Search NASA⌕ Search

SEARCH · Search NASA

Results for “Layered cathode”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

Impact of surface coating on electrochemical and thermal behaviors of a Li-rich Li 1.2 Ni 0.16 Mn 0.56 Co 0.08 O 2 cathode

Lithium-rich layered oxide materials are considered as potential cathode materials for future high-performance lithium-ion batteries (LIBs) owing to their high operating voltage and relatively high specific capacity. However, perceptible issues such as poor rate performance, poor capacity retention, and voltage degradation during cycling need to be improved before the successful commercialization of the material. In this report, zirconia coated Li 1.2 Ni 0.16 Mn 0.56 Co 0.08 O 2 2 = 1.0, 1.5 and 2.0 wt%) materials are synthesized using a sol–gel assisted ball milling approach. A comparison of structural, morphological and electrochemical properties is examined to elucidate the promising role of ZrO 2 coating on the performance of the NMC cathode. A uniform and homogeneous ZrO 2 coating is observed on the surface of NMC particles as evident by TEM elemental mapping images. The ZrO 2 coated NMCs exhibit significantly improved electrochemical performance at a higher C-rate as compared to pristine material. 1.5% ZrO 2 coated NMC demonstrates better cycling stability (95% capacity retention) than pristine NMC (77% capacity retention) after 50 cycles. All ZrO 2 coated NMC materials demonstrated improved thermal stability compared to pristine material. The difference in onset temperature of 2 wt% ZrO 2 coated and pristine NMC is 20 °C. The improved electrochemical performance of ZrO 2 coated NMC can be attributed to the stabilization of its surface structure due to the presence of ZrO 2 .

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A green closed-loop process for selective recycling of lithium from spent lithium-ion batteries

As the economy started to recover from the COVID pandemic, the price of Li 2 CO 3 skyrocketed to its highest. This situation has aggravated concerns about the supply chain for lithium-ion batteries (LIBs). Recycling spent LIBs is a potential solution to alleviate the bottleneck of the supply chain and prevent environmental pollution, and has attracted lots of attention. However, lithium recycling is generally disregarded because of the complex recycling process and its low recycling efficiency. Here, in this work we developed a sustainable lithium recovery process, which can selectively leach and recover lithium with formic acid before recycling valuable metals. With the reported method, lithium can be 99.8% recovered from layered oxide cathode materials with 99.994% purity. In addition, this lithium recovery process is affordable, compared to the typical hydrometallurgical process, by saving 11.15% per kilogram of spent LIBs. Therefore, this research provided a new solution to eliminating the effects of lithium ions on valuable metal separation and the co-precipitation reaction and precluding the influence of other metal ions on lithium recovery. Finally, this simplified lithium recovery process provides new opportunities for sustainable recycling of LIBs and economical restoration of the lithium supply chain.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Ultra-high efficient lithium recovery via terephthalic acid from spent lithium-ion batteries

The recovery of lithium from spent lithium-ion batteries (LIBs) is a critical step in advancing sustainability within the battery industry. Traditional lithium extraction methods from end-of-life LIBs predominantly rely on chemical leaching techniques. However, these methods often involve the excessive use of acids, leading to substantial environmental concerns. Additionally, their non-selective nature can compromise the purity of the recovered lithium salt. To achieve battery-grade purity, further purification and recovery processes are necessary. In this study, we introduce a universal and eco-friendly process for lithium recovery, employing terephthalic acid to selectively extract lithium prior to the recycling of other valuable metals. This innovative method achieves lithium recovery rates exceeding 98.53% from layered oxide cathodes and 98.53% from lithium iron phosphate cathodes, delivering an exceptional purity level of 99.95%. By demonstrating applicability across a variety of cathode materials, this approach establishes a universal, sustainable and efficient solution for LIB recycling. The high-purity lithium extraction enabled by this process supports the comprehensive utilization of valuable resources, contributing significantly to the development of a circular economy for battery materials.

Hou, Jiahui [Worcester Polytechnic Institute, MA (↗

Toward garnet electrolyte–based Li metal batteries: An ultrathin, highly effective, artificial solid-state electrolyte/metallic Li interface

Solid-state batteries are a promising option toward high energy and power densities due to the use of lithium (Li) metal as an anode. Among all solid electrolyte materials ranging from sulfides to oxides and oxynitrides, cubic garnet–type Li 7 La 3 Zr 2 O 12 (LLZO) ceramic electrolytes are superior candidates because of their high ionic conductivity (10 -3 to 10 -4 S/cm) and good stability against Li metal. However, garnet solid electrolytes generally have poor contact with Li metal, which causes high resistance and uneven current distribution at the interface. To address this challenge, we demonstrate a strategy to engineer the garnet solid electrolyte and the Li metal interface by forming an intermediary Li-metal alloy, which changes the wettability of the garnet surface (lithiophobic to lithiophilic) and reduces the interface resistance by more than an order of magnitude: 950 ohm·cm2 for the pristine garnet/Li and 75 ohm·cm 2 for the surface-engineered garnet/Li. Li 7 La 2.75 Ca 0.25 Zr 1.75 Nb 0.25 O 12 (LLCZN) was selected as the solid-state electrolyte (SSE) in this work because of its low sintering temperature, stabilized cubic garnet phase, and high ionic conductivity. This low area-specific resistance enables a solid-state garnet SSE/Li metal configuration and promotes the development of a hybrid electrolyte system. The hybrid system uses the improved solid-state garnet SSE Li metal anode and a thin liquid electrolyte cathode interfacial layer. This work provides new ways to address the garnet SSE wetting issue against Li and get more stable cell performances based on the hybrid electrolyte system for Li-ion, Li-sulfur, and Li-oxygen batteries toward the next generation of Li metal batteries.

25 ENERGY STORAGE↗

Materials and Design Selection to Improve High Current Density Performance in PEMFC

Performance at high current density is dominated by transport losses from resistance to oxygen and proton transport. The materials selection and their properties can have a significant impact on the transport resistance. Here, in this study, the impact of catalyst carbon support microstructure and its properties impacting performance at high current density is studied in detail. Platinum-cobalt alloy catalysts supported on different carbon supports were analyzed for pore size distribution characteristics. Catalyst layer electrochemical diagnostics such as oxygen limiting current and H 2 /N 2 impedance tests were conducted to measure local oxygen transport resistance and bulk proton transport resistance. For the first time, the local-oxygen transport and the bulk-proton transport resistances in the catalyst layer are directly correlated to the micropore and macropore properties of the carbon support.

08 HYDROGEN↗

Predicted Impacts of Pt and Ionomer Distributions on Low-Pt-Loaded PEMFC Performance

Low-cost, high performance proton exchange membrane fuel cells (PEMFCs) have been difficult to develop due to limited understanding of coupled processes in the cathode catalyst layer (CCL). Low-Pt-loaded PEMFCs suffer losses beyond those predicted solely due to reduced catalyst area. Although consensus links these losses to thin ionomer films in the CCL, a precise mechanistic explanation remains elusive. In this publication, we present a physically based PEMFC model with novel structure-property relationships for thin-film Nafion, validated against PEMFC data with low Pt loading. Results suggest that flooding exacerbates kinetic limitations in low-loaded PEMFCs, shifting the Faradaic current distribution. As current density increases, protons travel further into the CCL, resulting in higher Ohmic overpotentials. We also present a parametric study of CCL design parameters. We find that graded Pt and ionomer loadings reduce Ohmic losses and flooding, but individually do not provide significant improvements. However, a dual-graded CCL (i.e., graded Pt and ionomer) is predicted to significantly improve the maximum power density and limiting current compared to uniformly loaded CCLs. This work highlights the importance of accurate transport parameters for thin-film Nafion and provides a pathway to low-cost PEMFCs via precise control of CCL microstructures.

08 HYDROGEN↗

Meso-Structured Polymer Electrolyte Fuel Cell Electrode

Increasing the utilization of Pt and Pt alloy catalysts in polymer electrolyte fuel cell cathodes is critical to improving the high power density operation, particularly at low Pt loadings. State of the art electrodes are fabricated in an ink deposition process that leads to uncontrolled electrode architecture with random aggregates of functional domains (catalyst, ionomer, and pore volume) (1). The randomness in the domains induces high tortuosity transport pathways for ions and fluids, which cause severe transport resistance during high current density operation. Thin ionomer films cause additional transport resistance and poisoning of the Pt catalyst, which becomes more significant at low Pt loadings. Reducing the amount of ionomer in the catalyst domain without affecting the ionic transport resistance is key to improving the utilization of the Pt and reducing the transport resistance at low Pt loading. Rational design of the electrode structure with controlled low tortuous ionic transport pathways could improve performance. The introduction of the ionomer pathways could also enable reduction of the ionomer volume in the catalyst domain, reducing the transport resistance. Middelmen et al. proposed electrode structures consisting of aligned components in a low tortuosity configuration to improve performance (2). In this work, we present an alternative electrode structure based on a vertically aligned array of Nafion pillars in the cathode catalyst layer, as shown in Figure 1a. Figure 1b shows the SEM image of the Nafion pillars. Furthermore, Pt supported on carbon catalyst was deposited on the Nafion pillars to fabricate a meso-structured electrode. Nafion pillars provide high conductive and low tortuous pathways for protons, reducing the effective transport distance, and enabling reduction of the ionomer binder in the catalyst domain.

25 ENERGY STORAGE↗

Carbon Corrosion in Polymer Electrolyte Fuel Cells: A Complex Interplay between Morphological Changes and Electrochemical Performance

Due to the high gravimetric energy density of hydrogen, the focus of implementation of polymer electrolyte fuel cells (PEFCs) has shifted from light duty passenger vehicles to heavy duty vehicles such as buses, trucks, locomotives and marine vessels. A mechanistic understanding of degradation is therefore necessary to improve durability and efficiency. During start-up and shut-down (SUSD) of PEFC systems, the catalyst (Pt nanoparticles embedded on carbon support) undergoes local potentials ~ 1 - 1.5 V caused by a combination of fuel (H 2 ) starvation, mixed fuel region and cell reversal. This leads to a series of degradation phenomenon including reduction in cathode catalyst layer (cCL) thickness and porosity, loss in electrochemical surface area (ECSA), ionomer degradation and loss in electrical contact, therefore resulting in severe performance loss. The convoluted relationship between these individual degradation mechanisms, their chronology and their effects on electrochemical performance are yet unresolved. Here, the complex interplay between morphological changes due to carbon corrosion and its effects on the electrochemical performance were analyzed using a combination of detailed electrochemical characterization, spectroscopy, and electron microscopy techniques.

25 ENERGY STORAGE↗

XPS Studies of LSCF Interfaces after Cell Testing

The motivation of this investigation is to explore the possibility of using the depth profile capability of XPS to study interfaces after SOFC button cell testing. The literature uses XPS to study various cathode materials but has devoted little to the understanding of various cathode interfaces especially after testing. In this work, an SOFC button cell is first tested, and then, the LSCF cathode, barrier layer, and electrolyte are sputtered away to study the behavior of different interfaces. This work has shown that some elements have moved into other layers of the SOFC cell. It is argued that the migration of the elements is partly due to a redeposition mechanism after atoms are sputtered away, while the rest is due to interdiffusion between the SDC and YSZ layers. However, additional work is needed to better understand the mechanism by which atoms move around at different interfaces. In conclusion, the cell electrochemical performance is also discussed in some details but is not the focus.

42 ENGINEERING↗

Final Project Report: Development of Micro-Structural Mitigation Strategies for PEM Fuel Cells: Morphological Simulations and Experimental Approaches

The durability of PEM fuel cells is a primary requirement for large scale commercialization of these power systems in transportation and stationary market applications that target operational lifetimes of 5,000 hours and 40,000 hours by 2015, respectively. Key degradation modes contributing to fuel cell lifetime limitations have been largely associated with the platinum-based cathode catalyst layer. Furthermore, as fuel cells are driven to low cost materials and lower catalyst loadings in order to meet the cost targets for commercialization, the catalyst durability has become even more important. While over the past few years significant progress has been made in identifying the underlying causes of fuel cell degradation and key parameters that greatly influence the degradation rates, many gaps with respect to knowledge of the driving mechanisms still exist; in particular, the acceleration of the mechanisms due to different structural compositions and under different fuel cell conditions remains an area not well understood. The focus of this project was to address catalyst durability by using a dual path approach that coupled an extensive range of experimental analysis and testing with a multi-scale modeling approach.

08 HYDROGEN↗

Performance enhancement of a polymer-electrolyte membrane H2O and CO2 co-electrolysis system for the production of syngas

Co-electrolysis of water and CO 2 to produce hydrogen and CO would provide an alternative pathway to making chemicals and fuels. The process could provide a way to use excess renewable electricity, or could be coupled to nuclear or carbon-based power generation. Opus 12 has overcome barriers to using a proton exchange membrane (PEM) reactor for this reaction by modifying the cathode catalyst layer to enhance simultaneous electrochemical H 2 production and CO 2 reduction. Current reactor performance metrics in terms of selectivity, current density, and applied voltage meet or exceed internal targets. However, the cell lifetime must be extended for a commercial product to be feasible. Through this H2@Scale project, we propose to work with the Weber Group at LBNL to diagnose performance decay mechanisms that currently limit the lifetime of the electrochemical syngas generator. LBNL is host to a number of advanced PEM diagnostic tools and lab scientists have unique experience in exploring performance and lifetime tradeoffs at the component to cell scales. Using the results of this study, the identified limiting mechanisms will be mitigated through improved cell and catalyst design.

10 SYNTHETIC FUELS↗

Active and Durable PGM-free Cathodic Electrocatalysts for Fuel Cell Application

Platinum Group Metal-free (PGM-free) Oxygen Reduction Reaction (ORR) electrocatalysts possess high intrinsic activity measured by a Rotating Disk Electrode (RDE) method. However, under fuel cell operating conditions, PGM-free ORR electrocatalysts have underperformed compared to platinum catalysts. PGM-free ORR electrocatalyst’s fuel cell performance can be improved by designing and optimizing the cathodic catalyst layer (CL) and Membrane Electrode Assembly (MEA) construction such that: 1) it efficiently provides oxygen access to ORR active sites (through catalyst morphology control); 2) it removes water from the CL (by tuning the hydrophobicity of the PGM-free catalysts and the catalyst layer structure); and 3) it increases proton conductivity (by homogeneous mixing of catalysts and ionomer). Studying the CL is complex due to the absence of well-established protocols of MEA activation, especially compared to platinum-containing catalysts. PGM-free fuel cell testing protocols would need to optimize potentiostatic vs galvanostatic measurements, scan rates, parameters of Electrochemical Impedance Spectroscopy (EIS) and Beginning of Experiment (BOE) criteria. To make the PGM-free catalyst’s fuel cell performance comparable to platinum, the synergistic effort of materials design, fine tuning of the catalyst layer and comprehensive electrochemical analysis is required.

08 HYDROGEN↗

Synthesis, structural and electrochemical properties of V4O9 cathode for lithium batteries

Single-phase three-dimensional vanadium oxide (V 4 O 9 ) was synthesized by reduction of V 2 O 5 using a gas stream of ammonia/argon (NH 3 /Ar). The as-synthesized oxide, prepared by this simple gas reduction method was subsequently electrochemically transformed into a disordered rock salt type-“Li3.7V4O9” phase while cycling over the voltage window 3.5 to 1.8 V versus Li. The Li-deficient phase delivers an initial reversible capacity of ∼260 mAhg −1 at an average voltage of 2.5 V vs. Li + /Li 0 . Further cycling to 50 cycles yields a steady 225 mAhg −1 . Ex situ X-ray diffraction studies confirmed that (de) intercalation phenomena follows a solid-solution electrochemical reaction mechanism. As demonstrated, the reversibility and capacity utilization of this V 4 O 9 is found to be superior to battery grade, micron-sized V 2 O 5 cathodes in lithium cells.

25 ENERGY STORAGE↗

Stabilizing Li-rich NMC Materials by Using Precursor Salts with Acetate and Nitrate Anions for Li-ion Batteries

Lithium-rich layered oxide cathode materials of Li 1.2 Mn 0.5100 Ni 0.2175 Co 0.0725 O 2 have been synthesized using metal salts with acetate and nitrate anions as precursors in glycerol solvent. The effects of the precursor metal salts on particle size, morphology, cationic ordering, and ultimately, the electrode performance of the cathode powders have been studied. It was demonstrated that the use of cornstarch as a gelling agent with nitrate-based metal salts results in a reduction of particle size, leading to higher surface area and initial discharge capacity. However, the cornstarch gelling effect was minimized when acetate salts were used. As observed in the Fourier-transform infrared spectroscopy analysis, cornstarch can react with acetates to form acetyl groups during the synthesis, effectively preventing the cornstarch gel from capping the particles, thus leading to larger particles. A tradeoff was found when nitrate and acetate salts were mixed in the synthesis. It was shown that the new cathode powder has the best cationic ordering and capacity retention, promising a much stable Li-rich cathode material for lithium-ion batteries.

25 ENERGY STORAGE↗

Supersonic CO electric-discharge lasers

Laser modeling activity is described which involved addition of an option allowing N2 as a second diatomic gas. This option is now operational and a few test cases involving N2/CO mixtures were run. Results from these initial test cases are summarized. In the laboratory, a CW double-discharge test facility was constructed and tested. Features include: water-cooled removable electrodes, O-ring construction to facilitate cleaning and design modifications, increased discharge length, and addition of a post-discharge observation section. Preliminary tests with this facility using N2 yielded higher power loadings than obtained in the first-generation facility. Another test-section modification, recently made and as yet untested, will permit injection of secondary gases into the cathode boundary layer. The objective will be to vary and enhance the UV emission spectrum from the auxiliary discharge, thereby influencing the level of photoionization in the main discharge region.

Hason, R. K.↗

Observations of a double-layer in a hot-cathode discharge

The meniscus region of a hot cathode discharge was selected for an analysis of the nonlinear interaction of a convectively amplifying wave with a background plasma. A potential step, resulting from rectification of the wave fields is observed, and it is noted that predicted values for the step are in good agreement with empirical data. Attention is given to the determination of plasma parameters (using a Langmuir probe placed in front of the cathode) in terms of their relation to the pondermotive force.

Levine, J. S.↗