Influence of Austenitizing Temperature on the Microstructure and Mechanical Properties of an Fe-Cr-Ni-Mo-Ti Maraging Stainless Steel

The influence of austenitizing temperature on the microstructure and mechanical properties of an Fe-Cr-Ni-Mo-Ti maraging stainless steel was investigated. The grain size, Laves phase, and retained austenite in steels given different solution treatments were observed using optical microscopy, scanning electron microscopy, and x-ray diffraction. Relationships with mechanical properties were measured by tensile testing. The grain growth rate was relatively slow at temperatures of 800-1000 °C then rapidly increased at higher temperatures. Low-temperature austenitization augmented the retention of austenite, the fraction of which decreased with an increase in austenitizing temperature. The Laves phases, which precipitated in austenite during austenitization at 800-900 °C, were preserved after quenching. The solution treatment had a significant effect on the final tensile properties of the steel after aging, due to the presence of retained austenite and Laves phase reducing its strength.

36 MATERIALS SCIENCE↗

Brazing ZrO{sub 2} ceramic to Ti–6Al–4V alloy using NiCrSiB amorphous filler foil: Interfacial microstructure and joint properties

Reliable brazing of ZrO{sub 2} ceramic and Ti–6Al–4V alloy was achieved using NiCrSiB amorphous filler foil. The interfacial microstructure of ZrO{sub 2}/Ti–6Al–4V joints was characterized by scanning electron microscope, energy dispersive spectrometer and micro-focused X-ray diffractometer. The effects of brazing temperature on the interfacial microstructure and joining properties of brazed joints were investigated in detail. Active Ti of Ti–6Al–4V alloy dissolved into molten filler metal and reacted with ZrO{sub 2} ceramic to form a continuous TiO reaction layer, which played an important role in brazing. Various reaction phases including Ti{sub 2}Ni, Ti{sub 5}Si{sub 3} and β-Ti were formed in brazed joints. With an increasing of brazing temperature, the TiO layer thickened gradually while the Ti{sub 2}Ni amount reduced. Shear test indicated that brazed joints tend to fracture at the interface between ZrO{sub 2} ceramic and brazing seam or Ti{sub 2}Ni intermetallic layer. The maximum average shear strength reached 284.6 MPa when brazed at 1025 °C for 10 min. - Graphical Abstract: Interfacial microstructure of ZrO{sub 2}/TC4 joint brazed using NiCrSiB amorphous filler foil was: ZrO{sub 2}/TiO/Ti{sub 2}Ni + β-Ti + Ti{sub 5}Si{sub 3}/β-Ti/Widmanstätten structure/TC4. - Highlights: • Brazing of ZrO{sub 2} ceramic and Ti-6Al-4V alloy was achieved. • Interfacial microstructure was TiO/Ti{sub 2}Ni + β + Ti{sub 5}Si{sub 3}/β/Widmanstätten structure. • The formation of TiO produced the darkening effect of ZrO{sub 2} ceramic. • The highest joining strength of 284.6MPa was obtained.

36 MATERIALS SCIENCE↗

The comparison of microstructures and mechanical properties between 14Cr-Al and 14Cr-Ti ferritic ODS alloys

In this study, two kinds of 14Cr ODS alloys (14Cr-Al and 14Cr-Ti) were investigated to reveal the different effects between Al and Ti on the microstructures and mechanical properties of 14Cr ferritic ODS alloys. The microstructure information such as grains, minor phases of these two alloys has been investigated by high-energy X-ray diffraction and transmission electron microscopy (TEM). The in situ synchrotron X-ray diffraction tensile test was applied to investigate the mechanical properties of these two alloys. The lattice strains of different phases through the entire tensile deformation process in these two alloys were analyzed to calculate their elastic stresses. From the comparison of elastic stress, the strengthening capability of Y 2 Ti 2 O 7 is better than TiN in 14Cr-Ti, and the strengthening capability of YAH is much better than YAM and AlN in 14Cr-Al ODS. The dislocation densities of 14Cr-Ti and 14Cr-Al ODS alloys during tensile deformation were also examined by modified Williamson-Hall analyses of peak broadening, respectively. In conclusion, the different increasing speed of dislocation density with plastic deformation reveals the better strengthening effect of Y-Ti-O particles in 14Cr-Ti ODS than that of Y-Al-O particles in 14Cr-Al ODS alloy.

36 MATERIALS SCIENCE↗

Effect of Ni Addition to Sn0.7Cu Solder Alloy on Thermal Behavior, Microstructure, and Mechanical Properties

The addition of Ni on lead-free solder alloys Sn0.7Cu was tested in this study. A small amount of Ni was added to the solder alloys to evaluate the thermal behavior, microstructure, and mechanical properties of the composite solders after sintering and isothermal aging for 3 days and then compared with the results of the binary Sn0.7Cu solder. The results indicated that the ultimate tensile strength and yield tensile strength changed when adding 0.25 wt.% of Ni. The tested results of the differential scanning calorimeter showed that the addition of Ni (such as 0.5 and 1 wt.%) could obviously increase the solidification temperature of Sn0.7Cu alloys in the cooling process. When the Ni content was increased to 0.25 wt.% in the ternary condition, which includes the Sn0.7Cu-xNi (x = 0, 0.1, 0.25, 0.5, and 1 wt.%) solder alloys for the indentation creep test, the minimum creep rate reached the maximum; however, the trend was reversed as the Ni content was higher than this level. In addition, the microstructure of Sn-0.7Cu-xNi solder alloys was obviously different with the eutectic Sn-0.7Cu solder, such that the Ni gradually accumulated in the (Cu, Ni){sub 6}Sn{sub 5} IMCs within the Ni-containing solder alloys. Additionally, this process refined the microstructure of the Sn-0.7Cu solder. The fracture surface of the eutectic Sn-0.7Cu solder revealed ductile fracture modes; however, there was no mixed ductile–brittle fracture mode occurred when the Ni content was in the range of 0-1 wt.%.

36 MATERIALS SCIENCE↗

Correlating microstructure and mechanical properties of harvested high dose Zorita light water reactor internals

Here, in this study, microstructural studies and micro-mechanical testing of an ex-plant material harvested from the decommissioned pressurized water reactor (PWR) is carried out. Irradiated 304 stainless steel (SS) components were harvested by the Electric Power Research Institute, U.S. Nuclear Regulatory Commission, and members of the José Cabrera Nuclear Power Station (Zorita) in Spain. The bi-crystalline micro-tensile specimens, atom probe tomography (APT) tips, and transmission electron microscopy (TEM) lamellae were fabricated from the baffle plate materials irradiated to 0.05, 15 and 50 dpa to elucidate microstructural, microchemical, and local mechanical properties changes as a function of dose. TEM and APT studies reveal radiation induced Ni, Cr, and Si rich precipitates in the 15 dpa sample that become smaller and partially redissolve into the matrix of the 50 dpa sample (decreasing size and number density). Dislocation loop and cavity number density and size were quantified as a function of dose as well as swelling. Intergranular Ni and Si enrichments with concomitant Fe and Cr depletion were observed in the 15 dpa sample and were more pronounced in the 50 dpa sample. Micro-tensile testing performed in the scanning electron microscope (SEM) at room temperature and 300 °C shows that the material's local yield strength and ultimate tensile strength decreases with increased dose and elevated test temperature and provides further insights via localized strain mapping. Current and previous mechanical data was compared with calculated values using the dispersed barrier hardening model with inputs of dislocation loops, precipitates, and cavities from microstructural characterization.

36 MATERIALS SCIENCE↗

Effect of braze processing on the microstructure and mechanical properties of SCS-6/beta21S titanium matrix composites

An investigation is conducted of the effects of braze processing on the microstructure and tensile properties of SiC fiber-reinforced Ti-15Mo-2.7Nb-3Al-0.25Si-matrix composite (TMC) laminates; the brazing alloy was the commercial Ti-15Cu-15Ni, in both its conventional and metglass forms. Tensile tests conducted at room temperature, 1200 F, and 1500 F showed that the braze processes (1) had little effect on tensile properties, and (2) appeared to degrade neither the reinforcing fibers not the fiber/matrix interfacial bondline.

Hoffman, Eric K.↗

Comparative investigation on microstructures and mechanical properties of (TiB + TiC)/Ti-6Al-4V composites from Ti-B4C-C and Ti-TiB2-TiC systems

Highlights: • The (TiB{sub w}+TiC{sub p})/Ti-6Al-4V composites were fabricated from Ti-B{sub 4}C-C and Ti-TiB{sub 2}-TiC systems by reactive hot-pressed sintering. • Microstructures and mechanical properties of the two kinds of composites were comparatively investigated. • The composites from Ti-TiB{sub 2}-TiC system possess higher elastic modulus and Vickers hardness than those from Ti-B{sub 4}C-C system. • The composites from Ti-TiB{sub 2}-TiC system have higher bending strength than the other system while employing same conditions. • The composites from Ti-B{sub 4}C-C system present better abrasion resistance than those from Ti-TiB{sub 2}-TiC system. - Abstract: Two percentages of TiB + TiC reinforced Ti-6Al-4V composites from Ti-B{sub 4}C-C and Ti-TiB{sub 2}-TiC systems were fabricated by reactive hot-pressed sintering. Their microstructures and mechanical properties involving elastic modulus, Vickers hardness, bending strength and wear property were investigated comparatively. The experimental results show that needle-like TiB whiskers and near-equiaxed TiC particles are evenly distributed in the Ti-6Al-4V matrix. The mechanical properties of the (TiB + TiC)/Ti-6Al-4V composites are closely related with the nominal composition and synthesis system of TiB + TiC reinforcement and the microstructures of composites. With increasing the nominal volume fraction of reinforcement, both elastic modulus and Vickers hardness increase more or less and the bending strength decreases in varying degrees. A certain increase of pores in the composites with the sintering temperature increasing to 1300 °C can markedly affect the bending strength. Moreover, no matter what the sintering temperature and nominal volume fraction of reinforcement, the elastic modulus and Vickers hardness of composites from the Ti-TiB{sub 2}-TiC system are higher than those from the Ti-B{sub 4}C-C system. Similarly, the composites from the Ti-B{sub 4}C-C system present better abrasion resistance than those from the Ti-TiB{sub 2}-TiC system due to the difference of interfacial bonding between the TiC particles and Ti-6Al-4V matrix in the two kinds of composites.

36 MATERIALS SCIENCE↗

Optimization of the microstructure and mechanical properties of electron beam welded high-strength medium-entropy alloy (NiCoCr) 94 Al 3 Ti 3

For this work, the weldability and effects of subsequent heat treatment on the microstructure and mechanical properties of the medium-entropy alloy (MEA) (NiCoCr) 94 Al 3 Ti 3 have been explored using electron beam welding (EBW). It was found that EBW joints consist of a supersaturated f.c.c. matrix with coarse, asymmetric columnar grains (17.7–24 μm). The fraction of twins and Σ3 n CSL boundaries in weld joints was only 10% of that in the base metal, a value which increased to 30% after aging at 800 °C. The aging also led to improvements in the hardness, tensile strength, and work hardening rate, a result of the precipitation of a high volume fraction (0.29–0.33) of ultrafine (15–17.4 nm dia.) coherent spherical L1 2 -structured particles. The contributions of the L1 2 nanoparticles and Hall-Petch strengthening to the yield strength were estimated to be 537–573 MPa and 105–123 MPa, respectively. The MEA shows excellent weldability and, after aging, good strength (YS~1098 MPa, UTS~1368 MPa) and elongation to failure (~11%) by ductile fracture.

36 MATERIALS SCIENCE↗

Microstructure and Mechanical Properties of Ni-Based Superalloy Nimonic 105 with Varying Carbon Content

High carbon levels have been found to improve the fabricability of high-strength cast and wrought Ni-based superalloys, enabling the development of superior cast/wrought materials. However, carbon also strongly influences the microstructure and mechanical properties of the alloys. Nimonic 105 variants with three different carbon concentrations were manufactured. A bimodal grain size was found in the intermediate carbon content variant, while the high (low) carbon resulted in fine (coarse) grains thereby significantly affecting creep performance. The variations in grain structure were attributed to the primary carbides. An intermediate carbon level showed the best combination of strength and ductility in tension at high-temperature but little improvement in, or even inferior, creep performance. Discussion of the results will establish an understanding of the influence of carbon on the microstructure and mechanical properties of high strength cast and wrought superalloys, providing insights into obtaining high-quality alloys for future high-temperature applications.

Fang, Xiaotian↗

Effect of extrusion ratio on microstructure and mechanical properties of Mg-Nd-Zn-Zr alloys prepared by a solid recycling process

Microstructures and room temperature mechanical properties of Mg-2.4Nd-0.6Zn-0.6Zr alloys prepared by a solid recycling process with different extrusion ratios were studied. The tensile properties of the materials were evaluated for the magnesium alloys in as-extruded and extruded-T6 conditions. With increasing extrusion ratio, the tensile strength and elongation to failure increases. The heat treatment results in a significant increase in tensile yield strength and ultimate tensile strength because of dispersive particles or fine precipitates. Moreover, the ductility decreases from as-extruded condition to extruded-T6 condition. The morphology of the fracture surfaces was examined by employing scanning electron microscope. The fracture mode is a mix mechanism with brittle fracture and gliding fracture.

36 MATERIALS SCIENCE↗

Effect of Rolling Temperature on the Microstructure and Tensile Properties of 47Zr-45Ti-5Al-3V Alloy

The 47Zr-45Ti-5Al-3V (wt.%) alloy was solution-treated at 850 and 780 °C for 30 min and then rolled at different temperatures. The effect of rolling temperature on microstructure and tensile properties was investigated. The results showed that the microstructure contained a large amount of α phase at a rolling temperature of 600 °C. As the rolling temperature increased, the amount of α phase decreased, whereas the amount of β phase increased. When the rolling temperature was higher than 700 °C, the alloy was composed of a single β phase. The tensile properties of the alloy depended strongly on rolling temperature. The yield strength and tensile strength decreased with increasing rolling temperature, whereas the elongation increased. At a given rolling temperature, low solution treatment temperature resulted in higher strength and lower elongation than high solution treatment temperature. The fracture mode changed from cleavage fracture and quasi-cleavage fracture to dimple fracture with increasing rolling temperature.

36 MATERIALS SCIENCE↗

The effects of aluminum concentration on the microstructural and electrochemical properties of lithium lanthanum zirconium oxide

Cubic lithium lanthanum zirconium oxide (Li 7-x Al x La 3 Zr 2 O 12 , LLZO) garnet has gained attention as a promising next-generation electrolyte for lithium batteries due to its high ionic conductivity and chemical stability with lithium metal. The high conductivity can be achieved through doping over a range of aluminum concentrations. In this study, we hot-pressed samples to achieve <2% nominal porosity with aluminum concentrations from x = 0.25–0.55 mol to understand the effect of aluminum on microstructure and electrochemistry. It was observed that beyond the aluminum solubility limit (x = ~0.40), resistive secondary phases formed at the grain boundaries. As a result, the percent grain boundary resistance increased from 17.6 to 41.2% for x = 0.25 and x = 0.55, respectively. Both the grain boundary and bulk activation energies remained relatively constant as the aluminum concentrations increased (~0.44 eV and ~0.39 eV, respectively). It was, therefore, surmised that the mobility term of the Nernst–Einstein equation was roughly independent of aluminum concentration and the major variable controlling bulk conductivity was the number of lithium charge carriers. As a result, as the aluminum concentration increased from x = 0.25 to x = 0.55 the bulk conductivity decreased from 0.56 to 0.15 mS cm -1 . Following these trends of increasing grain boundary resistance and decreasing bulk conductivity with increasing aluminum concentration, x = 0.25 had the highest total conductivity (0.46 mS cm -1 ). We demonstrated that aluminum concentration has a significant effect on the microstructure and electrochemical properties of LLZO. In conclusion, we believe this work could help understand how to link processing, microstructure, and electrochemical properties to guide the manufacturing of LLZO for use in solid-state batteries.

25 ENERGY STORAGE↗

Microstructure and mechanical properties of Ti–B–C–N–Si nanocomposite films deposited by unbalanced magnetron sputtering

Quinary Ti–B–C–N–Si nanocomposite thin films were deposited on AISI 304 stainless steel substrates by d.c. unbalanced magnetron sputtering from a TiB{sub 2}–TiC compound target and a pure Si target. The relationship between microstructure and mechanical properties of the films was investigated in terms of the nanosized crystallites/amorphous system. The synthesized Ti–B–C–N–Si films were characterized using x-ray diffraction, x-ray photoelectron spectroscopy, atomic force microscopy, and high resolution transmission electron microscopy. The results showed that the Ti–B–C–N–Si films were nanocomposites composed of nanosized TiB{sub 2}, TiC, and TiSi{sub 2} crystallites (2-3 nm in size) embedded in an amorphous matrix. The addition of Si to the Ti–B–C–N film led to precipitation of nanosized crystalline TiSi{sub 2} and percolation of amorphous SiC phases. The Ti–B–C–N–Si films with up to 7 at. % Si content presented high hardness (≥35 GPa), H/E (≥0.0095), and W{sub e} (>50%) with compressive residual stress (∼0.5 GPa). A systematic investigation on the microstructure and mechanical properties of Ti–B–C–N–Si films containing different Si contents is reported.

36 MATERIALS SCIENCE↗

From Solidification Processing to Microstructure to Mechanical Properties: A Multi-scale X-ray Study of an Al-Cu Alloy Sample

We follow an Al-12 at. pct Cu alloy sample from the liquid state to mechanical failure, using in situ X-ray radiography during directional solidification and tensile testing, as well as three-dimensional computed tomography of the microstructure before and after mechanical testing. The solidification processing stage is simulated with a multi-scale dendritic needle network model, and the micromechanical behavior of the solidified microstructure is simulated using voxelized tomography data and an elasto-viscoplastic fast Fourier transform model. This study demonstrates the feasibility of direct in situ monitoring of a metal alloy microstructure from the liquid processing stage up to its mechanical failure, supported by quantitative simulations of microstructure formation and its mechanical behavior.

36 MATERIALS SCIENCE↗

Investigation of the changes in microstructure and transport properties of leached cement pastes accounting for mix composition

Ca-leaching of cement-based materials induces detrimental effects on properties related to long-term durability. A better understanding of leaching degradation in terms of alterations in mineralogy, microstructure, and transport properties is important for long-term assessments of concrete and reinforced concrete structures used in nuclear waste disposal systems or in hydro structures. However, the decalcification process is not easy to study because it is extremely slow. In this study, an ammonium nitrate (NH{sub 4}NO{sub 3}) solution of 6 mol/l was used to accelerate the leaching kinetics. The experiments were performed on cement paste samples with different water/powder (w/p) and limestone filler (LS) replacement ratios. Both the change of sample mass over time and the amount of calcium ion leached out were monitored during the test. Different post-analysis techniques including SEM/SEM-EDX, XRD/QXRD, MIP, ion chromatography, and N{sub 2}-adsorption were used to characterize the microstructural and mineralogical changes. The effect of accelerated leaching on transport properties was studied by measuring the changes in water permeability and diffusivity of dissolved gases. Results showed that the square-root-time law of degradation was applicable under accelerated conditions. Both higher w/p ratios and LS replacements increased the rate of leaching propagation; the former had a more significant effect. The accelerated leaching significantly altered the microstructure of the cement paste to a material with a higher specific surface area, increased total porosity and a shift to larger pore sizes. Those changes led to a significant increase in water permeability (one to two orders of magnitude) and diffusivity (less than one order) depending on degradation state.

36 MATERIALS SCIENCE↗

Accumulative Roll Bonding of Alloy 2205 Duplex Steel and the Accompanying Impacts on Microstructure, Texture, and Mechanical Properties

The mechanical and microstructural evolution of Alloy 2205 during severe plastic deformation is examined in this study. A combination of accumulative roll bonding (ARB) and cold rolling results in the successful formation of a nanograined dual-phase microstructure of austenite and ferrite with some transformed martensite. Severe deformation to cumulative reductions of 80.5, 92.5, 95, and 97 pct were performed. Microscopy indicates that grain dimensions in the sheet normal direction is less than 100 nm for reductions ≥ 92.5 pct. Shear banding is observed at reductions ≥ 95 pct while twinning is only observed at reductions < 92.5 pct. Neutron diffraction measurements indicated the presence of martensite for reductions ≥ 95 pct at ~ 8 pct volume fraction. Taken in conjunction, it appears that during initial ARB processing, both slip and twinning are active plastic mechanisms. As twinning becomes exhausted, martensitic transformation, slip, and intermittent shear banding account for the active plasticity mechanisms. Material hardness saturates at 92.5 pct reduction, with a maximum hardness of 45 HRC. Sub-sized tensile testing confirms this approximate hardness with measurements indicating a UTS of ~ 1440 MPa. Texture analysis of crystal orientation distributions in the plate normal direction suggest an approximate Kurdjumov–Sachs orientation relationship at all reductions above 80 pct indicating stability of the orientation relationship at high strains. The intragranular structure develops a fine scale sub-grain content with increasing deformation, resulting in a continual evolution of texture up to and including 97 pct reduction. The final structure presents strong components of Goss and rotated cube texture in both the austenite and ferrite. In this body of work we aim to compare ARB of an industrially relevant FCC/BCC system (Alloy 2205) to historical model FCC/BCC systems such as Cu/Nb.

36 MATERIALS SCIENCE↗

Impact of microstructure on elastic properties in the alloy Ti-42Al-8.5 Nb

The microstructure of a γ-TiAl alloy containing niobium undergoes continuous transformations during annealing at 550 °C. These take place within the α 2 -phase of lamellar (α 2 +γ) colonies. We have characterized these changes by transmission electron microscopy and made a correlation to the elastic constants determined by resonant ultrasonic spectroscopy during in-situ annealing at the same temperature. Further, the results show a continuous increase of the E-modulus. This can be attributed to elastic strains acting within α 2 lamellae as a result of lattice transformations. After 5000h, a thermodynamic equilibrium was established with equal fractions of α 2 -phase and O-phase that differ only in lattice symmetry and Nb content. Generally, the presence of O-phase should contribute to lower elastic moduli, however in the present case the evolving microstructural characteristics were responsible for the observed increase in the E-modulus.

36 MATERIALS SCIENCE↗

Effect of cold rolling on the microstructure and mechanical properties of Al 0.25 CoCrFe 1.25 Ni 1.25 high-entropy alloy

Cold rolling can break down the as-cast dendrite microstructure and thus may have pronounced impact on the mechanical behavior of the alloy. In the present study, the effect of cold rolling on the microstructure and mechanical properties of Al 0.25 CoCrFe 1.25 Ni 1.25 high-entropy alloy in the face-centered cubic structure was investigated. With increasing the thickness reduction from cold rolling, the hardness, the yield strength, and the fracture strength increased at the cost of reducing ductility. At the thickness reduction of 80%, the tensile strength (hardness) was 702 MPa (406 MPa), 1.62 (2.43) times that in the as-cast condition. Compared to traditional alloys, Al 0.25 CoCrFe 1.25 Ni 1.25 has the highest hardening rate with respect to CR thickness reduction. Lastly, the phase relation and the mixing properties of Gibbs free energy, enthalpy and entropy of Al x CoCrFe 1.25 Ni 1.25 were predicted using the CALPHAD method.

36 MATERIALS SCIENCE↗