Search NASA⌕ Search

SEARCH · Search NASA

Results for “sintering”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 775 records · Page 43

Impact of electrode porosity architecture on electrochemical performances of 1 mm-thick LiFePO4 binder-free Li-ion electrodes fabricated by Spark Plasma Sintering

Thick electrodes with high active material loadings have been intensively studied over the last couple of decades in pursuit of achieving high energy density systems. To optimize and enhance the electrochemical performance of such electrodes, one has to control the pore morphology by, for example, varying the pore size and shape, and the level of porosity. In the present work, the fabrication of thick binder-free LiFePO4 (LFP) electrodes with two different pore sizes (12 and 20 mu m) and porosities (21 vol% and 44 vol%) using Spark Plasma Sintering (SPS) and templating approach is reported. The well-controlled porous architecture inside the thick electrodes is realized by fine-tuning experimental parameters. The impact of porosity architecture on electrochemical performance is quantified and correlated with the 3D tortuosity values determined from both micro-computed tomography and electrochemical impedance-based experimental methods. Based on the micro-computed tomography data analysis, estimated tortuosity values along X, Y, and Z axes reveal an anisotropic effect perpendicularly to the SPS compression axis (Z-direction). This is particularly profoundly observed in the samples with larger pores (20 mu m). The correlation between morphological properties and the rate capability performance is established indicating that the capacity loss happens mainly due to the Li-ion diffusion limitations.

Cathode material↗

Enhanced thermoelectric properties of bismuth sulfide polycrystals prepared by mechanical alloying and spark plasma sintering

Bismuth sulfide powders were synthesized by mechanical alloying (MA) and then consolidated by spark plasma sintering (SPS) technique. In order to improve the electrical transport properties of bismuth sulfides, the carrier concentration was optimized by modifying chemical composition of sulfur through producing sulfur vacancies, and the carrier mobility was enhanced by a two-step SPS as a hot-forging process through increasing grain orientation. The electrical resistivity of bismuth sulfides was reduced to 10{sup -4} from 10{sup -2} {omega} m by optimizing sulfur content, and further lowered by hot-forging, whereby the power factor was significantly increased from 91 to 254 {mu}W/mK{sup 2}. The hot-forged Bi{sub 2}S{sub 2.90} sample showed the highest ZT=0.11 (at 523 K), which is higher than the reported value. The present work revealed that bismuth sulfide compounds as a promising candidate of thermoelectric materials can be synthesized by a simple process. - Abstract: Electrical properties of bismuth sulfides were improved by optimizing carrier concentration through modifying compositions of sulfur and enhancing carrier mobility through SPSed hot-forging. The ZT value of 0.11 was obtained, which is the maximum reported so far . Display Omitted.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Characterization using thermomechanical and differential thermal analysis of the sinterization of Portland clinker doped with CaF{sub 2}

In this work, the sintering process of Portland cement was studied by combining thermomechanical analysis (TMA) and differential thermal analysis (DTA), together with X-ray diffraction (XRD) and scanning electron microscopy (SEM). Thermal analysis results employing both techniques indicted that phase transformations appeared at lower temperatures when CaF{sub 2} was incorporated in the raw materials. Besides, it was observed at high temperature that in some phase transformations TMA conducts to better resolution compared with the DTA measurements. Furthermore, mechanical properties and X-ray diffraction patterns corroborate the TMA and DTA results, corroborating that the final amount of alite (Ca{sub 3}SiO{sub 5}) is higher when a certain amount of CaF{sub 2} was present during the clinkerization process.

36 MATERIALS SCIENCE↗

Investigation of deformation micro-mechanisms in nickel consolidated from a bimodal powder by spark plasma sintering

Bulk polycrystalline nickel compact was processed by spark plasma sintering from heterogeneous powder consisting of a mixture of nanometer and micrometer sized particles. The consolidated samples inherited the bimodal structure of the starting powder and was composed of ~ 55 vol.% coarse-grained (with the grain size larger than 1 μm) and ~ 45 vol.% ultrafine-grained (with an average grain size of ~ 550 nm) components. The deformation mechanisms were established by EBSD, X-ray line profile analysis and in-situ TEM observations. In the ultrafine-grained volume, the deformation occurred mainly through the activation of dislocation sources emitting full or partial dislocation either from grain interior or grain boundaries. Besides dislocation activity, rolling and sliding of nanograins were also observed during deformation by in-situ transmission electron microscopy, which have a considerable contribution to the observed high strain rate sensitivity of the bimodal microstructure. The cracks formed during deformation easily propagated in the nanograin regions due to the weaker particle bonding caused by the relatively high fraction of native oxide layer on the surface of the initial nanoparticles. - Highlights: • Bulk bimodal polycrystalline Ni was processed by SPS from a heterogeneous powder. • High SRS of the flow stress was observed which enhanced ductility and strength. • In-situ TEM revealed dislocation sources inside and at the boundaries of UFGs. • Twinning, partial dislocation and NG rolling were observed at crack tip vicinity. • The high SRS pertained to both dislocation activity in CG and NG rolling.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

The distribution and mechanism of pore formation in copper foams fabricated by Lost Carbonate Sintering method

In this research, utilizing X-ray computed tomography (XCT), geometrical characterization, and pore formation mechanisms of highly porous copper foams manufactured by powder metallurgical (PM) process are investigated. Open-cell copper foams with porosity percentages of 60% and 80% and with a pore size within the range of 300–600 μm were manufactured by using potassium carbonate as a space holder agent via the Lost Carbonate Sintering (LCS) technique. XCT and SEM were also employed to investigate the three-dimensional structure of foams and to find the effect of the parameters of the space holders on the structural properties of copper foams. The result showed an excellent correlation between the structural properties of the foams including the size and shape of the pores, porosity percentage, volume percentage, particle size, and the shape of the sacrificial agent used. Also, the advanced image analysis of XCT images indicated fluctuations up to ± 10% in porosity distribution across different cross-sections of the foams. Simultaneous thermal analysis (STA: DTA–TG) was also used to study the thermal history of the powders used during the manufacturing process of the foams. The results indicated that the melting and thermal decomposition of the potassium carbonate occurred simultaneously at 920 °C and created the porous structure of the foams. By combining the STA result with the result of the tension analysis of cell walls, the mechanisms of open-pore formation were suggested. In fact, most open pores in the samples were formed due to the direct contact of potassium carbonate particles with each other in green compact. Also, it was found that the thermal decomposition of potassium carbonate particles into gaseous CO{sub 2} led to the production of gas pressure inside the closed pores, which eventually caused the creation of cracks on the cell walls and the opening of the pores in foam's structure. - Highlights: • Structural characterization of copper foam produced by LCS method is investigated by tomography images. • The ability of LCS technique to control structural features of produced foams was proved. • The mechanisms of open pores formation were presented.

36 MATERIALS SCIENCE↗

Effect of ZnO addition on the sintering and electrical properties of (Mn,W)-doped PZT-PMS-PZN ceramics

The effect of ZnO addition on the phase structure, microstructure and dielectric and piezoelectric properties of 0.2 wt.% MnO{sub 2} and 0.6 wt.% WO{sub 3}-doped Pb(Zr{sub 0.52}Ti{sub 0.48})O{sub 3}-Pb(Mn{sub 1/3}Sb{sub 2/3})O{sub 3}-Pb(Zn{sub 1/3}Nb{sub 2/3})O{sub 3} (PZT-PMS-PZN) ceramics was investigated. X-ray diffraction shows that the phase structure of ceramics is transformed from rhombohedral to tetragonal with the increasing of ZnO addition. The bulk density significantly increases when ZnO is added and then it slightly decreases for ZnO addition above 0.2 wt.%. SEM micrographs show the grains of ceramics are uniform and well developed by adding 0.1 wt.% ZnO. The Curie temperature (T{sub c}) of 270 deg. C is obtained at the 0.1 wt.% ZnO addition. Mechanical quality factor (Q{sub m}), electromechanical coupling factor (K{sub p}) and piezoelectric constant (d{sub 33}) increase firstly, and then decrease with the increasing of ZnO addition, while dielectric loss tan {delta} drops all the time. The Q{sub m}, K{sub p}, d{sub 33}, tan {delta} and T{sub c} of the ceramics show the optimum values of 1899, 0.55, 300 (pC/N), 0.0063 and 270 deg. C, respectively, at the lower sintering temperature of 1120 deg. C and with 0.1 wt.% ZnO addition.

36 MATERIALS SCIENCE↗

Dislocation density in fine grain-size spark-plasma sintered aluminum measured using high brightness synchrotron radiation

In this study, three-dimensional orientation mapping of samples of aluminum prepared by spark plasma sintering (SPS) with average grain sizes of 5 μm and 1 μm has been carried out using high-brightness synchrotron radiation, from which the geometrically necessary dislocation (GND) density has been determined. The low average measured GND density values confirm that the SPS process can be used to produce samples containing grains with dislocation density similar to that of fully recrystallized coarse-grained samples. Values of GND density are also compared to those obtained from electron back-scatter diffraction studies on the same material, highlighting the significantly higher angular resolution of the synchrotron data. For the 5 μm grain-size sample the measured GND density can account for a large fraction of the previously observed positive Hall-Petch deviation of this material. For the 1 μm grain-size sample, however, the GND-based strengthening contribution is much smaller than the reported positive Hall-Petch deviation, such that the additional strength may be reliably associated with dislocation source-limited strengthening.

36 MATERIALS SCIENCE↗

Solid-state reaction mediated microstructural evolution in a spark plasma sintered in situ Ti–B 4 C composite

For this study, a novel porosity-free in situ Ti–B 4 C composite was fabricated via spark plasma sintering (SPS). Detailed analysis of the phase evolution, coupling results from XRM, XRD and SEM-EBSD-EDS, indicate that primarily TiB 2 precipitates formed due to the in-situ reactions between the boron-carbide and titanium powders. The precipitation of TiB 2 resulted in the formation of a graphitic C-rich thin layer circumscribing the partially reacted B 4 C particles. Further progression of the in-situ reaction leads to the out-diffusion of the excess carbon from the B 4 C particles, across the graphite and TiB 2 phases, forming TiC upon reacting with the titanium matrix. Therefore, the final microstructure primarily consisted of TiB 2 , TiC, and partially reacted B 4 C phases, with small amounts of TiB, α-Ti, and graphite. Furthermore, the microstructure in these SPS processed in situ composites appeared to be the product of a solid-state Ti–B 4 C diffusion couple, substantially different from their fusion-based additively manufactured counterparts. Nano-indentation tests revealed a remarkably high average hardness of ~25 GPa for this SPS-processed Ti–B 4 C composite and comparable (with literature) phase-specific hardness and modulus values for the constituent TiB 2 , TiC, and B 4 C phases.

36 MATERIALS SCIENCE↗

Electric-field-assisted-sintering of rare-earth oxide dispersion strengthened Fe-Cr-Mo alloys

Oxide dispersion-strengthened (ODS) alloys are widely recognized for their exceptional high-temperature strength, creep resistance, and radiation tolerance, making them indispensable for advanced nuclear reactors, aerospace, and energy systems. Achieving a fine and stable dispersion of oxide nanoparticles is critical, as these particles act as strong barriers to dislocation motion and effective sinks for irradiation-induced defects, ensuring structural integrity under extreme conditions. Here, in this study, Fe–Cr–Mo-based ODS alloys were fabricated via mechanical alloying and consolidated using electric-field-assisted sintering (EFAS) with additions of Y 2 O 3 , La 2 O 3 , and CeO 2 . EFAS processing produced ultrafine-grained microstructures (average grain size <1 μm) with uniformly distributed oxide clusters (2–4 nm). Atom probe tomography revealed that La 2 O 3 -containing alloys exhibited the highest nanoparticle number density, resulting in superior tensile strength compared to yttria- and ceria-bearing counterparts. The combined effect of grain refinement and rare-earth oxide dispersion significantly enhanced mechanical performance, demonstrating the potential of EFAS for developing high-strength ferritic alloys for demanding environments such as nuclear systems.

36 - MATERIALS SCIENCE↗

Amorphous complexion-aided sintering enables scalable processing of bulk nanocrystalline Cu-Zr with high strength and compressive plasticity

Nanocrystalline alloys can have exceptional strengths, yet due to limited microstructural stability it is difficult to fabricate bulk pieces through traditional processing routes that retain nanosized grains. In this study, centimeter-sized Cu-Zr alloy pellets were fabricated via a simple and improved powder metallurgy processing route. Different consolidation temperatures and times were employed to investigate the effect of amorphous grain boundary complexions on densification and the resulting mechanical properties. Bulk compression tests were carried out, with the samples that were hot pressed at 900 °C for 10 h exhibiting an excellent combination of average yield strength of 722 ± 45 MPa and average failure strain of 25.3 ± 2.4 %. Furthermore, we find that a powder processing route which enables amorphous complexion-assisted sintering leads to samples that (1) reach full density without requiring quenching treatments or other complex processing, (2) demonstrate appreciable plasticity, and (3) have strength that competes with commercially available high-strength Cu alloys.

Bulk nanocrystalline alloy↗

Radiative Properties of Coal Ash Deposits with Sintering Effects

The heat-transfer characteristics in the fireside of a pulverized-coal furnace are affected, among other factors, by the physical and chemical characteristics of the ash deposits. Indeed, the physical state of the ash deposits and their chemical composition determine the radiative and conductive properties of the furnace walls. Particularly, several complex mechanisms are involved in the radiative heat-transfer process at the walls that restricts the absorption of the incident radiation of the flame, particles, and hot gases. These mechanisms involve dependencies on the radiation spectrum due to the ash chemical composition and ash-sintering effects that enhance or hinder the overall heat transfer. In this work, the complex mechanisms that describe the heat exchange in the presence of ash deposits and their impact on the prediction of the wall emissivity and ultimately the wall heat transfer in a real system are discussed.

01 COAL, LIGNITE, AND PEAT↗

Pelletization with Spark Plasma Sintering and Characterization of Metal Iodides: An Assessment of Long-Term Radioiodine Immobilization Options

Four promising iodine “getter” materials (Ag, Cu, Bi, and Sn) for radioiodine capture were assessed in their pure metal-iodide (MI x ) pelletized forms to compare relative chemical durabilities. To study chemical durability, commercial MI x compounds of AgI, BiI 3 , BiOI, CuI, and SnI 4 were converted to dense monolithic pellets using spark plasma sintering. Semidynamic leach testing in the form of modified ASTM C1308 tests was then performed on the pellets in two different forms including unmounted (as-pressed) specimens (i.e., “U”) and epoxy-mounted specimens (i.e., “M”) with polished surfaces. The chemical durability results and sample characterizations showed that three of the five MI x compounds tested (i.e., AgI, CuI, and BiOI) displayed moderate to high leach resistances. Further, the remaining two MI x compounds (i.e., BiI 3 and SnI 4 ), which are both desirable iodine waste forms due to their high iodine loading capacities, readily decomposed during leach testing, indicated by crystallographic changes in the specimens as well as large amounts of iodine detected in the leachate solutions. The instabilities of BiI 3 and SnI 4 raise uncertainties for using the base metals/cations (i.e., Bi 0 /Bi 3+ and Sn 0 /Sn 4+ , respectively) as viable getters for radioiodine capture due to likely poor waste form chemical durabilities after capture and consolidation into waste forms.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Toward the Design of a Hierarchical Perovskite Support: Ultra-Sintering-Resistant Gold Nanocatalysts for CO Oxidation

We report that an ultrastable Au nanocatalyst based on a heterostructured perovskite support with high surface area and uniform LaFeO 3 nanocoatings was successfully synthesized and tested for CO oxidation. Strikingly, small Au nanoparticles (4–6 nm) are obtained after calcination in air at 700 °C and under reaction conditions. The designed Au catalyst not only possessed extreme sintering resistance but also showed high catalytic activity and stability because of the strong interfacial interaction between Au and the heterostructured perovskite support.

36 MATERIALS SCIENCE↗

Effect of fly ash on catalytic removal of gaseous dioxins over V{sub 2}O{sub 5}-WO{sub 3} catalyst of a sinter plant

A PCDD/F (polychlorinated dibenzo-p-dioxin and dibenzofuran)-containing gas stream generating system was developed to investigate the efficiency and effectiveness of V{sub 2}O{sub 5}-WO{sub 3} catalyst for PCDD/F destruction. Catalytic decomposition of PCDD/Fs (simulated gas streams) was evaluated with lab-scale pelletized and plate-type catalyst based on V{sub 2}O{sub 5}-WO{sub 3}/TiO{sub 2} at controlled temperature, space velocity, and inlet PCDD/F concentration. Due to the lower porosity of the pelletized catalyst, PCDD/F destruction efficiencies reach 72.9-83.2% for different levels of inlet PCDD/F concentrations (1.08-3.04 ng-TEQ/Nm{sup 3}) of the gas stream (space velocity: 5000 h-1). As the surface area is increased from 287 m{sup 2}/m{sup 3} (plate-type A) to 550 m{sup 2}/m{sup 3} (plate-type B), the PCDD/F destruction achieved with plate-type catalyst increases from 76.0% to 85.3% at 320{sup o}C (space velocity: 5000 h{sup -1}). In addition, the results of pilot-scale experiment (real flue gases of a sinter plant) indicate that relatively lower PCDD/F destruction efficiencies (62.1-65.7%) were achieved with the plate-type B catalyst as the solid-phase PCDD/F and fly ash passed through the reactor (space velocity: 5000 h{sup -1}). Overall, the lab-scale and pilot-scale experiments indicate that PCDD/F destructions achieved with pelletized and plate-type catalysts strongly depend on the operating temperature of the catalyst. The results also indicate that the presence of fly ash lowers PCDD/F destruction due to significant PCDD/F formation via de novo synthesis at 320{sup o}C. 20 refs., 5 figs., 3 tabs.

01 COAL, LIGNITE, AND PEAT↗

Rapid liquid phase sintered Mn doped BiFeO{sub 3} ceramics with enhanced polarization and weak magnetization

Single-phase BiFe{sub 1-x}Mn{sub x}O{sub 3} multiferroic ceramics have been synthesized by rapid liquid phase sintering method to study the influence of Mn substitution on their crystal structure, dielectric, magnetic, and ferroelectric behaviors. From XRD analysis it is seen that Mn substitution does not affect the crystal structure of the BiFe{sub 1-x}Mn{sub x}O{sub 3} system. An enhancement in magnetization was observed for BiFe{sub 1-x}Mn{sub x}O{sub 3} ceramics. However, the ferooelectric hysteresis loops were not really saturated, we observed a spontaneous polarization of 10.23 {mu}C/cm{sup 2} under the applied field of 42 kV/cm and remanent polarization of 3.99 {mu}C/cm{sup 2} for x=0.3 ceramic.

36 MATERIALS SCIENCE↗

Spark plasma sintering-fabricated one-dimensional nanoscale 'crystalline-amorphous' carbon heterojunction

One-dimensional (1D) nanoscale 'crystalline-amorphous' carbon heterojunction is fabricated by post-treatment of an amorphous carbon nanofiber in a spark plasma sintering (SPS) system. It is proposed that the unique SPS process is responsible for the heterojunction formation. Studies of the electrical transport property show that the nanoscale heterojunction exhibits a typical rectification behavior. The heterojunctions may have broad potential applications in nanoelectronics and optoelectronics and the SPS technique could be a distinctive approach to construct 1D functional nanomaterials with high throughput.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Large-size ultrahigh strength Ni-based bulk metallic glassy matrix composites with enhanced ductility fabricated by spark plasma sintering

Ni-based bulk glassy alloy composites (GACs) simultaneously with ultrahigh strength and enhanced ductility and satisfying large-size requirements were fabricated by spark plasma sintering of gas-atomized Ni{sub 52.5}Nb{sub 10}Zr{sub 15}Ti{sub 15}Pt{sub 7.5} glassy alloy powder blend with ceramic or metal powders. No crystallization of metallic glassy matrix and good bonding state between the particles are responsible for good mechanical properties of the fabricated bulk GACs. The improvement of plastic ductility of the fabricated bulk GACs originates from the structural inhomogeneity caused by the particles inclusion. The additional particulates act as a resisting media causing deviation, branching, and multiplication of shear bands.

36 MATERIALS SCIENCE↗

Structure and magnetic properties of bulk nanocrystalline Dy metal prepared by spark plasma sintering

The structure and magnetic properties were studied for bulk nanocrystalline dysprosium (Dy) metal prepared by spark plasma sintering method. All the as-prepared samples have hexagonal close packed structure. A decrease in grain size results in remarkable changes in magnetic ordering temperature of the nanocrystalline Dy metal. At 5 K, the magnetization drops by 3.35%, and the coercive force increases by three times for nanocrystalline Dy compared to those of coarse-grained bulk Dy sample. These results indicate the remarkable influence of the nanostructure on the magnetism of Dy due to finite size effect.

36 MATERIALS SCIENCE↗