Evaluation of Cyclic Behavior of Aircraft Turbine Disk Alloys

An evaluation of the cyclic behavior of three aircraft engine turbine disk materials was conducted to compare their relative crack initiation and crack propagation resistance. The disk alloys investigated were Inconel 718, hot isostatically pressed and forged powder metallurgy Rene '95, and as-hot-isostatically pressed Rene '95. The objective was to compare the hot isostatically pressed powder metallurgy alloy forms with conventionally processed superalloys as represented by Inconel 718. Cyclic behavior was evaluated at 650 C both under continuously cycling and a fifteen minute tensile hold time cycle to simulate engine conditions. Analysis of the test data were made to evaluate the strain range partitioning and energy exhaustion concepts for predicting hold time effects on low cycle fatigue.

Shahani, V.↗

Effect of microstructure on Na/+/ diffusion in beta alumina

The effect of microstructural features, such as grain size and orientation, on sodium ion diffusion in polycrystalline beta alumina is investigated; the ionic solid is suitable for use in high-energy and power density batteries. Two types of hot-pressed polycrystalline samples are studied, one with grains highly oriented in the direction normal to the pressing direction, the other with significantly less preferred orientation normal to the pressing direction. Results of the experimental assessments indicate that grain size and diffusion path tortuosity have little effect on diffusion kinetics, while grain boundary type and grain aspect ratio are important factors in determining the diffusion rate.

Sarian, S.↗

Consolidation of silicon nitride without additives

The use of ceramics for gas turbine engine construction might make it possible to increase engine efficiency by raising operational temperatures to values beyond those which can be tolerated by metallic alloys. The most promising ceramics being investigated in this connection are Si3N4 and SiC. A description is presented of a study which had the objective to produce dense Si3N4. The two most common methods of consolidating Si3N4 currently being used include hot pressing and reaction sintering. The feasibility was explored of producing a sound, dense Si3N4 body without additives by means of conventional gas hot isostatic pressing techniques and an uncommon hydraulic hot isostatic pressing technique. It was found that Si3N4 can be densified without additions to a density which exceeds 95% of the theoretical value

Sikora, P. F.↗

Development of silicon nitride of improved toughness

The application of reaction sintered Si2N4 energy absorbing surface layers to hot-pressed Si3N4 was investigated. The surface layer was formed by in-place nitridation of silicon powder. It was found that reaction sintered Si3N4 layers of 1 mm thickness, fabricated from either -100, +200, -200, or -325 mesh Si powder and nitrided in 96% N2/4% H2 so that approximately 20-25 vol % unnitrided Si remained in the layer, resulted in a sevenfold increase in ballistic impact resistance of a 0.64 cm thick hot-pressed SI3N4 substrate from RT 1370 C. Both NC-132 SI3N4, with MgO additive, and NCX-34 Si3N4, with Y2O3 additive, were evaluated as substrate material. The finer grain size -200 and -325 mesh nitrided Si layers were for their smoothness and relatively high density. It was found that nitriding in N2/H2 mixtures, rather than pure N2, resulted in a microstructure that did not substantially degrade the strength of the hot-pressed Si3N4 substrate. Thermal cycling tests on the RSSN/HPSN combinations from 200 C to 1370 C for 75 cycles in air did not degrade the impact resistance nor the interfacial bonding, although a large amount of internal silica formation occurred within the RSSN layer. Mach 0.8, 5 hr, hot gas erosion tests showed no surface recession of RSSN layers at 1200 C and slight surface recession at 1370 C.

Brennan, J. J.↗

Characterization and properties of controlled nucleation thermochemical deposited (CNTD) silicon carbide

The microstructure of controlled nucleation thermochemical deposition (CNTD) - SiC material was studied and the room temperature and high temperature bend strength and oxidation resistance was evaluated. Utilizing the CNTD process, ultrafine grained (0.01-0.1 mm) SiC was deposited on W - wires (0.5 mm diameter by 20 cm long) as substrates. The deposited SiC rods had superior surface smoothness and were without any macrocolumnar growth commonly found in conventional CVD material. At both room and high temperature (1200 - 1380 C), the CNTD - SiC exhibited bend strength approximately 200,000 psi (1380 MPa), several times higher than that of hot pressed, sintered, or CVD SiC. The excellent retention of strength at high temperature was attributed to the high purity and fine grain size of the SiC deposit and the apparent absence of grain growth at elevated temperatures. The rates of weight change for CNTD - SiC during oxidation were lower than for NC-203 (hot pressed SiC), higher than for GE's CVD - SiC, and considerably below those for HS-130 (hot pressed Si3N4). The high purity, fully dense, and stable grain size CNTD - SiC material shows potential for high temperature structural applications; however problem areas might include: scaling the process to make larger parts, deposition on removable substrates, and the possible residual tensile stress.

Dutta, S.↗

Effect of starting powder characteristics on density, microstructure and low temperature oxidation behavior of a Si3N48w/o Y2O3 ceramic

The densification and oxidation behavior of Si3N4 - 8w/oY2O3 prepared from three commercial starting powders were studied. Bars of SN 402, SN 502, and CP 85/15 were sintered for 3 to 4.5 hours at 1750 C. A second set was hot pressed for 2 hours at 1750 C. The microstructures were studied by transmission electron microscopy and scanning electron microscopy, densities were determined, and the phase compositions were determined by X-ray diffraction. Densification and microstructure were greatly influenced by the starting powder morphology and impurity content. Although SN 402 exhibited the maximum weight lose, the highest sintered and hot pressed densities were obtained with this powder. All powders had both equiaxed and elongated grains. Sintered bars were composed of beta silicon nitride and n-melelite. In contrast, hot pressed bars contained beta silicon nitride, H-phase, and J-phase, but no melelite. Yttria distribution in sintered bars was related to the presence of cation impurities such as Ca, Fe, and Mg. A limited oxidation study at 750 C in air showed no instability in these Si3N4 - 8 w/oY2O3 specimens, regardless of startin powder.

Schuon, S.↗

Completion of evaluation of manufacturing processes for B/Al composites containing 0.2mm diameter boron fibers

Four fabricators produced a total of 54 B/1100 Al, B/6061 Al, and B/2024 Al panels for evaluation. The 8 ply unidirectional, 45 to 50 volume percent, panels were made using 0.20 mm diameter boron fibers which were obtained from a single supplier. Hot press consolidation was carried out in vacuum except for one set of dry woven tape panels which were hot pressed in air. A single testing contractor conducted nondestructive inspection, metallography, fractography and mechanical property tests. The mechanical property tests included 21 and 260 C tensile tests and 21 C shear tests. Panel quality, as measured by nondestructive evaluation, was generally good as were the 21 C tensile properties. The panels hot pressed in air delaminated in the shear tests. Shear strength values were lower in these panels. But tensile strengths were not affected by the delaminations because of the relation between the tensile loading direction and the delaminations. Composite tensile strength was found to be proportional to the volume percent boron and the aluminum matrix rather than to the tape used or fabrication technique. Suitability of these composites for 260 C service was confirmed by tensile tests.

Moore, T. J.↗

Processing of sintered alpha SiC

Processing methods of sintered alpha SiC for engine applications are developed in a cost effective manner, using a submicron sized powder blended with sintering aids (boron and carbon). The processes for forming a green powder compact, such as dry pressing, cold isostatic pressing and green machining, slip casting, aqueous extrusion, plastic extrusion, and injection molding, are described. Dry pressing is the simplest route to component fabrication, and is carried out at approximately 10,000 psi pressure, while in the cold isostatic method the pressure could go as high as 20,000 psi. Surfactants are added to control settling rates and casting characteristics in the slip casting. The aqueous extrusion process is accomplished by a hydraulic ram forcing the aqueous mixture through a die. The plastic forming processes of extrusion and injection molding offer the potential of greater diversity in shape capacity. The physical properties of sintered alpha SiC (hardness, Young's modulus, shear modulus, and thermal diffusivity) are extensively tested. Corrosion resistance test results of silicon carbide are included.

Storm, R. S.↗

Photovoltaic-Panel Laminator

Two-piece unit heats and presses protective layers to form laminate. Rubber diaphragm between upper and lower vacuum chambers alternates between neutral position and one that presses against solar-cell array, supplying distributed force necessary to press layers of laminate together. Encapsulation helps to protect cells from environment and to ensure long panel life while allowing efficient generation of electricity from Sunlight.

Keenan, R.↗

Simple processing method for high-strength silicon carbide

Silicon carbide test bars were made by a simple wet-processing technique. The pressure casting method used the same equipment as conventional dry-pressing, but with a modified die. This casting technique was employed in order to produce test bars with improved strength and smaller fracture flaws than produced by dry-pressing. This was accomplished by eliminating pore clusters which were present in dry-pressed specimens and identified as a common source of failure in SiC MOR test bars.

Hurst, Janet B.↗

Preparation and evaluation of silicon nitride matrices for silicon nitride-SiC fiber composites

Continuous silicon carbide (SiC) fiber was added to three types of silicon nitride (Si3N4) matrices. Efforts were aimed at producing a dense Si3N4 matrix from reaction-bonded silicon nitride (RBSN) by hot-isostatic-pressing (HIP) and pressureless sintering, and from Si3N4 powder by hot-pressing. The sintering additives utilized were chosen to allow for densification, while not causing severe degradation of the fiber. The ceramic microstructures were evaluated using scanning optical microscopy. Vickers indentation was used to determine the microhardness and fracture toughness values of the matrices. The RBSN matrices in this study did not reach more than 80 percent of theoretical density after sintering at various temperatures, pressures, and additive levels. Hot-pressing Si3N4 powder produced the highest density matrices; hardness and toughness values were within an order of magnitude of the best literature values. The best sintering aid composition chosen included Y2O3, SiO2, and Al2O3 or AlN. Photomicrographs demonstrate a significant reduction of fiber attack by this additive composition.

Axelson, Scott R.↗

Effects of various consolidation techniques on microstructure, strength, and reliability of alpha-SiC

The effects of slurry pressing, HIP, and sinter-HIP on the strength, microstructure, and critical processing flaws in alpha-SiC are examined. Also, the feasibility of glass encapsulation is determined. Baseline strength was improved by about 25 percent by using slurry pressing instead of dry pressing. HIP further improved average strength to as high as 655 MPa. Sinter-HIP did not noticeably improve average strength. Although process-related flaws such as shrinkage cracks and large voids were not seen in HIPed alpha-SiC, surface-related flaws were observed. It is suggested that surface finishing by lapping, polishing, and heat treating might reduce the effect of surface-related flaws, improving the Weibull modulus in HIPed alpha-SiC.

Dutta, Sunil↗

Effect of Ga and P dopants on the thermoelectric properties of n-type SiGe

The purpose of this study was to hot-press improved n-type Si80Ge20/GaP samples directly (without any heat treatment) and to confirm that a Ga/P ratio less than one increases the solubility of P and, hence, improves the power factor and Z. One of the three samples (Ga/P = 0.43) had an improvement in Z of about 20 percent between 400 and 1000 C over that for standard SiGe. This demonstrates that improved samples can be pressed directly and that a Ga/P ratio less than one is necessary. The other two samples (Ga/P = 0.33 and 0.50) had Z's equal to or less than that of standard SiGe but had a lower hot-pressing temperature than the improved sample.

Draper, S. L.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glasss transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder x ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structure transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

Crystallization and properties of Sr-Ba aluminosilicate glass-ceramic matrices

Powders of roller quenched (Sr,Ba)O-Al2O3-2SiO2 glasses of various compositions were uniaxially pressed into bars and hot isostatically pressed at 1350 C for 4 hours or cold isostatically pressed and sintered at different temperatures between 800 to 1500 C for 10 or 20 hours. Densities, flexural strengths, and linear thermal expansion were measured for three compositions. The glass transition and crystallization temperatures were determined by Differential Scanning Calorimetry (DSC). The liquidus and crystallization temperature from the melt were measured using high temperature Differential Thermal Analysis (DTA). Crystalline phases formed on heat treatment of the glasses were identified by powder X ray diffraction. In Sr containing glasses, the monoclinic celsian phase always crystallized at temperatures above 1000 C. At lower temperatures, the hexagonal analog formed. The temperature for orthorhombic to hexagonal structural transformation increased monotonically with SrO content, from 327 C for BaO-Al2O3-2SiO2 to 758 C for SrO-Al2O3-2SiO2. These glass powders can be sintered to almost full densities and monoclinic celsian phase at a relatively low temperature of 1100 C.

Bansal, Narottam P.↗

A statistical comparison of two carbon fiber/epoxy fabrication techniques

A statistical comparison of the compression strengths of specimens that were fabricated by either a platen press or an autoclave were performed on IM6/3501-6 carbon/epoxy composites of 16-ply (0,+45,90,-45)(sub S2) lay-up configuration. The samples were cured with the same parameters and processing materials. It was found that the autoclaved panels were thicker than the platen press cured samples. Two hundred samples of each type of cure process were compression tested. The autoclaved samples had an average strength of 450 MPa (65.5 ksi), while the press cured samples had an average strength of 370 MPa (54.0 ksi). A Weibull analysis of the data showed that there is only a 30 pct. probability that the two types of cure systems yield specimens that can be considered from the same family.

Hodge, A. J.↗

Rhenium material properties

Tensile data were obtained from four different types of rhenium at ambient and elevated temperatures. The four types of rhenium included chemical vapor deposition (CVD) and three powder metallurgy (PM) types, i.e., rolled sheet and pressed and sintered bars, with and without hot isostatic pressure (HIP) treatment. Results revealed a wide range of values with ultimate strengths at ambient temperatures varying from 663 MPa for CVD rhenium to 943 MPa for rolled sheet. A similar spread was also obtained for material tested at 1088 K and 1644 K. The wide variance observed with the different materials indicated that the rhenium manufacturing process, material composition and prior handling strongly dictated its properties. In addition to tensile properties, CVD, pressed and sintered material and HIP rhenium successfully completed 100 cycles of low cycle fatigue. Creep data were also obtained showing that CVD and pressed and sintered rhenium could sustain five hours of testing under a tension of 27.5 MPa at 1922 K.

Biaglow, James A.↗

Stress Tuning of Laser Crystals

The topic of stress tunable laser crystals is addressed in this study with the purpose of determining the piezo-optic coefficients of a new laser material. This data was collected using a quadruple pass birefringence technique because of its high degree of sensitivity relative to the other methods examined including fringe shift analysis using a Mach-Zender interferometer. A green He-Ne laser was passed through a light chopper and Glan-Thompson prism before entering a crystal of Erbium doped Yttrium Aluminum Garnet (Er:YAG) (used in order to validate the experimental technique). The Er:YAG crystal is mounted in a press mechanism and the laser is quadruple passed through test specimen before being returned through the prism and the orthogonally polarized portion of the beam measured with a optical sensor. At a later stage, the Er:YAG crystal was replaced with a new crystal in order to determine the piezo-optic coefficients of this uncharacterized material. The applied load was monitored with the use of a 50 lb. load cell placed in line with the press. Light transmission readings were taken using a lock-in amplifier while load cell measurements were taken with a voltmeter from a 5 volt, 0.5 amp power supply. Despite the fact that an effective crystal press damping system was developed, size limitations precluded the use of the complete system. For this reason, data points were taken only once per full turn so as to minimize the effect of non uniform load application on the collected data. Good correlation was found in the transmission data between the experimentally determined Er:YAG and the previously known peizo-optic constants of non-doped crystal with which it was compared. The variation which was found between the two could be accounted for by the aforementioned presence of Erbium in the experimental sample (for which exact empirical data was not known). The same test procedure was then carried out on a Yttrium Gallium Aluminum garnet (YGAG) for the purpose of establishing values of its unknown piezo-optic constant tensor using experimentally collected transmission data. Significant variation between the piezo-optic constants of YAG and YGAG crystals was found however, the excellent data correlation of separate experimental runs carried out on the YGAG sample demonstrates the validity of these results. The data collected during the stressing of the YGAG was of high quality, however the amount of data collected was somewhat limited by a fracture of YGAG specimen which undoubted altered the crystalline lattice structure and hence precluded any further testing.

Carty, Atherton A.↗