Search NASA⌕ Search

SEARCH · Search NASA

Results for “WELDING”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Development of Friction Stir Welding Technologies for In-Space Manufacturing

Friction stir welding (FSW) has emerged as an attractive process for fabricating aerospace vehicles. Current FSW state-of-the-art uses large machines that are not portable. However, there is a growing need for fabrication and repair operations associated with in-space manufacturing. This need stems from a desire for prolonged missions and travel beyond low-earth orbit. To address this need, research and development is presented regarding two enabling technologies. The first is a self-adjusting and aligning (SAA) FSW tool that drastically reduces the axial force that has historically been quite large. The SAA-FSW tool is a bobbin style tool that floats freely, without any external actuators, along its vertical axis to adjust and align with the workpiece s position and orientation. Successful butt welding of 1/8 in. (3.175 mm) thick aluminum 1100 was achieved in conjunction with a drastic reduction and near elimination of the axial process force. Along with the SAA-FSW, an innovative in-process monitor technique is presented in which a magnetoelastic force rate-of-change sensor is employed. The sensor consists of a magnetized FSW tool that is used to induce a voltage in a coil surrounding the tool when changes to the process forces occur. The sensor was able to detect 1/16 in. (1.5875 mm) diameter voids. It is concluded that these technologies could be applied toward the development of a portable FSW machine for use in space.

42 ENGINEERING↗

Prediction of hardness minimum locations during natural aging in an aluminum alloy 6061-T6 friction stir weld

This study describes a simple model that can predict the evolution of hardness distribution as a function of natural aging time in a heat-treatable 6061-T6 Al alloy plate subjected to friction stir welding (FSW). First, two dimensional thermal distributions were simulated as a function of time in the FSW plate by finite element modeling. Second, the hardness changes during natural aging were measured as a function of aging time for a number of Al specimens that had been previously isothermally heat-treated to different hold temperatures in order to determine the natural aging kinetics. Finally, the simulated temperature profiles and the natural aging kinetics were correlated to predict the hardness profiles in the FSW plate. The predicted hardness variations are consistent with measured hardness profiles in that the location of minimum hardness moves away from the centerline as the aging time and/or heat input increases. The hardness variation was also related to the location of failure in cross-weld tensile samples.

36 MATERIALS SCIENCE↗

Analysis on the Fracture of Al-Cu Dissimilar Materials Friction Stir Welding Lap Joint

Friction stir welding (FWS) is regarded as a more plausible alternative to other welding methods for Al-Cu dissimilar joining. However, the structure of an FSW joint is different from others. In this study, lap joints of 6061 aluminum alloy and commercially pure copper were produced by FSW, and the effects of rotation rate on macromorphology, microstructure and mechanical properties were investigated. In addition, a fracture J integral model was used to analyze the effect of microstructure on the mechanical properties. The results revealed that the macrodefect-free joints were obtained at a feed rate of 150 mm/min and 1100 rpm and that the failure load of the joint reached as high as 4.57 kN and only reached 2.91 kN for the 900 rpm, where tunnel defects were identified. Particle-rich zones composed of Cu particles dispersed in an Al matrix, and “Flow tracks” were observed by the EDS. The J integral results showed that the microdefects on the advancing side cause serious stress concentration compared with the microdefects located on the Al-Cu interface, resulting in the fracture of the joints.

36 MATERIALS SCIENCE↗

The Effect of SiC Addition on Microstructure and Mechanical Properties of Gas Tungsten Arc-Welded Ti-6Al-4V Alloy

In the present study, SiC powder was added in situ for bead-on-plate weldments and fusion butt joints to modify the microstructure and the corresponding mechanical properties. Cross sections of bead-on-plate welds demonstrated that the SiC addition resulted in significant changes of the titanium microstructure. Specifically, a fine lamellar structure of α-phase with a small amount of intergranular β-titanium within the fusion zone could be established. Moreover, the size of prior β-grains was significantly reduced. After welding, no intermetallic silicides were observed. In the fusion zone of the SiC-enhanced samples, a small increase in hardness resulted, and the samples showed an increase in tensile strength, yield strength and elongation.

36 MATERIALS SCIENCE↗

Microstructure and Properties of 5083 Al/1060 Al/AZ31 Composite Plate Fabricated by Explosive Welding

A 5083 Al/1060 Al/AZ31 composite plate was fabricated by explosive welding. The microstructure and properties of the composite plate were investigated after explosive welding. The results showed that all bonding interfaces were wavy interfaces. With an increasing distance from the detonation point, the wavelength and the amplitude also increased. The EDS results indicated that a 5-μm diffusion layer was observed at the 1060 Al/AZ31 layer, including the Mg{sub 2}Al{sub 3} phase. Adiabatic shear bands and twin structures were observed in AZ31. The shear bond strength of the 5083 Al/1060 Al interface was 60 MPa, and the shear bond strength of the 1060 Al/AZ31 interface was 84 MPa.

36 MATERIALS SCIENCE↗

In Situ SEM Observations of Fracture Behavior of Laser Welded–Brazed Al/Steel Dissimilar Joint

Laser welding–brazing of 6061-T6 aluminum alloy to DP590 dual-phase steel with Al-Si12 flux-cored filler wire was performed. The microstructure at the brazing interface was characterized. Fracture behavior was observed and analyzed by in situ scanning electron microscope. The microstructure of the brazing interface showed that inhomogeneous intermetallic compounds formed along the thickness direction, which had a great influence on the crack initiation and propagation. In the top region, the reaction layer at the interface consisted of scattered needle-like Fe(Al,Si){sub 3} and serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the middle region, the compound at the interface was only serration-shaped Fe{sub 1.8}Al{sub 7.2}Si. In the bottom region, the interface was composed of lamellar-shaped Fe{sub 1.8}Al{sub 7.2}Si. The cracks were first detected in the bottom region and propagated from bottom to top along the interface. At the bottom region, the crack initiated and propagated along the Fe{sub 1.8}Al{sub 7.2}Si/weld seam interface during the in situ tensile test. When the crack propagated into the middle region, a deflection of crack propagation appeared. The crack first propagated along the steel/Fe{sub 1.8}Al{sub 7.2}Si interface and then moved along the weld seam until the failure of the joint. The tensile strength of the joint was 146.5 MPa. Some micro-cracks were detected at Fe(Al,Si){sub 3} and the interface between the steel substrate and Fe(Al,Si){sub 3} in the top region while the interface was still connected.

36 MATERIALS SCIENCE↗

Evaluating the Electrochemical Behavior of Friction Stir-Welded AA2219-O Alloy Joint in 3.5% NaCl Solution

Single-pass friction stir welding of AA2219-O aluminum alloy was carried out at high rotation speed (1180 rpm), and transverse travel rate of 33.5 mm/min was selected. The microstructural, mechanical and electrochemical characteristics of the weldment are investigated in this study. The high rotational tool speed resulted in a less uniform distribution of the intermetallic θ-phase (CuAl{sub 2}) in the thermo-mechanically affected zone (TMAZ) than in the weld nugget zone (WNZ). The higher transfer coefficient and lower charge transfer resistance (R{sub ct} + R{sub θ}) were observed in case of TMAZ as evaluated from potentiodynamic polarization and impedance spectroscopy, respectively. These results confirmed that microstructural variations could deteriorate the electrochemical performance of the weldment. TMAZ provided the least corrosion resistance than the base metal (BM) and WNZ due to the high concentration of cathodic intermetallic particles and possibly due to the large mechanical distortion of the grain structure.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Rapidly Cooled Friction Stir Welded Ti-6Al-4V Alloys

Two mm-thick Ti-6Al-4V alloy plates were friction stir butt welded under natural- and rapid-cooling conditions. The microstructures and mechanical properties of joints were investigated and compared. The rapid cooling via spraying cooling liquid nitrogen on the plate top surface was beneficial to obtaining a narrower cross section and finer and more uniform grains in the stir zone than those obtained by natural cooling. Joint tensile strength of 1021 MPa and elongation of 1.88% under the rapid-cooling condition respectively reached 102.7 and 150.4% of those under the natural-cooling condition, respectively. The uniform-and-compact equiaxed grains led to equiaxed dimples on the fracture surface, which demonstrated a ductile fracture of the welding joints.

36 MATERIALS SCIENCE↗

Microstructures and Mechanical Properties of Resistance Spot-Welded Steel/Aluminum Alloy Joints with Process Tapes

The microstructure and mechanical property of resistance spot-welded joints of steel and aluminum were studied by using process tapes. The steel/aluminum joint consists mainly of aluminum nugget and interface zone. The liquid nugget solidification has an epitaxial growth characteristic, and the interface zone displays a double-layer structure, Fe{sub 2}Al{sub 5} layer at steel side and Fe{sub 4}Al{sub 13} layer at aluminum nugget side. Compared with joints without process tape, the joint nugget diameter and tensile shear load increased by 35.45 and 10.98%, respectively, and its indentation ratio decreased by 56.25% due to the process tapes increasing heat input, producing larger nugget diameter and continuous interface layer, and protecting against deep indentation. The joining area of intermetallic layer and aluminum nugget is weak link in the joint. It is favorable to use the process tapes for improving welding quality, raising joint strength, and energy saving.

36 MATERIALS SCIENCE↗

Effects of Rotation Speed on Microstructure and Mechanical Properties of 2060 Al-Cu-Li Alloy in Friction Stir Welding

Microstructural and mechanical properties of 2.0-mm-thick 2060 Al-Cu-Li alloy joints obtained at different rotation speeds were assessed in this study. The rotation speeds ranged from 400 to 1300 rpm, with welding speed kept at a constant value of 100 mm/min. With the increase in rotation speed, grain coarsening occurred while the density of precipitation decreased in the stir zone (SZ), and great amounts of the Al{sub 2}CuLi and Al{sub 2}Cu phases were dissolved while only small amounts of the Al{sub 3}Zr and Al{sub 3}Li phases remained. The lowest hardness was found at the interface between the heat-affected zone (HAZ) and thermo-mechanically affected zone (TMAZ); the average hardness value of SZ increased, while the lowest hardness moved in the direction away from the center of joints. The ultimate strength (UTS) of weld first increased rapidly and then slowly decreased as rotation speed increased, with a maximum value of 443 MPa obtained at a rotation speed of 600 rpm, reaching 83.58% of the base metal (BM) strength. Three fracture modes were established to illustrate the growth mechanism of the crack. Analysis of the fracture surface showed that insufficient materials flowed and coarsened secondary phases caused the joint fracture.

36 MATERIALS SCIENCE↗

Influence of Annealing on the Properties of Explosively Welded Titanium Grade 1—AW7075 Aluminum Alloy Bimetals

Explosive welding of titanium Grade 1 to AW7075 aluminum alloy arranged in parallel setup was performed. The annealing of produced bimetals at the temperatures of 450, 500 and 550 °C for times ranging from 20 to 100 h was carried out after explosive welding. The produced bimetal was characteristic by its wavy interface typical for that bonding process. Increase in the microhardness at the interface was recorded due to work hardening. Delamination of titanium Grade 1 flyer sheet was firstly observed when annealing temperature of 500 °C for 40 h was carried out. Annealing at 550 °C also resulted in delamination of upper sheet. The intermetallic compound (IMC) layer was observed at the interface after annealing of bimetals. The higher the annealing temperature and time, the higher the thickness of continuous IMC layer. The maximum measured thickness of IMC layer averaged 13 µm. Energy dispersive x-ray spectroscopy (EDS) and x-ray diffraction (XRD) analyses revealed that the interface layer is consisted of Al{sub 18}Ti{sub 2}Mg{sub 3} IMC. Microhardness at the interface increased dramatically up to 439 HV0.1 after annealing of bimetal due to the presence of above-mentioned IMC.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Exothermic-Reaction-Assisted Friction-Stir-Welded Nickel-Aluminum Bronze Alloy

In the present work, nickel-aluminum bronze alloy is joined using conventional friction stir welding (CFSW) and thermite heat-assisted friction stir welding (THAFSW). In this experiment, preheating technology was utilized using the thermite reaction of Al-CuO powder. A substantial rise in temperature was observed during THAFSW which is beneficial to the eliminations of tunnel defect. In THAFSW, a large amount of α-phase was observed from the top to the center in stir zone as a result of the rise in temperature. Transverse tensile strength of the THAFSW and CFSW was improved by 27 and 14%, respectively, in comparison with base metal tensile strength. A higher microhardness values observed at the bottom of the stir zone in the THAFSW, while this was seen higher in the surface zone and the center zone in the case of CFSW. Tool wear was reduced during the THAFSW process.

36 MATERIALS SCIENCE↗

Numerical Simulation of Residual Stresses in Multipass Gas Metal Arc-Welded Joints of Thick Aluminum Alloy Plates

Numerical simulation was utilized to investigate the residual stresses in the multipass gas metal arc-welded joints of high-strength Al-Zn-Mg alloy plates. In order to elevate the reliability of numerical simulation, the heat source model, parameters characterizing the thermal and mechanical properties, boundary conditions, material constitutive model and finite element meshing were discussed in detail. As a novelty of this paper, the modified Arrhenius constitutive equation of the base material and the filled material was obtained according to the results of high-temperature tensile tests. Distributions of stress on the upper and bottom surface of the joint were obtained based on numerical simulation. Special attention was paid to the evolutions of local residual stress on the bottom surface of the joint, and it’s found that residual stresses on the bottom surface of the joint were almost unchanged after the weld seam approached a certain thickness. Blind-hole method and x-ray method were adopted to detect the residual stresses on the surfaces to verify the accuracy of the results obtained by numerical simulation.

36 MATERIALS SCIENCE↗

Numerical Simulation of Residual Stress for Laser Welding of Ti-6Al-4V Alloy Considering Solid-State Phase Transformation

In the present work, a thermal-metallurgical-mechanical model which considered the influence of phase transformation was used to predict the residual stress field of Ti-6Al-4V after laser welding. In this model, the Johnson–Mehl–Avrami equation was used to predict diffusional solid-state phase transformations: α phase to β phase during heating and β phase to α phase during cooling. The Koistinen–Marburger equation was used to predict diffusionless solid-state phase transformation of β phase to martensite during cooling. The properties of material were obtained using a mixing rule based on the phase fraction and the property of each pure phase. By applying this model, the effect of solid-state phase transformations of Ti-6Al-4V alloy on temperature field and stress field during laser welding was considered in the simulation. In addition, experiments were carried out for comparison, which significantly verified the accuracy of the applied model.

36 MATERIALS SCIENCE↗

Butt Laser Welding–Brazing of AZ31 Mg to Nickel-Coated Ti-6Al-4V

Mg and Ti alloy are hard to be bonded due to their huge discrepancy in physical and metallurgical characteristics. As an intermediate element, Ni is feasible for joining of Mg and Ti. The interfacial microstructure and mechanical properties of laser-welded–brazed AZ31 Mg/Ti-6Al-4V joints in butt configuration were investigated with different thicknesses of electrodeposited Ni interlayer. The interfacial reaction products evolved from an ultra-thin Ti{sub 3}Al layer to Ti{sub 2}Ni layer mingled with Ti{sub 3}Al, and more Mg{sub 3}AlNi{sub 2} compounds were produced in the fusion zone (FZ) as Ni coating thickness increased. Slag inclusions and cracks were observed in interfacial layer when coating thickness exceeded 2.5 μm. The quantity of Mg{sub 3}AlNi{sub 2} and the thickness of interfacial layer decreased from the top to bottom of groove of the same joint owing to high thermal gradient during laser welding. The chemical potential of Al and Ni indicated that Al-Ti reaction product was produced more easily than Ni-Ti in 0.001Mg-(Ni-Al-Ti) system. The thermodynamic calculation results of Gibbs free energy suggested the preferential formation Ti-Al phase and Ti-Ni phase along the interface while the Mg-Al-Ni ternary phase in the FZ. Fracture loads of joints increased first followed by a decline with the increase in coating thickness. The joint fractured at the Mg base metal, reaching a maximum value of 3900 N with the Ni coating thickness of 1.5 μm. In the case of using thinner or thicker Ni coating, crack propagated along the interface due to the insufficient metallurgical bonding or defects existed in the interfacial layer. The characteristic of fracture surface changed from the tear ridges and terraces to river pattern when interfacial failure occurred.

36 MATERIALS SCIENCE↗

Effect of a Zinc Interlayer on a Cu/Al Lap Joint in Ultrasound-Assisted Friction Stir Welding

This study proposes a welding process, ultrasound-assisted friction stir welding of dissimilar Al/Cu metals. Zinc foil is melted using the heat generated by a pinless stirring tool, and the molten intermediate layer is stirred by ultrasonic cavitation to achieve an effective connection. The metallurgical reaction behavior of the joint under the action of the sound field was studied, and the effects of different microstructures on the joint performance were analyzed. Specifically, the following observations were reported in this study: (1) When ultrasound assistance was used, the cavitation effect changed the brittle intermetallic compounds of Al{sub 2}Cu from a continuous distribution to a block distribution, and the mechanical properties of the joint were greatly improved; (2) the effects of the thickness of the zinc were also determined. The results showed that the highest shear tensile force was obtained when the thickness of the zinc foil was 0.2 mm. When the thickness was 0.3 mm, the ultrasound effect was weakened. The copper-side interface generated a zigzag-shaped Al{sub 4.2}Cu{sub 3.2}Zn{sub 0.7} layer with a thickness of 3.4 μm and had a continuous distribution. Increasing the thickness of the zinc to 0.5 mm, however, drastically decreased the mechanical properties of the joint due to incomplete melting of the zinc layer.

36 MATERIALS SCIENCE↗

Effects of Postweld Heat Treatment on Microstructure and Properties of Laser-Welded Ti-24Al-15Nb Alloy Joint

The microstructure evolution and mechanical properties of laser-welded joints of Ti-24Al-15Nb alloy under different postweld heat treatment (PWHT) conditions were systematically investigated. The results show that the microstructure is very sensitive to PWHT temperatures. The weld zone consists of B2 and O phases after PWHT. With the PWHT temperatures increasing from 850 to 1000 °C, the amount of O phase decreases gradually, while the grains of O precipitates become coarser. After PWHT, there are some thin acicular O precipitates in heat-affected zone (HAZ), and the decomposition of α{sub 2}-phase caused by niobium diffusion can be observed in the HAZ. The PWHT can significantly increase the microhardness of joints, resulting from O phase precipitation hardening effect. The tensile strength and elongation of joints can be remarkably improved after PWHT, which was closely related to the strengthening effect of O precipitates and slip transmission between O and B2 phases. In addition, the results indicate that the best mechanical properties can be achieved only when the number and size of O phase and B2 phase are the best match.

36 MATERIALS SCIENCE↗

Neutron Diffraction Residual Stress Study of a AA2219-T87 Self-Reacting Friction Stir Weld

2219-T87 is a precipitation hardenable aluminum-copper alloy which sees wide use in structural aerospace components. Thick panels of this alloy are joined via self-reacting friction welding (SRFSW); however, this thermomechanical process can result in significant loss of the alloy’s strengthening precipitates and large residual stresses which are detrimental to mechanical behavior and performance. High-resolution maps of the residual strain and stress states along the normal, transverse, and longitudinal directions of 2219-T87 SRFSW were obtained using neutron diffraction measurements. Residual stress had the highest tensile value in the heat-affected zone (HAZ) and the largest compressive stress in the base metal region of the normal and transverse directions. Line profile residual stress distributions displayed an “M”-shaped distribution in each direction with the longitudinal direction being the most pronounced while 2D residual stresses displayed an hourglass-shaped pattern. Further, average maximal longitudinal residual stress values ranged from 60.6 to 85.6% of yield. Microhardness testing across the transverse weld section produced a “V”-shaped curve with slight hardness recovery in the stir zone. Maximal and minimal microhardness values were observed in the base metal (154 HV) and thermomechanically affected zone (82 HV), respectively. Microstructural evolution was recorded using optical microscopy and showed decreasing grain size from the HAZ to the stir zone.

36 MATERIALS SCIENCE↗