Search NASA⌕ Search

SEARCH · Search NASA

Results for “EUTECTIC ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Effects of Laser Fluence on Microstructure and Bonding Characteristics of Wideband Laser-Deposited Nickel Composite Coatings

The wideband laser has shown great potential in metal–ceramic coatings deposition due to the high efficiency and low dilution rate. However, the effects of wideband laser process on microstructure evolution and bonding mechanism at the coatings/substrate interface are still a critical problem and need further investigation. In this work, nickel composite coatings are fabricated on the surface high-strength low-alloy steel. The effects of laser fluence on microstructure evolution, shear strength and fracture mechanism are studied. Results indicated the added WC particles were partly dissolved due to the high-power laser irradiation. Many block precipitates and dense eutectic were synthesized in composite coatings. Reinforced phases mainly consist of Cr{sub 5}B{sub 3}, Cr{sub 23}C{sub 6}, W{sub 2}C and Cr{sub 3}Ni{sub 2}. The dilution of Q550 steel contributed to the formation of nickel dendrites and facilitated a dense metallurgical bonding at coating/substrate interface when laser fluence was high. Shear strength tests indicated the laser fluence and shear strength had a positive correlation. For Ni60/WC composite coatings designed in these experiments, the recommend laser fluence should be higher than 55 J/mm{sup 2}, above which the shear strength could be greater than 200 MPa. Fracture surfaces indicated the failure mechanism of composite coatings was quasi-cleavage fracture.

36 MATERIALS SCIENCE↗

Solute diffusion behavior during heat treatment and its impact in Sc-microalloyed Al-Cu system

Scandium (Sc) is a promising microalloying element that enhances the strength and thermal stability of aluminum (Al) alloys. However, these benefits are not fully realized in aluminum-copper (Al-Cu) systems, and corrosion resistance often declines due to the complex phase evolution and diffusion behavior of Cu and Sc. Here, to clarify this, solute diffusion behavior and Cu-Sc interaction during heat treatment (HT) were investigated using in situ synchrotron-based transmission x-ray microscopy (TXM), wide-angle x-ray scattering (WAXS), and x-ray absorption near-edge structure (XANES) spectroscopy. The results, supported by electron microscopy, reveal strong Cu-Sc bonding that significantly impedes solute diffusion, leading to inhomogeneous solute distribution and non-uniform precipitation. Moreover, the Al-Cu-Sc eutectic phase exhibits high thermal stability, resisting dissolution even near the matrix liquidus. These findings quantitatively elucidate the sluggish diffusion kinetics of Cu and Sc, which can help redesign HT schedules to improve both mechanical properties and corrosion resistance in Sc-microalloyed Al-Cu alloys.

36 MATERIALS SCIENCE↗

Application of the Solute-Solvent EMF Cell to Measure Activity of NiF 2 in Molten FLiNaK

Electromotive force (emf) measurements made using a combination of solute- and solvent-based electrodes were used to determine the activity of NiF 2 in molten FLiNaK eutectic at 823 K across a concentration range of x NiF2 = 5.2 × 10 –4 –1.0 × 10 –2 . The solute emf values were measured using electrodes consisting of Ni wires immersed in FLiNaK with dissolved NiF 2 contained in graphite crucibles. The measured emf values were then converted to the FLiNaK Eutectic Potassium Electrode (FEKE) potential and used to quantify the activity of dissolved NiF 2 . This quantification was based upon comparative measurements of a reference solvent electrode consisting of a K-Bi alloy immersed in pure FLiNaK contained in a boron nitride crucible and a solute electrode. Short cell lives were characteristic of the measurements due to the corrosive nature of the fluoride salts. Quantifying the activity of NiF 2 will improve the utility of Ni 2+ /Ni reference electrodes in molten fluoride salts, which are notoriously difficult electrolytes to work with because of their reactivity. In conclusion, this work demonstrates the general nature of the solute-solvent approach as a repeatable, easily employed method for measuring the activity values of electroactive species in a variety of molten salts to improve understanding of the electroactive species behavior in these systems.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Rapid solidification of high-conductivity copper alloys

The main objective was to develop improved copper alloys of high strength and high thermal and electric conductivity. Chill block melt spinning was used to produce binary alloys of Cu-Cr and Cu-Zr, and ternary alloys of Cu-Cr-Ag. By quenching from the liquid state, up to 5 atomic percent of Cr and Zr were retained in metastable extended solid solution during the rapid solidification process. Eutectic solidification was avoided and the full strengthening benefits of the large volume fraction of precipitates were realized by subsequent aging treatment. The very low solid solubility of Cr and Zr in Cu result in a high conductivity Cu matrix strengthened by second phase precipitates. Tensile properties on as-cast and aged ribbons were measured at room and elevated temperatures. Precipitate coarsening of Cr in Cu was studied by changes in electrical resistance during aging. X-ray diffraction was used to measure the lattice parameter and the degree of supersaturation of the matrix. The microstructures were characterized by optical and electron microscopy.

Bloom, Theodore Atlas↗

Effects of Undercooling and Cooling Rate on Peritectic Phase Crystallization Within Ni-Zr Alloy Melt

The liquid Ni-16.75 at. pct Zr peritectic alloy was substantially undercooled and containerlessly solidified by an electromagnetic levitator and a drop tube. The dependence of the peritectic solidification mode on undercooling was established based on the results of the solidified microstructures, crystal growth velocity, as well as X-ray diffraction patterns. Below a critical undercooling of 124 K, the primary Ni{sub 7}Zr{sub 2} phase preferentially nucleates and grows from the undercooled liquid, which is followed by a peritectic reaction of Ni{sub 7}Zr{sub 2}+L → Ni{sub 5}Zr. The corresponding microstructure is composed of the Ni{sub 7}Zr{sub 2} dendrites, peritectic Ni{sub 5}Zr phase, and inter-dendritic eutectic. Nevertheless, once the liquid undercooling exceeds the critical undercooling, the peritectic Ni{sub 5}Zr phase directly precipitates from this undercooled liquid. However, a negligible amount of residual Ni{sub 7}Zr{sub 2} phase still appears in the microstructure, indicating that nucleation and growth of the Ni{sub 7}Zr{sub 2} phase are not completely suppressed. The micromechanical property of the peritectic Ni{sub 5}Zr phase in terms of the Vickers microhardness is enhanced, which is ascribed to the transition of the peritectic solidification mode. To suppress the formation of the primary phase completely, this alloy was also containerlessly solidified in free fall experiments. Typical peritectic solidified microstructure forms in large droplets, while only the peritectic Ni{sub 5}Zr phase appears in smaller droplets, which gives an indication that the peritectic Ni{sub 5}Zr phase directly precipitates from the undercooled liquid by completely suppressing the growth of the primary Ni{sub 7}Zr{sub 2} phase and the peritectic reaction due to the combined effects of the large undercooling and high cooling rate.

36 MATERIALS SCIENCE↗

The Effect of Sulfuric Acid Anodization on the Electrochemical Properties of Aluminum Alloy AlSi 10 Mg Prepared by Selective Laser Melting

Aluminum alloy, AlSi 10 Mg, prepared by selective laser melt (SLM) fabrication was anodized in 9.8% sulfuric acid (Type II) at 15 V for a total of 23 min. Experiments were performed to study the potentiostatic anodization process and its effects on the oxide coating morphology, thickness, and electrochemical properties of the alloy. Prior to anodization, the alloy microstructure is composed of aluminum cells encapsulated in a silicon network. Anodizing the abraded and polished AlSi 10 Mg surface produced a porous oxide layer with a thickness of 5μm. The oxide coating weight was 698 ± 29 mg/ft 2 . The oxide coating forms in the aluminum cells that are isolated from one another by the silicon eutectic phase. In electrochemical tests, the anodic and cathodic potentiodynamic polarization currents were suppressed by factors of 15× and 215×, respectively, as compared to the unanodized controls. The data indicate the anodic oxide coating suppresses the cathodic more than the anodic reaction rate. Linear polarization resistance (R p ) values increased by 279× after anodization. The corrosion current density values (j corr ) decreased by 133× after anodization. Taken together, the electrochemical data indicate the anodic oxide coating (unsealed) increases the corrosion resistance of the SLM alloy by two orders of magnitude.

Electrochemistry↗

Enhanced Tensile and Tear Toughness Properties of Thin-Wall Vacuum-Assisted High-Pressure Die-Cast Aural-5 Alloy by Friction Stir Processing

Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.

Friction stir processing, Aural-5, Strength, Tear ↗

Exploring Fission–Fusion Synergies to Accelerate Compatibility Understanding

To address the significant commercial interest in fusion energy, it will be necessary to accelerate the compatibility research associated with liquid breeders including Li, eutectic Pb–Li and LiF-BeF 2 (FLiBe) molten salt. Particularly for FLiBe, compatibility understanding is limited especially for fusion relevant materials such as reduced activation ferritic-martensitic steels, SiC and V alloys. The historical knowledge associated with molten salt reactors (MSRs) and recent work to commercialize MSRs can benefit fusion research. Recent experimental and modeling work has improved understanding and this knowledge can be applied to fusion relevant materials. For liquid metals (LMs), the comparisons to Li and Pb–Li are less direct but nevertheless can help guide the pathway toward commercialization. For Pb–Li, Al-rich coatings have been shown to inhibit dissolution and potentially increase operating temperatures. For commercialization, the experience with sensors and on-line cleanup can help guide future developments. Thus, it is worth considering the potential for fission-related research with LMs and molten salts to help accelerate fusion research.

36 MATERIALS SCIENCE↗

Overcoming time and complexity limitations in molecular dynamics investigations of equilibrium melting

Abstract A hybrid Monte-Carlo molecular-dynamics method for determining solidus and liquidus compositions in multicomponent systems is presented that overcomes both the time limitations in conventional molecular dynamics that prevent the evolution of distinct solid and liquid compositions via diffusion and the complexity challenge that prevents use of thermodynamic assessment in systems of many components. This hybrid method is validated in the Cu–Ni system against an independent assessment of solidus and liquidus compositions based on the regular solution model. Strategies for efficient mapping of different phase diagrams, based on the thermodynamic parameter T 0 , the temperature at which two phases of the composition X 0 have equal free energies, are presented and then demonstrated for the copper-nickel fully miscible system and the gold–silicon eutectic system. A calculation of the solidus and liquidus sampled during the equilibrium melting of equiatomic CrMnFeCoNi is performed, indicating that this method has potential to be extended to the study of many component alloys.

Au-Si↗

Materials and structural aspects of advanced gas-turbine helicopter engines

Advances in materials, coatings, turbine cooling technology, structural and design concepts, and component-life prediction of helicopter gas-turbine-engine components are presented. Stationary parts including the inlet particle separator, the front frame, rotor tip seals, vanes and combustors and rotating components - compressor blades, disks, and turbine blades - are discussed. Advanced composite materials are considered for the front frame and compressor blades, prealloyed powder superalloys will increase strength and reduce costs of disks, the oxide dispersion strengthened alloys will have 100C higher use temperature in combustors and vanes than conventional superalloys, ceramics will provide the highest use temperature of 1400C for stator vanes and 1370C for turbine blades, and directionally solidified eutectics will afford up to 50C temperature advantage at turbine blade operating conditions. Coatings for surface protection at higher surface temperatures and design trends in turbine cooling technology are discussed. New analytical methods of life prediction such as strain gage partitioning for high temperature prediction, fatigue life, computerized prediction of oxidation resistance, and advanced techniques for estimating coating life are described.

Freche, J. C.↗

Thermodynamic properties and crystallization kinetics at high liquid undercooling

The heat capacities of liquid and crystalline Au-Pb-Sb alloys in the glass-forming composition range were measured with droplet emulsion and bulk samples. Based on the measured C(sub p) data, the entropy, enthalpy, and Gibbs free energy functions of the eutectic, solid mixture, and undercooled liquid were determined as a function of undercooling and compared with theoretical predictions. The results indicate an isentropic temperature at 313 + or - 5 K, which agrees well with experimental data for the glass transition. A kinetics analysis of the nucleation undercooling response suggests that the proper choice for the Gibbs free energy change during crystallization is most important in analyzing the nucleation kinetics. By classical nucleation theory, the prefactors obtained, based on a variety of theoretical predictions for the driving force, can differ by six orders of magnitude. If the nucleation rates are extrapolated to high undercooling, the extrapolations based on measured heat capacity data show agreement, whereas the predicted nucleation rates are inconsistent with results from drop tower experiments. The implications for microg experiments are discussed.

Fecht, Hans J.↗

Effects of W on microstructure of as-cast 28 wt.%Cr–2.6 wt.%C–(0–10)wt.%W irons

Microstructures of as-cast 28 wt.%Cr–2.6 wt.%C irons containing (0–10)wt.%W with the Cr/C ratio about 10 were studied and related to their hardness. The experimental irons were cast into dry sand molds. Microstructural investigation was performed by light microscopy, X-ray diffractometry, scanning electron microscopy, transmission electron microscopy and energy-dispersive X-ray spectrometry. It was found that the irons with 1 to 10 wt.%W addition was hypereutectic containing large primary M{sub 7}C{sub 3}, whereas the reference iron without W addition was hypoeutectic. The matrix in all irons was austenite, partly transformed to martensite during cooling. The volume fractions of primary M{sub 7}C{sub 3} and the total carbides increased, but that of eutectic carbides decreased with increasing the W content of the irons. W addition promoted the formation of W-rich M{sub 7}C{sub 3}, M{sub 6}C and M{sub 23}C{sub 6}. At about 4 wt.%W, two eutectic carbides including M{sub 7}C{sub 3} and M{sub 6}C were observed together with primary M{sub 7}C{sub 3}. At 10 wt.%W, multiple carbides including primary M{sub 7}C{sub 3}, fish-bone M{sub 23}C{sub 6}, and M{sub 6}C were observed. M{sub x}C where x = 3 or less has not been found due possibly to the high M/C ratio in the studied irons. W distribution to all carbides has been determined increasing from ca. 0.3 to 0.8 in mass fraction as the W content in the irons was increased. W addition led to an increase in Vickers macro-hardness of the irons up to 671 kgf/(mm){sup 2} (HV30/15) obtained from the iron with 10 wt.%W. The formation of primary M{sub 7}C{sub 3} and aggregates of M{sub 6}C and M{sub 23}C{sub 6} were the main reasons for hardness increase, indicating potentially improved wear performance of the as-cast irons with W addition. - Highlights: • W addition at 1 up to 10 wt.%W to Fe–28Cr–2.6C produced “hypereutectic” structure. • W addition promoted the formation of W-rich M{sub 7}C{sub 3}, M{sub 6}C and M{sub 23}C{sub 6}. • M{sub 23}C{sub 6} has higher Fe/Cr and W/Cr atm% ratios than those in M{sub 7}C{sub 3}. • Si content and high W content over about 11 atm% are characteristics of M{sub 6}C. • Primary M{sub 7}C{sub 3} and aggregates of M{sub 6}C and M{sub 23}C{sub 6} increased the alloy macro-hardness.

36 MATERIALS SCIENCE↗

Additive Manufacturing of Pure Mo and Mo + TiC MMC Alloy by Electron Beam Powder Bed Fusion

A metal matrix composite powder of molybdenum (Mo) + TiC was produced by mechanical alloying (MA) and used in additive manufacturing by electron beam powder bed fusion along with pure Mo powder to form sandwich structures. The Mo + TiC solid layers formed mixed structures of Mo with discrete TiC particles, eutectic Mo + TiC, and Mo dendrites. Thermodynamic modeling showed that the system contained an invariant eutectic reaction in the composition range used and indicated that the system was highly sensitive to changes in composition and temperature.

36 MATERIALS SCIENCE↗

Phase relations in the Fe-FeSi system at high pressures and temperatures

The Earth's core is comprised mostly of iron and nickel, but it also contains several weight percent of one or more unknown light elements, which may include silicon. Therefore it is important to understand the high pressure, high temperature properties and behavior of alloys in the Fe–FeSi system, such as their phase diagrams. We determined melting temperatures and subsolidus phase relations of Fe–9 wt% Si and stoichiometric FeSi using synchrotron X-ray diffraction at high pressures and temperatures, up to ~200 GPa and ~145 GPa, respectively. Combining this data with that of previous studies, we generated phase diagrams in pressure–temperature, temperature–composition, and pressure–composition space. We find the B2 crystal structure in Fe–9Si where previous studies reported the less ordered bcc structure, and a shallower slope for the hcp+B2 to fcc+B2 boundary than previously reported. In stoichiometric FeSi, we report a wide B2+B20 two-phase field, with complete conversion to the B2 structure at ~42 GPa. The minimum temperature of an Fe–Si outer core is 4380 K, based on the eutectic melting point of Fe–9Si, and silicon is shown to be less efficient at depressing the melting point of iron at core conditions than oxygen or sulfur. At the highest pressures reached, only the hcp and B2 structures are seen in the Fe–FeSi system. We predict that alloys containing more than ~4–8 wt% silicon will convert to an hcp+B2 mixture and later to the hcp structure with increasing pressure, and that an iron–silicon alloy in the Earth's inner core would most likely be a mixture of hcp and B2 phases.

Fischer, Rebecca A.↗

Design of Novel Precipitate-Strengthened Al-Co-Cr-Fe-Nb-Ni High-Entropy Superalloys

Here, a series of non-equiatomic Al-Co-Cr-Fe-Nb-Ni high-entropy alloys, with varying levels of Co, Nb and Fe, were investigated in an effort to obtain microstructures similar to conventional Ni-based superalloys. Elevated levels of Co were observed to significantly decrease the solvus temperature of the γ' precipitates. Both Nb and Co in excessive concentrations promoted the formation of Laves and NiAl phases that formed either during solidification and remained undissolved during homogenization or upon high-temperature aging. Lowering the content of Nb, Co, or Fe prevented the formation of the eutectic type Laves. In addition, lowering the Co content resulted in a higher number density and volume fraction of the γ' precipitates, while increasing the Fe content led to the destabilization of the γ' precipitates. Various aging treatments were performed which led to different size distributions of the strengthening phase. Results from the microstructural characterization and hardness property assessments of these high-entropy alloys were compared to a commercial, high-strength Ni-based superalloy RR1000. Potentially, precipitation-strengthened high-entropy alloys could find applications replacing Ni-based superalloys as structural materials in power generation applications.

36 MATERIALS SCIENCE↗

Tungsten wire-nickel base alloy composite development

Further development and evaluation of refractory wire reinforced nickel-base alloy composites is described. Emphasis was placed on evaluating thermal fatigue resistance as a function of matrix alloy composition, fabrication variables and reinforcement level and distribution. Tests for up to 1,000 cycles were performed and the best system identified in this current work was 50v/o W/NiCrAlY. Improved resistance to thermal fatigue damage would be anticipated for specimens fabricated via optimized processing schedules. Other properties investigated included 1,093 C (2,000 F) stress rupture strength, impact resistance and static air oxidation. A composite consisting of 30v/o W-Hf-C alloy fibers in a NiCrAlY alloy matrix was shown to have a 100-hour stress rupture strength at 1,093 C (2,000 F) of 365 MN/square meters (53 ksi) or a specific strength advantage of about 3:1 over typical D.S. eutectics.

Brentnall, W. D.↗

Microstructures of niobium-germanium alloys processed in inert gas in the 100 meter drop tube

The 100 meter drop tube at NASA's Marshall Space Flight Center has been used for a series of experiments with niobium-germanium alloys. These experiments were conducted with electromagnetic levitation melting in a 200 torr helium environment. Liquid alloys experienced large degrees of undercooling prior to solidification in the drop tube. Several interesting metastable structures were observed. However, the recalescence event prevented extended solid solubility of germanium in the A-15 beta phase. Liquids of eutectic composition were found to undercool in the presence of solid alpha and solid Nb5Ge3.

Bayuzick, R. J.↗