Search NASA⌕ Search

SEARCH · Search NASA

Results for “EUTECTIC ALLOY”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 739 records · Page 41

Power Electronics Materials and Bonded Interfaces - Reliability and Lifetime

High temperature operation of wide bandgap devices continue to be a challenge for the power electronics packages. Thermal performance and reliability are important factors that determine the viability of a bonded interface for operation at high temperatures. In this presentation, we present the technical approach and key results from the research on sintered silver, transient liquid phase alloy, and polymeric materials. A lifetime prediction model that incorporates the thermomechanical behavior of sintered silver at 200C was developed. The copper-aluminum transient alloy completed 350 thermal cycles from -40C to 200C and little increase in the defect level was observed. In addition to material research, we initiated a time-series analysis on the scanning acoustic microscope images of eutectic solder to explore statistical forecasting methods and machine learning techniques. Initial results that report the accuracy of a few different statistical models are presented.

ADVANCED PROPULSION SYSTEMS↗

Mechanical Properties and Microstructure Investigation of Lead Free Solder

While the electronics industry appears to be focusing on Sn-Ag-Cu as the alloy of choice for lead free electronics assembly, ,the exact composition varies by geographic region, supplier and user. Add to that dissolved copper and silver from the printed circuit board traces and surface finish, and there can be significant variation in the final solder joint composition. A systematic study of the mechanical and microstructural properties of Sn-Ag-Cu alloys with Ag varying from 2wt% to 4wt% and Cu varying from 0.5wt% to lSwt%, was undertaken in this research study. Different sample preparation techniques (water quenched, oil quenched and water quenched followed by reflow) were explored and the resulting microstructure compared to that of a typical reflowed lead free chip scale package (CSP) solder joint. Tensile properties (modulus, 0.2% yield strength and the ultimate tensile strength) and creep behavior of selected alloy compositions (Sn-4Ag-1 X u , Sn-4Ag-OSCu, Sn- 2Ag-1 X u , Sn-2Ag-OSCu, Sn-3.5Ag-O.SCu) were determined for three conditions: as- cast; aged for 100 hours at 125OC; and aged for 250 hours at 125OC. There was no significant difference in Young's Modulus as a function of alloy composition. After an initial decrease in modulus after 100 hours at 125"C, there was an insignificant change with further aging. The distribution of 0.2% strain yield stress and ultimate tensile strength as a function of alloy composition was more significant and decreased with aging time and temperature. The microstructures of these alloys were examined using light and scanning electron microscopy (LM and SEM) respectively and SEM based energy dispersive x-ray spectroscopy (EDS). Fracture surface and cross-section analysis were performed on the specimens after creep testing. The creep testing results and the effect of high temperature aging on mechanical properties is presented for the oil quenched samples. In general the microstructure of oil quenched specimen exhibited a eutectic region of Sn with moderately dispersed Ag3Sn intermetallic, surrounded by a dendritic Sn-rich phase. The SEM images of the fracture surface indicated the presence of a tough shear surface at the initial cavity break area and a break line in the middle of specimen along the failure direction. A hyperbolic-sine creep model was adopted and used to fit the creep experiment data. The effect on the mechanical properties by adding the quaternary element bismuth to the Sn-3.5Ag-0.8Cu alloy was measured and compared with the mechanical properties of the ternary alloys. The results of this research study provide necessary data for the modeling of solder joint reliability for a range of Sn-Ag-Cu compositions and a baseline for evaluating the effects of subsequent quaternary additions.

Wang, Qing↗

Effects of a refractory metal protective barrier on uranium carbonitride ceramic–metallic composites exposed to a high temperature hydrogen environment

Uranium nitride has been under consideration at NASA and the Department of Energy for nuclear thermal propulsion applications intended for deep space exploration vehicles. It is critical to the success of the technology development that the behavior of the fuel system is properly characterized in operational environments. This body of work fabricated ceramic metal composites consisting of uranium ceramic fuel in a molybdenum and molybdenum–tungsten metal matrix, both with and without an exterior molybdenum barrier. Specimens were introduced to a high temperature hydrogen environment and characterized through x-ray diffraction, scanning electron microscopy, and energy dispersive spectroscopy to identify characteristic changes. A portion of the specimens was fabricated with a 1.27 mm thick molybdenum barrier in order to isolate the material from the hydrogen environment. Instability of the uranium nitride occurred as low as 2073 K, leading to aggressive instability approaching 2658 K. Carbon reactions with the metal matrix were observed as well as alloying between the uranium and metal matrix constituents. The liquid uranium resulting from the instability of the uranium nitride was observed to attack the grain boundaries of the refractory metal, resulting in the formation of a liquid uranium molybdenum eutectic melt. Specimens encased in a barrier experienced similar results. The authors conclude this is a significant challenge to applications of this cermet at these temperatures. Alternate configurations with resilient hermetic seals or lower temperature applications such as power reactors may have more success.

36 MATERIALS SCIENCE↗

Intermediate Temperature Fluids Life Tests - Experiments

There are a number of different applications that could use heat pipes or loop heat pipes (LHPs) in the intermediate temperature range of 450 to 725 K (170 to 450 C), including space nuclear power system radiators, fuel cells, and high temperature electronics cooling. Historically, water has been used in heat pipes at temperatures up to about 425 K (150 C). Recent life tests, updated below, demonstrate that titanium/water and Monel/water heat pipes can be used at temperatures up to 550 K (277 C), due to water's favorable transport properties. At temperatures above roughly 570 K (300 C), water is no longer a suitable fluid, due to high vapor pressure and low surface tension as the critical point is approached. At higher temperatures, another working fluid/envelope combination is required, either an organic or halide working fluid. An electromotive force method was used to predict the compatibility of halide working fluids with envelope materials. This procedure was used to reject aluminum and aluminum alloys as envelope materials, due to their high decomposition potential. Titanium and three corrosion resistant superalloys were chosen as envelope materials. Life tests were conducted with these envelopes and six different working fluids: AlBr3, GaCl3, SnCl4, TiCl4, TiBr4, and eutectic diphenyl/diphenyl oxide (Therminol VP-1/Dowtherm A). All of the life tests except for the GaCl3 are ongoing; the GaCl3 was incompatible. As the temperature approaches 725 K (450 C), cesium is a potential heat pipe working fluid. Life tests results are also presented for cesium/Monel 400 and cesium/70-30 copper/nickel heat pipes operating near 750 K (477 C). These materials are not suitable for long term operation, due to copper transport from the condenser to the evaporator.

Anderson, William G.↗

Control rods for light water reactors

A control rod for a nuclear fuel assembly is described herein that includes a neutron absorbing material having a melting point greater than 1500° C. that does not form a eutectic with a melting point less than 1500° C., and may further include a cladding material having a melting point greater than 1500° C. The cladding material is selected from the group consisting of silicon carbide, zirconium, a zirconium alloy, tungsten, and molybdenum. The absorbing material is selected from the group consisting of Gd2O3, Ir, B4C, Re, and Hf. The metal cladding or the absorbing material may be coated with an anti-oxidation coating of Cr with or without a Nb intermediate layer.

Lahoda, Edward J.↗

Low cycle fatigue behavior of AlSi10Mg(Cu) alloy at high temperature

Highlights: • The cyclic stress response of AlSi10Mg(Cu) alloy in LCF regime is temperature-dependent. • Precipitates transitions were observed after high temperature cycle loading. • Changes in the interaction mechanism between dislocations and nanoparticles lead to different cyclic stress responses. - Abstract: Low cycle fatigue (LCF) behavior of AlSi10Mg(Cu) alloy was investigated at 100 °C and 250 °C over a range of strain amplitude from 0.25% to 0.40%. Cycle stress response, hysteresis loops, fatigue life, as well as post-fatigue microstructure were studied in detail. Except 0.25%, the alloy performed cycle hardening behavior at 100 °C and softening behavior at 250 °C at any given strain amplitude, which corresponded well with the observed phenomena in hysteresis loops. At any given temperature, cyclic stress increases while fatigue life decreases with the increasing strain amplitude. The fatigue life of the studied alloy at 100 °C was higher than that at 250 °C under the same strain amplitude. Fractography indicated that most fatigue crack initiated from casting defects. The fatigue crack propagation was mainly characterized by fatigue striations and tear ridges in any conditions. Section inspection shows that the number of cracked eutectic Si increases with decreasing the temperature or increasing strain amplitude. Post-mortem transmission electron microscopy (TEM) investigations indicated that cyclic hardening behavior at 100 °C was due to the pinning effect of coherent precipitates (β″-Mg{sub 2}Si and GP zones). Most of tiny coherency precipitates and clusters transformed to large semi-coherency Q′ and β′-Mg{sub 2}Si precipitates after cyclic loading at 250 °C, leading to the sharp decrease of pinning number and dislocation density, which is a key reason for the cyclic softening. Another factor is that more dislocations can be activated and dislocation climb is easier at higher temperature.

36 MATERIALS SCIENCE↗

The structural-phase state of iron-carbon coatings formed by the ultradispersed particles

The methods of nuclear gamma-resonance spectroscopy, elemental microanalysis, and X-ray diffraction were used to study nanoscale coatings. The samples were prepared by magnetron sputtering of carbon and iron particles. They alternately were deposited on monocrystalline silicon or polycrystalline corundum substrate moving relative to the plasma flows in the form of sublayers with a thickness of less than 0.6 nm up to the total thickness of 150-500 nm. Solid solutions with the carbon concentrations of up to 7.5, 12.0, 17.6, and 23.9 at% were produced by co-precipitation of ultradispersed particles of iron and carbon. Using method of conversion electron Mössbauer spectroscopy, we detected the anisotropy of orientation of magnetic moments of iron atoms due to texturing of the formed coatings. The deviation of the crystallite orientation from the average value depends on the degree of carbonization. At 550°C, the pearlite eutectic α‐Fe(C)+Fe{sub 3}C is formed from the amorphous structure without formation of intermediate carbides. The relative content of cementite correlates with the amount of carbon in the coating. The formation of the solid solutions-alloys directly during the deposition process confirms the theory of thermal-fluctuation melting of small particles.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The Influence of Galvanizing Parameters on the Structural Development of Zn-Al-Based Coatings

The evolution of some layers’ characteristics, deposited by galvanization, was monitored according to the technological parameters of the process. Two types of alloys from the Zn-Al and Zn-Al-Ti-B systems were used for deposition. The structure of the deposited layers was analyzed by optical and electron microscopy. The chemical composition, phases and compounds in the structures were identified. The mechanical properties of the structural constituents of the layers were determined by nanoindentation. These techniques highlighted the typical non-uniformities in terms of composition and properties in the layers, mainly due to the diffusion and distribution of iron from the steel substrate in the deposited layers. The evaluation of iron diffusion in the deposited layer was done by differential thermal analysis. The values of the critical temperatures (melting temperature, eutectic temperature and solidification temperature) were correlated with the parameters used during deposition. It was observed that the structure of the coatings is layered, with a specific order from the steel substrate to the edge. In these layers, the constituents are mixtures of soft solid solutions of Al in Zn (η and β) and hard intermetallic compounds. Moreover, increasing the immersion time in the galvanizing bath and the bath temperature leads to an increase in iron diffusion in the coating layer, which contributes to lower coating thickness, thus reducing its durability in operation.

36 MATERIALS SCIENCE↗

Space Processing Applications Rocket project, SPAR 2

Experiment objectives, design/operational concepts, and final results are summarized for six materials science experiments conducted during the second space processing applications rocket mission flown by NASA. The individual experiments discussed are: (1) solidification of Pb-Sb eutectic; (2) feasibility of producing closed-cell metal foams; (3) direct observation of dendrite remelting and macrosegregation in castings; (4) agglomeration in immiscible liquids; (5) casting dispersion - strengthened composites at zero gravity; and (6) solidification behavior of Al-In alloys under zero gravity conditions.

Source record↗

High thermoelectric figure of merit and improved mechanical properties in melt quenched PbTe-Ge and PbTe-Ge{sub 1-x}Si{sub x} eutectic and hypereutectic composites.

We report the synthesis, microstructure, and transport properties of composite thermoelectric materials based on the eutectic phase relationship between PbTe and Ge. When quenched, these eutectic mixtures exhibit considerably stronger mechanical strength and reduced brittleness compared to PbTe itself, while at the same time they possess lower lattice thermal conductivity. Thermal conductivity measurements show values lower than expected based on the law of mixtures and multiphase composites. We find that the thermoelectric performance in these composites can be tuned through the use of hypereutectic compositions and alloying of Ge with Si. PbI{sub 2} was used as an n-type dopant, and precise control of the carrier concentration was achieved to optimize the electrical transport and thermoelectric properties. ZT values approaching 1.3 at 778 K have been obtained in samples of PbTe-Ge{sub 0.8}Si{sub 0.2}(5%), which represent an {approx}62% improvement over that of PbTe.

36 MATERIALS SCIENCE↗

Multimodal and multiscale strengthening mechanisms in Al-Ni-Zr-Ti-Mn alloy processed by laser powder bed fusion additive manufacturing

The unique thermokinetics of laser-powder bed fusion additive manufacturing (L-PBFAM) has been exploited for development of a novel high-strength Al-Ni-Ti-Zr-Mn alloy. The addition of 0.5 wt% Mn leads to extraordinary improvement in ultimate tensile strength (502 MPa) and work hardening due to the activation of two Mn-induced strengthening mechanisms. First, by a bimodal particle strengthening effect due to Al 31 Mn 6 Ni 12 nano-quasi-crystal particles rejected in inter-dendritic spaces and fibrous Al 3 Ni eutectic dendritic channels, which predominately contributes to the strength improvement, and second by solid solution strengthening from remaining Mn entrapped in Al. These mechanisms supplement the particle strengthening effect imparted by coherent and incoherent Al 3 (Ti,Zr) co-precipitates present at melt pool boundaries, dislocation strengthening due to solidification induced strain, and Hall-Petch and backstress strengthening effect due to heterogenous grain size distribution occurring at various length scales. In conclusion, the solidification dynamics and hierarchical heat distribution that are associated with L-PBFAM resulted in complex spatial variations in these strengthening phenomena and were investigated via a high-throughput multiscale structure–property correlation that involved thermokinetic simulation, X-ray diffraction, high-resolution nanoindentation mapping, and site-specific transmission electron microscopy of the alloy.

36 MATERIALS SCIENCE↗

Laser Weldability of AlSi{sub 10}Mg Alloy Produced by Selective Laser Melting: Microstructure and Mechanical Behavior

Selective laser melting (SLM) allows 3D complex parts to be produced with integrated functionalities but does not permit to realize large dimension parts, as the building chamber volume of commercial SLM systems is limited. Therefore, the possibility of joining SLM-built parts by welding appears as extremely valuable. In this work, laser weldability of SLMed AlSi{sub 10}Mg parts has been investigated. The cooling rates induced by the welding process are lower than the ones of SLM; therefore, typical eutectic silicon network of SLM-built parts appears broken in both the melted zone and part of the heat-affected zone, as confirmed by calorimetric measurement. This microstructural evolution caused a local decrease of hardness from 132 HV to 73 HV and a reduction of ductility caused by porosity formation in the weld bead. Moreover, the thermal treatment, performed at 320°C, can limit the gap of tensile response among welded bead and base SLM material.

36 MATERIALS SCIENCE↗

Fabrication and Performance of NiCuCoFeMn High Entropy Alloy Nanopastes for Brazing Inconel 718

Overview: High entropy alloys (HEAs) are a class of metallic alloys consisting of 5 plus elemental components and have four core effects - 1. High mixing entropy - 2. Sluggish diffusion kinetics - 3. High lattice distortion - 4. Cocktail effect; Boron-free, silicon-free brazing materials for nickel superalloys to avoid brittle intermetallic and eutectic phase formation; Size-dependent melting point depression can eliminate the need for boron, silicon and other melting point depressants; A Ni-Mn-Fe-Co-Cu HEA with low solidus and liquidus temperatures (1080 °C and 1150 °C) was developed; Low solidus and liquidus temperatures of the HEA combined with the nanoscale melting point depression in this study; Bulk HEA fabricated by induction melting of elemental powders; HEA nanoparticles (NPs) fabricated by ball milling of the HEA micropowder; Inconel 718 was laser brazed in air using the HEA and bulk and NP performances are compared.

Bridges, Denzel↗

Evaluation of Zn-rich coatings for IMC reaction control in aluminum-magnesium dissimilar welds

Highlights: • Thermodynamic and diffusion simulations have estimated the Zn conc. required to change the IMC reaction in Al-Mg dissimilar welding. • The selected coating alloy was effective in changing the Al-Mg reaction path by forming τ-(Al,Zn){sub 49}Mg{sub 32} as a substitute for β-Al{sub 3}Mg{sub 2}. • Refill™ friction stir spot welds produced with the coating alloy exhibited a thinner reaction layer and an increase in lap shear strength. - Abstract: The dissimilar welding of Al to Mg is very challenging owing to the rapid formation of an intermetallic (IMC) reaction layer at the joint interface, typically comprised of the binary phases γ-Al{sub 12}Mg{sub 17} and β-Al{sub 3}Mg{sub 2}. A potential metallurgical solution has been explored that aimed to change the reaction path by using Al-Zn alloy coatings to promote alternative IMCs with a slower growth rate. To determine the optimum composition for the coating, combined CALPHAD thermodynamic calculations and diffusion simulations were used to estimate the minimum Zn concentration (20 at.%) required to suppress the formation of the faster growing Al{sub 3}Mg{sub 2} phase. This prediction was verified by both static diffusion and Refill™ friction stir spot welding (FSSW) experiments. In each case the selected coating alloy was effective in changing the Al-Mg reaction path by forming the τ-(Al,Zn){sub 49}Mg{sub 32} phase as a substitute for β-Al{sub 3}Mg{sub 2}. However, in static heat treatments there was no reduction in the IMC reaction layer thickness due to the new phase having similar growth kinetics to the β-Al{sub 3}Mg{sub 2} phase it replaced. Nevertheless, Refill™ friction stir spot welds prepared with the new AL-Zn coating alloy exhibited a thinner reaction layer and an increase in lap shear strength. This benefit was attributed to the Zn addition reducing the joint interface liquation temperature, which resulted in a lower peak weld temperature and less IMC reaction; although an increase in local eutectic melting limited the improvement observed.

36 MATERIALS SCIENCE↗

Radionuclide tracing based in situ corrosion and mass transport monitoring of 316L stainless steel in a molten salt closed loop

In the study, we report an in situ corrosion and mass transport monitoring method developed using a radionuclide tracing technique for the corrosion study of 316L stainless steel (316L SS) in a NaCl–MgCl 2 eutectic molten salt natural circulation loop. This method involves cyclotron irradiation of a small tube section with 16 MeV protons, later welds at the hot leg of the molten salt flow loop, generating radionuclides 51 Cr, 52 Mn, and 56 Co at the salt–alloy interface. By measuring the activity variations of these radionuclides at different sections along the loop, both the in situ monitoring of the corrosion attack depth of 316L SS and corrosion product transport and its precipitation in flowing NaCl–MgCl 2 molten salt are achieved. While 316L SS is the focus of this study, the technique reported herein can be extended to other structural materials being used in a wide range of industrial applications.

36 MATERIALS SCIENCE↗

Surface grain refinement of casting A380 aluminum alloy by ultrasonic-assisted surface mechanical grinding treatment

A novel surface processing technique, ultrasonic-assisted surface mechnical grinding treatment (U-SMGT), was proposed and applied to modify the surface micriostructure of the casting aluminum alloy (A380). Comprehensive post-process chracterization techniques including 3D profilometry, optical microscope, scanning electric microscopy (SEM), and electron backscatter diffraction (EBSD) were carried out to investigate the surface morphology and microstructure of the processed region (PR). It was found that a surface layer of grain refinement with a thickness of about 50 µm was formed. In the as-received base material (BM), large clusters of dendritic eutectic phase with a size of approximately 20 µm were isolated by α-Al matrix. Nano-indentation tests showed that hardness of the eutectic and α-Al in the as-received BM was 2.15 GPa and 1.2 GPa respectively. After U-SMGT, the large dendritic eutectic phase was broken down into much fine particles with an average size of 0.57 µm. These fine particles were uniformly distributed into the α-Al matrix. Nano-indentation measurement exhibited a hardness of 2.27 GPa within the processed region. The overall high hardness in the processed region is a result of the pinning effect of uniformly distributed fine dendrites and grain refinement of Al-matrix.

36 MATERIALS SCIENCE↗

Microstructural characterization of ferrotitanium and ferroniobium

Ferroniobium and ferrotitanium, which are added during the steel-making process, may contain phases that do not melt or dissolve in molten steel. This can lead to the presence of coarse Ti- and Nb-rich particles in the resultant steel, which may have an adverse effect on the mechanical properties. In the present study, detailed microstructural characterization, using electron microscopy (both SEM and TEM) and X-ray diffraction (XRD), of commercial grades of ferrotitanium and ferroniobium alloys is carried out to identify the various phases. The ferrotitanium alloy was composed of mainly β-Ti solid solution and a Fe–Ti–Al ternary intermetallic. There were minor amounts of α-Ti solid solution, Ti(C{sub x}N{sub 1−x}) and FeTi. For the ferroniobium alloy, two main phases were present, a Nb-rich solid solution and μ-Fe{sub 7}Nb{sub 6}. The Fe{sub 7}Nb{sub 6} intermetallic phase exhibited two different morphologies, a proeutectic form that was slightly Fe-rich and a eutectic form that was slightly Nb-rich. - Highlights: ► Ferrotitanium has five phases — β-Ti and Ti–Fe–Al ternary are the main phases. ► Ferroniobium has two phases — Nb solid solution and μ-Fe{sub 7}Nb{sub 6} phases. ► The μ-Fe{sub 7}Nb{sub 6} phase has two morphologies — one heavily faulted.

36 MATERIALS SCIENCE↗

Composition optimization of chromium carbide based solid lubricant coatings for foil gas bearings at temperatures to 650 C

A test program to determine the optimum composition of chromium carbide based solid lubricant coatings for compliant gas bearings is described. The friction and wear properties of the coatings are evaluated using a foil gas bearing test apparatus. The various coatings were prepared by powder blending, then plasma sprayed onto Inconel 718 test journals and diamond ground to the desired coating thickness and surface finish. The journals were operated against preoxidized nickel-chromium alloy foils. The test bearings were subjected to repeated start/stop cycles under a 14 kPa (2 psi) bearing unit load. The bearings were tested for 9000 start/stop cycles or until the specimen wear reached a predetermined failure level. In general, the addition of silver and eutectic to the chromium carbide base stock significantly reduced foil wear and increased journal coating wear. The optimum coating composition, PS212 (70 wt% metal bonded Cr3C2, 15 wt% Ag, 15% BaF2/CaF2 eutectic), reduced foil wear by a factor of two and displayed coating wear well within acceptable limits. The load capacity of the bearing using the plasma-sprayed coating prior to and after a run-in period was ascertained and compared to polished Inconel 718 specimens.

Dellacorte, Christopher↗