Search NASA⌕ Search

SEARCH · Search NASA

Results for “solid solution”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 811 records · Page 45

Mapping growth windows in quaternary perovskite oxide systems by hybrid molecular beam epitaxy

Requisite to growing stoichiometric perovskite thin films of the solid-solution A ' 1-x A x B O 3 by hybrid molecular beam epitaxy is understanding how the growth conditions interpolate between the end members A'B O 3 and AB O 3 , which can be grown in a self-regulated fashion, but under different conditions. Using the example of La 1-x Sr x VO 3 , the two-dimensional growth parameter space that is spanned by the flux of the metal-organic precursor vanadium oxytriisopropoxide and composition, x , was mapped out. The evolution of the adsorption-controlled growth window was obtained using a combination of X-ray diffraction, atomic force microscopy, reflection high-energy electron-diffraction (RHEED), and Rutherford backscattering spectroscopy. It is found that the stoichiometric growth conditions can be mapped out quickly with a single calibration sample using RHEED. Once stoichiometric conditions have been identified, the out-of-plane lattice parameter can be utilized to precisely determine the composition x . This strategy enables the identification of growth conditions that allow the deposition of stoichiometric perovskite oxide films with random A-site cation mixing, which is relevant to a large number of perovskite materials with interesting properties, e.g., high-temperature superconductivity and colossal magnetoresistance, that emerge in solid solution A ' 1-x A x B O 3 .

36 MATERIALS SCIENCE↗

Synthesis, crystal structure and properties of SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ}

The solid solution formation range in the SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ} (0≤x≤2) system examined at 1100 °C in air corresponds to 0≤x≤1.1. The crystal structure of SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ} with x≤0.5 was described as orthorhombic (space group Pmmm), and with 0.6≤x≤1.1—as tetragonal (P4/mmm). The introduction of iron into the cobalt sublattice leads to a gradual increase of the unit cell parameters and volume, accompanied with increasing oxygen content determined by thermogravimetry. The dilatometric curves collected at 25–1100 °C in air exhibit moderate nonlinearities associated with the orthorhombic→tetragonal phase transition, as confirmed by the high-temperature X-ray diffraction analysis. Temperature dependencies of the electrical conductivity measured by 4-probe dc method in the temperature range 25–1000 °C in air display maxima at 300–350 °C, whilst the conductivity decreases with iron additions. These trends were discussed in terms of the defect structure and nature of the main charge carriers in SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ}. It was also shown that SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ} is chemically stable with respect to the Ce{sub 0.8}Sm{sub 0.2}O{sub 1.9} solid electrolyte up to 1100 °S, but reacts with Zr{sub 0.85}Y{sub 0.15}O{sub 1.93} even at 900 °S. Highlights: • The solid solution formation range in the SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ} system at 1100 °C in air corresponds to 0≤x≤1.1. • The unit cell volume and oxygen content in the solid solutions increase with x. • Oxygen nonstoichiometry of SmBaCo{sub 2−x}Fe{sub x}O{sub 5+δ} solid solutions. • Temperature dependencies of the electrical conductivity exhibit maxima at the temperatures when oxygen exchange with the gaseous phase becomes significant.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Selectivity Principles in Anion Separation by Crystallization of Hydrogen-Bonding Capsules

The fundamental factors controlling anion selectivity in the crystallization of hydrogen-bonding capsules [Mg(H2O)6][X L2] (X = SO42-, 1a; SeO42-, 1b; SO32-, 1c; CO32-, 1d; L = tris[2-(3-pyridylurea)ethyl]-amine) from water have been investigated by solution and solid-state thermodynamic measurements, anion competition experiments, and X-ray structural analysis. The crystal structures of 1a-d are isomorphous, thereby simplifying the interpretation of the observed selectivities based on differences in anion coordination geometries. The solubilities of 1a-d in water follow the order: 1a < 1b < 1c < 1d, which is consistent with the selectivity for the tetrahedral sulfate and selenate anions observed in competitive crystallization experiments. Crystallization of the capsules is highly exothermic, with the most favorable {Delta}H{sub cryst}{sup o} of -99.1 and -108.5 kJ/mol corresponding to SO42- and SeO42-, respectively, in agreement with the X-ray structural data showing shape complementarity between these tetrahedral anions and the urea-lined cavities of the capsules. Sulfite, on the other hand, has a significantly less negative {Delta}H{sub cryst}{sup o} of -64.6 kJ/mol, which may be attributed to its poor fit inside the capsules, involving repulsive interactions. The more favorable entropy of crystallization for this anion, however, partly offsets the enthalpic disadvantage, resulting in a solubility product very similar to that of the selenate complex. Because of their very similar shape and size, SO42- and SeO42- have a propensity to form solid solutions, which limits the selectivity between these two anions in competitive crystallizations. In the end, a comprehensive picture of contributing factors to anion selectivity in crystalline hydrogen-bonding capsules emerges.

36 MATERIALS SCIENCE↗

Enhancement of the colossal magnetoresistance in Eu{sub 1-x}Ca{sub x}B{sub 6}

The transport and magnetic properties of single crystal samples of substitutional solid solutions Eu{sub 1-x}Ca{sub x}B{sub 6} (0 {<=} x {<=} 0.26) have been studied at temperatures 1.8-300 K in magnetic fields up to 80 kOe. It has been shown that an increase in the calcium concentration results in the suppression of the charge transport accompanied by an increase in the amplitude of the colossal magnetoresistance (CMR) up to the value ({rho}(0) - {rho}(H))/{rho}(H) {approx} 7 x 10{sup 5} detected for x = 0.26 at liquid-helium temperature in a field of 80 kOe. The transition from the hole-like conductivity to the electron-like conductivity has been observed in the Eu{sub 0.74}Ca{sub 0.26}B{sub 6} solid solution in the CMR regime at T < 40 K. The Hall mobility values {mu}H = 200-350 cm{sup 2}/(V s) estimated for charge carriers in the strongly disordered matrix of the Eu{sub 0.74}Ca{sub 0.26}B{sub 6} solid solution are comparable with the charge carrier mobility {mu}H = 400-600 cm{sup 2}/(V s) for the undoped EuB{sub 6} compound. The anomalous behavior of the transport and magnetic parameters of the Eu{sub 1-x}Ca{sub x}B{sub 6} solid solutions is discussed in terms of a metal-insulator transition predicted within the double exchange model for this system with low carrier density.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Crystal structure and dielectric properties of a new Na2O-Nd2O3-CeO2 ceramic system at microwave frequencies

Highlights: • A large amount of Na evaporation can make τ{sub f} more negative in present ceramics. • Na-excess evaporation results in the formation of Ce{sub 1-x}Nd{sub x}O{sub 2-x/2} solid solution. • Ce{sub 1-x}Nd{sub x}O{sub 2-x/2} (x = 0.25 and 0.5) solid solutions belong to the same fluorite-type. - Abstract: Na{sub 2}O-Nd{sub 2}O{sub 3}-CeO{sub 2} ceramic systems of the form Na{sub 3x−1}Nd{sub 1−x}CeO{sub 3} (x = 0.4, 0.5, and 0.6) were prepared via a solid-state reaction method. X-ray diffraction analyses indicated that the samples with x = 0.4, 0.6 and those with x = 0.5 formed Nd{sub 0.25}Ce{sub 0.75}O{sub 1.875} and Nd{sub 0.5}Ce{sub 0.5}O{sub 1.75} solid solutions, respectively, which resulted from a large degree of Na{sup +} ion evaporation. Both the Nd{sub 0.25}Ce{sub 0.75}O{sub 1.875} and Nd{sub 0.5}Ce{sub 0.5}O{sub 1.75} phases belonged to the same cubic structure with an Fm-3m (225) space group. Additionally, the microstructures, sintering behaviors, and microwave dielectric properties were considered to be strongly related to the Na content in the Na{sub 3x−1}Nd{sub 1−x}CeO{sub 3} ceramics. A relatively large degree of Na{sup +} ion evaporation could increase the negative temperature coefficient of the resonant frequency (τ{sub f}) for these ceramic systems. Moreover, after sintering at 1380 °C for 2 h, the x = 0.6 specimen possessed a low permittivity (ε{sub r}) of approximately 9.13, a moderate quality factor (Q × f) of approximately 23,800 GHz (at 9.14 GHz) and a negative τ{sub f} value of approximately −61.7 ppm/°C. As a result, it could be a promising microwave dielectric material for achieving a near-zero τ{sub f} value by solidifying one or more microwave dielectric ceramics with a high positive τ{sub f} value.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Structural and magnetic properties of a mechanochemically activated Ti-Fe{sub 2}O{sub 3} solid mixture

The mechanochemical effects on the reactivity and properties of a titanium/hematite powder mixture with molar ratio of 1/2 are investigated. Crystalline-phase structure, composition, hyperfine and magnetic behaviors were analyzed as a function of activation time by means of X-ray diffraction, scanning electron microscopy, Moessbauer spectroscopy and vibrating sample magnetometry. The results showed that at relatively short activation times metallic Ti reduces part of the ferric ions, yielding a complex product formed mainly by a mix of two solid solutions Fe{sub 3-x}Ti{sub x}O{sub 4} (titanomagnetites), both with very different x values (0 < x < 1). Also metallic iron and superparamagnetic hematite particles were detected by Moessbauer spectroscopy. As the mechanical treatment extends the composition of the reactive mixture changes, prevailing in the end the solid solution with higher x value. In contrast, when these activated samples are thermally treated the fraction of the solid solution which is richer in Ti diminishes. This fact produces a significant variation of the saturation magnetization of the obtained material.

36 MATERIALS SCIENCE↗

New solid acids in the triple-layer Dion-Jacobson layered perovskite family

Research highlights: {yields} New triple-layer Dion-Jacobson layered perovskite solid solutions synthesized. {yields} New series of Ta-doped layered perovskite solid acids, HCa{sub 2}Nb{sub 3-x}Ta{sub x}O{sub 10}. {yields} New series of Sr-doped layered perovskite solid acids, HCa{sub 2-x}Sr{sub x}Nb{sub 3}O{sub 10}. {yields} Layered perovskites with highest Ta content are weaker solid acids than HCa{sub 2}Nb{sub 3}O{sub 10}. -- Abstract: Dion-Jacobson type layered perovskites such as A'Ca{sub 2}Nb{sub 3}O{sub 10} (A' = K, Rb, H) have continued to be of great interest due to their compositional variability, rich interlayer chemistry, and wide range of physical properties. In this study, we investigated the range and effects of substitutional doping of Ta{sup 5+} for Nb{sup 5+} and of Sr{sup 2+} for Ca{sup 2+} in A'Ca{sub 2}Nb{sub 3}O{sub 10}. We have prepared and characterized three new solid solutions: KCa{sub 2}Nb{sub 3-x}Ta{sub x}O{sub 10}, RbCa{sub 2}Nb{sub 3-x}Ta{sub x}O{sub 10}, and RbCa{sub 2-x}Sr{sub x}Nb{sub 3}O{sub 10}. These materials all readily undergo proton exchange to form two new series of hydrated solid acid phases, which in most cases can be dehydrated to form stable HCa{sub 2}Nb{sub 3-x}Ta{sub x}O{sub 10} and HCa{sub 2-x}Sr{sub x}Nb{sub 3}O{sub 10} compounds. Intercalation studies with n-hexylamine and pyridine were carried out to gauge the relative Bronsted acidities across the HCa{sub 2}Nb{sub 3-x}Ta{sub x}O{sub 10} series, and we determined that materials with the highest tantalum contents are weaker acids than the parent compound HCa{sub 2}Nb{sub 3}O{sub 10}. Preliminary intercalation studies with pyridine for the HCa{sub 2-x}Sr{sub x}Nb{sub 3}O{sub 10}.yH{sub 2}O solid acids, however, showed no significant difference in acidity with varying strontium content.

36 MATERIALS SCIENCE↗

Thermodynamic model for the solubility of BaSeO4(cr) in the aqueous Ba2+-SeO42--Na+-H+-OH--H2O system: Extending to high selenate concentrations

The solubility of Ba(SeO4, SO4) precipitates was determined as a function of the BaSeO4 mole fractions, ranging from 0.0015 to 0.3830, and time with an equilibration period extending to as long as 302 days. Equilibrium/steady state conditions in this system are reached in ≤ 65 days. Pitzer’s ion interaction model was used to calculate solid and aqueous phase activity coefficients. Thermodynamic analyses showed that the data do not satisfy Gibbs-Duhem equation, thereby demonstrating that a single-solid solution phase does not control both the selenate and sulfate concentrations. Our extensive data with log10 [Ba]) ranging from -3.6 to -5.9 mol.kg-1, log10 [SeO4]) ranging from -3.6 to -5.2 mol.kg-1, and log10 [SO4] ranging from -4.0 to -5.3 mol.kg-1 can be explained with the formation of an ideal BaSeO4 solid solution phase that controls the selenium concentrations and a slightly disordered/less-crystalline BaSO4(s) (log10 K0sp = -9.5 instead of -10.05 for barite) that controls the sulfate concentrations. In these experiments the BaSO4 component of the solid solution phase never reaches thermodynamic equilibrium with the aqueous phase. Thermodynamic interpretations of the data show that both the ideal BaSeO4 solid solution phase and less-crystalline BaSO4(s) phase are in equilibrium with each other in the entire range of BaSeO4 mole fractions investigated in this study.

Rai, Dhanpat↗

Atomic Ordering-Induced Ensemble Variation in Alloys Governs Electrocatalyst On/Off States

The catalytic behavior of a material is influenced by ensembles—the geometric configuration of atoms. Traditional approaches, mainly utilizing solid-solution alloys in electrocatalysis, have often overlooked the challenges posed by concurrent changes in the electronic structure (i.e. d-band center) when the composition is altered. Here, this study introduces a methodology that distinctly separates the geometric effects (i.e. ensembles) from the electronic structure. We compare the reactivity of compositionally identical, but structurally different Pd 3 Bi ordered intermetallic and solid-solution alloys. Remarkably, we find that Pd 3 Bi intermetallics display nearly no reactivity for the methanol oxidation (MOR), while their solid-solution counterparts have significant reactivity. This highlights a unique case where materials with identical chemical compositions demonstrate drastically different catalytic behavior underscoring the critical importance of ensembles in electrocatalysis. Specifically, Pd 3 Bi intermetallics form smaller ensembles (average coordination number: 4.5 ± 1.6) with almost no measurable MOR activity at room temperature, in contrast to the solid-solution Pd 3 Bi that exhibit larger ensembles (average coordination number: 6.8 ± 0.9) and considerable MOR reactivity (0.5 mA cm −2 Pd ). An ordered Pd 3 Bi alloy, with an intermediate ensemble size (average coordination number: 5.3 ± 1.2), displays moderate MOR activity (0.1 mA cm −2 Pd ), further confirming the direct correlation between ensemble size and catalytic activity. Notably, all Pd 3 Bi alloys maintain similar electronic structures, because the chemical composition of the alloys is fixed, indicating that the differences in reactivity are predominantly from changes to the ensemble size. Our findings offer an approach for precisely controlling catalytic activity through manipulating the geometric configuration of the atoms within an alloy, paving the way for more efficient catalyst design.

alloys↗

Thermodynamic Model for the Solubility of Ba(SeO 4 , SO 4 ) Precipitates

The solubility of Ba(SeO 4 , SO 4 ) precipitates was determined as a function of the BaSeO 4 mole fractions, ranging from 0.0015 to 0.3830, and time with an equilibration period extending to as long as 302 days. Equilibrium/steady state conditions in this system are reached in ≤ 65 days. Pitzer’s ion interaction model was used to calculate solid and aqueous phase activity coefficients. Thermodynamic analyses showed that the data do not satisfy Gibbs-Duhem equation, thereby demonstrating that a single-solid solution phase does not control both the selenate and sulfate concentrations. Our extensive data with log 10 [Ba] ranging from -3.6 to -5.9 mol kg -1 , log 10 [SeO 4 ] rangingfrom-3.6 to -5.2 mol kg -1 , and log 10 [SO 4 ] ranging from-4.0 to -5.3 mol kg -1 can be explained with the formation of an ideal BaSeO 4 solid solution phase that controls the selenium concentrations and a slightly disordered/less-crystalline BaSO 4 (s) (log 10 Κ° sp = -9.5 instead of -10.05 for barite) that controls the sulfate concentrations. In these experiments the BaSO 4 component of the solid solution phase never reaches thermodynamic equilibrium with the aqueous phase. Thermodynamic interpretations of the data show that both the ideal BaSeO 4 solid solution phase and less-crystalline BaSO 4 (s) phase are in equilibrium with each other in the entire range of BaSeO 4 mole fractions investigated in this study.

Rai, D.↗

Phase Diagram and Dielectric Properties of (1–x)Ba(Ti{sub 1–y}Zr{sub y})O{sub 3} · xPbTiO{sub 3} Ceramics

Ceramic (1–x)Ba(Ti1–yZry)O{sub 3} · xPbTiO{sub 3} (0 ≤ x, у ≤ 1) samples have been characterized by X-ray diffraction and dielectric measurements. The results have been used to map out the phase diagram of the system, which demonstrates the variation in the phase composition of the samples. It has been shown that, in the composition regions adjacent to the BaTiO{sub 3}–PbTiO{sub 3} side and BaZrO{sub 3} corner of the composition triangle, the samples consist of perovskite solid solutions that have tetragonal and cubic structures, respectively, at room temperature. In the intermediate composition region, the samples consist of different perovskite solid solutions similar in composition and structure. We have obtained composition dependences of the unit-cell symmetry and parameters for the solid solutions, their ferroelectric Curie temperature T{sub C}, characteristic dielectric relaxation temperatures, dielectric permittivity ε, and dielectric loss tangent tanδ (at temperatures from 100 to 800 K and frequencies from 25 to 106 Hz) and analyzed the evolution of their dielectric properties with increasing BaZrO{sub 3} content: from ferroelectric to properties of ferroelectric relaxors, reentrant relaxors, and dielectric relaxors of the dipole glass type.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Intrinsic thermal expansion and tunability of thermal expansion coefficient in Ni-substituted Co 2 V 2 O 7

Abstract Framework oxide materials are well-known for exhibiting not only negative thermal expansion (NTE), but also demonstrating thermal expansion that can be controlled using composition as a tuning parameter. In this work, we study the intrinsic thermal expansion properties of Co 2 V 2 O 7 , which has shown bulk linear NTE, and attempt to understand how substituting Ni 2+ for Co 2+ will affect the thermal expansion. The isomorphic solid solution is synthesized through solid-state methods and characterized using x-ray diffraction (XRD), diffuse reflectance spectroscopy, and neutron diffraction. The size difference between Ni 2+ and Co 2+ as well as the polyhedral volume of each Co 2+ metal coordination environment in the crystal structure allows Ni 2+ to partially be directed toward one crystallographic site over the other. Variable temperature synchrotron XRD data are employed to understand intrinsic thermal expansion. Across the solid solution, no intrinsic NTE is observed at the microscopic level, yet a degree of tunability in the thermal expansion coefficient with Ni substitution is demonstrated. The disparities between the intrinsic and bulk thermal expansion properties suggest that a morphological mechanism may have resulted in NTE in the bulk.

Materials Science↗

Crystal structure and magnetic properties of complex oxides Mg{sub 4-x}Ni{sub x}Nb{sub 2}O{sub 9}, 0{<=}x{<=}4

In the Mg{sub 4-x}Ni{sub x}Nb{sub 2}O{sub 9} (0{<=}x{<=}4) system two ranges of solid solution have been found. One of the solid solutions has a corundum-related structure type (space group P3-barc1); the second one adopts the II-Ni{sub 4}Nb{sub 2}O{sub 9} structure type (space group Pbcn). The unit cell constants and atomic positions have been determined and refined using neutron powder diffraction data. Electron diffraction and high-resolution transmission electron microscopy (HRTEM) from MgNi{sub 3}Nb{sub 2}O{sub 9} crystals identify the presence of planar defects and the intergrowth of several (structurally related) phases. The magnetic susceptibility of Mg{sub 3}NiNb{sub 2}O{sub 9}, measured in the temperature range T=2-300 K, shows no indications of magnetic ordering at low temperatures, while for MgNi{sub 3}Nb{sub 2}O{sub 9} there is a magnetic ordering at temperatures below 45.5 K. - Graphical abstract: HREM image showing planar defects in MgNi{sub 3}Nb{sub 2}O{sub 9} and their schematic representation.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Structural investigations on Co{sub 3-x}Mn{sub x}TeO{sub 6}; (0 < x ≤ 2); High temperature ferromagnetism and enhanced low temperature anti-ferromagnetism

In the quest of materials with high temperature ferromagnetism and low temperature anti-ferromagnetism, we prepare Co{sub 3-x}Mn{sub x}TeO{sub 6}; (0 < x ≤ 2) solid solutions. Room temperature structural investigations on these solid solutions as a function of Mn concentration using Synchrotron X-ray diffraction (SXRD) and X-ray absorption near edge structure measurements in corroboration with magnetism are presented. Phase diagram obtained from Rietveld Refinement on SXRD data as a function of Mn concentration indicates doping disproportionate mixing of both monoclinic (C2/c) and rhombohedral (R 3{sup ¯}) structure for x < 0.5, while only R 3{sup ¯} structure for x ≥ 0.5. Further, it shows increase in both lattice parameters as well as average transition metal-oxygen (Co/Mn-O) bond lengths for x ≥ 0.5. Co and Mn K-edge XANES spectra reveal that both Co and Mn are in mixed oxidation state, Co{sup 2+}/Mn{sup 2+} and Co{sup 3+}/Mn{sup 3+}. Relative ratios of Co{sup 3+}/Co{sup 2+} and Mn{sup 3+}/Mn{sup 2+} obtained using Linear combination fit decrease with increasing x (for x ≥ 0.5). These structural and spectroscopic evidences are used to provide possible interpretation of the observed paramagnetic to ferromagnetic transition at around 185 K followed by an enhanced antiferromagnetic transition ∼45 K for x = 0.5.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Phase equilibria and crystal chemistry of the CaO–½Sm 2 O 3 –CoOz system at 885 °C in air

The CaO–½Sm 2 O 3 –CoOz system prepared at 885 °C in air consists of two calcium cobaltate compounds, namely, the 2D thermoelectric oxide solid solution, (Ca 3$-$x Sm x )Co 4 O 9$-$z (0 ≤ x ≤ 0.5) which has a misfit layered structure, and the 1D Ca 3 Co 2 O 6 which consists of chains of alternating CoO 6 trigonal prisms and CoO 6 octahedra. Ca 3 Co 2 O 6 was found to be a point compound without the substitution of Sm on the Ca site. A solid solution region of distorted perovskite, (Sm 1$-$x Ca x )CoO 3$-$z (0 ≤ x ≤ 0.22, space group Pnma) was established. The reported Sm 2 CoO 4 phase was not observed at 885 °C, but a ternary Ca-doped oxide, (Sm 1+x Ca 1$-$x )CoO 4$-$z (Bmab) where 0 < x ≤ 0.15 was found to be stable at this temperature. In the peripheral binary systems, Sm was not present in the Ca site of CaO, while a small solid solution region was identified for (Sm 1$-$x Ca x )O(3 $-$z)/2 (0 ≤ x ≤ 0.075). Lastly, ten solid solution tie-line regions and six three-phase regions were determined in the CaO–½Sm 2 O 3 –CoO z system in air.

36 MATERIALS SCIENCE↗

Special features of the excitation spectra and kinetics of photoluminescence of the Si{sub 1-x}Ge{sub x}:Er/Si structures with relaxed heterolayers

Luminescent properties of heteroepitaxial Si{sub 1-x}Ge{sub x}:Er/Si structures with relaxed heterolayers are studied. The results of combined studies of the excitation spectra and kinetics of photoluminescence (PL) are used to single out the components providing the largest contribution to the PL signal of the Si{sub 1-x}Ge{sub x}:Er/Si structures in the wavelength region of 1.54 {mu}m. It is shown that relaxation of elastic stresses in the Si{sub 1-x}Ge{sub x}:Er heterolayer affects only slightly the kinetic characteristics of erbium luminescence and manifests itself in insignificant contribution of the defects and defect-impurity complexes to the luminescent response of the Si{sub 1-x}Ge{sub x}:Er/Si structures. In the excitation spectra of the erbium PL, special features related to the possibility of the rare-earth impurity excitation at energies lower than the band gap of the Si{sub 1} {sub -x}Ge{sub x} solid solution are revealed. It is shown that a peak the width of which depends on the band gap of the solid solution and the extent of its relaxation is observed in the excitation spectra of the erbium-related PL in the Si{sub 1-x}Ge{sub x}:Er/Si structures in the wavelength region of 1040-1050 nm. The observed specific features are accounted for by involvement of intermediate levels in the band gap of the Si{sub 1-x}Ge{sub x}:Er solid solution in the process of excitation of an Er{sup 3+} ion.

36 MATERIALS SCIENCE↗

A study of microstructure of Fe-Cu-Ni-Sn and Fe-Cu-Ni-Sn-VN metal matrix for diamond containing composites

Highlights: • A nanocrystalline sample of coarse-grained powders of iron, copper, nickel, tin was obtained. • The structure of the sample consists of a supersaturated solid solution of nitrogen and vanadium in α-Fe. • Grain refinement occurs as a result of the decomposition of supersaturated solid solution of nitrogen and vanadium in α-Fe. To obtain bulk of 51Fe–32Cu–9Ni–8Sn and 49.47Fe–31.04Cu–8.73Ni–7.76Sn–3VN nanocomposites, a pressing method at room temperature and subsequent hot pressing in a vacuum was used. The microstructure of the sintered composites by X-ray diffraction and transmission electron microscopy was investigated. It is shown that in the 49.47Fe–31.04Cu–8.73Ni–7.76Sn–3VN composite there was a dissolution of vanadium nitride in γ‑iron and formation of a supersaturated solid solution of nitrogen and vanadium in the α‑iron. As a result, there was a substantial grinding of ferrite grains (from 5 to 50 μm to 20–400 nm) as compared to a sample without vanadium nitride (from 5 to 50 μm to 400–800 nm). Nanocomposites are considered as promising materials to create a new generation of diamond containing composites.

77 NANOSCIENCE AND NANOTECHNOLOGY↗