Improved primer for bonding polyurethane adhesives to metals

Primer ensures effective bonding integrity of polyurethane adhesives on metal surfaces at temperatures ranging from minus 423 degrees to plus 120 degrees F. It provides greater metal surface protection and bond strengths over this temperature range than could be attained with other adhesive systems.

Constanza, L. J.↗

High vacuum adhesion test apparatus.

Vacuum apparatus for measuring uniaxially loaded metal surfaces interfacial adhesion, showing surface oxide removal effectiveness influence in adhesion strength

Hordon, M. J.↗

Nondestructive sonic testing of adhesive-bonded composites

System detects and determines the location, depth, and areas of crushed core or of breaks in bonding between core and adhesive, adhesive and face sheet, or face sheet and external doubler. It is applicable to honeycomb panels of metal and/or plastics and to metal-to-metal laminates.

Caustin, E. L.↗

Nonflammable organic adhesives effective over wide temperature range

Series of highly fluorinated polyurethanes have been prepared as basis for development of nonflammable structural adhesives for use over wide temperature range. Backbone of polyurethanes is polyether of perfluoropropylene oxide. Adhesive system is developed that exhibits adequate strength properties and is self-extinguishing in oxygen-rich atmospheres.

Mc Leod, A.↗

Improvement of adhesive-bonded structural joints

Investigation is described of methods for obtaining uniform shear stress distribution in adhesives used in double-lap bonded joints. Design rules for reducing adhesive peak shear stresses are listed. Test results of an analysis of straight-lap joint design and stepped-lap joint design are given.

Evensen, H. A.↗

Instant acting adhesive system

Adhesive developes 80 percent of minimum bond strength of 250 psi less than 30 sec after activation is required. Adhesive is stable, handles easily, is a low toxic hazard, and is useful in industrial and domestic prototype bonding and clamping operations.

Davis, T. R.↗

Development of an adhesively bonded beryllium propulsion structure for the Mariner Mars 1971 spacecraft

The design, testing, and fabrication of the support truss structure for the propulsion system of the Mariner 9 spacecraft are described. Support is provided by an 8.9-kg (19.5-lbm) truss assembly consisting of beryllium tubes adhesively bonded to magnesium end fittings. Beryllium was selected for the tubular struts in the truss because of its exceptionally high stiffness-to-weight ratio. Adhesive bonding, rather than riveting, was utilized to join the struts to the end fittings because of the low toughness (high notch sensitivity) of beryllium. Magnesium, used in the end fittings, resulted in a 50% weight saving over aluminum since geometric factors in the fitting design resulted in low stress areas where magnesium's lower density is a benefit.

Stevens, J. H.↗

Effect of metallurgical structure and properties on adhesion and friction behavior of cobalt alloys

The metallurgical structure and some of the mechanical properties of two cobalt alloys, cobalt-50% iron and cobalt-25% molybdenum-10% chromium, were determined under various heat treated conditions. The mechanical properties of the bcc disordered Co-50Fe alloy, which was found to be very brittle, indicated an exceedingly low fracture strength, low hardness, and very weak grain boundary strength. Ordering by suitable heat treatment only produced a more brittle material with a lower fracture strength and a slightly higher hardness value. Work hardening was found to produce a finer grain structure and a greater grain boundary strength. Tensile properties were examined. It was found that the Co-25Mo-10Cr alloy was difficult to place in the alpha Co solid solution condition, which limited the ability to use precipitation as a hardening reaction. Over two hundred adhesion cycles from zero contact load, to maximum load, to fracture were conducted between couples for each of the above alloys in an ultrahigh vacuum system which would permit the sample surfaces to be cleaned of all contaminant layers. In the Co-50Fe case, the calculated fracture stress from the adhesion tests showed values in the range of 80 to 150 k.s.i., which is about ten times greater than the values from tension tests.

Keller, D. V., Jr.↗

Adhesive coating eliminated in new honeycomb-core fabrication process

Technique eliminates use of silicone-based adhesive material as bonding medium. Adhesive requires precise time-temperature cure. Prepreg resin is used as bonding medium, and each layer is laminated together to form honeycomb billet. Process can be used in any application where nonmetallic honeycomb core is being fabricated.

Batty, W. L.↗

The atomic nature of polymer-metal interactions in adhesion, friction and wear

Adhesion experiments with polytetra-fluoroethylene (PTFE) and polyimide contacting tungsten indicate that the polymers bond chemically to the clean metal surface. Polymer chain fragments which transfer to the surface of tungsten in field ion microscopy adhesion studies are highly oriented. Auger emission spectroscopy of PTFE transfer films to various metal surfaces indicates that the PTFE is bonded to the metal surface via the carbon atom. With PTFE in sliding contact with different orientations of aluminum, metal orientation is found to influence surfaces in sliding. The lowest friction and least amount of surface damage is detected on the highest atomic density (111) plane. The friction process itself can initiate polymer film formation from simple organic molecules.

Buckley, D. H.↗

Feasibility study for the development of low temperature curing adhesives

The feasibility of a new approach for the development of stable, easily handled, room temperature (293 K - 311 K) curing adhesives was studied and demonstrated. The work concentrated on a family of unsaturated amide/ester resins. Twelve candidate resins were synthesized and tested for completeness of cure at room temperature, adhesion to aluminum and titanium, shear strength, moisture resistance and heat stability. The three most promising candidate resins were selected and recommended for further development.

Green, H. E.↗

The effects of plasticity in adhesive fracture

An energy-balance analysis is presented for adhesive failure in end loaded cantilever beams. The analysis includes the effects of input work, stored strain energy, dissipated plastic energy, and specific adhesive surface energy. Experimental results obtained with 6061-T6 aluminum are presented as evidence for the validity of the approach.-

Chang, M. D.↗

Advances in the analysis and design of adhesive-bonded joints in composite aerospace structures

Several aspects of adhesive-bonded joint analysis and design are presented from the reference of size of structure or load intensity. This integrates the individual characterizations of double-lap, single-lap, stepped-lap, tapered-lap and scarf joints. The paper includes an overview of bonded joint selection from the standpoints of design, fabrication, and processing, each bearing in mind the influence of such considerations on the strength of the joint. A case study is presented of the optimization of a specific relatively thick titanium-to-graphite epoxy stepped-lap joint, using the digital computer analysis program A4EG. The factors accounted for are adhesive plasticity, adherend stiffness imbalance, adherend thermal mismatch, and change of material properties within the range of temperature environment and with load direction. The strength increases obtainable by refining the initial design are demonstrated.

Hart-Smith, L. J.↗