Search NASA⌕ Search

SEARCH · Search NASA

Results for “Powder”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 757 records · Page 42

Mechanical behavior and shear band of a powder-metallurgy-fabricated CoCrFeMnNi high-entropy alloy during high strain-rate deformation

High-entropy alloys (HEAs) fabricated by powder metallurgy are considered to exhibit extremely-great potential application values in the field for high-speed impact deformation due to their uniform microstructures and compositions. The mechanical behavior of a powder-metallurgy-fabricated (PM) CoCrFeMnNi HEA was investigated at room temperature with strain rates ranging from 1200 s -1 to 2800 s -1 . It was found that the serration behavior and shear localization of the alloy under dynamic conditions occurred. Results also indicated that the serrated flow took place in the PM CoCrFeMnNi HEA during mechanical deformation at high strain rates (>1000 s -1 ) and became more pronounced as the strain rate increased. Furthermore, it was determined that the yield-strength values of the PM CoCrFeMnNi HEA were sensitive to strain rates, where the values increased from 500 MPa to 700 MPa when the strain rates increased from 1200 s -1 to 2800 s -1 . Shear bands with a width of about 20 μm were generated in the PM CoCrFeMnNi HEA after the shear stress reached a maximum value of 635 MPa, which corresponded to a nominal strain of about 8.71. Nanotwins and ultrafine-equiaxed grains with a diameter of about 150 nm also developed at the core of the shear band during deformation. The results revealed that the strength of the shear band was much higher than that of the matrix grain. Nanotwins in the shear band were composed of a single face-centered-cubic (FCC) structure with the twin plane of ($\bar{1}$1$\bar1$), which could be formed via a rotational dynamic recrystallization (RDR).

36 MATERIALS SCIENCE↗

Uranium silicide pellet fabrication by powder metallurgy for accident tolerant fuel evaluation and irradiation

In collaboration with industry, Idaho National Laboratory is investigating uranium silicide for use in future light water reactor fuels as a more accident resistant alternative to uranium oxide base fuels. Specifically this project was focused on producing uranium silicide (U 3 Si 2 ) pellets by conventional powder metallurgy with a density greater than 94% of the theoretical density. This work has produced a process to consistently produce pellets with the desired density through careful optimization of the process. Milling of the U 3 Si 2 has been optimized and high phase purity U 3 Si 2 has been successfully produced. Results are presented from sintering studies and microstructural examinations that illustrate the need for a finely ground reproducible particle size distribution in the source powder. The optimized process was used to produce pellets for the Accident Tolerant Fuel-1 irradiation experiment. The average density of these pellets was 11.54 ±0.06 g/cm 3 . Additional characterization of the pellets by scaning electron microscopy and X-ray diffraction has also been performed. As a result, pellets produced in this work have been encapsulated for irradiation, and irradiation in the Advanced Test Reactor is expected soon.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Infrared absorptive properties of Al-doped ZnO divided powder

Al-doped ZnO powders were synthesised by a Pechini process in order to obtain visible non-absorbent and near-Infrared absorbent particles. Firstly, it has been shown that synthesis under argon combined with the lowest synthesis temperatures (700 deg. C) allows getting the optimal properties for pure ZnO compounds due to creation of n-type defects segregated on oxide grain surface (Zn/O ratio superior to 1). Nevertheless, the near-Infrared absorption properties of the pure ZnO compounds remain low. The Al{sup 3+} doping of ZnO compounds was then investigated. The Al solubility limit inside ZnO doped compounds decreases drastically with the grain size, i.e. with the synthesis temperature. Then, the Al cations distribution varies inside ZnO grains, Al{sup 3+} segregation at the grain surfaces taking place for high synthesis temperatures. The optimal optical properties (high near-Infrared absorption) are reached combining Al-doping and adequate synthesis conditions: annealing under argon at low temperatures. In these conditions, the highest extrinsic (via Al doping) and intrinsic n-types defects rates are indeed reached. - Graphical abstract: Al-doped ZnO powders synthesised from Pechini routes after annealing under argon at low temperatures exhibit high optical selectivity: large Infrared absorption/high visible transparency. Highlights: > ZnO synthesis route with low T/low pO{sub 2} promotes extrinsic defects. > Highly divided Al-doped ZnO oxides (hdAZO) exhibit high Al solubility limit. > hdAZO are IR absorbent because of their high intrinsic/extrinsic defects concentrations.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Synthesis and crystal chemical evolution of fresnoite powders

(Ba,Sr){sub 2}TiSi{sub 2}O{sub 8} fresnoite powders were prepared via a Pechini process in which citric acid and ethylene glycol were used as complexing agents. The resulting gel contained a homogeneous distribution of the metal ions that suppressed the formation of (Ba,Sr)TiO{sub 3} perovskite as a secondary phase during calcination. Phase development was examined as by isochronal and isothermal reaction analysis. A combination of thermo- and differential gravimetric analysis (TGA-DGA), quantitative X-ray diffraction (XRD) and Fourier transform infrared spectroscopy (FTIR) confirmed that calcination at 900 Degree-Sign C/12 h yielded finely crystalline ({approx}70 nm) Ba{sub 2}TiSi{sub 2}O{sub 8} (BTS) and Sr{sub 2}TiSi{sub 2}O{sub 8} (STS). The endmembers and compositional intermediates crystallized directly from the Pechini resin and indirectly through reaction of (Ba,Sr)CO{sub 3}, (Ba,Sr)TiO{sub 3} and a silica-rich glass intermediates. This new method for preparing fresnoite yields materials suitable for consolidation as dense monolithic dielectrics or for use as high surface area catalytic powders. - Graphical abstract: The Pechini synthesis of (Ba, Sr){sub 2}TiSi{sub 2}O{sub 8} titano-silicate fresnoites delivers finely divided precursors for applications as diverse as solid electrolytes and photocatalysis that exploit the unique Ti-O and Si-O bonding and structural morphology of these materials. Highlights: Black-Right-Pointing-Pointer A Pechini method for synthesizing (Ba,Sr){sub 2}TiSi{sub 2}O{sub 8} fresnoites is demonstrated. Black-Right-Pointing-Pointer The method minimizes a persistent glassy intermediate phase. Black-Right-Pointing-Pointer The Pechini process is generally applicable for tailoring fresnoites as functional materials.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Surface characterization of ZnO/ZnMn{sub 2}O{sub 4} and Cu/Mn{sub 3}O{sub 4} powders obtained by thermal degradation of heterobimetallic complexes

From the selective transformation of the heterometallic (Zn-Mn or Cu-Mn) carboxylate complexes with 2,2 Prime -bipyridyl by thermal degradation at relatively low (350 Degree-Sign C) temperature, it was possible to get either well defined spinel ZnMn{sub 2}O{sub 4} over zinc oxide or well dispersed copper particles surrounded by a manganese oxide (Mn{sub 3}O{sub 4}) in a core-shell like structure. Morphology of the powder surface was examined by scanning electron microscopy with energy dispersive X-ray microanalysis (SEM/EDX). Surface composition was determined by X-ray photoelectron spectroscopy (XPS). Specific surface of the powders by nitrogen adsorption was found to be 33{+-}0.2 and 9{+-}0.06 m{sup 2} g{sup -1} for Zn-Mn and Cu-Mn samples, respectively, which is comparable to those of commercial products. - Graphical abstract: From the selective transformation of heterometallic (Zn-Mn or Cu-Mn) carboxylate complexes, it was possible to get either well defined spinel ZnMn{sub 2}O{sub 4} over zinc oxide or well dispersed copper particles surrounded by a manganese oxide (Mn{sub 3}O{sub 4}) in a core-shell like structure. Highlights: Black-Right-Pointing-Pointer Thermal degradation of heterometallic complexes results in fine disperse particles. Black-Right-Pointing-Pointer Core-shell Cu/Mn{sub 3}O{sub 4} particles are obtained. Black-Right-Pointing-Pointer ZnMn{sub 2}O{sub 4} spinel layer covers ZnO particles.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

A-site deficient perovskites in the SrO-ZrO{sub 2}-Nb{sub 2}O{sub 5} system: Composition dependent structures from neutron powder diffraction data

A series of A-site deficient perovskite-type phases was synthesised and characterised in the SrO-ZrO{sub 2}-Nb{sub 2}O{sub 5} system. The composition range was established as Sr{sub 0.70+x}Zr{sub 0.40+2x}Nb{sub 0.60-2x}O{sub 3}, {approx}0.02{<=}x{<=}0.30, and the resulting structures refined using high resolution neutron powder diffraction data. While structures in this composition range are closely related to the cubic perovskite parent, the symmetry for all investigated compositions is lowered to tetragonal or orthorhombic. For x<0.15 the resulting space group is tetragonal I4/mcm, for x>0.15 it is orthorhombic Pnma and for x=0.15 two phases co-exist, in space groups I4/mcm and Pnma. - Graphical abstract: Structured diffuse intensity indicating additional short range order in the defect perovskite Sr{sub 0.72}Zr{sub 0.44}Nb{sub 0.56}O{sub 3}. Highlights: Black-Right-Pointing-Pointer A-site deficient perovskites synthesised in Sr{sub 0.70+x}Zr{sub 0.40+2x}Nb{sub 0.60-2x}O{sub 3}, {approx}0.02 {<=}x{<=}0.30. Black-Right-Pointing-Pointer Space groups established from X-ray, electron and neutron powder diffraction. Black-Right-Pointing-Pointer Structures refined and phase transition established from neutron diffraction data.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High pressure powder X-ray diffraction of sillenites Bi{sub 12}MO{sub 20} (M=Si, Ge, Ti) and Bi{sub 4}Ti{sub 3}O{sub 12}

Powder X-ray diffraction experiments of sillenites Bi{sub 12}M O{sub 20} (M=Si, Ge, Ti) were performed with synchrotron radiation at the ESRF, Grenoble, at pressures up to 39 GPa (M=Si), 50 GPa (M=Ge), and 37 GPa (M=Ti), respectively. These three sillenites were investigated for the first time over such a large pressure range and they show no phase transition up to the highest pressures achieved. Birch–Murnaghan equations of state of third order were fitted to the pressure dependence of the lattice parameters. The resulting bulk moduli B{sub 0} and their pressure derivatives B′ are B{sub 0}=63(1)GPa with B′=6.6(3) (M=Si), B{sub 0}=63.0(5)GPa with B′=5.90(7) (M=Ge), and B{sub 0}=48(1)GPa with B′=9.4(5) (M=Ti). In the case of Bi{sub 12}SiO{sub 20} and Bi{sub 12}TiO{sub 20} the equation of state fits were restricted to pressures below 15 GPa, because the experimental data were affected by non-hydrostatic stress at higher pressures. The equation of state of neon was redetermined (V{sub 0}=11.7(6)cm{sup 3}/mol, B{sub 0}=5(1)GPa, B′=5.5(3)GPa) and its use as an internal pressure standard for diffraction experiments is discussed. A second cubic phase could be identified in our Bi{sub 12}TiO{sub 20} sample. This was attributed to eulytite-type Bi{sub 4}Ti{sub 3}O{sub 12}, which has B{sub 0}=50.9(8)GPa and B′=6.9(3). - Graphical abstract: X-ray diffraction at high pressure → Equation of state. - Highlights: • Powder X-ray diffraction experiments of sillenites were performed at high pressures. • Equations of state of sillenites Bi{sub 12}MO{sub 20} (M=Si, Ge, Ti) were determined. • The sillenite structure was shown to be stable at high hydrostatic pressure. • Sillenites are sensitive to non-hydrostatic pressure conditions in neon-loaded DACs. • An eulytite-type Bi{sub 4}Ti{sub 3}O{sub 12} phase was found to exist up to 10 GPa.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Magnetic and low temperature phonon studies of CoCr{sub 2}O{sub 4} powders doped with Fe(III) and Ni(II) ions

Extensive temperature-dependent phonon studies and low-temperature magnetic measurements of CoCr{sub 2−x}Fe{sub x}O{sub 4} (for x=0.5, 1 and 2) and Co{sub 0.9}Ni{sub 0.1}Cr{sub 2}O{sub 4} polycrystalline powders are presented. The main aim of these studies was to obtain information on phonon and structural properties of these compounds as well as strength of spin–phonon coupling in the magnetically ordered phases. IR and Raman spectra show that doping of CoCr{sub 2}O{sub 4} with Fe(III) ions leads to broadening of bands and appearance of new bands due to the formation of inverted spinel structure. In contrast to this behavior, doping with 10 mol% of Ni(II) ions leads to weak increase of band width only. Magnetization measured as a function of temperature and external magnetic field showed that magnetic properties of Co{sub 0.9}Ni{sub 0.1}Cr{sub 2}O{sub 4} sample are similar to those reported for pure CoCr{sub 2}O{sub 4}, i.e., partial substitution of Ni(II) for Co(II) leads to slight shift of the ferrimagnetic phase transition at T{sub C} and spiral spin order transition at T{sub S} towards lower values. The change of crystallization preference induced by incorporation of increasing concentration of Fe(III) ions in the spinel lattice causes significant increase of T{sub C} and decrease of T{sub S}. The latter transition disappears completely for higher concentrations of Fe(III). The performed temperature-dependent IR studies revealed interesting anomalous behavior of phonons below T{sub C} for CoCr{sub 1.5}Fe{sub 0.5}O{sub 4} and Co{sub 0.9}Ni{sub 0.1}Cr{sub 2}O{sub 4}, which was attributed to spin–phonon coupling. - Graphical abstract: Visualization of normal spinel-type AB{sub 2}O{sub 4} structure, where blue octahedrons denote BO{sub 6} and red tetrahedrons AO{sub 4} units as well as IR and Raman spectra of Co{sub 0.9}Ni{sub 0.1}Cr{sub 2}O{sub 4} powder. - Highlights: • T{sub C} (T{sub S}) increases (decreases) with increasing Fe(III) concentration. • Ni(II) ions doping up to 10 mol% does not change remarkably T{sub C} and T{sub S}. • Doping with Fe(III) ions causes increase of spinel inversion parameter. • Spin–phonon interactions in Co{sub 0.9}Ni{sub 0.1}Cr{sub 2}O{sub 4} and CoCr{sub 1.5}Fe{sub 0.5}O{sub 4} were evidenced.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Low temperature synthesis and characterization of BiNbO{sub 4} powders

BiNbO{sub 4} powders, a potential microwave dielectric ceramic were prepared by both co-precipitation and solid state techniques. In the former method, an aqueous ammonium hydroxide was used to precipitate Bi{sup 3+} and Ta{sup 5+} cations as hydroxides simultaneously under basic conditions. It is observed that the co-precipitation produces BiNbO{sub 4} phase on heating at 600 deg. C, whereas complete phase formation occurs only at 800 deg. C in the case of solid state method. The phase contents and lattice parameters were studied by powder X-ray diffraction. The sequence of the reaction and phase evolution of BiNbO{sub 4} were also studied by the X-ray diffraction. The samples were characterized by the differential-thermal/thermo-gravimetric analyses and scanning electron microscopy techniques.

36 MATERIALS SCIENCE↗

Macroporous glass monoliths prepared from powdered niobium phosphate glass by fast sintering

Macroporous monoliths were prepared by very fast sintering (between 3 and 15 min) of niobophosphate glass powders at low temperature (1018 K) using cellulose as a foaming agent. The porous materials were analyzed by thermal analysis, Raman spectroscopy, scanning electron microscopy and powder X-ray diffraction, and further investigated using X-ray microtomography, a non-destructive technique capable of reconstructing three-dimensional models of samples and providing structural measurements. The progression of the porosity of the monoliths depends on the sintering time (3 to 15 min) and the amount (up to 50% in mass) of cellulose used. The macroporous glass monoliths may find application in integrated chemical systems and in filtering processes.

36 MATERIALS SCIENCE↗

Characterization by X-ray tomography of granulated alumina powder during in situ die compaction

Compaction process, the aim of which being to obtain green bodies with low porosity and small size, is often used before sintering treatment. Prior to die filling, the ceramic powder is generally granulated to improve flowability. However during compaction, density heterogeneity and critical size defects may appear due to intergranule and granule-die wall frictions. In this work, the influence of granule formulation on the compact morphology has been studied. To do so, a compaction setup was installed inside an X-ray tomography equipment so that the evolution of the compact morphology could be analysed during the whole compaction process. We have demonstrated that high humidity rate and the addition of binder in the granule formulation increase density heterogeneity and generate larger defects. - Highlights: • An original compaction set up was installed inside an X-Ray tomography equipment. • The compaction process of granulated ceramic powder is imaged. • The compact green microstructure is quantified and related to the compaction stages. • The most detrimental defects of dry-pressed parts are caused by hollow granules. • Formulations without binder allow a reduction of the number of large defects.

36 MATERIALS SCIENCE↗

Characterization of 430L porous supports obtained by powder extrusion moulding for their application in solid oxide fuel cells

The characterization of 430L stainless steel planar porous supports obtained by powder extrusion moulding was performed in this work. A thermoplastic multicomponent binder based on high density polyethylene and paraffin wax was selected for the process. Green supports were shaped by extrusion moulding, and subsequently the binder was removed by a thermal cycle previously optimized. Sintering was carried out at different temperatures in low vacuum. Density of sintered parts was measured by Archimedes' method and porosity was also evaluated through a microstructural analysis by optical microscopy. The porosity degree of samples sintered at low temperature was close to 35% which is a very suitable value for their application in SOFCs. Tensile tests were carried out in order to determine mechanical strength as a function of porosity degree. Based on these results, the best feedstock composition and processing parameters were selected. The oxidation behaviour in static air at high temperature was studied, and formed oxides were characterized in a scanning electron microscope equipped with energy dispersive analysis of X-rays. X-ray diffraction experiments were performed in order to identify the formed oxides based on formula Fe{sub 2−x}Cr{sub x}O{sub 3}. The results of these studies showed that this kind of ferritic stainless steel would be more suitable to be used as anodic supports where a rich hydrogen atmosphere is employed. Preliminary deposition tests allowed obtaining a homogeneous Ni–YSZ anode layer with a thickness of 10 μm on the porous metallic substrates. - Highlights: • 430L stainless steel porous supports were obtained by powder extrusion moulding. • Porosity degree was controlled sintering at different temperatures in low vacuum. • Tensile tests allowed determining mechanical strength of porous supports. • A study about its oxidation behaviour in static air at high temperature was realized. • After oxidation, formed oxides were characterized by EDS–SEM and XRD.

36 MATERIALS SCIENCE↗

Comprehensive characterization of ball-milled powders simulating a tribofilm system

A model system was used to simulate the properties of tribofilms which form during automotive braking. The model system was prepared by ball milling of a blend of 70 vol.% iron oxides, 15 vol.% molybdenum disulfide and 15 vol.% graphite. The resulting mixture was characterized by X-ray powder diffraction (XRD), X-ray photoelectron spectroscopy (XPS), and various transmission electron microscopic (TEM) methods, including energy dispersive X-ray spectroscopy (EDXS), high resolution investigations (HRTEM) with corresponding simulation of the HRTEM images, diffraction methods such as scanning nano-beam electron diffraction (SNBED) and selected area electron diffraction (SAED). It could be shown that the ball milling caused a reduction of the grain size of the initial components to the nanometer range. Sometimes even amorphization or partial break-down of the crystal structure was observed for MoS{sub 2} and graphite. Moreover, chemical reactions lead to a formation of surface coverings of the nanoparticles by amorphous material, molybdenum oxides, and iron sulfates as derived from XPS. - Highlights: • Ball milling of iron oxides, MoS{sub 2}, and graphite to simulate a tribofilm • Increasing coefficient of friction after ball milling of the model blend • Drastically change of the diffraction pattern of the powder mixture • TEM & XPS showed the components of the milled mixture and the process during milling. • MoS{sub 2} and graphite suffered a loss in translation symmetry or became amorphous.

36 MATERIALS SCIENCE↗

Texture development in magnetostrictive Fe-Ga alloys processed by laser powder bed fusion

Iron-gallium (Fe-Ga, Galfenol) alloys are promising magnetostrictive materials for actuators, sensors, and energy harvesting, but their performance is highly sensitive to microstructure and texture. Additive manufacturing by laser powder bed fusion (LPBF) offers a pathway to engineer texture and integrate functional materials into complex geometries. Here, we fabricate Fe-Ga alloys (Fe 82.2 Ga 17.8 ) by LPBF of gas-atomized powders and systematically optimize laser power and scan speed to maximize density and control texture. Nearly full-density parts (up to 99.6 %) are achieved within a narrow processing window. Electron backscatter diffraction (EBSD) reveals a strong <100> fiber texture aligned with the build direction and columnar grains up to 1 mm long. Magnetostriction measurements show saturation magnetostriction of 190 ppm in the build direction. Correlating texture data with macroscopic magnetostriction, we estimate intrinsic magnetostriction constants (λ 100 = 228 ppm, λ 111 = 12 ppm), closely matching single crystal-derived values. These results demonstrate the critical interplay between processing, texture, and functional performance in additively manufactured Fe-Ga alloys and establish LPBF as a viable route for high-performance magnetostrictive materials.

Additive manufacturing↗

Fabrication of cerium active terbium aluminum garnet (TAG:Ce) phosphor powder via the solid-state reaction method

A modified solid-state reaction method for the formation of terbium aluminum garnet (TAG:Ce) powder was studied. The starting materials, which included terbium oxide (Tb{sub 4}O{sub 7}), boehmite and cerium chloride (CeCl{sub 3}.7H{sub 2}O), were pre-aged at pH 3. This pre-aging process helps to form the core-shell structure, which leads to the formation of TAG:Ce phosphor powder via a solid-state reaction more easily. The emission intensity at 551 nm of the product pre-aged at pH 3 is higher than that formed without pre-aging.

36 MATERIALS SCIENCE↗

Preparation and characterization of nanometer-scale powders ceria by electrochemical deposition method

Ceria (CeO{sub 2}) nanoparticles of 10-30 nm in average particle size have been synthesized via electrochemical deposition method in cerium(III) chloride solution with an undivided cell as electrochemical cell and ethanol-acetylacetone as additives. X-ray diffraction (XRD), transmission electron microscopy (TEM), Fourier transformation infrared spectroscopy (FT-IR) and thermal analysis (TG-DTA) are introduced to characterize the samples. The results indicate that the as-prepared powders after being treated at 650 deg. C are nanocrystalline with the cubic fluorite structure and the sphericity in shape. It is revealed that the size of ceria nanoparticles can be decreased effectively by adding the ethanol-acetylacetone solution. In addition, the possible formed mechanism of CeO{sub 2} nanometer-scale powder. The role of additive is also investigated in this paper.

36 MATERIALS SCIENCE↗

Fine-grained multiferroic BaTiO{sub 3}/(Ni{sub 0.5}Zn{sub 0.5})Fe{sub 2}O{sub 4} composite ceramics synthesized by novel powder-in-sol precursor hybrid processing route

Dense, homogeneous, and fine-grained multiferroic BaTiO{sub 3}/(Ni{sub 0.5}Zn{sub 0.5})Fe{sub 2}O{sub 4} composite ceramics are synthesized by a novel powder-in-sol precursor hybrid processing route. This route includes the dispersion of nanosized BaTiO{sub 3} ferroelectric powders prepared via conventional sold-state ceramic process into (Ni{sub 0.5}Zn{sub 0.5})Fe{sub 2}O{sub 4} ferromagnetic sol-gel precursor prepared via sol-gel wet chemistry process. Uniformly distributed slurry is obtained after ball milling and used in the fabrication of the ceramics with low sintering temperatures. The ceramics show coexistence of ferromagnetic and ferroelectric phases with obvious ferromagnetic and ferroelectric hysteresis loops at room temperature, besides exhibiting excellent magnetic and dielectric properties in a wide range of frequency. The combination of high permeability and permittivity with low losses in the ceramics enables significant miniaturization of electronic devices based on the ceramics.

36 MATERIALS SCIENCE↗

Fabrication of ultrafine tungsten-based alloy powders by novel soda reduction process

A novel reduction method has been developed to fabricate ultrafine tungsten heavy alloy powders, with ammonium metatungstate (AMT), iron(II) chloride tetrahydrate (FeCl{sub 2}.4H{sub 2}O), nickel(II) chloride hexahydrate (NiCl{sub 2}.6H{sub 2}O) as source materials and sodium tungstate dihydrate (Na{sub 2}WO{sub 4}.2H{sub 2}O) as a reductant. In the preparation of mixtures the amounts of the source components were chosen so as to obtain alloy of 93W-5Ni-2Fe composition (wt.%). The obtained powders were characterized by X-ray diffraction, XPS, field-emission scanning microscope (FESEM), and chemical composition was analyzed by EDX.

36 MATERIALS SCIENCE↗