Study of bound hydrogen in powders of diamond nanoparticles

In order to access feasibility of increasing albedo of very cold neutrons from powder of diamond nanoparticles, we studied hydrogen bound to surface of diamond nanoparticles, which causes unwanted losses of neutrons. We showed that one could decrease a fraction of hydrogen atoms from a ratio C{sub 7.4{+-}0.15}H to a ratio C{sub 12.4{+-}0.2}H by means of thermal treatment and outgasing of powder. Measurements of atomic excitation spectra of these samples, using a method of inelastic incoherent neutron scattering, indicate that residual hydrogen is chemically bound to carbon, while a removed fraction was composed of adsorbed water. The total cross section of scattering of neutrons with a wavelength of 4.4 Angstrom-Sign on residual hydrogen atoms equals 108 {+-} 2 b; it weakly changes with temperature. Thus preliminary cleaning of powder from hydrogen and its moderate cooling do not improve considerably neutron albedo from powder of nano-diamonds. An alternative approach is isotopic replacement of hydrogen by deuterium.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

X-ray diffraction characterization of epitaxial CVD diamond films with natural and isotopically modified compositions

Comparative investigations of homoepitaxial diamond films with natural and modified isotopic compositions, grown by chemical vapor deposition (CVD) on type-Ib diamond substrates, are carried out using double-crystal X-ray diffractometry and topography. The lattice mismatch between the substrate and film is precisely measured. A decrease in the lattice constant on the order of (Δa/a){sub relax} ∼ (1.1–1.2) × 10{sup –4} is recorded in isotopically modified {sup 13}C (99.96%) films. The critical thicknesses of pseudomorphic diamond films is calculated. A significant increase in the dislocation density due to the elastic stress relaxation is revealed by X-ray topography.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Ground-state properties of boron-doped diamond

Boron-doped diamond undergoes an insulator-metal or even a superconducting transition at some critical value of the dopant concentration. We study the equilibrium lattice parameter and bulk modulus of boron-doped diamond experimentally and in the framework of the density functional method for different levels of boron doping. We theoretically consider the possibility for the boron atoms to occupy both substitutional and interstitial positions and investigate their influence on the electronic structure of the material. The data suggest that boron softens the lattice, but softening due to substitutions of carbon with boron is much weaker than due to incorporation of boron into interstitial positions. Theoretical results obtained for substitution of carbon are in very good agreement with our experiment. We present a concentration dependence of the lattice parameter in boron-doped diamond, which can be used for to identify the levels of boron doping in future experiments.

36 MATERIALS SCIENCE↗

Thermal conductivity of polycrystalline CVD diamond: Experiment and theory

The temperature dependences of thermal conductivity {kappa} of polycrystalline CVD diamond are measured in the temperature range from 5 to 410 K. The diamond sample is annealed at temperatures sequentially increasing from 1550 to 1690{sup o}C to modify the properties of the intercrystallite contacts in it. As a result of annealing, the thermal conductivity decreases strongly at temperatures below 45 K, and its temperature dependence changes from approximately quadratic to cubic. At T > 45 K, the thermal conductivity remains almost unchanged upon annealing at temperatures up to 1650{sup o}C and decreases substantially at higher annealing temperatures. The experimental data are analyzed in terms of the Callaway theory of thermal conductivity [9], which takes into account the specific role of normal phonon-phonon scattering processes. The thermal conductivity is calculated with allowance for three-phonon scattering processes, the diffuse scattering by sample boundaries, the scattering by point and extended defects, the specular scattering by crystallite boundaries, and the scattering by intercrystallite contacts. A model that reproduces the main specific features of the thermal conductivity of CVD diamond is proposed. The phonon scattering by intercrystallite contacts plays a key role in this model.

36 MATERIALS SCIENCE↗

Dynamics of charge carriers at the place of the formation of a muonic atom in diamond and silicon

The space-time distribution of charge carriers at the place of the location of a muonic atom formed when a negative muon is captured by an atom of the lattice has been numerically simulated taking into account the self-consistent electric field. The results of {mu}SR experiments with negative muons in diamond crystals have been explained and reasons for the difference in the behavior of the spin polarization of the negative muon in boron-doped diamond and in silicon have been revealed. The condition of the validity of the analytical solution of this problem has been obtained. It has been shown that the muonic atom in diamond, in contrast to silicon, does not form a neutral acceptor center in the paramagnetic state during the muon experiment and remains in the diamagnetic state of a positive ion.

74 ATOMIC AND MOLECULAR PHYSICS↗

Photoluminescence of silicon after deposition of polycrystalline diamond films

Low-temperature (5K) photoluminescence of silicon substrates in the range 0.8-1.2 eV is studied before and after deposition of polycrystalline diamond films. The diamond films were deposited in the microwave plasma onto high-purity dislocation-free silicon (with the resitivity {rho} {approx} 3 k{Omega} cm) subjected to mechanical polishing or more delicate chemical and mechanical polishing. The deposition temperature was 750-850 deg. C. In the photoluminescence spectra of the samples with the substrates polished chemically and mechanically, two lines, D{sub 1} and D{sub 2}, corresponding to the dislocation-related emission are recorded. Generation of dislocations in the substrates is caused by efficient adhesion of the diamond film and, as a result, by internal stresses that relax with the formation of dislocations. The experimental spectra are practically identical to the photoluminescence spectra observed in silicon ({rho} {approx} 100 {Omega} cm) with the density of dislocations {approx}10{sup 4} cm{sup -2}.

36 MATERIALS SCIENCE↗

Study of the Structural and Morphological Properties of HPHT Diamond Substrates

The morphological and structural properties of a series of high-pressure high-temperature (HPHT) single-crystal diamond substrates are comprehensively studied by white-light optical interference microscopy, atomic-force microscopy, and X-ray diffraction analysis. Procedures that provide a means for characterizing the substrate parameters most critical for epitaxial application with the laboratory equipment are described. It is shown that the jewelry-type characterization of diamond substrates is insufficient to assess the possibility of their use for the epitaxial growth of chemical-vapor-deposited (CVD) diamond.

36 MATERIALS SCIENCE↗

Evolution of Triplet Paramagnetic Centers in Diamonds Obtained by Sintering of Detonation Nanodiamonds at High Pressure and Temperature

The electron paramagnetic resonance (EPR) spectra of triplet centers in detonation nanodiamonds (DNDs) and diamond single crystals of submicrometer size, synthesized from those DNDs at high pressures and temperatures, are studied. In the EPR spectra of DNDs, signals from negatively charged nitrogen- vacancy centers (NV)/sup(-) with a g factor of g{sub 1} = 4.24 and multivacancies with g{sub 2} = 4.00 are observed. The signals from (NV)/sup(-) centers disappear in the spectra of diamond single crystals, and a quintet signal with g = 4.00 is detected at the position of the signal from multivacancies. Analysis of the shape and position of the quintet’ lines showed that this ESR signal is due to the pairs of nitrogen substitution centers in diamond, separated from each other by distances not exceeding 0.7 nm, between which a strong exchange interaction takes place. A comparison of the experimental data and the simulation results allows determining the spin-Hamiltonian parameters of the exchange-coupled pairs of paramagnetic impurity nitrogen atoms.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Ion Modification of the Field-Emission Properties of Diamond-Graphite Film Structures

The patterns of variation of structure-phase, morphological, and field-emission parameters of nanocomposite diamond-graphite film structures, which were synthesized in microwave plasma of ethanol vapors, with the dose of irradiation with nitrogen ions with an energy of 20 keV are studied. It is found that the morphological parameters of diamond-graphite structures subjected to small-dose irradiation differ only slightly from those of nonirradiated samples. In contrast, the field-emission properties of irradiated samples are altered significantly. The maximum density of field-emission currents increases when the field-emission excitation thresholds are raised. The optimum doses of nitrogen ion implantation resulting in a more than fivefold increase (relative to nonirradiated structures) in the maximum density of field-emission currents are determined. The physical and chemical mechanisms involved in the modification of surface and near-surface properties of diamond-graphite structures subjected to various doses of ion irradiation are examined.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Influence of Cobalt on the Adhesion Strength of Polycrystalline Diamond Coatings on WC–Co Hard Alloys

The influence of cobalt on the phase composition and adhesion strength of polycrystalline diamond coatings has been studied using scanning electron microscopy, Raman spectroscopy, and X-ray microanalysis. The coatings have been deposited on WC–Co hard alloy substrates in glow discharge plasma. It has been found that the catalytic amorphization of carbon only takes place during the direct synthesis of the diamond coating, when the cobalt vapor pressure over the substrate is high and the cobalt-related degradation of the synthesized diamond is absent.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

On a Possibility of the Overgrowth of Diamonds in the Hydrocarbon Atmosphere

The possibility to increase sizes of diamond crystals at least 25 μm by means of their annealing at a temperature of 1450 K in a hydrocarbon atmosphere has been studied. The initial diamond crystals are incorporated in the polyvinyl acetate layer on the surface of a silicon monocrystal and subjected to the annealing in methane atmosphere with low pressure in the presence of an external electric field with intensity up to 0.04 V/μm. Under these conditions the charged ions of methane dissociation products are accelerated and acquire the kinetic energy that is comparable with energy sufficient to form sp{sup 3}-hybride bonds, which can lead to an increase in the sizes of initial seed crystallites. The obtained substrates of a composite with a typical thickness not higher than 1.2 mm, which contain a joined diamond crystal in the carbon matrix, can be used as thermal conductive and electrical insulating spacers in devices for cooling items of electronic engineering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Simulation of a Detector of Visible and Near-IR Electromagnetic Radiation Based on Artificial Diamond

A method for calculation of the I–V characteristic is proposed for a detector of visible and near-IR electromagnetic radiation based on artificial diamond with allowance for vertical flow of electric current. The method can be used when the free-path length of carriers in diamond is less than the scale of variations in the concentration of carriers. The method is used to determine the following detector characteristics: the dependence of current on voltage, distribution of carrier concentration, and electric potential for a particular variant of a photodetector based on polycrystalline diamond film consisting of nanosized single crystals doped with boron.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A CVD Diamond-Based Photodetector for the Visible and Near-IR Spectral Range

A photodetector for the visible and near-IR spectral range has been created on the basis of a chemical- vapor-deposited diamond modulation-doped with boron. The detected electromagnetic radiation is absorbed in a thin Cr (7 nm)–Au (5.5 nm) bimetallic sublayer deposited on the surface of a modulationdoped diamond film comprising a highly doped (up to 5 × 10{sup 19} cm{sup –3}) 3-nm-thick delta-layer, low-doped (~10{sup 17} cm{sup –3}) 800-nm-thick sublayer, and highly doped (10{sup 20} cm{sup –3}) ~10-μm-thick sublayer with an ohmic Ti(50 nm)/Pt(15 nm)/Au(30 nm) contact. Holes generated in the bimetallic sublayer diffuse into diamond and are accelerated by an electric field in the low-doped sublayer to form a response photocurrent. The ampere/watt responsivity of the photodetector reaches 1 μA/W at a radiation wavelength of 445 nm and 0.18 μA/W at 1.06 μm.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

New Cluster Secondary Ions for Quantitative Analysis of the Concentration of Boron Atoms in Diamond by Time-of-Flight Secondary-Ion Mass Spectrometry

A new approach to quantitative analysis of the concentration of boron atoms in diamond using secondary- ion mass spectrometers with time-of-flight mass analyzers is proposed. Along with the known boron-containing lines (B, BC, BC{sub 2}), many lines related to cluster secondary ions BC{sub N} have been found in the mass spectrum; their intensity increases by one or two orders of magnitude when Bi{sub 3} probe ions are used. Lines BC{sub 4}, BC{sub 6}, BC{sub 2}, and BC{sub 8} have the highest intensity (in the descending order); when they are summed, the sensitivity increases by an order of magnitude in comparison with the known mode of detecting BC{sub 2}. The parameters of the boron δ-layer in single-crystal diamond films grown under optimal conditions have been measured to be unprecedented: the δ-layer width is about 2 nm, and the concentration is 6.4 × 10{sup 20} cm{sup –3} (the boron concentrations for doped and undoped diamonds differ by four orders of magnitude).

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Vacancy induced structural changes in diamond.

Although optically active defects in nanodiamond are being considered as candidates for optical labeling in biomedical applications, development in this area is being hindered the fact that suitable defects are rarely seen in diamond nanoparticles in the size regime required. These defects usually form as a complex with an impurity and a neutral of charged vacancy, so a measurable concentration of vacancy point defects is also necessary. Presented here are results of density functional tight binding computer simulations investigating the stability of vacancies in diamond nanoparticles with different surface structures. The results indicate that both neutral and charged vacancies alter the structure of as-grown diamond nanoparticles and are likely to diffuse out of the particle during synthesis or irradiation. We also find that suitable passivation of the particle may alleviate this problem, and hence facilitate the formation of defect complexes.

36 MATERIALS SCIENCE↗

Hydrogen Storage in Nano-Phase Diamond at High Temperature and Its Release

The objectives of this proposed research were: 91) Separation and storage of hydrogen on nanophase diamonds. It is expected that the produced hydrogen, which will be in a mixture, can be directed to a nanophase diamond system directly, which will not only store the hydrogen, but also separate it from the gas mixture, and (2) release of the stored hydrogen from the nanophase diamond.

08 HYDROGEN↗

Frictional Coefficients between Aluminum–Silicon Alloy and Cutting Inserts with MPCVD Diamond Coatings

The frictional coefficients at the front and rear surfaces of a VK6 hard-alloy cutter with experimental nano- and microcrystalline CVD diamond coatings applied in microwave plasma are determined by extrapolation to zero cut-layer thickness. It is found that, for diamond coatings with a single microcrystalline layer and those with both a microcrystalline layer and a nanocrystalline layer, the frictional coefficients are less than for an uncoated hard-alloy cutter and also for a cutter with a Sandvik diamond coating.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Undulatory Diamond Smoothing of Machine-Part Surfaces

The use of an industrial robot for undulatory diamond smoothing of machine-part surfaces is considered. The design of a robot for diamond smoothing of cylindrical and complex surfaces is described, and an example of an automatic machining line that includes a two-column industrial robot for undulatory smoothing is presented. In tests, the wear resistance of samples subjected to diamond smoothing on a lathe and to undulatory smoothing is compared.

42 ENGINEERING↗