Formation of homologous In{sub 2}O{sub 3}(ZnO){sub m} thin films and its thermoelectric properties
Homologous In{sub 2}O{sub 3}(ZnO){sub 5} thin films were produced on a synthetic quartz glass substrate by thermal annealing of magnetron sputtered In{sub 2}O{sub 3}-ZnO compound films. When the annealing temperature was increased to 700 °C, the sputtered In{sub 2}O{sub 3}-ZnO film with In{sub 2}O{sub 3} microcrystalline changed to a c-oriented homologous In{sub 2}O{sub 3}(ZnO){sub 5} structure, for which the crystallization is suggested to begin from the surface and proceed along with the film thickness. The annealing temperature of 700 °C to form the In{sub 2}O{sub 3}(ZnO){sub 5} structure was substantially lower than temperatures of conventional solid state synthesis from In{sub 2}O{sub 3} and ZnO powders, which is attributed to the rapid diffusional transport of In and Zn due to the mixing of In{sub 2}O{sub 3} and ZnO in the atomic level for sputtered In{sub 2}O{sub 3}-ZnO compound films. The homologous structure collapsed at temperatures above 900 °C, which is attributed to (1) zinc vaporization from the surface and (2) a gradual increase of zinc silicate phase at the interface. This c-oriented layer structure of homologous In{sub 2}O{sub 3}(ZnO){sub 5} thin films along the film thickness allowed the thin film to reach a power factor of 1.3 × 10{sup −4} W/m K{sup 2} at 670 °C, which is comparable with the reported maximum value for the textured In{sub 2}O{sub 3}(ZnO){sub 5} powder (about 1.6 × 10{sup −4} W/m K{sup 2} at 650 °C).