Electrochemical and Thermodynamic Properties of U in LiCl-KCl-UCl{sub 3} salt system

Pyro-processing technology has been considered and examined by several countries as a promising method for the recovery and recycle of uranium and actinide elements from used nuclear fuel. One of the key processes in pyro-processing is an electro-refiner (ER) where the metallic fission products are loaded into an anode basket and dissolved into lithium-potassium chloride (LiCl-KCl) eutectic salt at 773 K. Many researchers have been exploring the fundamental characterizations of U in LiCl-KCl system by using various electrochemical methods, resulting in several reported values of diffusion coefficient, apparent standard potential, and activity coefficient of U in the salt system. In addition, several researchers measured kinetic parameter of U (exchange current density, i{sub 0}) by using Tafel and linear polarization (LP) methods. Despite available data sets on this ternary salt system, there are discrepancies due to different experimental conditions, design, size of the cell, and measurement techniques. In addition, the i{sub 0} for U/U{sup 3+} reaction has only been measured since 2009; therefore, only few data sets are available to date although the i{sub 0} is critical for the development of dynamic ER model. The value of i{sub 0} is a kinetic characteristic in an ideal equilibrium state; therefore, it is very challenging to be measured by experiments. The authors have estimated the values of i{sub 0} via Tafel and linear polarization methods (LP); however, these methods are lack of maintaining electrode surface area during the measurements. In addition, some data are not following the trends from other literature studies due to its difficulties of the measurement. Therefore, further experimental determinations have to be accomplished to understand the i{sub 0} kinetics and the database for the i{sub 0} of U/U{sup 3+} couple in LiCl-KCl eutectic salt needs to be established systematically. In the present study, an experimental setup was designed and used in a consistent manner to build a meaningful database for U in LiCl-KCl system. LiCl-KCl-UCl{sub 3} salt was prepared at different concentrations and temperatures ranging from 0.5 wt% to 4 wt% and 723 K to 798 K, respectively. Then, CV, open circuit potential (OCP), and electrochemical impedance spectroscopy (EIS) were performed to understand the electrochemical, thermodynamic, and kinetic properties of U. Specially, i{sub 0} values have not been measured via EIS method; therefore, this study provides a good chance to confirm the i{sub 0} values with the new technique.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Enhanced Tensile and Tear Toughness Properties of Thin-Wall Vacuum-Assisted High-Pressure Die-Cast Aural-5 Alloy by Friction Stir Processing

Steadily rising demand for glider weight reduction has driven the development of vacuum-assisted high-pressure die-cast (HPDC) Al-alloys for automotive structural components. Aural-5 is a strontium-modified HPDC alloy utilizing manganese (Mn) to reduce die soldering, eliminating detrimental needle-shaped Fe-bearing ß-phase intermetallic and improving ductility. HPDC Aural-5 contains shrinkage porosity, dendrites with Al-Si eutectic colonies, externally solidified crystals (ESCs), shear-band structure, and large second-phase particulates. Porosity, ESCs and large second-phase particles work as crack initiation sites, negatively impacting tensile properties. In this study, friction stir processing (FSP) is employed for microstructural modification of a thin-walled HPDC Aural-5 by eliminating porosity and breaking down dendrites, second-phase particles, eutectic colonies, ESCs and shear-band structures to create wrought microstructure with homogenized particle distribution. Mechanical property characterization indicates ~30% and ~35% enhancement in yield strength and ductility and associated marked effects on ~69% improvement in tear toughness according to the ASTM B871 test.

Friction stir processing, Aural-5, Strength, Tear ↗

Design and Characterization of Hierarchically-Strengthened, Cast Al-Ce-Ni-Mn-Sc-Zr Alloys for High-Temperature Applications

We characterize the microstructure and mechanical properties of cast Al-Ce-Ni-Mn-Sc-Zr alloys designed for structural use above 300 °C. We first report on the effect of Ni on the as-cast phase formation, where all alloys consist of fine Al11Ce3 and Ni-rich eutectic phases, but the identity of the Ni-rich phase varies with Ni content. Furthermore, these alloys contain four coarsening-resistant strengthening phases as determined from SEM and APT investigations: (i) Al11Ce3 and (ii) Ni-rich micron-scale platelets formed during eutectic solidification, (iii) L12-Al3(Sc,Zr) nanoprecipitates formed during secondary aging, and (iv) Mn solute in the α-Al matrix. The Al-Ce-Ni-Mn-Sc-Zr alloy possesses higher microhardness and creep resistance than compositionally simpler alloys containing fewer of the strengthening phases, indicating that these strengthening mechanisms synergize to provide increased ambient- and elevated-temperature strength.

Ekaputra, Clement↗

Synthesis, Spectral Characterization, Thermal and Optical Studies of Novel Complexes: 4-(Dimethylamino)benzylidene-4-acetamideaniline and 4-(Dimethylamino)benzylidene-4-nitroaniline

The phase diagram representing solid–liquid equilibrium of entire range of composition and thermodynamic studies of two binary organic systems of 4-dimethylaminobenzaldehyde (DMAB) with two NLO active compounds, p-aminoacetanilide (PAA) and p-nitroaniline (PNA), have been studied by solid state synthetic route. Both systems are independently forming a new entity called intermolecular complex (IMC) and two eutectics on either side of intermolecular complexes. The various thermodynamic parameters such as heat of mixing, entropy of fusion, roughness parameter, interfacial energy and excess thermodynamic functions of IMCs and eutectics were calculated using the heat of fusion values. The TGA and DTA studies were performed to understand the physico-chemical, thermal behavior and unique identity of newly synthesized organic complexes, 4-(dimethylamino)benzylidene-4-acetamideaniline (DMABPAA) and 4-(dimethylamino)benzylidene-4-nitroaniline (DMABPNA), and their respective enthalpy of fusion values were found to be 30.01 and 37.26 kJ mol{sup − 1}. The higher melting point of both the novel complexes than their parent’s compounds reveal the strong molecular interaction between parent components to yield the complex. The FTIR spectral analysis predicts the disappearance of aldehyde peaks of DMAB and NH{sub 2} peaks of PAA and PNA while the appearance of entirely new peaks than that of parent’s compounds are the supportive for the formation of new molecular entities. These findings are further supported by FTNMR spectrum studies by observation of disappearance of proton peak of aldehyde of DMAB and amine peaks of PAA and PNA rather formation of new imine proton peak or peaks were observed. The appearance of new peaks in Powder XRD of complexes than those of parent components is further indicative for the formation of complexes. The absorption spectrum of DMABPAA and DMABPNA showed intra-molecular charge-transfer (ICT) excited state absorption at 258 and 241 nm, respectively. Both the IMCs, DMABPAA and DMABPNA, show strong fluorescence with quantum yield 0.66 and 0.93, respectively, in methanol solution.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Dechlorination of molten chloride waste salt from electrorefining via ion-exchange using pelletized ultra-stable H-Y zeolite in a fluidized particle reactor

Dechlorination of eutectic LiCl–KCl based electrorefner (ER) salt is reported via ion-exchange reaction with protonated ultrastable Y-type (USHY) zeolite bound into mechanically fuidized 45–250 μm diameter particles. Evidence of exchange of cations from the salt (Li + , K + , and fission product cations) into the zeolite lattice replacing H + ions was found based on a change in unit cell size, ICP-MS, XRD and TEM–EDS in addition to detection of HCl of gas. Ion exchange reaction was carried out at 625 and 650 °C, temperatures above the melting point of eutectic LiCl–KCl. Experiments were carried out to optimize zeolite drying temperature, estimate maximum ion-exchange capacity, and determine the thermal stability of USHY zeolite. The results indicate over 90% dechlorination can be achieved without zeolite structure collapse at 625 °C. Finally, this provides a promising route to stabilizing waste from radioactive chloride salts into dechlorinated waste forms for permanent geologic disposal.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Effects of Silicon and Niobium Concentration on the Solidification Behavior and Microstructure of Cast Monel Alloys

Cast Monel alloys are used in applications requiring a combination of good mechanical properties and excellent resistance to corrosion. Despite prevalent industrial use, relatively few studies have been conducted to investigate the relationships between composition, solidification behavior, and microstructure. Given that these alloys are used in the cast and welded conditions, these factors have a significant influence over the material properties. Here, in this work, microstructural characterization, electron probe microanalysis, X-ray diffraction, and differential scanning calorimetry were used to study how changes in Si and Nb concentrations affected the solidification path and microstructure of Monel alloys. It was found that increasing Nb concentration stabilized higher amounts of MC carbides and suppressed graphite formation during solidification. It was also found that the high nominal concentration and segregation of Si to the liquid led to the formation of Ni 31 Si 12 and other silicides via terminal eutectic reactions at the end of solidification. A pseudo-binary solidification diagram was constructed using experimental data and was applied to predict the mass fraction of solidified eutectic as a function of composition. The modeled microstructures were found to be in good agreement with experimentally measured phase fractions.

36 MATERIALS SCIENCE↗

In-Situ Synchrotron X-Ray Diffraction of Ultrasonic Microstructural Refinement During Solidification in a Commercial Al–Si–Mg Alloy

This study reports the first use of in-situ synchrotron X-ray diffraction (SXRD) to study the effects of ultrasonic melt processing (USMP) on phase and grain size evolution during solidification in a commercial Al–Si–Mg casting alloy. USMP is a technique that, when applied to aluminum as it solidifies, can be used to refine the local microstructure of large-scale castings. Analysis of the in-situ SXRD data to estimate the average grain size of primary α-Al grains during USMP demonstrates that USMP slows the growth rate of α-Al grains and reduces grain size by 36 pct. Furthermore, there is also evidence that USMP causes the primary α-Al grains to move relative to the X-ray beam; such motion increases the probability of primary α-Al grains colliding and fragmenting. This movement becomes constrained at the onset of the Al–Si binary eutectic, suggesting that USMP ceases to effectively refine the microstructure once the Al–Si binary eutectic begins to form. Complementary laboratory-scale X-ray diffraction (XRD) data were used to correlate the lattice parameters of the α-Al and Si (D-A4) phases with temperature to estimate cooling rate during solidification. Thus, this study can guide the design of novel castings with spatially distributed fine-grained regions produced using local ultrasonic processing.

Aluminum Alloys↗

Sensitivity of Liquation Cracking to Deposition Parameters and Residual Stresses in Laser Deposited IN718 Alloy

The laser deposited IN718 alloys were fabricated with laser cladding system under different conditions to estimate the sensitivity of weld metal liquation cracking. The microstructure and the crack characterization of the laser deposited IN718 alloy were investigated, and the effect of metallurgical factors and residual stress on the crack sensitivity was analyzed. The results showed that the continuous dendritic Laves was precipitated and formed a Lave–austenite interface with ambiguous nanohardness distribution. The weld metal liquation cracking was propagated along the laser scanning direction and the buildup direction in the laser deposited IN718 alloy simultaneously, and the Nb-/Mo-riched fine granular clusters were formed in the crack surface. The precipitation amount of the coarse eutectic phases, presented as dendrite or network, was increased in the laser deposited alloy fabricated with IN718/C-Fe-Cr composite powder and slow cooling rate. The total crack length and the maximum crack length were decreased by increasing cooling rate, and the transverse residual stress was increased with increasing buildup layer number. The crack sensitivity of the laser deposited IN718 alloy was increased by the crack initiation provided by the metallurgical defects and the eutectic phases with low melting temperatures, and then, crack propagated along the continuous phase under the transverse residual stress.

36 MATERIALS SCIENCE↗

Laser Welding-Brazing of Immiscible AZ31B Mg and Ti-6Al-4V Alloys Using an Electrodeposited Cu Interlayer

Metallurgical bonding between immiscible system AZ31B magnesium (Mg) and Ti-6Al-4V titanium (Ti) was achieved by adding Cu interlayer using laser welding-brazing process. Effect of the laser power on microstructure evolution and mechanical properties of Mg/Cu-coated Ti joints was studied. Visually acceptable joints were obtained at the range of 1300 to 1500 W. The brazed interface was divided into three parts due to temperature gradient: direct irradiation zone, intermediate zone and seam head zone. Ti{sub 3}Al phase was produced along the interface at the direct irradiation zone. Ti-Al reaction layer grew slightly with the increase in laser power. A small amount of Ti{sub 2}(Cu,Al) interfacial compounds formed at the intermediate zone and the (α-Mg + Mg{sub 2}Cu) eutectic structure dispersed in the fusion zone instead of gathering when increasing the laser power at this zone. At the seam head zone, Mg-Cu eutectic structure was produced in large quantities under all cases. Joint strength first increased and then decreased with the variation of the laser power. The maximum fracture load of Mg/Cu-coated Ti joint reached 2314 N at the laser power of 1300 W, representing 85.7% joint efficiency when compared with Mg base metal. All specimens fractured at the interface. The feature of fracture surface at the laser power of 1100 W was characterized by overall smooth surface. Obvious tear ridge and Ti{sub 3}Al particles were observed at the fracture surface with increase in laser power. It suggested atomic diffusion was accelerated with more heat input giving rise to the enhanced interfacial reaction and metallurgical bonding in direct irradiation zone, which determined the mechanical properties of the joint.

36 MATERIALS SCIENCE↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

The Effects of Heat Treatment on Microstructure and Mechanical Properties of Tribaloy 400 Coatings Deposited by Laser Cladding

The effects of heat treatment on the microstructure, microhardness, nanohardness and wear resistance of Tribaloy 400 coatings prepared by laser cladding on 304 stainless steel were studied in this paper. The results show that the microstructures of Tribaloy 400 laser cladding layer are cobalt matrix dendrites and eutectic structure. After the heat treatment at 1250 °C for 1 h, the eutectic structure disappears and the strip-like Laves phase is formed on the Co matrix. Meanwhile, the hardness is obviously improved. After the heat treatment at 1250 °C for 1 h and then 900 °C for 4 h, a small amount of ε-Co appears, the strip-like Laves phases become coarser and blunter, and some of the strip structures combine together to form blocky structures, and the hardness is decreased. The wear resistance of the samples at 600 °C is better than that at RT since the hardness of the Laves phase increases with the rise in temperature.

36 MATERIALS SCIENCE↗

The Effect of Boron Content on Wetting Kinetics in Si-B Alloy/h-BN System

In this work, the effect of boron content on the high-temperature wetting behavior in the Si-B alloy/h-BN systems was experimentally examined. For this reason, hypoeutectic, eutectic and hypereutectic Si-B alloys (Si-1B, Si-3.2B and Si-5.7B wt.%, respectively) were produced by electric arc melting method and then subjected to sessile drop/contact heating experiments with polycrystalline h-BN substrates, at temperatures up to 1750 °C. Similar to pure Si/h-BN system, wetting kinetics curves calculated on a basis of in situ recorded drop/substrate images point toward non-wetting behavior of all selected Si-B alloy/h-BN couples. The highest contact angle values of ~ 150° were obtained for hypoeutectic and eutectic Si-B alloys in the whole examined temperature range.

36 MATERIALS SCIENCE↗

Microstructural and Mechanical Characterization of Directionally Solidified Conventional and Nb-Modified Mar-M247 Superalloy

This study analyzes the effects of replacing Ta by Nb (at.% basis) in the phase transformation temperatures, Scheil solidification behavior, and microstructural mechanical features of a Nb-modified as well as conventional Mar-M247 superalloys. Both alloys were directionally solidified at a withdrawal rate of 18 cm/h under a thermal gradient of about 80 °C/cm. DSC results were compared to thermodynamic simulations of phase transformation temperatures and showed a good correlation. The replacement of Ta by Nb has not altered the solidification path of Mar-M247, keeping the sequence L → L + γ → L + γ + MC → L + γ + MC + γ/γ′ eutectic. Due to the segregation of Hf and Zr to the very last liquid to solidify, a low melting point γ/Ni{sub 5}(Hf,Zr) constituent was observed. The as-solidified microstructures of both Mar-M247(Nb) and Mar-M247 were constituted of columnar dendrites of gamma matrix (γ) phase with cuboidal gamma-prime (γ′) precipitates. In addition, γ/γ′-eutectic was observed in the interdendritic region along with MC carbides in blocky, script (blocky dendritic), needle-like and fine nodular morphologies. Both alloys contained about 1.5 vol.% of MC carbides. The MC carbides in Mar-M247(Nb) and Mar-M247 are, respectively, Nb-rich and Ta-rich, with only a limited amount of Hf being detected in the MC phase. The yield stress of Nb-modified Mar-M247 showed higher values up to 750 °C. For higher temperatures, above 800 °C, a conventional Mar-M247 presented a higher value of yield stress.

36 MATERIALS SCIENCE↗

Notch Tensile Behavior of the Mg-Zn-Gd-Zr Alloy

The Mg-Zn-Gd-Zr alloy is one of the important aerospace alloys in the aircraft gearbox applications. The complex geometry of the gearbox introduces several stress concentration points with various intensities. These regions are susceptible to catastrophic failure under mixed loading condition. Therefore, it is important to understand the deformation and failure mode of this alloy for various plastic constraint conditions. In the present work, Mg-4%Zn-1.5%Gd-0.5%Zr alloys were prepared with four different increasing notch root radii (1, 2, 4 and 8 mm). These samples were tested for tensile properties and compared with the smooth condition. In addition, notch sensitivity was determined analytically. The microstructure and fracture samples of the alloy were characterized with the aid of an optical/scanning electron microscope. Tensile test results show that the alloy is notch sensitive and shows notch-strengthening effects. The notch strength ratio increases with the decrease in the notch root radius due to the strong plastic constraint. The predicted and experimental results of the fracture strain with the notch root radius are in qualitative agreement. The void growth rate prediction is qualitatively in agreement with the tensile and fractography results and suggests that the notch geometry has a significant influence on the plastic strain of the alloy. The microstructure of the alloy has equiaxed grains of 74 ± 24 µm with the grain boundary eutectic. The eutectic is composed of Gd-rich Mg phase. The fracture surface has a distinct change from mixed mode to complete cleavage with the increasing notch root radius. The fractography results show that the fracture mode is predominantly intergranular for all the cases.

36 MATERIALS SCIENCE↗

Additive Manufacturing of Pure Mo and Mo + TiC MMC Alloy by Electron Beam Powder Bed Fusion

A metal matrix composite powder of molybdenum (Mo) + TiC was produced by mechanical alloying (MA) and used in additive manufacturing by electron beam powder bed fusion along with pure Mo powder to form sandwich structures. The Mo + TiC solid layers formed mixed structures of Mo with discrete TiC particles, eutectic Mo + TiC, and Mo dendrites. Thermodynamic modeling showed that the system contained an invariant eutectic reaction in the composition range used and indicated that the system was highly sensitive to changes in composition and temperature.

36 MATERIALS SCIENCE↗

Multi-scale characterization of supersolidus liquid phase sintered H13 tool steel manufactured via binder jet additive manufacturing

Additive manufacturing (AM) of H13 tool steel by binder jet 3D printing (BJ3DP) followed by pressureless supersolidus liquid phase sintering (SLPS) provides a low-cost alternative manufacturing method for components with intricate geometric features. However, the microstructure-mechanical property relationships for BJ3DP-SLPS produced H13 tool steel are not well understood, which makes it challenging to develop printing and post-processing methods that maximize part performance. In this work, we leverage atom probe tomography and transmission electron microscopy along with thermodynamic calculations to rationalize the microstructure-mechanical property relationships in as-sintered BJ3DP H13 tool steel. Here, we report for the first time, the presence of a continuous eutectic film-like carbide in H13 along with the more commonly observed cuboidal MX carbides in the prior liquid channels of the microstructure. Further, atom probe tomography revealed the interconnected nature of the MX carbides that appear to be discrete in two-dimensional micrographs. These continuous eutectic carbides and interconnected MX carbides result in brittle failure of the material. Characterization of these microstructural features will be critical in developing appropriate post-processing heat treatments for the improved mechanical performance of BJ3DP H13.

36 MATERIALS SCIENCE↗

High performance Nb/TiNi nanocomposites produced by packaged accumulative roll bonding

Taking full advantage of intrinsic high strength of nano-reinforcements has been proven difficult in a composite until the concept of strain matching was experimental verified in a nanowire Nb/TiNi in-situ composite, which was obtained via solidifying eutectic Nb/TiNi and subsequent severe wire drawing. However, the volume fraction of the nano-reinforcement was dictated by eutectic reaction, which severely limited the development of high-performance composites. Here, the martensitic transformation nanocomposites were successfully acquired with increased volume fraction and changeable morphology of the nano-reinforcement through hot packaged ARB (PARB) and subsequent wire drawing. The nano-reinforcement with lamellar configuration in the composite could exhibit a large lattice strain of similar to 3.8%, which demonstrated the applicability and effectiveness of the strain matching principle in nano-lamellar composite. The obtained composites show a yield strength over 2.0 GPa and a quasi-linear elastic strain as larger as similar to 6.5% with adjustable apparent elastic modulus from 30 to 50 GPa.

42 ENGINEERING↗

Superconducting properties of commercially available solders for low-field applications

Solders with superconducting transitions around 4K are useful in low magnetic field environments for AC current leads or in electrical and mechanical bonds. Accurate knowledge of these solders’ superconducting properties is essential for improving high precision experiments. We have measured the electrical resistance of five commercially-available eutectic or near-eutectic solders: 50%Sn-50%Pb, 60%Sn-40%Pb, 60%Sn-40%Pb-0.3%Sb, 52%In-48%Sn, and 96.5%Sn-3.5%Ag, down to 2.3K and in applied magnetic fields from 0 to 0.1 T . We report critical temperatures T c (B), 90%–10% transition widths ΔT c , and zero-temperature critical fields B c,0 . Our best candidate for low-loss AC current wiring in low fields is 50%Sn-50%Pb, which has a zero-field T c,0 = 7.1K (with ΔT c = 0.6 K), and remained high at T c (0.1 T) = 6.9K (ΔT c = 0.6K ). We also report, for the first time, T c and B c of 60%Sn-40%Pb-0.3%Sb and B c,0 of 96.5%Sn-3.5%Ag. Our T c,0 - 3.31K (ΔT c = 0.08K) for 96.5%Sn-3.5%Ag disagrees with a widely adopted value.

Hickman, C. [North Carolina State University, Rale↗