Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Computation of Effective Radiative Properties of Powders for Selective Laser Sintering Simulations

Selective laser sintering (SLS) is an additive manufacturing technique for rapidly creating parts directly from a computer-aided design (CAD) model by using a laser to fuse successive layers of powder. However, better understanding of the effect of particle-level variations on the overall build quality is needed. In this work, we investigated these effects computationally by considering the role of the particle size distribution and variations in the powder bed depth to mimic the part complexity found in overhangs and protrusions. In addition, the results from these studies can be distilled to obtain better effective material properties such as laser absorptivity and laser extinction coefficient that are needed for continuum models of the process. We implement a Monte Carlo ray-tracing algorithm within the discrete element model in the open-source simulation software MFiX. Random, loose-packed, particle bed structures are generated, and effective absorptivity and extinction coefficients are calculated. Results are compared against previous computational and experimental measurements for free, monodisperse, and deep powder beds, with good agreement being obtained. Correlations along with uncertainties are developed to allow the effective absorptivity and extinction coefficient as a function of various particle and operational parameters to be accurately set in SLS macroscale models.

Moser, Daniel↗

In Situ Analysis of Laser Powder Bed Fusion Using Simultaneous High-Speed Infrared and X-ray Imaging

Laser powder bed fusion is a metal additive manufacturing technique that has received significant scientific and industrial attention over the past decades. However, the quality and reproducibility of parts manufactured by this technique is still a problem. Overcoming this issue requires an understanding of multiple complex physical phenomena which occur simultaneously during the process. Here, we illustrate a powerful new technique which synchronizes high-speed x-ray imaging with high-speed infrared imaging to study laser powder bed fusion processes in real time. Using this technique, we demonstrate the simultaneous observation of multiple phenomena including three-dimensional melt pool visualization, vapor plume dynamics, spatter formation, thermal history, and point cooling rates. The paired observation of these dynamic phenomena is critical to understanding the fundamentals of laser powder bed fusion, and the overall impact of process parameters on print quality.

36 MATERIALS SCIENCE↗

Additive Manufacturing of Pure Mo and Mo + TiC MMC Alloy by Electron Beam Powder Bed Fusion

A metal matrix composite powder of molybdenum (Mo) + TiC was produced by mechanical alloying (MA) and used in additive manufacturing by electron beam powder bed fusion along with pure Mo powder to form sandwich structures. The Mo + TiC solid layers formed mixed structures of Mo with discrete TiC particles, eutectic Mo + TiC, and Mo dendrites. Thermodynamic modeling showed that the system contained an invariant eutectic reaction in the composition range used and indicated that the system was highly sensitive to changes in composition and temperature.

36 MATERIALS SCIENCE↗

Laser powder-bed fusion additive manufacturing: Physics of complex melt flow and formation mechanisms of pores, spatter, and denudation zones

Our study demonstrates the significant effect of the recoil pressure and Marangoni convection in laser powder bed fusion (L-PBF) of 316L stainless steel. A three-dimensional high fidelity powder-scale model reveals how the strong dynamical melt flow generates pore defects, material spattering (sparking), and denudation zones. The melt track is divided into three sections: a topological depression, a transition and a tail region, each being the location of specific physical effects. The inclusion of laser ray-tracing energy deposition in the powder-scale model improves over traditional volumetric energy deposition. It enables partial particle melting, which impacts pore defects in the denudation zone. Different pore formation mechanisms are observed at the edge of a scan track, at the melt pool bottom (during collapse of the pool depression), and at the end of the melt track (during laser power ramp down). Finally, we discuss remedies to these undesirable pores are discussed. The results are validated against the experiments and the sensitivity to laser absorptivity.

36 MATERIALS SCIENCE↗

Multiscale investigations of nanoprecipitate nucleation, growth, and coarsening in annealed low-Cr oxide dispersion strengthened FeCrAl powder

A major challenge in the design of oxide dispersion strengthened (ODS) FeCrAl alloys is the optimization of the fine-scale particle size distribution that provides both beneficial mechanical properties and irradiation resistance. To address this obstacle, the nucleation, growth, and coarsening of the fine-scale (Y,Al,O) nanoprecipitates within an ODS FeCrAl powder was studied using atom probe tomography (APT) and small-angle neutron scattering (SANS). Mechanically alloyed Fe10Cr-6.1Al-0.3Zr + Y 2 O 3 wt.% (CrAZY) powders were heated in-situ from 20 to 1000 °C to capture the nucleation and growth of the nanoprecipitates using SANS. Furthermore, CrAZY powders were annealed at 1000 °C, 1050 °C, and 1100 °C for ageing times from 15 min to 500 h followed by either APT or magnetic SANS to study the structure, composition, and coarsening kinetics of the nanoprecipitates at high temperature. In-situ SANS results indicate nanoprecipitate nucleation and growth at low temperatures (200–600 °C). APT results revealed compositions corresponding to the cubic Y 3 Al 5 O 12 garnet (YAG) stoichiometry with a possible transition towards the perovskite YAlO3 (YAP) phase for larger precipitates after sufficient thermal ageing. However, magnetic SANS results suggest a defective structure for the nanoprecipitates indicated by deviations of the calculated A-ratio from stoichiometric (Y,Al,O) phases. Particle coarsening kinetics follow n = 6 power law kinetics with respect to particle size, but the mechanism cannot be explained through the dislocation pipe diffusion mechanism. In conclusion, the potential effect of precipitate coarsening during pre- and post-consolidation heat treatments on the irradiation resistance of ODS FeCrAl alloys is discussed with respect to sink strength maximization.

36 MATERIALS SCIENCE↗

Powders and pellets – Extrusion engineering for a Cu/BEA syngas-to-hydrocarbons catalyst

Converting high-performing powder catalysts from the laboratory reactor scale into effective extruded catalysts at the industrial scale remains a hurdle for advancing sustainable catalytic processes, such as the conversion of biogenic syngas into high octane gasoline. Recently, a process-intensified syngas-to-hydrocarbons (STH) reaction in a single reactor under relatively mild conditions (220–250 ºC, 0.75–2.0 MPa) was reported, enabled by the development of a dimethyl ether (DME) homologation catalyst, Cu-modified H-BEA (Cu/BEA) zeolite. In this study, we explore approaches for synthesizing engineered Cu/BEA catalysts for use in the STH reaction to retain the high performance observed with the powder catalyst. We demonstrate that changes to the order of manufacturing steps (i.e., Cu deposition, alumina binder addition, and extrusion) result in observable changes to key active sites (Brønsted acid sites and zeolitic Cu + species), and ultimately, catalyst performance. When the Cu precursor was added directly to BEA before extrusion, both types of active sites were stabilized, preserving the activity of the powder catalyst. However, when the Cu precursor was added after extrusion, the resulting Cu species were mobile, destabilizing Brønsted acid sites and leading to near-zero activity.

09 BIOMASS FUELS↗

Fatigue of additive manufactured Ti-6Al-4V, Part I: The effects of powder feedstock, manufacturing, and post-process conditions on the resulting microstructure and defects

Additive manufacturing provides an appealing means to process titanium alloy parts with new levels of conformability, complexity, and weight reduction. However, due to the heating/cooling rates and heat transfer associated with directed energy source material processing, the as-built AM parts contain unique material and microstructural features. In order to confidently manufacture fatigue critical additive manufactured (AM) Ti-6Al-4V parts, a better understanding of the interrelationships between powder feedstock, AM processes, structure of the processed parts, their resulting mechanical properties, and their performance under realistic loadings is necessary. Part I of this two-part collection focuses on the powder-process-structure relationships and how powder feedstock, manufacturing, and post-processing conditions can affect the microstructure and defect features that ultimately contribute to the fatigue performance of Ti-6Al-4V parts. The material and physical phenomena inherent to the AM process of Ti-6Al-4V are discussed in detail and related to the phase composition/structure, grain morphology, surface characteristics, defect size/distribution, and post-process treatments available for AM parts. This investigation is the foundation for the structure-performance relationships that will be covered in detail in Part II.

36 MATERIALS SCIENCE↗

Microstructural evolution and intermetallic formation in Zn-3Mg (wt%) powder mixture processed by high-pressure torsion

Severe plastic deformation (SPD) techniques have been used extensively over the past 40 years for producing strong metals and alloys. High-pressure torsion (HPT) is one of the most promising SPD techniques for achieving high strength through nanoscale grain refinement and phase transformation. In this research, a mixture of pure zinc (Zn) and magnesium (Mg) powders, Zn-3Mg (wt%), was HPT-processed under a pressure of 6 GPa for 1, 5, 10, 20, and 30 turns at room temperature to achieve a high strength biodegradable material. In order to understand the effects of pre-consolidation on the resulting microstructure and hardness, HPT processing was performed on loose powders placed in the die and also on a pre-compacted powder mixture and the resulting HPT disks were characterized by X-ray diffraction, scanning electron microscopy, atom probe tomography, and Vickers microhardness. In both cases, the HPT disk microstructures contained nanoscale grains, and stable and metastable strain-induced intermetallics, but an unusual softening appeared at large shear strains. Grain size, grain morphology, and the formation of different intermetallics were analyzed to explain the unusual hardness distribution, and it was found that an inverse Hall-Petch relationship between hardness and grain size exists. It is suggested that thermally-activated phenomena such as grain boundary sliding contributed to the strain-induced softening of this nano-structured biomaterial due to its low melting point. Finally, the current results are compared with those for HPT-processed cast alloys and hybrids of the same composition.

36 MATERIALS SCIENCE↗

Studies on in situ magnetic alignment of bonded anisotropic Nd-Fe-B alloy powders

We presented some considerations for achieving high degree of alignment in polymer bonded permanent magnets via the results of a study on in situ magnetic alignment of anisotropic Nd-Fe-B magnet powders. Contributions from effect of the alignment temperature, alignment magnetic field and the properties of the polymer on the hard magnetic properties of the bonded magnet were considered. Moreover, the thermo-rheological properties of the polymer and the response of the magnet powders to the applied magnetic field indicate that hard magnetic properties were optimized at an alignment temperature just above the melting temperature of the EVA co-polymer. This agrees with an observed correlation between the change in magnetization due to improved magnetic alignment of the anisotropic powders and the change in viscosity of the binder. Finally, manufacturing cost can be minimized by identifying optimum alignment temperatures and magnetic field strengths.

36 MATERIALS SCIENCE↗

Single particle impact explorations on the role of powder heat treatments in cold spray: Effects of strength and oxide structure

In cold spray, the optimization of the powder feedstock for improving the final properties of the coating and for improving the process itself are two different objectives. This paper explores the latter, studying the relationship between powder pre-heat treatment and the kinetic bonding between the individual particles and the substrate. Using a laser-induced particle impact test (LIPIT), we investigate the effect of different heat treatments on the critical adhesion velocity of Al 6061. Although heat treatments change the strength of the powders as well as the thickness of the native oxide layer each by as much as ∼50 %, the critical adhesion velocity remains constant to within only ∼10 %. A deeper analysis reveals that these two factors change in somewhat complementary ways for the heat treatments explored here, leading to counteracting effects. By quantitatively evaluating these two microstructural factors in tandem, we find that they are roughly equally important in determining the critical adhesion velocity. These observations thus provide insight for the development of new heat treatment regimens that might lower the adhesion velocity.

Al 6061↗

Structural characterisation of the Ce{sub 1-x}La{sub x}NbO{sub 4+{delta}} solid solution series: In-situ high-temperature powder diffraction studies

High-resolution neutron powder diffraction has been utilised to investigate the effect of lanthanum substitution on the structure of cerium niobate, CeNbO{sub 4+{delta}}, as a function of temperature. Two members of the Ce{sub 1-x}La{sub x}NbO{sub 4+{delta}} solid solution series, Ce{sub 0.8}La{sub 0.2}NbO{sub 4+{delta}} and Ce{sub 0.2}La{sub 0.8}NbO{sub 4+{delta}}, were examined over a temperature range of 293-923 K under a positive pressure of O{sub 2} (500 mbar). From this data it was found that on increasing lanthanum substitution there was an associated reduction in the temperature of the monoclinic-to-tetragonal phase transition. The data also suggested that increasing lanthanum substitution caused an associated decrease in the excess oxygen content. In addition, high-temperature X-ray powder diffraction data recorded in static air were also examined for four compositions of the Ce{sub 1-x}La{sub x}NbO{sub 4+{delta}} series (x=0.2, 0.4, 0.6 and 0.8). These data corroborated the results of the neutron diffraction experiments and also suggested that there was formation of an intermediate phase, analogous to the CeNbO{sub 4.08} phase of the parent material, during the phase transitions of the x=0.8 and 0.6 compositions. - Graphical abstract: Tetragonal scheelite-type structure (left) and in-situ X-ray powder diffraction data highlighting the oxidation and phase transformation of end member CeNbO{sub 4+{delta}}.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Neutron powder diffraction study of the layer organic-inorganic hybrid iron(II) methylphosphonate-hydrate, Fe[(CD{sub 3}PO{sub 3})(D{sub 2}O)]

The crystal and magnetic structures of the hybrid organic-inorganic layer compound Fe[(CD{sub 3}PO{sub 3})(D{sub 2}O)] have been studied by neutron powder diffraction as a function of temperature down to 1.5 K. The neutron diffraction pattern recorded at 200 K shows that the fully deuterated compound crystallizes in one of the two known forms of the undeuterated Fe[(CH{sub 3}PO{sub 3})(H{sub 2}O)]. The crystal structure is orthorhombic, space group Pmn2{sub 1}, with the following unit-cell parameters: a=5.7095(1) A, b=8.8053(3) A and c=4.7987(1) A; Z=2. The crystal structure remains unchanged on cooling from 200 to 1.5 K. Moreover, at low temperature, Fe[(CD{sub 3}PO{sub 3})(D{sub 2}O)] shows a commensurate magnetic structure (k=(0,0,0)). As revealed by bulk susceptibility measurements on Fe[(CH{sub 3}PO{sub 3})(H{sub 2}O)], the magnetic structure corresponds to a canted antiferromagnet with a critical temperature T{sub N}=25 K. Neutron powder diffraction reveals that below T{sub N}=23.5 K the iron magnetic moments in Fe[(CD{sub 3}PO{sub 3})(D{sub 2}O)] are antiferromagnetically coupled and oriented along the b-axis, perpendicular to the inorganic layers. No ferromagnetic component is observable in the neutron powder diffraction experiment, due to its too small value (<0.1{mu}{sub B}). - Graphical abstract: Crystal structure and magnetic structure of Fe[(CD{sub 3}PO{sub 3})(D{sub 2}O)].

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Self-powdering and nonlinear optical domain structures in ferroelastic beta'-Gd{sub 2}(MoO{sub 4}){sub 3} crystals formed in glass

Ferroelastic beta'-Gd{sub 2}(MoO{sub 4}){sub 3}, (GMO), crystals are formed through the crystallization of 21.25Gd{sub 2}O{sub 3}-63.75MoO{sub 3}-15B{sub 2}O{sub 3} glass (mol%), and two scientific curious phenomena are observed. (1) GMO crystals formed in the crystallization break into small pieces with a triangular prism or pyramid shape having a length of 50-500 {mu}m spontaneously during the crystallizations in the inside of an electric furnace, not during the cooling in air after the crystallization. This phenomenon is called 'self-powdering phenomenon during crystallization' in this paper. (2) Each self-powdered GMO crystal grain shows a periodic domain structure with different refractive indices, and a spatially periodic second harmonic generation (SHG) depending on the domain structure is observed. It is proposed from polarized micro-Raman scattering spectra and the azimuthal dependence of second harmonic intensities that GMO crystals are oriented in each crystal grain and the orientation of (MoO{sub 4}){sup 2-} tetrahedra in GMO crystals changes periodically due to spontaneous strains in ferroelastic GMO crystals. - Graphical abstract: This figure shows the polarized optical photograph at room temperature for a particle (piece) obtained by a heat treatment of the glass at 590 deg. C for 2 h in an electric furnace in air. This particle was obtained through the self-powdering behavior in the crystallization of glass. The periodic domain structure is observed. Ferroelastic beta'-Gd{sub 2}(MoO{sub 4}){sub 3} crystals are formed in the particle, and second harmonic generations are detected, depending on the domain structure.

36 MATERIALS SCIENCE↗

Neutron powder diffraction analysis of (Tm{sub 0.50}Ca{sub 0.50})MnO{sub 3} and (Lu{sub 0.50}Ca{sub 0.50})MnO{sub 3}

The crystal and magnetic structures of (Tm{sub 0.50}Ca{sub 0.50})MnO{sub 3} and (Lu{sub 0.50}Ca{sub 0.50})MnO{sub 3} have been investigated between 5 K and 300 K by means of high resolution neutron powder diffraction followed by Rietveld refinement and dc magnetic measurements. During cooling orbital ordering at the Mn sub-lattice takes place at T{sub OO}{approx}280 K in both compounds, inducing an orthorhombic to monoclinic phase transition. As the temperature is further decreased an antiferromagnetic CE-type structure occurs in both compounds at T{sub N}{approx}105 K. The comparison with other (Ln{sub 0.50}Ca{sub 0.50})MnO{sub 3} compounds reveals that at room temperature the average Jahn-Teller distortion increases sharply with the decrease of the ionic radius for lanthanides heavier than Sm. The ordered magnetic moment progressively decreases as the lanthanide ionic radius decreases on account of the decreased values of the Mn-O-Mn bond angles. - Graphical abstract: Rietveld refinement plot for (Tm{sub 0.50}Ca{sub 0.50})MnO{sub 3} obtained from neutron powder diffraction data collected at 5 K; the inset shows the CE-type spin ordering taking place at the Mn sub-lattice. Highlights: Black-Right-Pointing-Pointer The crystal and magnetic structures of (Tm{sub 0.50}Ca{sub 0.50})MnO{sub 3} and (Lu{sub 0.50}Ca{sub 0.50})MnO{sub 3} were analyzed by neutron powder diffraction. Black-Right-Pointing-Pointer Orbital ordering takes place below T{sub OO}{approx}280 K in both compounds. Black-Right-Pointing-Pointer An antiferromagnetic CE-type structure occurs in both compounds below T{sub N}{approx}105 K. Black-Right-Pointing-Pointer A Comparison with other (Ln{sub 0.50}Ca{sub 0.50})MnO{sub 3} compounds is reported.

36 MATERIALS SCIENCE↗

Search for octupolar order in NpO 2 by neutron powder diffraction

The magnetic structure of neptunium dioxide (NpO 2 ) remains a mystery despite decades of research. We revisited the search for magnetic ordering in NpO 2 by performing a powder neutron diffraction experiment at low temperatures and relatively large values of Q. Diffraction data were collected for 300 MK, 15 K, and 35 K to understand the phase transition near 25 K. However, no significant changes in the neutron diffraction pattern were identified. Using the octupolar magnetic form factor j 6 , the maximum theoretical expected value of the magnetic moment (3.27 μ B ), the calculated magnetic Bragg peak intensities would not be observable in neutron powder diffraction data. This value is much larger than the previously estimated magnetic moment of ~0.1 μ B . In conclusion, supported by experimental results, these calculations suggest that unpolarized neutron powder diffraction is unsuitable for measuring octupolar ordering in NpO 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Electrochemical hydrogen storage in LaNi{sub 4.25}Al{sub 0.75} alloys: A comparative study between film and powder materials

A comparison is made of the electrochemical and structural properties of LaNi{sub 4.25}Al{sub 0.75} alloys in thin film and powder forms. X-ray diffraction (XRD) revealed that both the LaNi{sub 4.25}Al{sub 0.75} thin film and powder materials are crystalline. Atomic force microscopy (AFM) and focused ion beam microscopy (FIB) proved that the film appeared to have a hill-like surface morphology, but was rather dense with a thickness of about 4.2 {mu}m. Simulated battery tests indicate that both exhibit similar electrochemical behavior, possibly due to their crystal structure, as it requires a primary activation to reach its fully active state. However it took a longer activation period for the film to be activated; an apparent initial decrease of charging voltage with cycle number was observed, as were abnormal discharge processes during activation. After 30 charge/discharge cycles, small needle-shaped aluminium oxide particles were formed on both the powder and film surfaces.

36 MATERIALS SCIENCE↗

Magnetic and structural properties of nanostructured Fe–20Al–2Cr powder mixtures

Nanostructured Fe–20Al–2Cr (wt.%) powders have been prepared using high energy planetary ball-mill. Changes in structural, morphological and magnetic properties of the powders during mechanical alloying (MA) and during subsequent annealing have been examined by X-ray diffraction, scanning electron microscopy (SEM) and vibrating sample magnetometer (VSM). The observed structural and microstructural changes have been related to several processes occurring during MA. After MA, the material becomes significantly disordered and refines to nanoscale grain sizes (~ 14 nm). The obtained bcc α-Fe(Al,Cr) solid solution shows a ferromagnetic behavior. Upon subsequent annealing at 400 °C, α-Fe{sub 2}O{sub 3} and spinel oxides are formed at the surface of particles, while structural defects disappeared as Fe(Al,Cr) solid solution becomes more ordered and grain growth occurs. The saturation magnetization (Ms) shows lower values after annealing, attributed to the formation of metal oxides with low magnetic moment. - Graphical abstract: Display Omitted - Highlights: • Nanostructured Fe–Al–Cr powders were prepared by MA. • Careful analysis of the XRD patterns by using the Rietveld refinement • The lattice distortion is evidenced by the increase of both the lattice parameter and the static Debye Waller parameter. • Annealing at 400 °C stabilizes the microstructure at the nanometer range and leads to the formation of Fe{sub 3}O{sub 4} and Fe{sub 2}O{sub 3} oxides. • Both the milled and annealed samples are ferromagnetic.

36 MATERIALS SCIENCE↗

Low-temperature synthesis of AlN powder with multicomponent additive systems by carbothermal reduction-nitridation method

AlN powders were synthesized at low temperatures (1300 and 1400 {sup o}C) by the carbothermal reduction-nitridation (CRN) method using multicomponent additive systems. The synthesis treatments were conducted in a graphite furnace with flowing nitrogen gas between 1200 and 1500 {sup o}C using powder mixtures with Al{sub 2}O{sub 3}:C molar ratio of 1:3 and 0.5-3 wt% of CaF{sub 2}, Y{sub 2}O{sub 3}, Li{sub 2}CO{sub 3} and/or SrCO{sub 3} as additives. In relation to the conventional CRN process, the use of multicomponent additive systems reduced the synthesis temperature in 200 {sup o}C (CaF{sub 2}-SrCO{sub 3}), 100 {sup o}C (CaF{sub 2}-Li{sub 2}CO{sub 3} and CaF{sub 2}-Y{sub 2}O{sub 3}-Li{sub 2}CO{sub 3}) or <100 {sup o}C (CaF{sub 2}-Y{sub 2}O{sub 3} and CaF{sub 2}-Y{sub 2}O{sub 3}-Li{sub 2}CO{sub 3}-SrCO{sub 3}). X-ray diffraction patterns showed that the additives reacted with the alumina powder forming aluminate phases, which vaporized with the increase of synthesis temperature. The enhanced AlN conversion rate was discussed in terms of the vaporization of aluminates in the reducing atmosphere.

36 MATERIALS SCIENCE↗