Reducing Intermetallic Compounds of Mg/Al Joint in Friction Stir Lap Welding

To reduce intermetallic compounds (IMCs) of Al{sub 12}Mg{sub 17} and Al{sub 3}Mg{sub 2} in Mg/Al friction stir lap welding joint, pin tip was plunged into the lower sheet at a small distance. Results showed that at a fixed welding speed of 50 mm/min, sound joints were obtained using rotating speeds from 750 to 500 rpm, and the IMCs zones were rather small. Cracks easily appeared inside IMCs inside onion ring and at lap interface. Therefore, reducing the IMC was beneficial for reducing the crack. Joint lap shear stress firstly increased and then decreased with decrease in the rotating speed. The maximum shear stress of 50.2 MPa was attained at a rotating speed of 500 rpm because of reduced IMC.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Welded Q235 Low-Carbon Steel

Three-millimeter-thick Q235 steel plates were friction stir welded using a tool made of tungsten-rhenium alloy in the present study. The microstructure and mechanical properties of welded joints at various traverse speeds from 50 to 150 mm/min were analyzed. It was demonstrated that traverse speed had great impacts on microstructure and mechanical properties of the joints. Phase transformation accompanied with recrystallization occurred during FSW process which resulted in different microstructures in the WNZ, and the grain size in other zones was significantly affected by traverse speed. The highest hardness was located in the nugget zone, while the lowest hardness was found in the heat-affected zone. The transverse tensile test suggested that all the joints showed slightly lower tensile strength than that of the base material, and the tensile strength increased with increasing traverse speed. All the joints fractured in the heat-affected zone with ductile fracture mode. The impact test showed that the impact toughness decreased with the increasing traverse speed and the impact fracture surface could be divided into shear lip zone and fibrous zone which showed a typical ductile fracture.

36 MATERIALS SCIENCE↗

Precipitate evolution in friction stir welding of 2219-T6 aluminum alloys

Precipitate evolution in friction stir welding of 2219-T6 aluminum alloys was characterized by transmission electron microscopy. In the weld nugget zone and the thermo-mechanically affected zone some metastable precipitates overaged to equilibrium phase while others solutionized into the aluminum solid solution. In the heat-affected zone the precipitates coarsened.

36 MATERIALS SCIENCE↗

Microstructures in a resistance spot welded high strength dual phase steel

The microstructure of a high strength dual phase steel resistance spot welded with tempering-pulse technology is characterized in this paper. In the fusion zone, there is a needle-like microstructure identified as acicular or side plate ferrite that has a cube-on-cube orientation relationship with respect to the surrounding martensite. In contrast to the microstructures produced by the lower cooling rate arc or laser welding techniques, the nucleation of this fine intragranular ferrite takes place independent of inclusions. Further, a leaf-like microstructure within the martensitic matrix is found to contain primitive orthorhombic Cr{sub 3}C{sub 2} and face-centered cubic CrC chromium carbides, rather than Cr{sub 23}C{sub 6} or Cr{sub 7}C{sub 3} as is commonly observed in steel alloys. The formation histories of both the ferrite phase and the chromium carbides are analyzed.

36 MATERIALS SCIENCE↗

Microstructural evolution of fusion zone in laser beam welds of pure titanium

Microstructural evolution of fusion zone in laser beam welds of pure titanium was studied by means of electron backscattering diffraction. The microstructural evolution is strongly affected by the {beta} {yields} {alpha} transformation mechanism dependent on the cooling rate during phase transformation. The long-range diffusional transformation mainly occurs in the fusion zone at the low cooling rate, and the massive transformation dominantly takes place at the high cooling rate. For this reason, the grain morphologies probably change from the granular-like to columnar-like grains with the cooling rate increasing. - Highlights: Black-Right-Pointing-Pointer Microstructures of fusion zone in laser beam welds of pure titanium are studied. Black-Right-Pointing-Pointer Increasing cooling rate changes grain morphology from granular to columnar one. Black-Right-Pointing-Pointer Final microstructures depend on the {beta}{yields}{alpha} transformation mechanisms.

36 MATERIALS SCIENCE↗

Microstructure evolution in the fusion zone of laser-welded Mg–Gd–Y–Zr alloy during solution and aging treatment

The microstructure evolution in the fusion zone of laser-welded Mg-Gd-Y-Zr alloy during solution and aging treatment is investigated. The morphology of the Mg{sub 24}(Gd,Y){sub 5} in the divorced eutectic at the grain boundary transforms from a continuous network to disconnected and fragmentized islands and then to spheroidal particles before complete dissolution during the solution treatment at 430 °C. During the subsequent aging treatment at 225 °C, the precipitation sequence in the fusion zone follows the order of supersaturated solid solution (SSSS) → βʺ(D0{sub 19}) → βʹ(cbco) → β{sub 1}(fcc) → β(fcc). High-density precipitates are present at the original grain boundaries of the fusion zone from the welded structure but there are less precipitates in the interior of the original grains. The grain growth during the solution treatment at 430 °C comprises the slowly increasing stage, rapidly increasing stage, and stable stage. The network-distributed Mg{sub 24}(Gd,Y){sub 5} impedes migration of the grain boundaries, restricts grain growth in the first slowly increasing stage, and segregation of zirconium near the grain boundaries also affects migration of the grain boundaries. - Highlights: •Different quantities of precipitates are present at different location of grain. •The network-distributed Mg{sub 24}(Gd,Y){sub 5} restricts grain growth. •Segregation of Zr affects migration of grain boundaries.

36 MATERIALS SCIENCE↗

Microstructure, texture, and mechanical properties of friction stir welded commercial brass alloy

Microstructural evolution during friction stir welding of single-phase brass and corresponding mechanical properties were investigated. For this purpose, 2 mm thick brass plate was friction stir welded at a rotational speed of 450 rpm and traverse speed of 100 mm/min. The microstructure of the joint was studied using optical microscopy, scanning electron microscopy equipped with electron back scattered diffraction system, and scanning transmission electron microscopy. The mechanical properties were measured using hardness and tensile tests. The formation of subgrains and their transformation into new grains in conjunction with existence of A{sub 1}{sup ⁎}, A{sub 2}{sup ⁎} and C texture components revealed that the continuous dynamic recrystallization plays a dominant role in the microstructural evolution. However, grain boundary bulging, along with the formation of twin boundaries, and presence of the G texture component showed that the discontinues dynamic recrystallization may participate in the new grain formation. Furthermore, the different strengthening mechanisms, which caused the higher strength of the joint, were discussed. - Highlights: •Microstructural evolution during FSW of a single phase brass was investigated. •CDRX and DDRX were the main mechanisms of the grain structure formation during FSW. •GDRX and SRX were not contributed in grain structure formation. •The lamellas TBs were formed in the SZ of the joints. •Grain boundary, dislocation, and texture effects resulted in higher strength.

36 MATERIALS SCIENCE↗

In situ investigation of the tensile deformation of laser welded Ti{sub 2}AlNb joints

The tensile deformation behavior of laser welded Ti{sub 2}AlNb joints was investigated using in situ analysis methods. The fracture mode of the single-B2-phase fusion zone was quasi-cleavage at room temperature and intergranular at 650 °C, while that of base metal was microvoid coalescence at both room temperature and 650 °C. Tensile deformation at room temperature was observed using in situ SEM tensile testing. In base metal, microcracks nucleated and propagated mainly within the O phase or along O/B2 phase boundaries. While both the cross- and multi-slips were found in the single-B2-phase fusion zone, a confocal laser scanning microscopy was used to observe the crack initiation and propagation process in situ at 650 °C. Cracks mainly formed along the B2/O phase boundaries in base metal, along the fragile grain boundaries of B2 phase in the fusion zone. The thermal simulation experiment and following TEM analysis indicated that the precipitation of continuous O-phase films along the B2 grain boundaries resulted in the high temperature brittleness of laser welded Ti{sub 2}AlNb joints. - Highlights: •Cracks formed within O phase or along B2/O boundaries in the base metal. •Cross- and multi-slips relieved stress in the fusion zone at room temperature. •Cracks mainly formed along the B2/O boundaries at 650 °C. •In the fusion zone, intergranular cracks were in situ observed at 650 °C. •O-phase films along B2 grain boundaries caused the high temperature brittleness.

36 MATERIALS SCIENCE↗

Microstructure of a safe-end dissimilar metal weld joint (SA508-52-316L) prepared by narrow-gap GTAW

The microstructure, residual strain and interfacial chemical composition distribution of a safe-end dissimilar metal weld joint (DMWJ, SA508-52-316L) prepared by narrow-gap gas-tungsten arc welding (NG-GTAW) were studied by optical microscope (OM) and scanning electron microscope equipped with an energy dispersive X-ray microanalysis (SEM/EDX) and an electron back scattering diffraction (EBSD) system. Complex microstructure and chemical composition distribution are found, especially at the SA508-52 interface and the 52-316L interface. In brief, a complicated microstructure transition exists within the SA508 heat affected zone (HAZ); the residual strain, the fraction of high angle random grain boundaries and low angle boundaries decrease with increasing the distance from the fusion boundary in 316L HAZ; neither typical type II boundary nor obvious carbon-depleted zone is found near the SA508-52 interface; dramatic and complicated changes of the contents of the main elements, Fe, Cr and Ni, are observed at the distinct interfaces, especially at the SA508-52 interface. No carbon concentration is found at the SA508-52 interface. - Highlights: •Residual strain and GBCD change as a function of the distance from FB in 316L HAZ. •Neither type II boundary nor obvious carbon-depleted zone is found in SA508 HAZ. •No carbon concentration is found at the SA508-52 interface. •The middle part of the DMWJ has the highest residual strain.

36 MATERIALS SCIENCE↗

Synchrotron experiment and simulation studies of magnesium-steel interface manufactured by impact welding

The effective weight reduction in the automotive industry by the wide adoption of lightweight magnesium (Mg) alloys demands high-quality joint between magnesium alloys and massively-used steels in order to wring the excess weight with strength and safety assurance. However, Mg-steel joint is difficult to achieve because there is no mutual solubility between magnesium and steel and huge disparity in physical properties. An impact-based welding method recently showed successful Mg-steel joining. In this work, the characteristics of Mg-steel interface joined by the impact welding method were investigated. Synchrotron high-energy X-ray computed tomography and diffraction were applied to characterize the microstructure across Mg-steel interface. Results revealed a deposit layer formed at the joint interface where Fe-rich particles spread deep into the Mg matrix. High-resolution 3D morphology of Mg-steel interface demonstrated the trapped pores and cracks inside the deposit layer. Finally, the formation of the deposit layer and the void/cracking evolution were analyzed by using finite element models. These findings provide insights into the immiscible Mg-steel joining process.

36 MATERIALS SCIENCE↗

Eutectic structures in friction spot welding joint of aluminum alloy to copper

A dissimilar joint of AA5083 Al alloy and copper was produced by friction spot welding. The Al-MgCuAl{sub 2} eutectic in both coupled and divorced manners were found in the weld. At a relatively high temperature, mass transport of Cu due to plastic deformation, material flow, and atomic diffusion, combined with the alloy system of AA5083 are responsible for the ternary eutectic melting.

36 MATERIALS SCIENCE↗

Features of the microstructure development under conditions, reproducing the process of friction stir welding. Molecular-dynamics study

Friction stir welding is a recently developed technology which is used in various branches of modern engineering. The basis of this technology is the friction of the rotating cylindrical or specially shaped tool between two metal plates brought together either to meet their ends of one above another with the overlap. When applying the FSW process in various economical sectors, the important task is to study the mechanisms and identify the physical laws and factors leading to formation of structural inhomogeneities and discontinuities in the weld seam. This paper analyzes the basic mechanisms behind the structural state generation in the material subjected to severe plastic deformation and heating. To investigate the atomic mechanisms of structural changes in FSW, the modeling at atomic scale has been carried out. Results of work can be a basis for new knowledge about the microstructure evolution in FSW.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Microstructure based modeling of friction stir welded joint of dissimilar metals using crystal plasticity

We report the friction stir welding (FSW) process shows promising results in joining dissimilar metals which are otherwise almost impossible to join using traditional welding techniques. Being a new technique, the deformation and the failure mechanism of the joints made by the FSW process needs to be investigated. In this work, a joint between AZ31 Mg alloy and DP590 steel is modeled using phenomenological crystal plasticity formulation on the mesoscale in the form of a representative volume element (RVE). The interface of the two materials is modeled using a cohesive zone model. A parametric study has been performed to understand the effect of grain size and interface fracture toughness as well as strength on the mechanical performance of the joint. It was found that the grain size of AZ31 Mg alloy, as well as DP590 steel, has little effect on the overall joint performance. On the other hand, interface fracture toughness and strength have a significant impact on the mechanical properties of the joint

36 MATERIALS SCIENCE↗

Ultrasonic Evaluation of Two Dissimilar Metal Weld Overlay Specimens

Two dissimilar metal weld (DMW) pipe-to-nozzle specimens were implanted with thermal fatigue cracks in the 13% to 90% through-wall depth range. The specimens were ultrasonically evaluated with phased-array probes having center frequencies of 0.8, 1.0, 1.5, and 2.0 megahertz (MHz). An Alloy 82/182 weld overlay (WOL) was applied and the specimens were ultrasonically re-evaluated for flaw detection and characterization. The Post-WOL flaw depths were approximately 10% to 56% through-wall. This study has shown the effectiveness of ultrasonic examinations of Alloy 82/182 overlaid DMW specimens. Phased-array probes with center frequency in the 0.8- to 1.0-MHz range provide a strong coherent signal but the greater ultrasonic wavelength and larger beam spot size prevent the reliable detection of small flaws. These small flaws had nominal through-wall depths of less than 15% and length in the 50-60 mm (2-2.4 in.) range. Flaws in the 19% and greater through-wall depth range were readily detected with all four probes. At the higher frequencies, the reflected signals are less coherent but still provide adequate signal for flaw detection and characterization. A single inspection at 2.0 MHz could provide adequate detection and sizing information but a supplemental inspection at 1.0 or 1.5 MHz is recommended.

36 MATERIALS SCIENCE↗

Friction Stir Processed Repair Welding of Dry Storage Canisters and Mitigation Strategies: Effect of Engineered Barrier Layer on Environmental Degradation

The proposed project aims to develop a friction sir based repair technique to heal cracks of stainless steel dry storage canisters (DSCs), created by the effect of stress corrosion cracking (SCC). In real service conditions, the welded parts of the canisters become prone to SCC under exposure to aggressive chemical environment. The focus of the project is on developing a mitigation strategy that can be implemented for countering SCC in DSCs following a two-pronged approach: (i) apply friction stir processing (FSP) as a crack repair technique while creating compressive residual stresses at the canister material surface, thus improving resistance against SCC; (ii) add molybdenum and/or nitrogen by friction stir based alloying process to create compositions that improve pitting resistance and thus enhance resistance against SCC. The specific project objectives are listed below: • Investigate FSW of 304L SS a potential repair welding technique of dry storage canisters; • Optimize the FSW parameters to introduce surface compressive stress profiles in the weldments; • Develop a FSP method to surface alloy the 304L with nitrogen and Mo by adding CrN and Mo powders; • Evaluate the surface compressive residual stress profile during FSW and FSP processes; • Evaluate the localized corrosion resistance of the FSW and FSP samples as a function of temperature, chloride concentration, and surface alloy composition; • Evaluate the SCC behavior of the FSW and FSP samples as a function of stress, chloride concentration, and temperature at different surface chemistries and induced residual stress profiles.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The Role of Friction Stir Welding in Nuclear Fuel Plate Fabrication

The friction bonding process combines desirable attributes of both friction stir welding and friction stir processing. The development of the process is spurred on by the need to fabricate thin, high density, reduced enrichment fuel plates for nuclear research reactors. The work seeks to convert research and test reactors currently operating on highly enriched uranium fuel to operate on low enriched uranium fuel without significant loss in reactor performance, safety characteristics, or significant increase in cost. In doing so, the threat of global nuclear material proliferation will be reduced. Feasibility studies performed on the process show that this is a viable option for mass production of plate-type nuclear fuel. Adapting the friction stir weld process for nuclear fuel fabrication has resulted in the development of several unique ideas and observations. Preliminary results of this adaptation and process model development are discussed.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Ultrasonic Spot Welding of AZ31B to Galvanized Mild Steel

Ultrasonic spot welds were made between sheets of 0.8-mm-thick hot-dip-galvanized mild steel and 1.6-mm-thick AZ31B-H24. Lap-shear strengths of 3.0-4.2 kN were achieved with weld times of 0.3-1.2 s. Failure to achieve strong bonding of joints where the Zn coating was removed from the steel surface indicate that Zn is essential to the bonding mechanism. Microstructure characterization and microchemical analysis indicated temperatures at the AZ31-steel interfaces reached at least 344 C in less than 0.3 s. The elevated temperature conditions promoted annealing of the AZ31-H24 metal and chemical reactions between it and the Zn coating.

36 MATERIALS SCIENCE↗

THE ROLE OF FRACTURE PROPERTIES ON LAP JOINT STRENGTH OF FRICTION STIR WELDED AA7055-T6 SHEETS

Friction stir lap welded (FSLW) joints have weight-saving potential in aluminum-intensive automotive assembly. However, FSLW also modifies the material microstructure close to the joint. Optimizing the FSLW process requires understanding the relationship between the strength and the joint's microstructure. In previous studies, efforts have been dedicated to determining the effects of local softening, the shape of the oxide line, and porosity. However, the impact of changes to the fracture properties on the joint's strength has not been studied. In this work, strength testing, and simulations, aided by material characterization, were used to determine the role of fracture properties on the shear strength of a 3-sheet (aluminum alloys 7055-7055-6022) lap joint. Characterization involved testing for fracture properties in the weld region. This data was then implemented into finite element simulations. As a result, the joint strength was predicted with a deviation of less than 6% from the experimental value. Comparison with strength prediction using only the base metal properties indicates that fracture property in the nugget region determines the strength of AA7055 FSLW.

Finite element analysis, Friction stir welding, ma↗