Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 721 records · Page 40

Characteristics of Bi-metallic Interfaces Formed During Direct Energy Deposition Additive Manufacturing Processing

Various additive manufacturing processes are being evaluated to reduce the time and cost for fabrication of low volume, complex, and multifunctional assemblies. This study evaluated two direct energy deposition processes for the fabrication of large bi-metallic structures. The materials evaluated were Inconel 625 and copper alloy C18150, which are used in various high heat flux applications. Inconel was deposited onto the C18150 substrate using blown powder and wire-fed processes. Complete bonding was obtained in both processes and the resulting interfaces were evaluated using microscopy and indentation testing. Differences were observed in the interface region suggesting the kinetic energy of the blown powder process resulted in more residual stress at the interface, promoting recrystallization and enhanced diffusion. This created a broader interface in the blown powder specimens compared to a narrower mechanically mixed interface with the wire-fed process.

36 MATERIALS SCIENCE↗

Microstructure and Properties of Inconel 718 Fabricated by Directed Energy Deposition with In-Situ Ultrasonic Impact Peening

Many inherent issues, such as the detrimental residual stress, columnar grains with anisotropy, and weak mechanical properties, have severely impeded the adoption of metal additive manufacturing (AM) techniques including powder bed fusion and directed energy deposition (DED) processes. In this study, a hybrid AM process that consists of layer-wise laser metal deposition (i.e., a DED process) and in-situ ultrasonic impact peening (UIP) was applied to obtain Inconel 718 superalloy workpieces. Also, for further property enhancement, a post-heat treatment was applied to the deposited material obtained by the hybrid AM process. Scanning electron microscopy and transmission electron microscope were used to investigate the microstructure morphology and reveal the underlying strengthening mechanism. Electron backscatter diffraction was employed to quantitatively study the microstructure resulted from the hybrid AM process and the post-heat treatment. The profile of residual stress along the depth direction was obtained through X-ray diffraction. The results demonstrate that this hybrid AM process is capable of producing high-quality metal parts with significantly refined microstructure, and beneficial compressive residual stress along the depth into surface. Severe plastic strains are introduced by UIP, and the resulted mechanical twinning and dynamic recrystallization play an important role in refining microstructure. The material microstructure is further refined down to 100 µm, and the texture anisotropy is significantly diminished after solution treatment at 980 °C for 1 hour. Under the as-built condition, in-situ ultrasonic peening alters the residual stress component from a tensile state to an overall compressive state with a maximum value of − 190 MPa within the range of measurement depth.

36 MATERIALS SCIENCE↗

Effect of Aging Treatment on the Precipitation Behavior and Mechanical Properties of Mg-9Gd-3Y-1.5Zn-0.5Zr Alloy

Aging heat treatments of an extruded Mg-9Gd-3Y-1.5Zn-0.5Zr (wt.%) alloy at 200, 225, and 250 °C for various times were studied. The results show that dynamic recrystallization (DRX) occurred during the extrusion process and the alloy exhibited a significant aging hardening response at temperatures ranging from 200 to 225 °C. The precipitation sequence of the alloy at 225 °C was supersaturated solid solution (SSSS) → β″ (D0{sub 19}, Mg{sub 3}RE) → β′ (bco, Mg{sub 15}RE{sub 3}), where the β′ phase was the primary precipitated phase. A large amount of discontinuous lamellar-shaped 14H-structure long period stacking ordered (LPSO) phase was also observed in the α-Mg matrix before and after aging treatments. Owing to the combined strengthening effect of fine DRXed grains, β′ nanoparticles, and widespread LPSO phases, the ultimate tensile strength and tensile yield strength of the peak-aged extruded alloy reached 409 and 303 MPa, respectively. The elongation in this circumstance was ~7.1%, which was slightly lower than that of the alloy before aging treatment.

36 MATERIALS SCIENCE↗

Effect of Microstructural Evolution on Sagging Behavior of Cold-Rolled Aluminum Foil During the Brazing Thermal Cycle

Effect of microstructural evolution on sagging behavior of aluminum foil was investigated during the brazing thermal cycle. During the brazing thermal cycle, the sagging behavior consists of three stages: slight sagging stage, accelerative sagging stage and slow sagging stage. The sagging of cold-rolled aluminum foil mainly occurs in the accelerative sagging stage, which is governed by recovery under external stress in the sagging test. The coarse recrystallized grain is responsible for the slow sagging stage by reducing grain boundary sliding. Increasing cold-rolled reduction and addition of final annealing heat treatment can improve sagging resistance by shortening recovery process during the brazing thermal cycle. Dissolution of dispersoids has few effects on sagging deformation.

36 MATERIALS SCIENCE↗

Effects of Roughing on Finish Rolling Simulations in Microalloyed Strip Steels

The effects of a roughing pass in hot rolling simulations were assessed in VN and Nb-Ti steels. Continuous cooling phase transformation temperatures, flow curves, softening mechanisms (dynamic transformation DT and dynamic recrystallization DRX), and deformed microstructure morphologies were analyzed. The application of one or more roughing passes eliminates the effects of prior microstructural history and ensures that all stock material experiences equivalent hot working conditions and state of the microalloying elements. It has been shown that roughing in hot simulation has the following positive influences: (1) provide more reliable flow stress data; (2) give greater consistencies and accuracy in analysis of softening mechanisms giving three distinct regimes (DT regime at temperatures below 800 °C, DT/DRX inter-mode regime between 800 and 950 °C and DRX regime for temperatures above 950 °C for VN steel); (3) promotion of softening mechanisms as evidence by low critical strains (ε{sub c DT} was within the range 0.08-0.12, while for finishing-only pass, the ε{sub c DT} was in the range of 0.11-0.14 at ε-dot =0.1 s{sup −1}); (4) for roughing and finishing schedules, DT was verified to occur at temperatures 117 and 133 °C above Ae{sub 3} for VN steel and Nb-Ti steel, respectively, compared to the F-only schedules which showed that DT can only occur at temperatures below the Ae{sub 3}; (5) RF schedules promoted uniform microstructural morphologies compared to inhomogeneous microstructures realized in F-only schedules.

36 MATERIALS SCIENCE↗

Effect of 0.1 wt.% Co on the Hot Deformation and Toughness of Fine-Grained Low-Carbon Steel at Sub-zero Temperatures

The effect of 0.1 wt.% Co on the hot deformation behavior of fine-grained low-carbon microalloyed steel was investigated at temperatures of 850-1200 °C and a strain rate of 5 s{sup −1}. Furthermore, the toughness of the steel with and without Co at sub-zero temperatures was evaluated. The results suggest that the addition of 0.1 wt.% Co increases the flow stress and delays the occurrence of dynamic recrystallization (DRX) at the same deformation temperature and strain. The DRX fraction of steel specimens without and with 0.1 wt.% Co was about 67.4 and 43.9% at 850 °C, respectively. Then, it increased to 100% at 1100 °C. Compared with steel without Co, cementite particles in the tempered sorbite of steel with 0.1 wt.% Co decreased in size but increased in quantity, yield strength increased from 756 to 787 MPa, and Charpy V-notch energy at − 20 and − 50 °C improved from 69 and 41 to 102 and 65 J, respectively. The fracture morphology and crack propagation characteristics were consistent with the variation in impact energy.

36 MATERIALS SCIENCE↗

The Effect of Grain Size on the Strain Hardening Behavior for Extruded ZK61 Magnesium Alloy

The effects of grain size on the tensile and compressive strain hardening behaviors for extruded ZK61 alloys have been investigated by uniaxial tensile and compressive tests along the extrusion directions. Cylindrical tension and compression specimens of extruded ZK61 alloys with various sized grain were fabricated by annealing treatments. Tensile and compressive tests at ambient temperature were conducted at a strain rate of 0.5 × 10{sup −3} s{sup −1}. The results indicate that both tensile strain hardening and compressive strain hardening of ZK61 alloys with different grain sizes have an athermal regime of dislocation accumulation in early deformation. The threshold stress value caused dynamic recovery is predominantly related to grain size in tensile strain hardening, but the threshold stress values for different grain sizes are almost identical in compressive strain hardening. There are obvious transition points on the tensile strain hardening curves which indicate the occurrence of dynamic recrystallization (DRX). The tensile strain hardening rate of the coarse-grained alloy obviously decreases faster than that of fine-grained alloys before DRX and the tensile strain hardening curves of different grain sizes basically tend to parallel after DRX. The compressive strain hardening rate of the fine-grained alloy obviously increases faster than that of coarse-grained alloy for twin-induced strain hardening, but compressive strain hardening curves also tend to parallel after twinning is exhausted.

36 MATERIALS SCIENCE↗

Microstructure Characteristic and Mechanical Properties of High-Strength Mg-Nd-Zn-Zr Alloy Seamless Tube Produced by Integrated Extrusion

Large size seamless tubes of Mg-3.0Nd-0.4Zn-0.4Zr alloy (NZ30K, in weight percent) were prepared by integrating backward extrusion with forward extrusion. Microstructure, mechanical properties, aging behavior and texture of the tubes were investigated. The microstructure of as-extruded tube is characterized by the blend of considerably elongated grains and fine equiaxed grains. The maximum values of yield strength and ultimate tensile strength, i.e., 191 and 245 MPa, were obtained in the as-extruded tubes, and these values were increased to 212 and 267 MPa in the peak-aged tubes (T5), implying an increasing ratio of 9 and 11%, respectively. The peak value of the Vickers’ micro-hardness of the NZ30K tubes extruded at 673, 723 and 753 K are 66, 64 and 60 (kilogram-force per square millimeter), respectively. The texture of NZ30K tube is weak, the primary mechanism behind which is suggested to be the particle-induced nucleation responsible for the promotion of recrystallization.

36 MATERIALS SCIENCE↗

Constitutive Model for Hot Deformation of the Cu-Zr-Ce Alloy

Hot compressive deformation behavior of the Cu-Zr-Ce alloy has been investigated according to the hot deformation tests in the 550-900 °C temperature range and 0.001-10 s{sup −1} strain rate range. Based on the true stress–true strain curves, the flow stress behavior of the Cu-Zr-Ce alloy was investigated. Microstructure evolution was observed by optical microscopy. Based on the experimental results, a constitutive equation, which reflects the relationships between the stress, strain, strain rate and temperature, has been established. Material constants n, α, Q and ln A were calculated as functions of strain. The equation predicting the flow stress combined with these materials constants has been proposed. The predicted stress is consistent with experimental stress, indicating that developed constitutive equation can adequately predict the flow stress of the Cu-Zr-Ce alloy. Dynamic recrystallization critical strain was determined using the work hardening rate method. According to the dynamic material model, the processing maps for the Cu-Zr and Cu-Zr-Ce alloy were obtained at 0.4 and 0.5 strain. Based on the processing maps and microstructure observations, the optimal processing parameters for the two alloys were determined, and it was found that the addition of Ce can promote the hot workability of the Cu-Zr alloy.

36 MATERIALS SCIENCE↗

The Precipitation Behavior and Hot Deformation Characteristics of Electron Beam Smelted Inconel 740 Superalloy

The Inconel 740 superalloy was prepared by the electron beam smelting (EBS) technology, the precipitation behavior and strengthening mechanism were studied, and the hot deformation characteristics of EBS 740 superalloy were investigated. The results indicate that the EBS 740 superalloy is mainly strengthened by the mechanism of weakly coupled dislocation shearing, and the resulting critical shear stress is calculated to be 234.6 MPa. The deformation parameters show a great influence on the flow behavior of EBS 740 superalloy. The strain rate sensitivity exponent increases with the increasing of deformation temperature, and the strain hardening exponent shows a decreasing trend with the increasing of strain. The activation energy of EBS 740 above 800 °C is measured to be 408.43 kJ/mol, which is higher than the 740H superalloy. A hyperbolic-sine-type relationship can be observed between the peak stress and Zener–Hollomon parameter. Nevertheless, the influence of deformation parameters is found to be considerably different at temperatures below and above 800 °C. The size of dynamic recrystallization (DRX) grains decreases with the increasing of strain rate when the strain rate is lower than 1/s, and reverse law can be found at higher strain rate. As a result, a piecewise function is established between the DRX grain size and hot working parameters.

36 MATERIALS SCIENCE↗

The Evolution of Second-Phase Particles in 6111 Aluminum Alloy Processed by Hot and Cold Rolling

The evolution of coarse Al{sub 9.9}Fe{sub 2.65}Ni{sub 1.45} phase, spherical Al{sub 12}(Mn,Fe){sub 3}Si phase and rod-like Q phase in a 6111 aluminum alloy during hot and cold rolling deformation processes was systematically investigated in this work. The results showed that the coarse Al{sub 9.9}Fe{sub 2.65}Ni{sub 1.45} particles are mainly distributed at the grain boundaries, accompanied by the co-formation of Al{sub 12}(Fe,Mn){sub 3}Si phase and Mg{sub 2}Si phase, while the spherical Al{sub 12}(Mn,Fe){sub 3}Si particles are mainly distributed in the grain interiors. Hot rolling has little effects on the size and distribution of both phases, but cold deformation can severely decrease the size of the particles by breaking the particles into small pieces. In addition, the temperature of 450 °C is not high enough for the dissolution of Q phase in the Al matrix, but the Q particles can be broken into small pieces due to the stress concentration during both hot and cold rolling deformation. In addition, the influences of phase evolution, dislocations and recrystallization on the mechanical properties evolution were also discussed.

36 MATERIALS SCIENCE↗

Deformation Mechanisms and Formability Window for As-Cast Mg-6Al-2Ca-1Sn-0.3Sr Alloy (MRI 230D)

The hot deformation characteristics of MRI 230D alloy have been evaluated in the temperature range 260-500 °C and strain rate range 0.0003-10 s{sup −1}, on the basis of processing map. The processing map exhibited two domains in the ranges: (1) 300-370 °C and 0.0003-0.001 s{sup −1} and (2) 370-480 °C and 0.0003-0.1 s{sup −1}. Dynamic recrystallization occurs in the both domains with basal slip dominating in the first domain along with climb as recovery process and second-order pyramidal slip dominating in the second with the recovery by cross-slip. In Domains (1) and (2), the apparent activation energy values estimated using the kinetic rate equation are 143 and 206 kJ/mole, respectively, the first one being close to that for lattice self-diffusion confirming climb. It is recommended that the alloy is best processed at 450 °C and strain rates less than 0.1 s{sup −1}, where non-basal slip and cross-slip occur extensively to impart excellent workability. The alloy exhibits flow instability in the form of adiabatic shear band formation and flow localization at lower temperatures and higher strain rates. Forging of a cup-shaped component was performed under various conditions, and the results validated the predictions of the processing map on the workability domains as well as the instability regimes.

36 MATERIALS SCIENCE↗

Properties of Rolled AZ31 Magnesium Alloy Sheet Fabricated by Continuous Variable Cross-Section Direct Extrusion

Rolling is currently a widely used method for manufacturing and processing high-performance magnesium alloy sheets and has received widespread attention in recent years. Here, we combined continuous variable cross-section direct extrusion (CVCDE) and rolling processes. The microstructure and mechanical properties of the resulting sheets rolled at different temperatures from CVCDE extrudate were investigated by optical microscopy, scanning electron microscope, transmission electron microscopy and electron backscatter diffraction. The results showed that a fine-grained microstructure was present with an average grain size of 3.62 μm in sheets rolled from CVCDE extrudate at 623 K. Dynamic recrystallization and a large strain were induced by the multi-pass rolling, which resulted in grain refinement. In the 573-673 K range, the yield strength, tensile strength and elongation initially increased and then declined as the CVCDE temperature increased. The above results provide an important scientific basis of processing, manufacturing and the active control on microstructure and property for high-performance magnesium alloy sheet.

36 MATERIALS SCIENCE↗

Tensile Properties and Fracture Characteristics of Nanostructured Copper and Cu-SiC Nanocomposite Produced by Mechanical Milling and Spark Plasma Sintering Process

The presence of large grains within nanometric and ultrafine grain matrix is an effective method in order to enhance strength while keeping the high ductility of metals. For this purpose, in this research, spark plasma sintering (SPS) was used to consolidate milled Cu and Cu-SiC powders. In SPS process, local sparks with high temperature between particles take place and locally lead to intense grain growth, and therefore, this method has the ability to produce bimodal grain structures in copper and copper-based composites. Microstructural and mechanical studies showed ≈ 185 and ≈ 437 nm matrix grain sizes, high tensile yield strength values of ≈ 188.4 and ≈ 296.9 MPa, and fracture strain values of 15.1 and 6.7% for sintered Cu and Cu-4 vol.% SiC nanocomposite materials, respectively. The presence of nanoparticles promoted the occurrence of static recrystallization and decreased the fraction of coarse grains in microstructure. The high tensile properties of the produced materials are attributed to fine grain size, homogenous dispersion of nanoparticles and retarded grain boundary migration during sintering.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Characterization of the Hot Deformation Behavior of a Newly Developed Nickel-Based Superalloy

To clarify the microstructural evolution and hot workability of GH4282 during hot forming processes, the hot deformation behavior of this superalloy was investigated by isothermal compression tests in the temperature interval of 950-1210 °C and the strain rate range of 0.01-10 s{sup −1} with a true strain of 0.7. The results show that the flow stresses decrease with an increase in the deformation temperature and a decrease in the strain rate. The characteristic of dynamic recrystallization is revealed by the flow curves. The variation rule of the flow stress can be well described by the hyperbolic sine type equation, and the thermal deformation activation energy is determined to be 498.118 kJ/mol. The optimum hot working parameters are 1100-1180 °C and 0.01-0.1 s{sup −1}, under which the fine and uniform microstructure can be obtained.

36 MATERIALS SCIENCE↗

Effect of Hot Deformation on Texture and Microstructure in Fe-Mn Austenitic Steel During Compression Loading

Hot compression tests of a new high-Mn austenitic steel were carried out at deformation temperatures of 700, 800, 900, and 1000 °C under strain rate of 0.01 s{sup −1}. The hot deformation behavior was investigated by the analyses of flow curves, texture, and deformed microstructures. Microstructures of the deformed specimens and macrotexture were examined using electron backscatter diffraction and x-ray diffraction methods, respectively. The results showed that the flow stress depended strongly on the deformation temperature and decreased by increasing deformation temperature. The microstructural evidence indicated that the dynamic recrystallization (DRX) process of experimental steel was initiated at 800 °C with necklace structure. The volume fraction of DRX grains was considerably increased by increasing deformation temperature to 1000 °C. Texture of the DRX grains tended to become a weak texture and was associated with the formation of Goss and R-Cube components. Meanwhile, martensitic transformation was detected in the hot-deformed austenite. The martensitic transformation was the most difficult in the DRX grains because of the effect of small grain size. The tendency of transformation was decreased after compression at 1000 °C.

36 MATERIALS SCIENCE↗

X-ray Diffraction Investigation of Annealing Behavior of Peened Surface Deformation Layer on Precipitation Hardening Stainless Steel

In order to investigate the recrystallization behavior of peened surface deformation layer of precipitation hardening stainless steel, a classic x-ray diffraction line profile analysis, Voigt method, was carried out on peened 17-4PH with different isothermal annealing temperatures. The activation energy of domain boundary migration (Q{sub a}) and the activation energy of microstrain relaxation (Q{sub b}) were calculated by regression analysis in different annealing temperature conditions. The results show that the value of Q{sub a} decreases with annealing temperature increasing, which is due to the influence of precipitation (ε-Cu) size on the movements of grain and subgrain boundaries. The maximum growth rate of ε-Cu particles occurs during 400 to 500 °C interval. Compared with growth behavior of domain size, microstrain relaxation behavior is less sensitive to precipitation particle size. The effects of annealing temperature and time on dislocation density are both significant when annealing temperature is lower than 500 °C. However, the effect of annealing temperature on dislocation density becomes insignificant when annealing temperature is higher than 500 °C. 300 °C annealing temperature only leads to the microstrain relaxation but nearly cannot lead to the domain size growth even if prolonging annealing time. Microstructure enhancement effect still exists in plastic deformation layer when 300 °C annealing temperature lasts for 60 min but nearly disappears when 600 °C annealing temperature lasts for 20 min.

36 MATERIALS SCIENCE↗

Effect of Ceramic Rolling and Annealing on Mechanical Properties of AlCoCrFeNi{sub 2.1} Eutectic High-Entropy Alloys

It was firstly proved that AlCoCrFeNi{sub 2.1} could optimize the strength-ductility combination by ceramic rolling at room temperature. The technique greatly enhanced the strength of the materials at the price of slight ductility, which is different from the previous studies. When the thickness reduction was 23.06%, the yield strength and compressive strength were 1611.42 and 2212.99 MPa, respectively, with the plastic strain of 28.36%. Such an excellent combination of strength and ductility was attributed to the distribution of the residual stress, the high hydrostatic stress and the shear bands in ceramic rolling process. The plastic strain of the material increased to 38.54%, and the strength reduced to 1900.73 MPa after annealing at 800 °C for 1 h. A lot of like-flower patterns of recrystallized ultrafine grain were observed after annealing at 800 °C due to the sluggish diffusion in HEAs and the effect of ceramic rolling. In addition, after annealing at 800 °C, the fracture mode changed to shearing fracture of microvoid aggregation from cleavage/quasi-cleavage fracture of as-rolled sample due to the deposition of the second phase in the tested sample.

36 MATERIALS SCIENCE↗