Search NASA⌕ Search

SEARCH · Search NASA

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Atomic Layer-Deposited TiO{sub 2} Coatings on NiTi Surface

NiTi shape-memory alloys may release poisonous Ni ions at the alloys’ surface. In an attempt to prepare a well-performing surface layer on an NiTi sample, the thermally grown TiO{sub 2} layer, which formed during the heat treatment of NiTi, was removed and replaced with a new TiO{sub 2} layer prepared using the atomic layer deposition (ALD) method. Using x-ray photoelectron spectroscopy, it was found that the ALD layer prepared at as low a temperature as 100 °C contained Ti in oxidation states + 4 and + 3. As for static corrosion properties of the ALD-coated NiTi samples, they further improved compared to those covered by thermally grown oxide. The corrosion rate of samples with thermally grown oxide was 1.05 × 10{sup −5} mm/year, whereas the corrosion rate of the ALD-coated samples turned out to be about five times lower. However, cracking of the ALD coating occurred at about 1.5% strain during the superelastic mechanical loading in tension taking place via the propagation of a localized martensite band.

36 MATERIALS SCIENCE↗

Formation of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) Nano-composites via Mechanical Alloying and Friction Stir Processing

Combination of mechanical alloying and friction stir processing was used for the fabrication of Al/(Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3}) nano-composites. Pre-milled hematite + Al powder mixture was introduced into the stir zone generated on 1050 aluminum alloy sheet by friction stir processing. Uniform and active milled powder mixture reacted with plasticized aluminum to produced Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles. Al{sub 13}Fe{sub 4} intermetallic showed elliptical shape with a typical size of ~ 100 nm, while nano-sized Al{sub 2}O{sub 3} exhibited irregular floc-shaped particles that formed clusters with the remnant of iron oxide particles in the fine recrystallized aluminum matrix. As the milling time (1-3 h) of the introduced powder mixture increased, the volume fraction of Al{sub 13}Fe{sub 4} + Al{sub 2}O{sub 3} particles increased in the fabricated composite. The hardness and ultimate tensile strength of the fabricated nano-composites varied from 54.5 to 75 HV and 139 to 159 MPa, respectively; these are much higher than those of the friction stir processed base alloy (33 HV and 97 UTS). The highest hardness and strength were achieved for the nano-composite fabricated using the 3-h milled powder mixture; hard nano-sized reaction products and fine recrystallized grains of Al matrix had major and minor roles on enhancing these properties, respectively.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Friction Stir Process Derived Al-TiO{sub 2} Nanocomposite

Aluminum-based composites have many advantages over their conventional counterparts. A major problem in such composites is the clustering of particles in the matrix. Friction stir processing (FSP) can homogenize particle distribution in aluminum-based composites. In this study, unannealed TiO{sub 2} particles were used to prepare Al-TiO{sub 2} nanocomposite using FSP. The TiO{sub 2} particles, about 1 µm, were dispersed into an aluminum matrix by 6 passes of FSP. The TiO{sub 2} particles were fractured by multiple FSP passes, leading to a nano-size particle distribution in the matrix. Nanoscale dispersion was confirmed by scanning electron microscopy and transmission electron microscopy. The fractured TiO{sub 2} particles reacted with the aluminum matrix to form Al{sub 3}Ti intermetallic and Al{sub 2}O{sub 3} ceramic. The progression of the Al-TiO{sub 2} reaction from the fourth to the sixth pass of FSP was revealed by x-ray diffraction. Due to the nanoscale dispersion, the yield and ultimate tensile strength of the composite increased to 97 and 145 MPa, respectively. Ductility of the composite decreased marginally compared to the as-received aluminum. As the dispersed particles pin dislocations, the strain-hardening rate of the composite was considerably increased and the same was seen in the Kocks-Mecking plot. The TiO{sub 2} particles are mechanically activated due to their fracture during FSP, hence leading to reaction with the matrix. The particle refinement and dispersion lead to a homogeneous matrix with higher strength.

36 MATERIALS SCIENCE↗

Effect of Al on Grain Refinement and Mechanical Properties of Mg-3Nd Casting Alloy

The effect of Al on the grain refinement and mechanical properties of as-cast Mg-3Nd alloy was investigated systematically by a series of microstructural analysis, solidification analysis and tensile tests. The results show that Al has an obvious refining effect on the as-cast Mg-3Nd alloy. With increasing Al content, the grain size of the as-cast Mg-3Nd alloy decreases firstly, then increases slightly after the Al content reaching 3 wt.%, and the minimum grain size of the Mg-3Nd alloy is 48 ± 4.0 μm. The refining mechanism can be attributed to the formation of Al{sub 2}Nd particles, which play an important role in the heterogeneous nucleation. The strength and elongation of the Mg-3Nd alloy refined by Al also increase with increasing Al content and slightly decrease when the Al content is more than 3 wt.%, and the strengthening mechanism is attributed to the grain refinement as well as dispersed intermetallic particles. Furthermore, the microstructural thermal stability of the Mg-3Nd-3Al alloy is higher than that of the Mg-3Nd-0.5Zr alloy. Overall, the Mg-3Nd alloy with Al addition is a novel alloy with wide and potential application prospects.

36 MATERIALS SCIENCE↗

The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B{sub 4}C and (Cr, Fe, Mo, Ni, Ti){sub 3}B{sub 2} phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

36 MATERIALS SCIENCE↗

Interfacial Microstructure and Mechanical Properties of Friction Stir Welded Joints of Commercially Pure Aluminum and 304 Stainless Steel

In the present investigation, friction stir welding of commercially pure aluminum and 304 stainless steel was carried out at varying tool rotational speeds from 200 to 1000 rpm in steps of 200 rpm using 60 mm/min traverse speed at 2 (degree) tool tilt angle. Microstructural characterization of the interfacial zone was carried out using optical microscope and scanning electron microscope. Energy-dispersive spectroscopy indicated the presence of FeAl{sub 3} intermetallic phase. Thickness of the intermetallic layer increased with the increase in tool rotational speed. X-ray diffraction studies indicated the formation of intermetallic phases like FeAl{sub 2}, Fe{sub 4}Al{sub 13}, Fe{sub 2}Al{sub 5}, and FeAl{sub 3}. A maximum tensile strength of ~ 90% that of aluminum along with ~ 4.5% elongation was achieved with the welded sample at tool rotational speed of 400 rpm. The stir zone showed higher hardness as compared to base metals, heat affected zone, and thermo-mechanically affected zone due to the presence of intermetallics. The maximum hardness value at the stir zone was achieved at 1000 rpm tool rotational speed.

36 MATERIALS SCIENCE↗

Syntheses and Characterization of Intermetallic Nanostructures Based on Mn

The nanocrystalline powders of Mn50Ni41Sn9 were prepared by ball milling using a PM 200-type RETSCH planetary ball mill. The morphological, microstructural, and structural characterizations of the nanostructured powders were carried out by scanning electron microscope, x-ray diffraction, first using the Williamson–Hall relation for the refinement of the diffraction peak profiles. The high-temperature thermal and magnetic properties of nanocrystalline alloy Mn50Ni41Sn9 were characterized at different temperatures using a vibrating sample magnetometer; differential scanning calorimetry was used to determine the transformation temperature and thermodynamic values in the Mn50Ni41Sn9 alloy.

36 MATERIALS SCIENCE↗

Electrochemical Behavior Assessment of As-Cast Mg-Y-RE-Zr Alloy in Phosphate Buffer Solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}) Using Electrochemical Impedance Spectroscopy and Mott–Schottky Techniques

In the present study, electrochemical behavior of as-cast Mg-Y-RE-Zr alloy (RE: rare-earth alloying elements) was investigated using electrochemical tests in phosphate buffer solutions (X Na{sub 3}PO{sub 4} + Y Na{sub 2}HPO{sub 4}). X-ray diffraction techniques and Scanning electron microscopy equipped with energy dispersive x-ray spectroscopy were used to investigate the microstructure and phases of the experimental alloy. Different electrochemical tests such as potentiodynamic polarization (PDP), electrochemical impedance spectroscopy (EIS) and Mott–Schottky (M–S) analysis were carried out in order to study the electrochemical behavior of the experimental alloy in phosphate buffer solutions. The PDP curves and EIS measurements indicated that the passive behavior of the as-cast Mg-Y-RE-Zr alloy in phosphate buffer solutions was weakened by an increase in the pH, which is related to formation of an imperfect and less protective passive layer on the alloy surface. The presence of the insoluble zirconium particles along with high number of intermetallic phases of RE elements mainly Mg{sub 24}Y{sub 5} in the magnesium matrix can deteriorate the corrosion performance of the alloy by disrupting the protective passive layer that is formed at pH values over 11. These insoluble zirconium particles embedded in the matrix can detrimentally influence the passivation. The M–S analysis revealed that the formed passive layers on Mg-Y-RE-Zr alloy behaved as an n-type semiconductor. An increase in donor concentration accompanying solutions of higher alkalinity is thought to result in the formation of a less resistive passive layer.

36 MATERIALS SCIENCE↗

Evaluating the Electrochemical Behavior of Friction Stir-Welded AA2219-O Alloy Joint in 3.5% NaCl Solution

Single-pass friction stir welding of AA2219-O aluminum alloy was carried out at high rotation speed (1180 rpm), and transverse travel rate of 33.5 mm/min was selected. The microstructural, mechanical and electrochemical characteristics of the weldment are investigated in this study. The high rotational tool speed resulted in a less uniform distribution of the intermetallic θ-phase (CuAl{sub 2}) in the thermo-mechanically affected zone (TMAZ) than in the weld nugget zone (WNZ). The higher transfer coefficient and lower charge transfer resistance (R{sub ct} + R{sub θ}) were observed in case of TMAZ as evaluated from potentiodynamic polarization and impedance spectroscopy, respectively. These results confirmed that microstructural variations could deteriorate the electrochemical performance of the weldment. TMAZ provided the least corrosion resistance than the base metal (BM) and WNZ due to the high concentration of cathodic intermetallic particles and possibly due to the large mechanical distortion of the grain structure.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗

Role of Centrifugal Casting on Electrochemical Corrosion Behavior of A356-SiCp Composite in 3.5 wt.% NaCl

Role of graded microstructure in a centrifugally cast A356-SiC particle (SiCp) composite alloy disk on passivity and localized corrosion behavior in 3.5 wt.% NaCl environment has been investigated. The area fraction of SiCp has been found to decrease from the outer periphery to the core of the disk, while the apparent size and area fraction of the intermetallics and Mg-rich phase increase from the periphery to the core. As a consequence, the corrosion resistance of the as-cast disk varies with the distance from the periphery in the order 45 < 65 < 25 < 5 mm. The corrosion resistance of the centrifugally cast disk can be significantly improved through solution annealing at 540 °C for 2 h and solution annealing + aging at 175 °C for 2 h. However, between the two, the former has shown a better corrosion resistance and passivity than the latter. In the latter case, the aging treatment resulted in the precipitation of Mg{sub 2}Si phase which is prone to the corrosion attack.

36 MATERIALS SCIENCE↗

Formation and Decomposition Process of the Filled Skutterudite Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} (0.40 ≤ x ≤ 1) as Revealed by Differential Thermal Analysis

Filled skutterudites are among the most promising thermoelectric materials, and the obtainment of monophasic samples is crucial for the study of their transport properties. In this work, a differential thermal analysis study was performed on samples belonging to the Sm{sub y}(Fe{sub x}Ni{sub 1-x}){sub 4}Sb{sub 12} system with the aim to determine the most proper annealing temperature to possibly obtain skutterudite monophasic samples, and to study the effect of Sm addition on the thermodynamics of the Fe-Ni-Sb system. Samples were prepared through the traditional procedure consisting in melting–quenching–annealing the starting elements. DTA analyses were carried out on annealed samples, and results were interpreted using the Fe{sub 25}Sb{sub 75}-Ni{sub 25}Sb{sub 75} pseudobinary phase diagram taken from the literature as a starting point. They reveal that 870 K is the best annealing temperature, being the formation of a liquid phase just above this point; moreover, the Sm introduction results in widening the one-phase skutterudite stability region toward both higher temperatures and higher Fe concentrations compared with the Sm-free system.

36 MATERIALS SCIENCE↗

Corrosion Behavior of Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} (0.40 ≤ x ≤ 0.80) in NaCl Solutions Studied by Electron Microscopy and ICP-AES

Filled skutterudites are currently studied as thermoelectric materials to be used in the automotive and nautical field; the study of their resistance to a saline environment is therefore mandatory. To this purpose, the corrosion behavior of several compositions belonging to the Sm{sub y}(Fe{sub x}Ni{sub 1−x}){sub 4}Sb{sub 12} skutterudites system was investigated by immersing samples in differently concentrated (0.1 and 0.5 M) NaCl solutions. The effect of the treatment was analyzed both by SEM–EDS on the sample surface and at fixed times by ICP-AES on the solution. The formation of an oxide layer was observed on the surface of all the samples: the film results uniformly grown on specimens treated in NaCl at the lower concentration, while it is cracked and not spread over the whole surface in the other samples. Relying on the oxide layer thickness, the oxidation resistance results to increase with increasing the Fe content; correspondingly, the Sb concentration in the more diluted solution decreases at each time considered with increasing the Fe amount, pointing at a strict correlation between the cationic release and the oxide formation, and suggesting a possible mechanism for the growth of the protective film.

36 MATERIALS SCIENCE↗

Influence of Oxygen Partial Pressure Variation on Oxidation Resistance of Ti-46.7Al-1.9W-0.5Si at 750, 850 and 950 °C

γ-TiAl intermetallic alloys can be potentially employed as structural materials for many industries where high temperature and access of atmosphere with variable oxygen partial pressures are often met. Different partial pressures of oxygen may influence oxidation behavior and induce different oxide scale phase constitutes. This study investigated the influences of oxygen partial pressures on the oxidation resistance of a γ-TiAl alloy, Ti-46.7Al-1.9W-0.5Si (at.%), in Ar-O{sub 2} environments (5%O{sub 2}, 20%O{sub 2} and 80%O{sub 2}) at 750, 850 and 950 °C, respectively. The oxidation products were characterized using scanning electron microscopy, energy-dispersive x-ray analysis, x-ray diffraction and transmission electron microscopy. The oxidation kinetic results achieved by a discontinuous gravimetric method revealed that the alloy oxidized following a parabolic rate law. The oxidation resistance of the alloy was enhanced with increasing the oxygen partial pressures at all three experimental temperatures. Multilayered oxide scales of TiO{sub 2}/Al{sub 2}O{sub 3} were developed during the oxidation process. The enhancement of oxidation resistance was resulted from preferential generation of Al{sub 2}O{sub 3} and the reduction in defects in TiO{sub 2} with increasing the oxygen partials pressures.

36 MATERIALS SCIENCE↗

Effect of Coherent Lattice Mismatch on the Morphology and Kinetics of Ordered Precipitates

The morphological evolution and precipitation kinetics of ordered precipitates under the influence of lattice mismatch were studied by using the phase field model. The variation of the average aspect ratio of the precipitates and their distributions was investigated quantitatively, and the relationship of particles shape and particles fraction with the variation of the aspect ratio was determined. As the lattice mismatch increases, the coarsening rate constants and the particles number density decrease, the particles size distribution (PSD) becomes narrower, and the peak value of the PSD becomes lower than the value obtained by the Lifshitz–Slyozov–Wagner theory, while it is close to the value obtained by the Brailsford–Wynblatt theory. The change rate of the particles number density shows four-stage characteristics and decreases as the lattice mismatch and time increase, indicating that the precipitation and coarsening are retarded for a large lattice mismatch and that a large lattice mismatch results in fewer particles being dispersed in the matrix phase. The morphology and the particles number density show that a suitable lattice mismatch can enhance the mechanical properties of the alloys.

36 MATERIALS SCIENCE↗

Microstructures and Mechanical Properties of Resistance Spot-Welded Steel/Aluminum Alloy Joints with Process Tapes

The microstructure and mechanical property of resistance spot-welded joints of steel and aluminum were studied by using process tapes. The steel/aluminum joint consists mainly of aluminum nugget and interface zone. The liquid nugget solidification has an epitaxial growth characteristic, and the interface zone displays a double-layer structure, Fe{sub 2}Al{sub 5} layer at steel side and Fe{sub 4}Al{sub 13} layer at aluminum nugget side. Compared with joints without process tape, the joint nugget diameter and tensile shear load increased by 35.45 and 10.98%, respectively, and its indentation ratio decreased by 56.25% due to the process tapes increasing heat input, producing larger nugget diameter and continuous interface layer, and protecting against deep indentation. The joining area of intermetallic layer and aluminum nugget is weak link in the joint. It is favorable to use the process tapes for improving welding quality, raising joint strength, and energy saving.

36 MATERIALS SCIENCE↗

Effect of Welding Parameters on the Corrosion Behavior of Dissimilar Alloy Welds of T6 AA6061 Al-Galvanized Mild Steel

Partial replacement of steel by Aluminium (Al) alloys is a promising approach adopted by automotive sector to improve fuel efficiency without compromising on the strength. However, this results in the generation of dissimilar welds of Al alloys and steel. Understanding the corrosion behavior of Al alloys–steel welds as a function of welding parameters is critical in the successful application of such alloys. The present study reports the intergranular corrosion behavior of T6 heat-treated AA6061 Al alloy-galvanized mild steel lap joints, welded by metal inert gas welding–brazing technique as a function of different welding parameters, viz. weld speed (4-6 m/min) and wire feed rate (0.8-0.9 m/min), following ASTM G 67-04. Weld characterization was performed by field emission scanning electron microscopy (FESEM), x-ray diffraction and nano-hardness measurement. Results indicate heavy dissolution and metal loss at the interface. A high volume fraction of Al-Fe intermetallics was precipitated at the weld interfaces, resulting in high hardness and higher localized corrosion. The thickness of Al-Fe intermetallic layer increased with increasing wire feed rate and lower weld speed which enhanced the severity of galvanic and intergranular corrosion.

36 MATERIALS SCIENCE↗

The Influence of Pr and Nd Substitution on Hydrogen Storage Properties of Mechanically Alloyed (La,Mg){sub 2}Ni{sub 7}-Type Alloys

The (La,Mg){sub 2}Ni{sub 7}-type alloys are candidates for hydrogen storage materials. In this study, mechanical alloying with subsequent annealing under the argon atmosphere at 1123 K for 0.5 h is applied to produce La{sub 1.5−x}Pr{sub x}Mg{sub 0.5}Ni{sub 7} and La{sub 1.5−x}Nd{sub x}Mg{sub 0.5}Ni{sub 7} alloys (x = 0, 0.25, 0.5, 1). A shaker-type ball mill is used in the study. The objective of the present study is to investigate the influence of the amount of Pr or Nd in the La-Mg-Ni alloy on the electrochemical, hydrogenation and dehydrogenation properties of (La,Mg){sub 2}Ni{sub 7}-type materials. The x-ray diffraction analysis reveals the formation of multi-phase structure materials. The obtained alloys were studied by a conventional Sievert’s type apparatus at 303 K. It has been observed that a chemical modification by Pr and Nd can affect the kinetics of the hydrogen absorption process and the maximum hydrogen storage capacity. Moreover, the stability of the electrochemical discharge capacity during cyclic work of the (La,Mg){sub 2}Ni{sub 7}-type alloys is improved by a substitution with the La by Pr or Nd atoms.

36 MATERIALS SCIENCE↗