Evaluation of Experimental Studies in the U-Rich Region of the U-Pu Phase Diagram

Upon the re-examination of two experimental studies, additional thermophysical data pertaining to the uranium-rich portion of the uranium-plutonium binary phase diagram have been elucidated. The first study involved the analysis of solidification cooling curves following the processing of U-Pu alloys. Two phase transitions (liquidus and bcc) were evaluated and the results agreed very well with the established boundaries. The second study was actually performed over sixty years ago but still warrants recognition due to the paucity of thermodynamic data on the U-Pu system to date. From the investigation, the activity coefficients of plutonium in liquid uranium from 1813 K to 2042 K were derived assuming Henry’s law from which the partial molar excess Gibbs energy change of plutonium was obtained: Δ G-bar {sup ex}=R∗T∗ln γ{sub Pu}{sup o}=− 76694+39.2∗T(J/mol).

36 MATERIALS SCIENCE↗

Dendritic Growth Under Natural and Forced Convection in Al-Cu Alloys: From Equiaxed to Columnar Dendrites and from 2D to 3D Phase-Field Simulations

The interaction between convection and solute transport during solidification has significant influence on the dendritic evolution. By employing the phase-field lattice-Boltzmann approach together with the parallel and adaptive-mesh-refinement algorithm, the dendritic evolution under convection is simulated in both 2D and 3D cases. The flow-induced redistribution of the solute alters both tip velocity and the development of dendritic arms. The effect of both convection and undercooling is quantified and compared using the length ratio of the dendritic arms. The effect of convection behavior (i.e., natural and forced) and domain dimension (i.e., 2D and 3D) on dendritic growth is discussed. Results show that the convection effect is mainly dominated by the convection mode, and the melt flow in 2D can produce biased results comparing with those in 3D.

36 MATERIALS SCIENCE↗

Characterization, Mechanism and Control Measures of V Segregation in Continuous Casting Billet of C-Mn Steel

To eliminate V segregation, which significantly deteriorates the homogeneity of continuous casting steel billets, V segregation in the C-Mn steel billet was observed by microscope, SEM and EDS. The formation mechanism and control measures for V segregation were proposed. Results show that many slim V segregation strips are distributed on an inverted conical surface and that most segregation strips start from the vertex of the inverted conical surface. A series of inverted conical surfaces containing V segregation strips periodically appears along the longitudinal direction of the billet. The microstructures in the V segregation strip are fine granular structures, while the microstructures outside the V segregation strip are coarse Widmanstätten. The V segregation strip also contains many inclusions and porosities. The formation mechanism for V segregation, which is illuminated by a physical simulation of Al-5wt pctCu alloy, is attributed to the fissure in the equiaxed dendritic network torn by solidification contraction. By controlling the percentage and distribution of equiaxed grains, the V segregation in the billet of C-Mn steel is completely eliminated.

36 MATERIALS SCIENCE↗

Precipitation Mechanism and Reduction of Amount of Primary Carbides During Electroslag Remelting of 8Cr13MoV Stainless Steel

The precipitation and growth of primary carbides in 8Cr13MoV steel during electroslag remelting (ESR) were studied. The effects of melting rate and fill ratio of ESR on the reduction of primary carbides were clarified. Primary carbides M{sub 7}C{sub 3} precipitated from liquid steel at the final stage of solidification, which is attributed to an enrichment of carbon and chromium in liquid steel. The carbon content in the residual liquid steel was the determining factor for the formation of primary carbides. The growth of primary carbides was affected mainly by the chromium-concentration and temperature-field gradients. An appropriate melting rate facilitated the nucleation and growth of dendrites, which caused dendrite closure and prevented the further enrichment of carbon atoms. Primary carbides were refined and their amount was reduced when using a lower ESR melting rate. The fill ratio can affect the uniformity of the temperature field in the liquid metal pool and heat transfer from the slag pool to the liquid metal pool, and an optimal fill ratio resulted in a minimum mushy zone and less primary carbides. The volume fraction of primary carbides was reduced by 23 pct when the melting rate decreased from 150 to 133 kg/h and the fill ratio increased from 0.23 to 0.33.

36 MATERIALS SCIENCE↗

Effect of Mg-Bearing Oxide(+TiN) Inclusion on Microstructure of Fe-16 Mass Pct Cr Ferritic Alloy and Its Evolution During Heating at 1573 K (1300 °C)

Both the effects of Mg-bearing oxide and Mg-bearing oxide +TiN inclusions on the microstructures of Fe-16 mass pct Cr alloy should be clarified. In this paper, the effects of Mg-bearing oxide(+TiN) inclusions on the microstructures of Fe-16 mass pct Cr ferritic alloy and changes due to the inclusions during heating at 1573 K (1300 °C) were studied by manual and automatic SEM-EDS analyses. Three alloys were used as specimens. The inclusions were Al{sub 2}TiO{sub 4} +TiN with a small amount of TiN in alloy #1, Al{sub 2}(Mg, Ti)O{sub 4} in alloy #2 and Al{sub 2}(Mg, Ti)O{sub 4} +TiN in alloy #3. The average grain size was smaller, and the ratio of columnar grains was lower in the as-cast alloy #2 and as-cast alloy #3 than that in the as-cast alloy #1. This is attributed to the heterogeneous nucleation of delta ferrite on Al{sub 2}(Mg, Ti)O{sub 4} during solidification. Refinement of the microstructures of ferritic steel by Mg-bearing oxide + multi-TiN inclusions is proposed. Changes in composition, aspect ratio, and size distribution of inclusions in each alloy during heating were investigated systematically. Mg-bearing oxide(+TiN) was dispersed in both the as-cast alloys and heated alloys, which contributed to microstructural refinement of the heated alloys through the pinning effect.

36 MATERIALS SCIENCE↗

Modeling and Simulation of Porosity in Spray Deposition

Numerical models, consisting of interstitial porosity model and gas porosity model, have been developed to predict the porosity in the spray deposition process. The interstitial porosity model is based on the assumption of liquid feeding in the porous mushy layer of the deposit. The porosity fraction is related to the particle packing density and the amount of the feeding flow during solidification. The gas porosity model is based on the diffusion kinetics of gas pore formation. A numerical simulation of spray deposition for a billet was carried out by coupling the porosity model with the shape and heat-transfer models. The volume fraction and distribution of the porosity were investigated. As a result of the experimental verification, the simulation results showed good agreement with the experimental data. As applications, the models were used to investigate the influence of spray process parameters on porosity formation. The investigation demonstrated that the porosity is substantially influenced by the temperature of the impinging layer and the preheating of the substrate.

36 MATERIALS SCIENCE↗

Understanding the Formation and Evolution of Oxide Inclusions in Si-Deoxidized Spring Steel

To illustrate the mechanism of the formation and evolution of inclusions in Si-deoxidized spring steel, pilot trials and systematic samplings were conducted, and detailed information about the inclusion density, morphology and composition was elucidated by electron probe X-ray microanalysis. The steel samples were collected from the vacuum degassing furnace, tundish furnace and spring rods after hot rolling. Based on the relationship between the mass ratio of X{sub (CaO)}/X{sub (SiO{sub 2)}} and diameters of inclusions, CaO-SiO{sub 2} inclusions were found to be formed by the coalescence between SiO{sub 2} and CaO-SiO{sub 2} inclusions. Most CaO-SiO{sub 2} inclusions > 10 μm were located in the melilite areas with liquidus temperatures < 1400 °C. The Al{sub 2}O{sub 3}-SiO{sub 2}-CaO inclusions in the steel samples from the vacuum degassing and tundish furnaces were considered to be formed by reduction of CaO-SiO{sub 2} inclusions by Al dissolved in steel. The increased number density of Al{sub 2}O{sub 3}-SiO{sub 2}-CaO inclusions in spring rods was primarily attributed to the entrapment of Na{sub 2}O-contained mould flux particles and inclusions crushed after hot rolling. Many Al{sub 2}O{sub 3}-SiO{sub 2}-MnO and SiO{sub 2}-MnO inclusions were observed in tundish furnace samples, which originated from inherent reactions between [Al], [Si], [Mn] and [O] in the molten steel. The SiO{sub 2} precipitation of Al{sub 2}O{sub 3}-SiO{sub 2}-MnO inclusions was attributed to the solubility decrease during the solidification process with temperature drop.

36 MATERIALS SCIENCE↗

Porosity Prediction in A356 Wheel Casting

A FLUENT™-based thermal-fluid-compositional model has been developed and applied to a low-pressure, die-cast, A356 aluminum alloy wheel to explore the effects of macro-segregation of hydrogen and late-stage liquid encapsulation on pore formation during solidification. Based on the evolution of temperature, pressure, and hydrogen concentration in the liquid output from FLUENT, the porosity size distribution has been predicted at a number of locations in a commercially produced wheel using an in-house micro-porosity model. The porosity model incorporates pore nucleation kinetics based on hydrogen supersaturation, and two modes of pore growth: the first, occurring at low solid fractions is based on hydrogen diffusion; and the second, occurring at high solid fractions is based on conservation of volume. Samples from a commercially cast wheel have been analyzed using X-ray micro-tomography to provide basic validation of the micro-porosity model. The predicted results showed that the evolution in pressure has the dominant effect on pore growth, but only under conditions where pores have nucleated prior to late-stage liquid encapsulation. Otherwise, the cooling rate appears to have the dominant effect. The accuracy of the model is discussed in terms of the predicted pore size distribution and number density of pores. Areas for continued development are presented.

36 MATERIALS SCIENCE↗

Numerical Simulation and Experimental Validation of Nondendritic Structure Formation in Magnesium Alloy Under Oscillation and Ultrasonic Vibration

In this study, the formation of nondendritic structures in the primary phase of magnesium alloy solidified under oscillation and ultrasonic vibration was investigated by numerical simulation and experimentally. The growth and motion of a dendrite during solidification was simulated by a combination of the lattice Boltzmann method and the phase-field method. The simulation and experimental results indicated that higher oscillation amplitudes and acoustic streaming made the microstructures change from dendritic to nondendritic in the α-Mg primary phases. A sufficient shear stress and an appropriate flow time in the barrel should be satisfied when a given inclined angle is selected. The effects of the flow and the thermal field on the nucleation behavior, the constitutional undercooling, and the growth morphology are also discussed. It was found that a high shear rate and high turbulence can help homogenize the temperature and the concentration fields and collide and rotate the α-Mg primary phases.

36 MATERIALS SCIENCE↗

Formation Mechanisms and Microstructure Characterization of Al/Al{sub 3}Ni In-situ Composite by Compound Casting

The Compound casting method was used to produce an Al/Ni bimetal composite. The mechanisms of formation of the reinforcing intermetallic phases were studied and the produced bimetal composite’s microstructure was then characterized. The results showed that the Al/Ni interface consisted of two intermetallic layers including Al{sub 3}Ni{sub 2} and Al{sub 3}Ni. It is suggested that the Al{sub 3}Ni reinforcing particles of the composite originated from two sources. (1) Some Al{sub 3}Ni particles detached from the Al{sub 3}Ni layer formed at the interface between the Ni core and the Al melt and dispersed in the liquid Al and (2) Al-Al{sub 3}Ni eutectic phase, which formed during the solidification process. The increase in the temperature led to the formation of more reinforcing particles and extended the depth of dispersion of the particles in the Al matrix.

36 MATERIALS SCIENCE↗

Comparison of Extensive Thermal Cycling Effects on Microstructure Development in Micro-alloyed Sn-Ag-Cu Solder Joints

Pb-free solder alloys based on the Sn-Ag-Cu (SAC) ternary eutectic have promise for widespread adoption across assembly conditions and operating environments, but enhanced microstructural control is needed. Micro-alloying with elements such as Zn was demonstrated for promoting a preferred solidification path and joint microstructure earlier in simple (Cu/Cu) solder joints studies for different cooling rates. This beneficial behavior now has been verified in reworked ball grid array (BGA) joints, using dissimilar SAC305 (Sn-3.0Ag-0.5Cu, wt.%) solder paste. After industrial assembly, BGA components joined with Sn-3.5Ag-0.74Cu-0.21Zn solder were tested in thermal cycling (-55 C/+125 C) along with baseline SAC305 BGA joints beyond 3000 cycles with continuous failure monitoring. Weibull analysis of the results demonstrated that BGA components joined with SAC + Zn/SAC305 have less joint integrity than SAC305 joints, but their lifetime is sufficient for severe applications in consumer, defense, and avionics electronic product field environments. Failure analysis of the BGA joints revealed that cracking did not deviate from the typical top area (BGA component side) of each joint, in spite of different Ag3Sn blade content. Thus, SAC + Zn solder has not shown any advantage over SAC305 solder in these thermal cycling trials, but other characteristics of SAC + Zn solder may make it more attractive for use across the full range of harsh conditions of avionics or defense applications.

36 MATERIALS SCIENCE↗

The Role of Elastic and Plastic Anisotropy of Sn in Recrystallization and Damage Evolution During Thermal Cycling in SAC305 Solder Joints

Because failures in lead-free solder joints occur at locations other than the most highly shear-strained regions, reliability prediction is challenging. To gain physical understanding of this phenomenon, physically based understanding of how elastic and plastic deformation anisotropy affect microstructural evolution during thermomechanical cycling is necessary. Upon solidification, SAC305 (Sn-3.0Ag-0.5Cu) solder joints are usually single or tricrystals. The evolution of microstructures and properties is characterized statistically using optical and orientation imaging microscopy. In situ synchrotron x-ray measurements during thermal cycling are used to examine how crystal orientation and thermal cycling history change strain history. Extensive characterization of a low-stress plastic ball grid array (PBGA) package design at different stages of cycling history is compared with preliminary experiments using higher-stress package designs. With time and thermal history, microstructural evolution occurs mostly from continuous recrystallization and particle coarsening that is unique to each joint, because of the specific interaction between local thermal and displacement boundary conditions and the strong anisotropic elastic, plastic, expansion, and diffusional properties of Sn crystals. The rate of development of recrystallized microstructures is a strong function of strain and aging. Cracks form at recrystallized (random) boundaries, and then percolate through recrystallized regions. Complications arising from electromigration and corrosion are also considered.

36 MATERIALS SCIENCE↗

Homogenizing Advanced Alloys: Thermodynamic and Kinetic Simulations Followed by Experimental Results

Segregation of solute elements occurs in nearly all metal alloys during solidification. The resultant elemental partitioning can severely degrade as-cast material properties and lead to difficulties during post-processing (e.g., hot shorts and incipient melting). Many cast articles are subjected to a homogenization heat treatment in order to minimize segregation and improve their performance. Traditionally, homogenization heat treatments are based upon past practice or time-consuming trial and error experiments. Through the use of thermodynamic and kinetic modeling software, NETL has designed a systematic method to optimize homogenization heat treatments. Use of the method allows engineers and researchers to homogenize casting chemistries to levels appropriate for a given application. The method also allows for the adjustment of heat treatment schedules to fit limitations on in-house equipment (capability, reliability, etc.) while maintaining clear numeric targets for segregation reduction. In this approach, the Scheil module within Thermo-Calc is used to predict the as-cast segregation present within an alloy, and then diffusion controlled transformations is used to model homogenization kinetics as a function of time and temperature. Examples of computationally designed heat treatments and verification of their effects on segregation and properties of real castings are presented.

36 MATERIALS SCIENCE↗

Process Evaluation of AISI 4340 Steel Manufactured by Laser Powder Bed Fusion

Laser powder bed fusion (L-PBF) involves the consolidation of metal powder, layer by layer, through laser melting and solidification. In this study, process parameters are optimized for AISI 4340 steel to produce dense and homogeneous structures. The optimized process parameters produce mechanical properties at the center of the build plate that are comparable to wrought in the vertical and horizontal orientations after heat treatment and machining. Four subsequent builds are filled with specimens to evaluate the mechanical behavior as a function of location and orientation. Variations in the mechanical properties are likely due to recoater blade interactions with the powder and uneven gas flow. The results obtained in this study are analyzed to assess the reliability and reproducibility of the process. A different build evaluates the performance of near-net-shaped tensile specimens angled 35°-90° from the build plate surface (horizontal). Ductility measurements and surface roughness vary significantly as a function of the build angle. In the stress-relieved and as-built conditions, the mechanical behavior of vertically oriented specimens exhibits somewhat lower and more variable ductility than horizontally oriented specimens. Therefore, several process variables affect the mechanical properties of parts produced by the L-PBF process.

36 MATERIALS SCIENCE↗

Abnormal Transient Liquid Phase Bondability of High-Volume Fraction SiC Particle-Reinforced A356 Composite for Cu Interlayer and the Interlayer Improvement Routes

Features of transient liquid phase (TLP) bondability of high-volume fraction (70 vol.%) SiC particle-reinforced A356 composite for popular Cu interlayer were investigated. Although Cu foil was melted, molten Cu was completely expulsed, indicating that the numerous SiC particles significantly deteriorated wettability not only at particle/braze metal (P/M) interface, but also at the matrix/braze metal (M/M) interface. For the reason of poor wettability at P/M interface, a model showing there is a “window period” for actual wetting reaction (allowing liquid phase to be in contact with surficial SiC particles) much shorter than nominal isothermal solidification time during TLP bonding of the composite containing sintered ceramic preform was proposed. For the poor wettability at M/M interface, both size effect of too small matrix unit (2 ~ 20 μm) and restraint effect of the rigid porous ceramic preform on suppressing oxide film crack on the small matrix unit surface were proposed. Thus, chemical route to disrupt oxide film on the small matrix unit surface should be preferred in braze composition design. For example, Al-27Cu-5Si-2Mg-1Ti braze was developed by co-addition of Mg and Ti to improve wettability and to in situ reinforce bond seam, respectively; Ti also could remedy Mg loss for improving wettability.

36 MATERIALS SCIENCE↗

Tribological Performance of Ni{sub 3}Al Matrix Self-Lubricating Composites Containing Multilayer Graphene Prepared by Additive Manufacturing

In order to improve tribological performance of Ni{sub 3}Al-based alloy, Ni{sub 3}Al matrix composites containing 1.5 wt.% multilayer graphene (MLG) are prepared through additive manufacturing (AM) and spark plasma sintering (SPS), which are denoted as NMAM and NMSPS, respectively. Tribological behaviors of NMAM and NMSPS against Si{sub 3}N{sub 4} balls are researched under constant speed (0.2 m/s) and varied loads (from 4 to 16 N) for evaluating the tribological properties of NMAM and NMSPS. The results present that NMAM exhibits the excellent tribological properties [low friction coefficients (0.26-0.40) and considerable wear resistance (2.8-4.6 × 10{sup −5} mm{sup 3} N{sup −1} m{sup −1})] as compared to NMSPS, which attributes to the uniform enrichment of MLG with properties of high tensile strength and being easily sheared off on the worn surfaces. Owing to the use of spherical prealloyed powder containing multilayer graphene and the characteristics of layer by layer depositing in the AM process, NMAM has a more compact and uniform substrate, which persistently provides a source of the formation of continuous and stable frictional layer. Due to the characteristics of AM rapid solidification, NMAM has the small grain size and well-compacted microstructure, which can effectively reduce the probability of spalling wear and lead to the increase in wear resistance of materials. The research can offer the reference for self-lubricating materials prepared by AM technology.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Nucleation and Grain Refinement of 7A04 Aluminum Alloy Under a Low-Power Electromagnetic Pulse

The effects of a low-power electromagnetic pulse on the grain size and cooling curve of high-strength aluminum alloy 7A04 were investigated for various pulse duty cycles. This electromagnetic pulse treatment was found to effectively produce fine grains with globular crystals and a uniform microstructure for pulse duty cycles between 20 and 40%. The key factors that affected grain refinement under the electromagnetic pulse included the electromagnetic energy and the conversion frequency between B and E. The nucleation rate increased as the nucleation period was extended. A new kinetic condition of magnetic nucleation was explored by decreasing the critical Gibbs free energy in the electromagnetic pulse, which was more sensitive under low undercooling. In addition, the crystal orientation was controlled in such a solidification environment.

36 MATERIALS SCIENCE↗