Si-doped β -(Al 0.26 Ga 0.74 ) 2 O 3 thin films and heterostructures grown by metalorganic vapor-phase epitaxy
We report on n-type degenerate doping in β-(Al 0.26 Ga 0.74 ) 2 O 3 epitaxial thin films grown by metalorganic vapor-phase epitaxy and modulation doping in β-(Al 0.26 Ga 0.74 ) 2 O 3 /β-Ga 2 O 3 heterostructures. Here, the alloy composition is confirmed using high-resolution X-ray diffraction measurements. Carrier concentration in the thin films is proportional to the silane molar flow. Room-temperature Hall measurements showed a high carrier concentration of 6 × 10 18 cm –3 to 7.3 × 10 19 cm –3 with a corresponding electron mobility between 53–27 cm 2 V –1 s –1 in uniformly doped β-(Al 0.26 Ga 0.74 ) 2 O 3 layers. Modulation doping is used to realize a total electron sheet charge of 2.3 × 10 12 cm –2 in a β-(Al 0.26 Ga 0.74 ) 2 O 3 /β-Ga 2 O 3 heterostructure using a uniformly doped β-(Al 0.26 Ga 0.74 ) 2 O 3 barrier layer and a thin spacer layer.