and dispersal is critical in the licensing and use of high-burnup (>62 GWd/MTU) nuclear fuel in light water reactors (LWRs). In this work, two test series are reported that examine the fragment dispersal during a burst event and an additional dispersal following the burst due to vibrations in the rod, such as those induced by accident recovery systems. To examine dispersal during the balloon and burst portion of a Loss-of-Coolant Accident event, HfO 2 fragments and yttria-stabilized zirconia pellets were filled into an as-fabricated cladding tube, which was then pressurized and subjected to loss-of-coolant accident testing in steam. Results from this test were found to be highly non-prototypic, and dispersal was both significantly more violent and significantly greater in magnitude than identified for actual fuel tests. These findings were attributed to the conservative (more dispersive) nature of the particles chosen for dispersal and to the details of the test conditions used that led to particularly wide bursts. Further, the second set of tests examined dispersal following the burst when vibrations were induced in the rod, primarily via recovery activities such as Emergency Core Cooling System actuation leading to rapid water addition. Post-burst dispersal testing was performed by inducing sinusoidal oscillations with 2–25 nm peak-to-peak amplitude and 2–5 Hz frequencies in pre-burst rods that had been refilled with HfO 2 fragments or high-burnup fragment surrogate mixture of HfO 2 fragments and yttria-stabilized zirconia sands. Testing revealed that rods with large burst openings (7 mm wide in this work) led to unmitigated dispersal from above the burst zone but that smaller bursts (5 mm wide), although still much larger than the mean fragment size of 3 mm, led to effectively no dispersal because of interparticle locking. Additionally, mixture and moisture were found to impact the amount of dispersal: mixtures increased dispersal, and moisture drastically reduced it. The implications of these findings on likely dispersal from actual fuel are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗