Search NASA⌕ Search

SEARCH · Search NASA

Results for “PERMANENT MAGNETS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

Phase transformation sequence and magnetic properties of melt-spun SmCo-based alloy after isochronal heat treatment

The phase transformation sequence, microstructure and compositions, and magnetic properties for a melt-spun Sm(Co{sub 0.68}Fe{sub 0.2}Cu{sub 0.1}Zr{sub 0.02}){sub 7.5} alloy after isochronal heat treatments have been studied by using x-ray diffraction, transmission electron microscopy, three-dimensional atom probe (3DAP), and magnetometry. The as-spun ribbons had a single phase with the Cu{sub 7}Tb structure. After being aged at 720 deg. C, the single phase decomposed into two major phases: 2:17R and 1:5H, and one minor CoFeZr-rich phase. The formation of the Z-phase happened after the cellular structure, requiring a higher temperature than that for the cellular structure. The 3DAP analysis showed that Zr was depleted from the 2:17R and 1:5H phases by a half while the other elements remained almost unchanged when the aging temperature increased from 720 to 840 deg. C. In contrast to the sintered permanent magnets, Cu was enriched in the 1:5H phase with a much higher concentration (>40 at. %). The Cu enrichment also occurred at the boundary of the Z-phase. The coercivity achieved was H{sub c}=4.34 kOe following aging at 720 deg. C. The highest maximum energy product, (BH){sub max}, was 6.48 MG Oe after aging at 800 deg. C and the remanence to saturation magnetization ratio, M{sub r}/M{sub s}, was 0.69. This relatively low H{sub c} and high M{sub r}/M{sub s} ratio may be a consequence of the formation of a significant volume fraction of the CoFeZr-rich nanocrystalline phase.

36 MATERIALS SCIENCE↗

Tetragonal structure and uniaxial magnetic anisotropy in the arc-melted (Ce,Zr) 2 (Fe,M) 17 (M = Mo, W, Co) alloys

The tetragonal ThMn 12 -type structure is stabilized in (Ce 1-x Zr x ) 2 T 16 M (x = 0.2 – 0.3; T = Fe or Fe/Co, M = Mo or W) arc-melted alloys. Approximately 5 at% of Mo or W admixture is sufficient to transform the hexagonal Th 2 Ni 17 -type structure of (Ce 1-x Zr x ) 2 Fe 17 into the tetragonal ThMn 12 -type structure of nearly single-phase (Ce 1-x Zr x ) 2 Fe 16 M and/or (Ce 1-x Zr x ) 2 Fe 15 CoM bulk alloys. X-ray Rietveld refinements reveal that Zr and Mo (W) substitute different sites in the tetragonal crystal structure. Zirconium preferentially replaces Ce, whereas Mo (W) substitutes Fe. At room temperature, the tetragonal phases exhibit strong ferromagnetism and a uniaxial magneto-crystalline anisotropy with anisotropy fields of 15 – 17 kOe. These materials possess room-temperature saturation magnetizations of 95 – 105 emu/g and Curie temperature of 420 – 505 K. At some concentrations, concurrent Zr and Mo (W) site occupancy facilitates 1:12 structure formation in bulk alloys with minimal presence of non-magnetic element in the Fe sublattice, thus securing the highest known magnetic moment per Fe atom (∼ 1.37 µ B ) in this type of materials. The intrinsic magnetic characteristics, as well as the absence of critical rare earths (RE), make these compounds interesting for development as low-cost permanent magnets. In conclusion, small Co additions improve the Curie temperature, especially if combined with W.

36 MATERIALS SCIENCE↗

Heat treatment effects on dielectric properties of SRFe{sub 12}O{sub 19} hexaferrite prepared by an SHS route

The M-type Strontium Hexaferrite SRFe{sub 12}O{sub 19} particles were prepared by a Self propagating High temperature Synthesis (SHS) route. Precursors were heated under two different conditions: microwave heating for 30 minutes and sintered at 950 deg C for 4 hrs. The dielectric properties: dielectric constant ({epsilon}{sup '}), dielectric loss (tan {delta} ) and ac conductivity ({sigma}{sub ac}) were measured at room temperature in the frequency range from 100 Hz to 2 MHz. The samples present a non-linear behavior for the dielectric constant at 1 kHz, 100 kHz and 2 MHz. The dielectric properties of prepared Strontium Hexaferrite samples were discussed in view of applications as a material for microwave devices, permanent magnets and high density magnetic recording media. (author)

36 MATERIALS SCIENCE↗

Laser plasma in a magnetic field

Laser Ion Source (LIS) is a candidate among various heavy ion sources. A high density plasma produced by Nd:YAG laser with drift velocity realizes high current and high charge state ion beams. In order to obtain higher charged particle ions, we had test experiments of LIS with a magnetic field by which a connement effect can make higher charged beams. We measured total current by Faraday Cup (FC) and analyzed charge distribution by Electrostatic Ion Analyzer (EIA). It is shown that the ion beam charge state is higher by a permanent magnet.

72 PHYSICS OF ELEMENTARY PARTICLES AND FIELDS↗

Selective Extraction and Recovery of Nd and Dy from Nd-Fe-B Magnet Scrap by Utilizing Molten MgCl{sub 2}

Fundamental experiments are conducted with the aim of developing an efficient recycling process for rare earth elements (REEs) from neodymium-iron-boron (Nd-Fe-B) permanent magnet scrap. Molten magnesium dichloride (MgCl{sub 2}) was chosen as an extraction medium, which can selectively chlorinate and extract REEs in magnet alloys. Dysprosium-containing Nd-Fe-B magnet alloy was immersed in molten MgCl{sub 2} at 1273 K (1000 °C) for 3 to 12 hours. The results of the experiments clearly show that the REEs in the magnetic alloy were successfully extracted into the molten salt, while the Fe-B alloy remained in a solid form. The extraction ratios of Nd and Dy were at most 87 and 78 mass pct, respectively. After the extraction experiment, excess MgCl{sub 2} and Mg were removed by vacuum distillation and the rare earth chlorides were recovered. Thus, the feasibility of this method for efficient recovery of rare earths using molten MgCl{sub 2} is demonstrated.

36 MATERIALS SCIENCE↗

Non-contact magnetically coupled rectilinear-rotary oscillations to exploit low-frequency broadband energy harvesting with frequency up-conversion

Ambient vibrations have a rectilinear and broadband nature and are particularly rich in the low-frequency regions. This letter reports an electromagnetic energy harvester to transform low-frequency broadband rectilinear vibrations into electricity with frequency up-conversion. The harvester consists of a rectilinear oscillator and a rotary oscillator coupled through magnetic force induced by four arc permanent magnets centrosymmetrically distributed on each oscillator. The rotary oscillator also includes two repulsive magnets and six stationary coils with steel screws inside to obtain and maintain four equilibrium positions with shallowed potential wells. The magnetic interaction between the rectilinear oscillator and the rotary oscillator is formulated using a magnetic dipole model. The restoring torque induced by the steel screws on the rotor is experimentally measured. Magnetically coupled governing equations are derived and their numerical solutions are used to characterize the dynamic response of the harvester under chirp excitations. Experimental results demonstrate its excellent harvesting capability of scavenging low-frequency wideband vibrational energy under slow-frequency-drifted excitations, simple harmonic excitations, and mixed-frequency excitations. Under harmonic excitations, the rectilinear oscillator vibrates non-harmonically but approximately periodically, while the rotary counterpart oscillates in a more complex pattern varying with the excitation frequency, which leads to the frequency up-conversion (up to 10 times increase) and broadened bandwidth (25% increase from its resonant frequency). Experiments show an output voltage of 5 V (RMS)/40 V (Peak to Peak) and an output power of 55 mW (RMS)/950 mW (Peak) at an optimal load of 465 Ω under harmonic excitation of 4 Hz at 0.7 g.

Deng, Wei (ORCID:0000000194598151)↗

Recycled Sm-Co bonded magnet filaments for 3D printing of magnets

Recycling of rare earth elements, such as Sm and Nd, is one technique towards mitigating long-term supply and cost concerns for materials and devices that depend on these elements. In this work recycled Sm-Co powder recovered from industrial grinding swarfs, or waste material from magnet processing, was investigated for use in preparation of filament for 3D printing of bonded magnets. Recycled Sm-Co powder recovered from swarfs was blended into polylactic acid (PLA). Up to 20 vol.% of the recycled Sm-Co in PLA was extruded at 160°C to produce a filament. It was demonstrated that no degradation of magnetic properties occurred due to the preparation or extrusion of the bonded magnet material. Good uniformity of the magnetic properties is exhibited throughout the filament, with the material first extruded being the exception. The material does exhibit some magnetic anisotropy, allowing for the possibility of the development of anisotropic filaments. Finally, this work provides a path forward for producing recycled magnetic filament for 3D printing of permanent magnets.

36 MATERIALS SCIENCE↗

Magnetic small-angle neutron scattering

Small-angle neutron scattering (SANS) is one of the most important techniques for microstructure determination, being utilized in a wide range of scientific disciplines, such as materials science, physics, chemistry, and biology. The reason for its great significance is that conventional SANS is probably the only method capable of probing structural inhomogeneities in the bulk of materials on a mesoscopic real-space length scale from roughly 1 to 300 nm. Moreover, the exploitation of the spin degree of freedom of the neutron provides SANS with a unique sensitivity to study magnetism and magnetic materials at the nanoscale. As such, magnetic SANS ideally complements more real-space and surface-sensitive magnetic imaging techniques, e.g., Lorentz transmission electron microscopy, electron holography, magnetic force microscopy, Kerr microscopy, or spin-polarized scanning tunneling microscopy. This review summarizes the recent applications of the SANS method to study magnetism and magnetic materials. Here, this includes a wide range of materials classes from nanomagnetic systems such as soft magnetic Fe-based nanocomposites, hard magnetic Nd-Fe-B-based permanent magnets, magnetic steels, ferrofluids, nanoparticles, and magnetic oxides to more fundamental open issues in contemporary condensed matter physics such as skyrmion crystals, noncollinear magnetic structures in noncentrosymmetric compounds, magnetic or electronic phase separation, and vortex lattices in type-II superconductors. Special attention is paid not only to the vast variety of magnetic materials and problems where SANS has provided direct insight, but also to the enormous progress made regarding the micromagnetic simulation of magnetic neutron scattering.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Furnace Blower Electricity: National and Regional Savings Potential

Currently, total electricity consumption of furnaces is unregulated, tested at laboratory conditions using the DOE test procedure, and is reported in the GAMA directory as varying from 76 kWh/year to 1,953 kWh/year. Furnace blowers account for about 80percent of the total furnace electricity consumption and are primarily used to distribute warm air throughout the home during furnace operation as well as distribute cold air during air conditioning operation. Yet the furnace test procedure does not provide a means to calculate the electricity consumption during cooling operation or standby, which account for a large fraction of the total electricity consumption. Furthermore, blower electricity consumption is strongly affected by static pressure. Field data shows that static pressure in the house distribution ducts varies widely and that the static pressure used in the test procedure as well as the calculated fan power is not representative of actual field installations. Therefore, accurate determination of the blower electricity consumption is important to address electricity consumption of furnaces and air conditioners. This paper compares the potential regional and national energy savings of two-stage brushless permanent magnet (BPM) blower motors (the blower design option with the most potential savings that is currently available in the market) to single-stage permanent split capacitor (PSC) blower motors (the most common blower design option). Computer models were used to generate the heating and cooling loads for typical homes in 16 different climates which represent houses throughout the United States. The results show that the potential savings of using BPM motors vary by region and house characteristics, and are very strongly tied to improving house distribution ducts. Savings decrease dramatically with increased duct pressure. Cold climate locations will see savings even in the high static pressure duct situations, while warm climate locations will see less savings overall and negative savings in the high static pressure duct situations. Moderate climate locations will see little or no savings.

32 ENERGY CONSERVATION, CONSUMPTION, AND UTILIZATI↗

Isotropic nanocrystalline Sm(Fe,Co) 11.3 Ti 0.7 magnets modified with B and Zr

Rare-earth-lean Sm(Fe,Co,Ti) 12 alloys with the ThMn 12 crystal structure and less than one Ti atom per formula unit have the potential of exceptionally powerful permanent magnets, but all prior attempts to develop high coercivity in bulk alloys, especially coercivity combined with crystallographic texture, have fallen short of the expectations. This study was aimed at improvement of the currently best Sm(Fe,Co,Ti) 12 magnets prepared through melt-spinning which are inherently isotropic. Modifications of the alloys with B and Zr, already demonstrated in earlier studies to be effective separately, have been implemented simultaneously. Here, a systematic study of Sm 1.1-x (Fe,Co) 11.3-y Ti 0.7 B y alloys melt-spun at a tangential speed of 50 m/s and annealed at 600–950 °C allowed for monitoring the continuous evolution of the two consecutive crystal structures, those of the TbCu 7 and ThMn 12 types. Zirconium was found to facilitate the formation of the 1:12 structure at the expense of the 1:7, whereas boron has the opposite effect, at certain concentrations completely suppressing the 1:12. When the two alloying elements are introduced simultaneously, they inhibit growth of the 1:12 crystallites at annealing temperatures higher than 800 °C, thus allowing for the development of a higher coercivity. Because of instrumental limitations, bulk magnets were prepared through a two-step process – compaction of the melt-spun ribbons at 650 °C and additional treatment at a higher temperature – and they were characterized by a reduced, 90–93%, density. Nevertheless, an isotropic Sm 0.9 Zr 0.2 (Fe,Co) 10.8 Ti 0.7 B 0.5 magnet exhibited fair values of the remanence (7.4 kG), maximum energy product (8.5 MGOe) and coercivity (5.4 kOe), as well as high Curie temperature of 525 °C and remarkably small temperature coefficient of the coercivity, -0.25%/°C.

36 MATERIALS SCIENCE↗

Effect of cobalt substitution on structure and magnetic properties of Nd 0.4 Zr 0.6 Fe 10–x Co x Si 2 (x = 0–3) alloys and their ribbons

This paper reports the stabilization of the RFe 12 -type based compounds where part of R and Fe are substituted with Zr and Co and Si, respectively, in order to examine whether these rare-earth-lean materials are suitable for applications as permanent magnets. Structural and magnetic characterization of the family of alloys with the general formula Nd 0.4 Zr 0.6 Fe 10–x Co x Si 2 (x = 0–3) and their melt-spun ribbons were carried out using X-ray diffraction and Mössbauer spectroscopy. The ThMn 12 -type structure is obtained for all samples as the majority phase with a minority α-Fe(CoSi) phase (less than 5 wt%) as it was estimated by XRD for x = 1 and 2. The Curie temperature increases linearly with Co substitution from 561 K for x = 0 to 712 K for x = 3. The saturation magnetization decreases slightly from 130.5 (x = 1) to 129.1 A·m 2 /kg (x = 3), while the anisotropy field is following the same trend.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Phase equilibria in iron-rich Sm–Fe–Ti and Sm–(Fe,Co)–Ti alloys at 1100–1200 °C

Iron-rich corners of ternary Sm–Fe–Ti phase diagram at 1100 °C and quasi-ternary Sm–Fe 0.8 Co 0.2 –Ti phase diagrams at 1100 and 1200 °C are constructed based on experimental investigation of equilibrated alloys with electron probe microanalysis, X-ray diffraction and thermomagnetic analysis. In addition, the upper boundaries of the temperature ranges of Sm(Fe,[Co,]Ti) 12 and Sm 3 (Fe,[Co,]Ti) 29 phases are determined with differential thermal analysis to update earlier rough estimates. The existence of a high-temperature phase of the Th 2 Ni 17 type, originally reported by Ivanova et al. [J. Alloys Compd. 224 (1995) 29], is confirmed. In the Sm–Fe 0.8 Co 0.2 –Ti system, the composition and equilibria of this hexagonal phase are established for 1200 °C; it is Sm-depleted (≈9.8 at.% Sm) compared to the 2:17 stoichiometry and it coexists with the rhombohedral 2:17 phase. The magnetic anisotropy of the cobalt-substituted Th 2 Ni 17 -type phase is planar, with the easy magnetization direction parallel to [100]. Equilibrium between a Sm-rich liquid phase and the 1:12 phase, which is important for the development of new high-performance permanent magnets, is absent up to 1000 °C, but does exist at 1100 °C (for the 1:12 phase with at least 8.7–8.9 at.% Ti) and at 1200 °C (for the 1:12 phase with as little as 7.4 at.% Ti). The development of magnets may be complicated, however, by an observed tendency of the high-temperature liquid to solidify into ferromagnetic phases including the Th 2 Ni 17 -type phase. The Curie temperatures of the α-(Fe,Ti), Sm(Fe,Ti) 12 , Sm 3 (Fe,Ti) 29 and rhombohedral Sm 2 (Fe,Ti) 17 phases are not only increased by the partial Co substitution for Fe, but their dependence on the Ti concentration is changed by this Co substitution from positive (or, for the 1:12 phase, zero) to negative values.

36 MATERIALS SCIENCE↗

Thermodynamics and Magnetism of SmFe12 Compound Doped with Co and Ni: An Ab Initio Study

Ni-doped Sm(Fe1−xCox)12 alloys are investigated for their magnetic properties. The Sm(Fe,Co)11M1 compound (M acts as a stabilizer) with the smallest (7.7 at.%) rare-earth-metal content has been recognized as a possible contender for highly efficient permanent magnets thanks to its significant anisotropy field and Curie temperature. The early transition metals (Ti-Mn) as well as Al, Si, and Ga stabilize the SmFe12 compound but significantly decrease its saturation magnetization. To keep the saturation magnetization in the range of 1.4–1.6 T, we suggest replacing a certain amount of Fe and Co in the Sm(Fe1−xCox)12 alloys with Ni. Ni plays the role of a thermodynamic stabilizer, and contrary to the above-listed elements, has the spin moment aligned parallel to the spin moment of the SmFe12 compound, thereby boosting its saturation magnetization without affecting the anisotropy field or Curie temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

A CW radiofrequency ion source for production of negative hydrogen ion beams for cyclotrons

A CW 13.56 MHz radiofrequency-driven ion source RADIS for production of H{sup −} and D{sup −} beams is under development for replacing the filament-driven ion source of the MCC30/15 cyclotron. The RF ion source has a 16-pole multicusp plasma chamber, an electromagnet-based magnetic filter and an external planar spiral RF antenna behind an AlN window. The extraction is a 5-electrode system with an adjustable puller electrode voltage for optimizing the beam formation, a water-cooled electron dump electrode and an accelerating einzel lens. At 2650 W of RF power, the source produces 1 mA of H{sup −} (2.6 mA/cm{sup 2}), which is the intensity needed at injection for production of 200 µA H{sup +} with the filament-driven ion source. A simple pepperpot device has been developed for characterizing the beam emittance. Plans for improving the power efficiency with the use of a new permanent magnet front plate is discussed.

43 PARTICLE ACCELERATORS↗

Coercivity of (Fe 0.7 Co 0.3 ) 2 B Nanowire and Its Bonded Magnet

(Fe 0.7 Co 0.3 ) 2 B are potential permanent magnets material due to its large saturation magnetization and high Curie temperature. However, it has moderate magnetocrystalline anisotropy (MCA) and low coercivity. One way to improve its coercivity is to combine the contributions from magnetocrystalline- and magnetic-shape anisotropy by preparing (Fe 0.7 Co 0.3 ) 2 B nanowires. We study the effects of size, morphology, and surface defects on the hard magnetic properties of nanowires using micromagnetic simulation. The hard magnetic properties of (Fe 0.7 Co 0.3 ) 2 B nanowire-bonded magnets are estimated, including the role of inter-wire magnetostatic interaction. By considering the existence of local reductions in MCA energy of up to 30% on the surface layer of nanowires, the anisotropic bonded magnet with a 65% vol. of (Fe 0.7 Co 0.3 ) 2 B nanowires would have typical remanence, B r = 7.6–8.4 kG, coercivity, H ci = 9.6–9.9 kOe, and maximum energy product, (BH) m = 14–17.8 MGOe. Developing effective technology for synthesizing nanowires and fabricating corresponding bonded magnets is promising for manufacturing practical magnets based on the magnetic phase with a relatively low or moderate MCA, such as (Fe 0.7 Co 0.3 ) 2 B.

36 MATERIALS SCIENCE↗

Thermodynamics and Magnetism of SmFe 12 Compound Doped with Zr, Ce, Co and Ni: An Ab Initio Study

Alloys that are Ni-doped, such as the (Sm 1—y Zr y )(Fe 1—x Co x ) 12 and (Ce 0.5 Sm 0.5 )Fe 10 Co 2 systems, are studied because of their magnetic properties. The (Sm 1—y Zr y )(Fe 1—x Co x ) 11—z Ti z and (Ce. 1—x Sm x )Fe 9 Co 2 Ti alloys are considered contenders for vastly effective permanent magnets because of their anisotropy field and Curie temperature. Ti can act as a stabilizer for the SmFe 12 compound but substantially suppresses saturation magnetization. To maintain the saturation magnetization in the scope of 1.3–1.5 T, we propose substituting a particular quantity of Fe and Co in the (Sm 1—y Zr y )(Fe 1—x Co x ) 12 and (Ce 0.5 Sm 0.5 )Fe 10 Co 2 alloys with Ni. By performing ab initio calculations, we show that Ni incorporation results in increased thermodynamic stability and, in contrast to Ti, has a parallel spin moment aligned to the moment of the SmFe 12 compound and improves its saturation magnetization without affecting the anisotropy field or Curie temperature.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Accelerating Nature: Induced Atomic Order in Equiatomic FeNi

Abstract The production of locally atomically ordered FeNi (known by its meteoric mineral name, tetrataenite) is confirmed in bulk samples by simultaneous conversion X‐ray and backscattered γ‐ray 57 Fe Mössbauer spectroscopy. Up to 22 volume percent of the tetragonal tetrataenite phase is quantified in samples thermally treated under simultaneous magnetic‐ and stress‐field conditions for a period of 6 weeks, with the remainder identified as the cubic FeNi alloy. In contrast, all precursor samples consist only of the cubic FeNi alloy. Data from the processed alloys are validated using Mössbauer parameters derived from natural meteoritic tetrataenite. The meteoritic tetrataenite exhibits a substantially higher degree of atomic order than do the processed samples, consistent with their low uniaxial magnetocrystalline anisotropy energy of ≈1 kJ·m −3 . These results suggest that targeted refinements to the processing conditions of FeNi will foster greater atomic order and increased magnetocrystalline anisotropy, leading to an enhanced magnetic energy product. These outcomes also suggest that deductions concerning paleomagnetic conditions of the solar system, as derived from meteoritic data, may warrant re‐examination and re‐evaluation. Additionally, this work strengthens the argument that tetrataenite may indeed become a member of the advanced permanent magnet portfolio, helping to meet rapidly escalating green energy imperatives.

36 MATERIALS SCIENCE↗

Comparison of Candidate Designs and Performance Optimization for an Electric Traction Motor Targeting 50 kW/L Power Density

The continued expansion of the global electric vehicle fleet is accompanied by an unprecedented demand for high power density electric traction motors. With the ambitious U.S. DRIVE 2025 target of 50 kW/L power density and an equally aggressive cost reduction goal, innovative approaches have to be utilized in terms of both the design and manufacturing of electric traction motors. In this paper, six motor options are compared and the best design is picked for each option to investigate the drive and excitation requirements and the weighted power efficiency over multiple load points, with necessary mechanical stress and demagnetization checks. State-of-the-art winding technologies, including high slot fill die compressed windings and hairpin windings, and rotors both with permanent magnet (PM) and PM-free are incorporated. The design of high flux density and low harmonic content magnetic field is also demonstrated.

33 ADVANCED PROPULSION SYSTEMS↗