Synthesis, thermal and electrical properties of Al-doped Bi{sub 4}V{sub 1.8}Cu{sub 0.2}O{sub 10.7}
Partial substitution of copper with aluminum in Bi{sub 4}V{sub 1.8}Cu{sub 0.2}O{sub 10.7} has led to the Bi{sub 4}V{sub 1.8}Cu{sub 0.2−x}Al{sub x}O{sub 10.7+x/2} solid solution. X-ray diffraction and thermal analysis have shown that the compounds with x=0.05 and x=0.10 are tetragonal with γ′ form of Bi{sub 4}V{sub 2}O{sub 11}, while the compound with x=0.15 is of β polymorph. The effect of Al{sup 3+} doping on electrical conductivity has been studied using Electrochemical Impedance Spectroscopy. The electrical conductivity of doped samples along with the amount of Al{sup 3+} has been studied by electrochemical impedance spectroscopy in the temperature range 250–700 °C. The slope changes observed in the Arrhenius plots agree with the microstructural transitions occurring in these compounds. The highest ionic conductivity values are obtained for the sample with x=0.05. - Graphical abstract: Arrhenius plots of the electrical conductivity of the of Bi{sub 4}V{sub 1.8}Cu{sub 0.2−x}Al{sub x}O{sub 10.7+x/2} compounds. Display Omitted.