The electrochemical properties of alloy 690 in simulated pressurized water reactor primary water: Effect of temperature
Not provided.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not provided.
Not provided.
Not provided.
Not provided.
Not provided.
Not provided.
The passive film on low-temperature-carburized AISI-316L austenitic stainless steel was studied in an oxygenated, simulated boiling-water-reactor environment with normal water chemistry. The microstructure was studied using scanning electron microscopy, grazing-incidence X-ray diffractometry, Auger electron spectroscopy, X-ray energy-dispersive spectroscopy, and transmission electron microscopy. For non-surface engineered AISI-316L, three distinct layers were observed after exposure: an outer layer of larger nickel-oxide enriched particles with the spinel structure, an intermediate layer of small Cr-oxide-enriched hematite particles, and a compact inner layer of Cr-enriched oxide also having the spinel structure. Exposure of low-temperature-carburized AISI-316L, in contrast, resulted in only two distinct layers. These layers did not include a compact Cr-rich inner layer. Instead, the innermost layer consisted of an oxide with the spinel structure that was a mixture of Fe, Cr and Ni oxide. The outer layer on the low-temperature-carburized specimen consisted of large loosely stacked particles with the spinel structure of mixed composition. In addition to passive-film characterization, the corrosion rate was studied by monitoring mass loss. Finally, after 500 h of immersion, the mass changes measured were relatively low for all specimens indicating good adhesion and low oxidation rates.
Irradiation growth of single-crystal Zr is modeled with a reduced set of cluster dynamics equations. Nucleation and growth of basal and prismatic dislocation loops are both accounted for in the model. Equations are developed for the time evolution of single point defects, a limited number of point defect clusters, interstitial and vacancy loop nucleation rates, as well as for the growth of vacancy loops on basal planes and interstitial loops on prismatic planes. Reduction of the usual infinite hierarchy of cluster dynamics equations to the simple set studied here is justified on the physical basis of the stability of small loops once nucleated. This simplified cluster dynamics model with a small number of adjustable parameters avoids the complexity of explicit representation of higher order point defect clusters. The model shows consistency with experimental observations of the following aspects: (1) the growth rates of Zr crystals along the a- and c-axes; (2) the onset dose for breakaway irradiation growth; (3) the saturation dislocation loop densities of vacancy and interstitial loops; (4) the effects of cold work and temperature on irradiation growth.
Tungsten-based materials are among the main candidate plasma-facing materials for future fusion reactors where extreme conditions of thermomechanical stresses, radiation, and energetic particles must be withstood. Here a hybrid X-pinch platform combined with a pulsed power machine was used to study damage mechanisms in 90W–4Cu–6Ni tungsten heavy alloy as a result of exposure to high energy density plasma, X-ray radiation, and the resulting thermal shock. It was found that the plasma-facing surface of the material undergoes severe melting and ablation with the extent of ablation being higher in the Cu–Ni phase than the W particles. Rapid melting and solidification transform the W particles into fine dendrite morphologies embedded in the Cu–Ni solid solution. Cracking was also observed in the subsurface layers at the interfaces between the W particles and the Cu-rich phase of the Cu–Ni matrix. X-ray radiation, on the other hand, cause slight melting on the surface without significant ablation and no cracking.
In this work, we use atomistic simulations to investigate the interaction of vacancies and interstitials with interfaces between a crystalline metal and an amorphous, covalently-bonded solid. We select the gold (Au)/silicon (Si) binary system as a model material and construct interface models along two different facets of crystalline Au and with amorphous Si (a-Si) created at three different quench rates. We compute formation energies of vacancies, self-interstitials, and interstitial impurities as a function of position relative to the interface and find that they have markedly lower values near the interface than in the interior of the adjoining phases. We conclude that crystal/amorphous, metal/covalent interfaces may be as effective at removing radiation-induced point defects as interfaces in polycrystalline metals composites. Moreover, irrespective of interface character, the average formation energies of all point defects at all the Au/a-Si interfaces we investigated are comparable. Thus, unlike in polycrystalline metals, where an interface’s crystallographic character has a marked effect on its interactions with point defects, all interface types in crystal/amorphous, metal/covalent composites may be equally effective at absorbing all radiation-induced defects.
Ferritic/Martensitic (F/M) steel T91 was irradiated in-situ to 4 and 10 dpa at 470 °C using 1 MeV Kr 2+ . Additionally, the microstructure evolution under irradiation was followed and characterized by in-situ Transmission Electron Microscopy (TEM), in terms of dislocation loop Burgers vector, average size and density as a function of dose. Furthermore, the influence of the presence of dislocations in the pre-irradiated matrix was investigated by comparing the radiation induced defect evolution in grains with and without initial dislocations.
In this paper, accident-tolerant fuel (ATF) cladding materials aim to improve fuel reliability and safety during accident scenarios in water-cooled reactors. These ATF cladding should also perform comparable or better than the current zirconium alloy cladding under reactor normal operating conditions. Surface-modified Zircaloy-4 was produced by depositing a protective coating of chromium by two different coating techniques, Physical Vapor Deposition (PVD) and Cold Spray (CS). The coating thickness, structure, composition, and mechanical properties of the coated Zircaloy were assessed with advanced materials characterization techniques. Results showed a strengthening effect of the Cr-coating, along with ~83% higher hardness compared to that of the Zircaloy-4 substrate. Surface topography and surface chemistry of the Cr-coated Zircaloy-4 were assessed with contact profilometry, atomic force microscopy, contact angle goniometry, and X-ray photoelectron spectroscopy. Deposited Cr-coating significantly improved surface wettability compared to the substrate Zircaloy-4. The formation of surface oxides on the coatings by prolonged exposure to ambient air showed a further increase in the hydrophobic behavior. Surface parameters and surface chemistry after flow boiling critical heat flux tests, conducted at atmospheric pressure, evidenced a slight increase in surface roughness with notable changes in wettability associated with the formation of surface oxides.
Atom probe tomography has characterised the microstructural changes in T91 steel after BOR60 reactor irradiation at five temperatures between 376 °C and 524 °C to doses between 14.6 dpa and 35.1 dpa. Irradiation-induced precipitation and segregation to carbide/matrix interface induced by neutron irradiation has been characterised. Atom probe tomography characterisation shows that Mn, Ni, Si -rich (MNS-rich) clusters form in T91 steel irradiated in BOR60 reactor at temperatures between 376 °C and 415 °C, which is not observed at higher temperatures 460 °C and 524 °C. Additionally, the number density, volume fraction and composition of MNS-rich clusters have been characterised. Ni, Mn, Si and P is found to segregate at carbide matrix interface after irradiation at lower temperature and only P segregation is observed at 524 °C.
For improved understanding of the behavior of Li plasma facing components (PFCs) in the presence of oxygen impurities, we report on the thermal stability of ultrathin (up to 1.0 nm) LiO x films on a titanium-zirconium-molybdenum (TZM) alloy substrate over the temperature range of 310–1400 K. LiO x films were prepared by either post-oxidation of Li films or Li films deposited on an oxygen-precovered TZM surface. Thermal stability of these films was studied using a combination of temperature programmed desorption (TPD), X-ray photoelectron spectroscopy (XPS), and low-energy ion scattering (LEIS). For post-oxidized Li films, TPD showed that no Li desorption occurred until temperatures above 620 K, and then Li desorbed from the surface via at least three desorption peaks. The O 1s XPS spectra on the post-oxidized films at 310 K indicate the formation of lithium oxide (Li2O) and peroxide/hydroxide (Li 2 O 2 /LiOH). The peroxide/hydroxide converts to oxide after heating to 680 K with no desorption of Li or O 2 , and then this film decomposes to liberate Li into the gas phase while leaving oxygen at the TZM surface. Heating the LiO x films to 1070 K led to a solid-state reaction with surface Mo atoms of the substrate to form a condensed binary lithium molybdenum oxide (LixMoOy) phase, which upon further heating decomposed to liberate gas phase binary lithium molybdenum oxide species. Li deposition on an oxygen-precovered TZM surface formed a complex, highly stable, oxygen rich, Li-O-Mo interfacial oxide. Li desorption from multilayer Li films on oxygen-precovered TZM surfaces occurred in a metallic Li multilayer peak and three other oxide-derived peaks. These results support the improved thermal stability of oxidized lithium as compared to metallic Li and have implications for Mo impurity transport into the plasma at high temperatures.
Not provided.
Not provided.
Not Available