Search NASA⌕ Search

SEARCH · Search NASA

Results for “recrystallization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Effect of Bi on the microstructure and mechanical properties of Sn-Zn alloys processed by rolling

Highlights: • Sn-Zn-Bi is proposed for the first time as the cladding in linear explosive device. • Bi can significantly refine the microstructure of Sn-Zn. • Bi can enhance both strength and ductility of Sn-Zn processed by rolling. • The 5 wt% Bi in Sn-3Zn leads to finest and most homogenous grains after rolling. - Abstract: Sn-Zn based alloys including Sn-3Zn, Sn-3Zn-1Bi, and Sn-3Zn-5Bi were prepared by casting and rolling, in efforts to assess their feasibility for the application as cladding materials in detonating and explosive cords. It was found that Bi significantly refined the solidification microstructure, changing the configuration of Sn-Zn eutectic from well-aligned Zn-rich precipitates/needles to misaligned Zn-rich flakes. During deformation, second phases like Zn-rich precipitates and Bi particles, and Bi solutes were effective in grain refinement since second phase particles provided more sites for nucleation and more obstacles to growth of new recrystallized grains. Tensile results revealed that Bi addition enhanced both strength and ductility of the rolled Sn-Zn-Bi alloys. The Sn-3Zn-5Bi alloy possessed superior strength and ductility (UTS: 84.4 MPa; Yield strength: 68.3 MPa; Elongation: 75.2%) due to its finest and most homogeneous equiaxed grains. Based on decent mechanical properties, the Sn-Zn-Bi alloys could be well qualified for the application as cladding materials.

36 MATERIALS SCIENCE↗

High-temperature deformation behavior of the extruded Ti-22Al-25Nb alloy fabricated by powder metallurgy

Highlights: • The high-temperature deformation behavior of the extruded Ti-22Al-25Nb alloy was analyzed. • A true strain-compensated Arrhenius-type constitutive model was established. • The processing maps of true strains 0.2, 0.4, and 0.6 were constructed to optimize the processing parameters. • Microstructural evolution and deformation mechanism in different conditions were explained. - Abstract: The hot-deformation behavior of the extruded Ti-22Al-25Nb alloy was investigated by compression testing in the 1213–1333 K temperature range, under a 0.001–1.0 s{sup −1} strain-rate range. The activation energy, Q, at a deformation strain of 0.3, was calculated to be 574.80 kJ mol{sup −1}. A strain-compensated Arrhenius-type constitutive model was established for this alloy, with an average absolute relative error (AARE) and correlation coefficient (R) of 7.64% and 0.994, respectively. Based on the dynamic materials model (DMM), processing maps were developed by combining the power dissipation and instability maps. An instability region was identified in the 1213–1278 K temperature range and 0.022–1.0 s{sup −1} strain-rate range. The microstructure of specimens deformed under different conditions were analyzed to characterize the corresponding deformation mechanisms. The main softening mechanisms in the stability regions were dynamic recrystallization (DRX) and dynamic globularization. The grain size of the specimen deformed at 1313 K/0.001 s{sup −1} was approximately 15.2 μm.

36 MATERIALS SCIENCE↗

Microstructure, texture and mechanical properties of 6061 aluminum laser beam welded joints

Highlights: • Strong cube texture ({001}<100>) is observed in columnar dendrites. • The ratio of equiaxed dendrites shows proportional relationship with the strength. • The relations between process-microstructure-property are accurately established. - Abstract: In the present study, laser beam welding was carried out with 6061 Al alloy plate to study the microstructural evolution under various welding heat input (ηP/v = 30 J/mm, 38 J/mm, 46 J/mm, and 58 J/mm). The width of the weld metals increased continuously with the heat input values. Quantitatively correlation of the microstructure distribution with welding parameters was developed based on the EBSD results. The weld metals mainly consisted of coarse columnar dendrites and equiaxed dendrites. The ratio of equiaxed dendrites which were controlled by constitutional supercooling and heterogeneous nuclei showed directly proportional relationship with the weld strength. Strong cube texture ({001}<100>) was observed in columnar dendrites, which showed harmful effect on the weld strength. Slight softening in heat affected zone due to recrystallization was identified by nanoindentation tests. All specimens failed in weld metal and the fracture surfaces showed the characteristics of ductile fracture.

36 MATERIALS SCIENCE↗

Influence of annealing temperature on microstructure and tensile property of cold-rolled Fe-0.2C-11Mn-6Al steel

To fully realize the potential of austenite characterized by strip-like and equiaxed structure and enhance the comprehensive mechanical properties of medium-Mn steel, the as-hot-rolled Fe-0.2C-11Mn-6Al steel was subjected to cold roll annealing to refine the grain size. The ultimate tensile strength of the cold-rolled steel annealed at 650 °C was significantly enhanced, while the total elongation was markedly decreased. The variation in tensile properties of the annealed cold-rolled steel was due to weakening of transformation induced plasticity (TRIP) effect and enhanced twinning induced plasticity (TWIP) effect with increase in quenching temperature. Furthermore, austenite had two different morphologies, strip-like and granular. Though the grain size of granular austenite increased with increased annealing temperature, the austenite stability increased with increase in quenching temperature, which is contrary to the expectations. This is attributed to refinement of large austenite strips induced by recrystallization.

36 MATERIALS SCIENCE↗

Refining whisker size of 2024Al/Al18B4O33w composite through extrusion and its effects on the material's micro-structures and mechanical properties

Highlights: • The nonuniform distributions of stress and velocity along whisker lead to whisker breakage. • The microcrack between broken whiskers can propagate into interface or matrix, related to the wedge angle of broken whisker. • The whisker breakage and staggered result in the decreasing distance between neighboring whiskers. • The smaller distance between neighboring whiskers reduces the resistance to the propagation of crack resulting in the lower ultimate tensile strength of extruded composite. - Abstract: Hot extrusion is used to improve the distribution of whiskers and refine the whisker sizes of 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite. The grain size and the ultimate tensile strength of the extruded 2024Al/Al{sub 18}B{sub 4}O{sub 33}w composite are analyzed. The results show that the average length of whiskers decreases due to the whisker breakage. The nonuniform distributions of stress and velocity along the whisker lead to whisker breakage. The microcrack between the broken whiskers can propagate into the interface or the matrix, related to the wedge angle of the broken whisker. The extrusion is beneficial to the whisker staggered and makes it easy for the microcracks filled with matrix. The whisker breakage and the whisker staggered result in the decreasing distance between the neighboring whiskers. Due to the dislocation motion constrained by matrix and the overlap of the deformation areas, the decreasing distance between the neighboring whiskers promoting the recrystallization results in the smaller grain size. During tensile tests, due to the smaller resistance with the smaller distance between the neighboring whiskers, the cracks between the progressive broken whiskers are easy to coalesce resulting in the lower ultimate tensile strength of the extruded composite.

36 MATERIALS SCIENCE↗

Characterization of texture and grain boundary character distributions of selective laser melted Inconel 625 alloy

Highlights: • <110> texture along layer build direction was generated in as-SLMed Inconel 625. • The stress relief process dominates texture and GBCD evolution. • SLMed IN 625 alloy can be GBEed via suitable post annealing. - Abstract: Select laser melting (SLM) is one of the practical metal additive manufacturing processes to fabricate complex structures. The inhomogeneous microstructure and high residual stress are typically resulted from a non-uniform melting and rapid solidification during a SLM process, which has the significant impact on part dimensional instability, corrosion resistance, and mechanical properties. The bulk of current research is limited to the general characterization of grain size, texture, and mechanical properties. However, grain boundary character distribution (GBCD) and its relationship with texture are yet to be understood. This study has shown that the preferred <110> along building direction and <100> along laser scanning direction were produced. The high density of low angle grain boundary (LAGB) can be an indicator of residual stress levels in the as-SLMed samples. The newly-developed ∑3, ∑9 and ∑27 grain boundaries were heavily populated, and the cluster of grains interfaced by ∑3{sup n} (n = 0, 1, 2…) was introduced at the expense of LAGB only at high recrystallization annealing (1150°C or over). The research results suggest that GBCD optimization be possible in the SLMed Inconel 625 alloy via suitable post annealing, which allows improving intergranular corrosion resistance and enhancing mechanical properties.

36 MATERIALS SCIENCE↗

Precipitation behavior of L12 Al3Zr phase in Al-Mg-Zr alloy

Highlights: • Precipitation behavior of the as-cast Al-3.0Mg-0.25Zr alloy was studied. • Discontinuous and continuous precipitation mechanisms of Al{sub 3}Zr phase are observed. • Precipitation type changes from discontinuous to continuous at two-step annealing. • Developed treatment mode provides high dispersoids dense and maximum aging effect. - Abstract: Increasing the recrystallization resistance and the mechanical properties of aluminum-based alloys is possible due to the formation of a nanoscale L1{sub 2}-structured Al{sub 3}Zr phase. Treatment conditions and alloys composition affect the size and density of dispersoids and their final properties. In this work we analyze the decomposition of the supersaturated solid solution in the as-cast Al-3%Mg-0.25%Zr alloy for different annealing modes to understand the precipitation kinetics of the Al{sub 3}Zr phase in the presence of Mg. We found that both discontinuous and continuous precipitation mechanisms of the Al{sub 3}Zr phase are possible in the studied low-alloyed material. One-step annealing leads to the formation of coarse (17 nm) spherical precipitates of a coherent L1{sub 2}-structured Al{sub 3}Zr phase and discontinuously formed fan-shaped aggregations of the same phase. Two-step annealing provided for the maximum precipitation hardening with the formation of high-density nanoscale (7 nm) dispersoids of the Al{sub 3}Zr phase. This study highlights the importance of the annealing mode of the as-cast material for achieving a high density of the fine L1{sub 2} structured Al{sub 3}Zr phase and the maximum hardening effect.

36 MATERIALS SCIENCE↗

Effect of stored strain energy heterogeneity on microstructure evolution of 90% cold rolled AISI 304L stainless steel during interrupted annealing treatment

Highlights: • Study of usefulness of stored strain energy distribution map of the material for variable temperature range. • Advantage of using stored strain energy distribution map • Variation observed in stored energy between isothermal annealing treatment and interrupted annealing treatment. - Abstract: This research work is an attempt to understand the effect of stored strain energy heterogeneity over macro-scale, induced during interrupted annealing treatment, on the micro structural evolution in a heavily cold rolled AISI 304L austenitic stainless steel. The cold rolled AISI 304L stainless steel (SS) samples were subjected to different annealing treatments. The microstructures obtained after each annealing treatment were characterized using optical and electron microscopy techniques. Further, an attempt was made to estimate the stored strain energy by a novel approach of micro hardness measurement both over small scale (area 3600 μm{sup 2}) and large scale (area ~0.25 mm{sup 2}). The stored strain energy was determined using hardness values. Using these data, spatial stored strain energy distribution contour maps were created. They were, in turn, used to characterize the local softening behavior both at micro and macro-scale levels after each interrupted annealing treatment. The results showed that, interrupted annealing treatment induces increased stored strain energy heterogeneity after each annealing interruptions. Also, it was possible to determine recrystallization kinetics of the material using stored strain energy map, which helps in designing annealing cycles for achieving ultrafine grained microstructure.

36 MATERIALS SCIENCE↗

Resolving the geometrically necessary dislocation content in severely deformed aluminum by transmission Kikuchi diffraction

Highlights: • Grain fragmentation and steady-state stages occur during HPT processing. • A gradual transformation of LAGBs to HAGBs is characterized in both regimes. • During plastic deformation, dislocations gather collectively as geometrical walls. • The presence of GNDs is more pronounced in the vicinity of already existing HAGBs. • The density of GNDs is greater in the fragmentation stage. - Abstract: In this paper, severe plastic deformation (SPD) is applied to commercially pure aluminum. Monotonic high pressure torsion (HPT) processing is employed at room temperature, and the microstructure of samples deformed up to an equivalent strain of 50 is investigated by electron backscatter diffraction (EBSD). The distribution pattern and the density of geometrically necessary dislocations (GNDs) are evaluated by examination of transmission Kikuchi diffraction (TKD) maps. Three different methodologies are utilized for assessment of the GND density. It was observed that two distinct stages of grain fragmentation and steady-state occur during processing. During the first stage, a severe grain refinement was observed as the average grain size decreased from ~85 μm to ~1 μm at an equivalent strain of 10. Quantification of the density of dislocations in both deformation regimes showed that, independent of the choice of model, the GND density is greater in the fragmentation stage than in the steady-state stage. This observation was linked with the prevalence of the continuous dynamic recrystallization (CDRX) phenomenon in each stage. Furthermore, a significant presence of GNDs in the steady-state stage was characterized. Formation of microstructure, grain refinement and saturation of grain size are discussed in the light of statistics of GNDs.

36 MATERIALS SCIENCE↗

Characteristics of kinetic sprayed Ta in terms of the deposition behavior, microstructural evolution and mechanical properties: Effect of strain-rate-dependent response of Ta at high temperature

Highlights: • The effect of high-temperature rate-dependent response of BCC Ta on the deposition state of kinetic sprayed Ta particles with synergistic effect of powder oxidation • Abnormal increase of dislocation density above certain powder preheating temperature under the lower condition (N{sub 2} carrier gas), whereas considerable occurrence of grain refinement under the higher condition (He carrier gas). • Most significant dislocation density with the smallest volume-averaged domain size under the condition of 600 {sup o}C powder pre-heating with N{sub 2} carrier gas due to characteristic response of Ta. - Abstract: Numerous efforts have been focused on the fundamental research regarding kinetic spraying processes, but previous studies were biased to only few kinds of metallic materials. In particular, for Ta with body-centered cubic crystal structure, systematic studies are currently lacking in the literature. In this study, the characteristic deposition behaviors, microstructures, and mechanical properties of kinetic sprayed Ta under various impact conditions were systematically investigated. Generally, unusual features were usually related to strain-rate-dependent response (i.e. Peierls-Nabarro short range barriers) of Ta at high-temperature. This made thermal softening effect to be saturated above a certain degree of temperature, contributing to inferior deposition efficiency for the pre-heating at 600 °C than those of 400 and 500 °C by creating synergy with powder oxidation. In terms of microstructural evolutions, the dislocation density was abnormally increased at a certain powder preheating temperature (i.e., 600 °C), owing to the strain-rate-dependent response of Ta at high-temperature. On the other hand, grain refinement generated by rotational dynamic recrystallization was mainly observed under the higher kinetic energy condition (He carrier gas) at RT. Especially, the dislocation density and volume-average domain size evaluated via high-resolution X-ray diffraction peak profile analysis were corresponding to the results of the microstructural observations. Additionally, the nanomechanical properties (i.e., nanohardness and elastic modulus) evaluated via nanoindentation tests were in good agreement with the results from transmission electron microscopy investigations.

36 MATERIALS SCIENCE↗

Mechanical property and microstructure evolution of nitrogen-modified Ti-6Al-4V alloy with core-shell structure by hot compression

Highlights: • Core-shell structured Ti-6Al-4 V is composed of α shells and α + β cores. • Nitrogen solution and core-shell structure significantly enhances the strength. • Core-shell structural alloy performs inhomogeneous deformation. - Abstract: Core-shell (CS) structured Ti-6Al-4 V (Ti64) alloy with single α shells and duplex α + β cores was fabricated by powder nitriding and spark plasma sintering. The mechanical property and microstructure evolution of CS-Ti64 alloy was investigated by compression at temperatures of 950–1100 °C and strain rates of 0.001–1 s{sup −1}. The nitrogen-induced solid solution strengthening and the nitrogen-stabilized CS structure significantly enhanced the compressive strength. Microstructure evolution of CS-Ti64, involved inhomogeneous deformation of the core and shell, which was quite different from that of the commercial Ti64. Regions adjacent to shells and central locations of cores suffered large strain and therefore preferentially underwent dynamic recrystallization (DRX). The deformation mechanism of the novel CS-Ti64 alloy was discussed in terms of the α shells, α laths and DRX.

36 MATERIALS SCIENCE↗

Asymmetric cross rolling (ACR): A novel technique for enhancement of Goss/Brass texture ratio in Al-Cu-Mg alloy

Highlights: • The main components of the ACR were Goss, Rotated Goss, Goss-Brass, and α-fiber. • The ACR process was obviously impactful to enhance the Goss/Brass texture ratio. • The Goss/Brass texture ratio increased to 1.51 after 30% ACR process. • During 30% rolling, the DRX occurred and the intensity of Goss and Cube increased. - Abstract: The present work focused on the effect of asymmetric cross rolling (ACR) process as a novel technique on microstructure and texture evolution of Al-Cu-Mg alloys. The microstructural observation and bulk texture from RD–TD plane of the initial and deformed samples were characterized by optical microscopy (OM) and X-ray diffraction (XRD). It was found that the deformed Al-Cu-Mg alloy consisted of strong Goss, Rotated Goss, Goss-Brass, and α-fiber textures. Usually, straight rolling leads to a significant strengthening of the Brass component with increasing strain in the Al-Cu-Mg alloy, but for asymmetrically cross rolled samples, the Goss orientation was stable after 40% deformation. Results showed that the ACR process was effective to intensify (up to 1.51 after 30% thickness reduction) the low Goss/Brass texture ratio often existing in the rolled Al-Cu-Mg alloy. During 30% ACR, the dynamic recrystallization (DRX) occurred, which led to increasing the intensity of Goss and Cube components and the fraction of extra high angle grain boundaries (EHAGBs).

36 MATERIALS SCIENCE↗

Effect of Mn addition on deformation behaviour of 23% Cr low nickel duplex stainless steel

Highlights: • Increasing Mn content obviously affects dynamic softening behaviour of flow curves. • More complete austenite DRX occurred with middle Mn addition of 10.3% at 1 s{sup −1}. • The constitutive equations for different Mn addition alloys are developed. • The values of activation energy and Z parameter are lowest with middle Mn addition. • Different Mn addition processing maps with increasing strain were established. - Abstract: Isothermal compression testing of 23% Cr low nickel duplex stainless steels, with different Mn concentrations, was investigated in the temperature range of 1173–1423 K, the strain rate range of 0.01–10 s{sup −1} and with a height reduction of 70%. Increasing the Mn content from 6.3 to 14.1% affected the deformation dynamic softening behaviour of flow curves at lower temperature and higher strain rate. It was also observed that increasing the deformation stain rate contributed to flow softening, and was caused by dynamic recrystallization (DRX) as a function of Mn addition. Deformation microstructure analysis demonstrated that more complete austenite phase DRX occurred with 10.3% Mn addition than that with 6.3% Mn addition at 1 s{sup −1}, but an excessive Mn content of 14.1% was unfavourable due to the increase of austenite fraction and stacking fault energy enhancement. Increasing the strain rate to 10 s{sup −1} promoted austenite phase DRX at 1323 K with the Mn addition under large strain. Meanwhile, the ferrite phase DRX occurred at 1173 K/1–10 s{sup −1} with 6.3% Mn, and was weakened with higher Mn addition. Compared to the 6.3% and 14.1% Mn, continuous DRX occurred at 1323 K/1 s{sup −1} with 10.3% Mn, due to the larger fraction of high angle misorientations. The values for the activation energy and Zener–Hollomon parameter decreased with Mn addition from 6.3 to 10.3%, and then increased with a higher Mn addition of 14.1%, indicating that a proper content of Mn addition can reduce the thermal deformation resistance and promote DRX. The constitutive equations for different Mn addition alloys were developed using a hyperbolic sine equation. Processing maps with different Mn addition for the strains of 0.3, 0.6 and 1.2 were established. The 10.3% Mn content sample corresponded to the lowest instability region, implying that the workability was improved with the middle Mn addition.

36 MATERIALS SCIENCE↗

Grain boundary inter-connections in polycrystalline aluminum with random orientation

Highlights: • The GBICs in a pure aluminum are not random, showing remarkable preference on the planes of low Miller index. • {1 1 1}/{1 1 1} is the most frequent GBIC in pure aluminum. • {1 1 1}/{1 1 1} GBIC is mainly coming from the GBs formed by rotations around , and axes. • {1 1 1}/{1 1 1} GBIC possesses higher PCSD and definite dislocation structures compared to the general GBs. • To pursue {1 1 1}/{1 1 1} GBIC is a pint-cut for the GBE research in high stacking fault energy FCC materials. - Abstract: Grain boundary inter-connection (GBIC) is the matching of two crystallographic planes from two abutting grains ending on the grain boundary (GB) position in polycrystalline materials, which can be expressed as {h_1k_1l_1}/{h_2k_2l_2}. GBIC is the critical parameter that intrinsically defines the character and properties of a GB. In current work, a zone-melted polycrystalline aluminum bar with a purity higher than 99.99% (mass fraction) was subjected to a multi-directional forging (MDF) with a true strain of 4 followed by a recrystallization annealing at 360 °C. Such process repeated at least 4 times until an equiaxed-grain microstructure with random orientation and averaged grain size approximate 30 μm was achieved. Then the GBICs were determined by electron backscatter diffraction (EBSD) measurement and stereology-based five-parameter analysis (FPA) coupled with crystallographic analysis after the grain boundaries (GBs) were filtered according to their misorientations (e.g. angle/axis pair). The results revealed that the GBICs for any group of GBs with a given misorientation are not random, showing remarkable preference on the planes of low Miller index forming mixed and twist GBs. The work also demonstrated that among the high angle boundaries (HABs), {1 1 1}/{1 1 1}, including coherent ∑3 boundaries, is the most frequent GBIC, mainly due to the GBs formed by rotations around <1 1 1>, <1 2 2> and <1 1 2> axes. Near coincidence site (NCS) and O-lattice theory analyses indicate that the {1 1 1}/{1 1 1} GBICs usually possess higher planar coincidence site density (PCSD) and definite dislocation structures compared to the general GBs, implying their more structural stability when only crystallography is taken into account. This result agrees very well with the recent results obtained by molecular dynamic simulations. It is significant to the grain boundary engineering (GBE) in the high stacking fault energy (SFE) face-centered cubic (FCC) materials such as aluminum and its alloys.

36 MATERIALS SCIENCE↗

Effect of microstructures on hot compression behavior of a Ti-43Al-2Si alloy fabricated by cold crucible continuous casting

Highlights: • TiAl alloys with different lamellar colonies were fabricated by cold crucible continuous casting. • EBSD was used to investigate the evolution of lamellae during the hot compression. • Lamellar colony boundaries promote the dynamic recrystallization process. - Abstract: To investigate the influence of lamellar orientation and colony boundary on deformation behavior, fully lamellar Ti-43Al-2Si alloys were prepared by cold crucible continuous casting and isothermal compression tests were conducted at different temperatures in the range 1373–1523 K with a strain rate of 0.01 s{sup −1}. The as-cast microstructures were elongated colony with lamellae oriented at nearly 45° to the compression direction and equiaxed colony with various lamellae orientations, respectively. The results revealed that serious cracking or sliding traces appeared on the surface of deformed specimens with elongated colony original microstructure and that their peak stresses were lower compared to those of specimens with equiaxed colony original microstructure. The relationship between deformation behaviors and as-cast microstructure was analyzed in detail. It was found that the recrystallization/globularization level is significantly lower than that in specimens with equiaxed colony original microstructure during hot deformation owing to the preferred nucleation sites in colony boundaries. Finally, the lamellae conversion process was characterized to reveal the softening mechanisms of full lamellar TiAl-based alloy during hot compression.

36 MATERIALS SCIENCE↗

Annealing-induced microstructural evolution and mechanical anisotropy improvement of the Mg-Gd-Y-Zr alloy processed by hot ring rolling

Highlights: • Growth of SRX grains in GBR is random, while that of TBR is anisotropic. • The new texture component in annealed MR weakens the anisotropy obviously. • T6 treatment leads to an excellent comprehensive mechanical property. - Abstract: Hot ring rolling (HRR) is widely used to fabricate large-size seamless ring-shape components. However, this process produces a severe mechanical anisotropy, which is not acceptable in practical industrial application and should be avoided. This paper reports the annealing-induced microstructural evolution and mechanical anisotropy improvement of HRRed Mg-8.12Gd-1.82Y-0.35Zr alloy ring. Results show that annealing treatment could improve the microstructural homogeneity of the ring owing to the occurrence of static recrystallization (SRX). SRX grains are preferentially formed at twin boundaries and initial grain boundaries due to high dislocation density, high level of stored energy, and stress concentration. Twin boundaries, to some extent, can suppress the migration of SRX grain boundaries. In addition, occurrence of SRX weakens the texture intensity and basal pole inclination, leading to a decrease in the mechanical anisotropy of the ring. Considering the weakened anisotropy, comparable strength, and improved ductility, annealing + aging (T6), compared with direct aging (T5), is a more suitable heat treatment schedule for the HRRed Mg-8.12Gd-1.82Y-0.35Zr alloy ring.

36 MATERIALS SCIENCE↗

Friction stir welding of a carbon-doped CoCrFeNiMn high-entropy alloy

Highlights: • Friction stir welding of a CoCrFeNiMn HEA doped with C was successfully obtained. • M{sub 23}C{sub 6} carbides with d≈150 nm form in the HEA due to addition of 0.9 at.% C. • Friction stir welding resulted in a decrease in grain size from 9.2 μm to 4.6 μm. • Smaller grain size and increased fraction of M{sub 23}C{sub 6} increase strength by 84 MPa. - Abstract: Butt-joint seam of a high entropy alloy (HEA) of the CoCrFeNiMn system was successfully obtained by friction stir welding (FSW). The HEA was produced by self-propagating high-temperature synthesis. Along with the principal elements, a small amount (0.9 at.%) of C was added to the alloy. The as-cast alloy was cold rolled and annealed at 900 °C to produce refined microstructure. The structure of the annealed alloy consisted of a recrystallized face-centered cubic matrix with a grain size of 9.2 μm and fine Cr-rich M{sub 23}C{sub 6} carbides. FSW of the HEA resulted in microstructure refinement to d = 4.6 μm in the stir zone. A noticeable rise in strength and some decrease in ductility of the processed alloy in comparison with the initial condition can be associated with the microstructure refinement and some increase in the volume fraction of M{sub 23}C{sub 6} carbides.

36 MATERIALS SCIENCE↗

Effect of niobium interlayer in dissimilar friction stir welding of aluminum to titanium

Highlights: • In the present study, FSW of Al to Ti with Nb interlayer has been characterized. • Fragmentation and distribution of Nb and Ti have been correlated with properties. • Ternary mixing and chemical reaction reduced the brittleness of the joint. • Al in the weld nugget showed a gradient in microstructural features. • The weld with Nb interlayer exhibited higher ductility. - Abstract: The most important issue associated with dissimilar welding is the formation of detrimental intermetallics and consequent reduction in mechanical properties of the weld. It was expected that addition of an interlayer would modify the pattern of the intermetallic formation. The present investigation deals with Friction Stir Welding of aluminum (Al) to titanium (Ti) in presence of niobium (Nb) interlayer. X-ray Computed Tomography results highlighted that fine particles of both Ti and Nb are homogeneously distributed. Large Ti particles are substantially fragmented whereas large Nb particles remain as flakes. Microstructural features of the nugget zone indicated a complex mixing of materials. Jointing had been perceived through elemental diffusion at the interfaces of Al/Ti and Ti/Nb. However, Nb restricted the reaction between Al and Ti, and acted as an efficient interlayer to retard the formation of brittle Al{sub 3}Ti intermetallic phase. Mechanisms of microstructural evolution in Al side of the weld have been identified as Dynamic Recovery, Dynamic Recrystallization and particle stimulated nucleation. Significant improvement in the tensile ductility had been observed due to the presence of finer particles. The presence of Nb in the weld nugget influences the microstructural evolution and tensile properties of the weld by reducing the formation of intermetallics.

36 MATERIALS SCIENCE↗