Search NASA⌕ Search

SEARCH · Search NASA

Results for “Pyrolysis”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 829 records · Page 46

Swell Behavior of Elastomers with a Hydrothermal Liquefaction Bio-Crude and a Fast Pyrolysis Bio-Oil

The compatibility of seventeen elastomer materials with two heavy biofuels (fast pyrolysis bio-oil and hydrothermal liquefaction (HTL) bio-crude) and diesel was assessed through volume change measurements. The elastomers included two fluorocarbons, six acrylonitrile rubbers (NBRs), and one each of fluorosilicone, neoprene, polyurethane, silicone, epichlorohydrin rubber (ECO), a blend of polyvinyl chloride and NBR (OZO), styrene butadiene rubber (SBR), hydrogenated NBR (HNBR) and ethylene propylene diene monomer (EPDM). The specimens were immersed in each test fuel for four weeks at 50°C and then measured for volume change. Afterwards, the specimens were dried, and the volume was remeasured. Ingeneral, the bio-oil produced unacceptable swelling in the fluoroelastomers, ECO, OZO, neoprene, polyurethane, SBR, HNBR, EPDM, silicone and five of the NBRs. In most cases, the HTL bio-crude produced lower (though still unacceptable) swelling than the bio-oil. Materials that showed good compatibility with the HTL biocrude were the fluoroelastomers, OZO, and silicone.

Kass, Michael↗

Electrochemical Corrosion Analysis of Stainless Steels in LALM Pyrolysis Bio-Oil with Organic Corrodents

Pyrolysis bio-oils are corrosive to low alloy steels, e.g., 2.25Cr-1Mo, 5Cr-1Mo, and 9Cr-1Mo grades. To identify the alloys with sufficient bio-oil compatibility, several commercial stainless steels were examined in bio-oil using electrochemical impedance spectroscopy to semi quantitatively assess their corrosion resistance. Low-Ash Low-Moisture (LALM) bio-oil, produced from a forest residue feedstock by the National Renewable Energy Laboratory in Golden, CO, was used as a test liquid for electrochemical impedance spectroscopy measurements. Three organic corrodents, formic acid, catechol, and lactobionic acid, were added into LALM bio-oil to produce test liquids with intentionally increased corrosivity. Corrosion reaction resistance, determined from the impedance data, was used to evaluate the corrosion compatibility of each stainless steel in LALM bio-oil and LALM bio-oil + organic corrodent(s). The results from corrosion reaction resistance indicated that the critical Cr content of stainless steels for corrosion resistance would be greater than 14 wt % if Ni and Mo contents are low but can be as low as 12–13 wt % with appreciable amounts of Ni and Mo.

Jun, Jiheon↗

Rapid pyrolysis to form super ionic conducting lithium garnets

A method of preparing a lithium-ion conducting garnet via low-temperature solid-state synthesis is disclosed. The lithium-ion conducting garnet comprises a substantially phase pure aluminum-doped cubic lithium lanthanum zirconate (Li 7 La 3 Zr 2 O 14 ). The method includes preparing nanoparticles comprising lanthanum zirconate (La 2 Zr 2 O 7 -np) via pyrolysis-mediated reaction of lanthanum nitrate (La(NO 3 ) 3 ) and zirconium nitrate (Zr(NO 3 ) 4 ). The method also includes pyrolyzing a solid-state mixture comprising the La 2 Zr 2 O 7 -np, lithium nitrate (LiNO 3 ), and aluminum nitrate (Al(NO 3 ) 3 ) to give the Li 7 La 3 Zr 2 O 14 and thereby prepare the lithium-ion conducting garnet. A lithium-ion conducting garnet prepared via the method is also disclosed.

Daemen, Luc L.↗

Microwave-assisted pyrolysis of hydrocarbons using iron-based alumina catalysts obtained via solution combustion synthesis

The demand for hydrogen is growing which makes the development of clean and efficient H2 synthesis technologies imperative. Microwave-assisted, thermocatalytic, dehydrogenation of hydrocarbons has demonstrated the ability to generate H2 with high yield and selectivity, leaving behind valuable solid carbon byproducts. However, this microwave-assisted process is unoptimized which prevents it from being utilized in industry. A critical component of optimization is the development of a catalyst that is catalytically active, a good microwave absorber, and can be regenerated for repeated dehydrogenation cycles. Previous studies that focused on plastic waste decomposition have used iron-based alumina (FeAlxOy) made via solution combustion synthesis (SCS). Unexplored is the effect of tuning SCS parameters on dehydrogenation performance, the use of these materials in hydrocarbon decomposition to H2, and the regeneration of these catalysts. This dissertation has three objectives: (1) characterize the relationship between SCS parameters and the material properties of FeAlxOy, (2) determine how differences in the material properties of FeAlxOy influence their performance as catalysts during microwave-assisted pyrolysis of fossil fuels, and (3) investigate the Boudouard reaction to regenerate the FeAlxOy post-dehydrogenation.

Chanoi, Zachary Aidan↗

Drivers of Thermal Instability of Catalytic Pyrolysis Oils During Hydrotreating and Co-Processing to Sustainable Fuels

This presentation goes over polymerization observed in CFPs driven by thermally labile oxygenates. Lower oxygen oils have improved stability and a few percent decrease in oxygen greatly improves stability. Further improvements could be realized via targeted catalytic development and further reduction in reactive species. High stability CFP will help enable refinery integration of biogenic carbon.

bio-oil↗

Novel preparation of N-doped SnO 2 nanoparticles via laser-assisted pyrolysis: Demonstration of exceptional lithium storage properties

Here, laser pyrolyzed SnO 2 nanoparticles with an option of nitrogen (N) doping are prepared using a cost-effective method. The electrochemical performance of N-doped samples is tested for the first time in Li-ion batteries where the sample with 3% of N-dopant exhibits optimum performance with a capacity of 522 mAh g active material –1 that can be obtained at 10 A g –1 (6.7C).

25 ENERGY STORAGE↗

Process Considerations for the Production of Hydrogen via Steam Reforming of Oxygenated Gases from Biomass Pyrolysis and Other Conversion Processes

Abstract In 2021, average CO 2 emissions was 9.7 g CO 2 /g H 2 produced, primarily based on steam methane reforming (SMR) technology that currently dominates hydrogen production. The substitution of natural gas (NG) and other fossil feedstocks in SMRs with renewable gases may be considered as an option for reducing greenhouse gas emissions. This analysis explores process impacts and constraints associated with the potential introduction of biogenic gases into SMRs. The results indicate that replacing NG in the fuel train of the SMR, followed by partial replacement of NG in the feed train may be a feasible approach. For the CO‐ and CO 2 ‐rich gas compositions assumed in this analysis the results indicate that feed train may accommodate up to 25 mole % of biogenic gases using allowances in existing designs and/or with small modifications, while maintaining similar hydrogen output. NG substitution in higher proportions require more major changes because of increased flow rates and heat exchange requirements in the system. Biogenic gases with lower CO 2 and higher calorific values are advantageous for NG substitution, and dry reforming using the CO 2 present in the feed gas can reduce steam consumption and increase process efficiency within limits where coking does not become a new constraint.

08 HYDROGEN↗

Pyrolysis of ground pine chip and ground pellet particles

In addition to particle size, biomass density influences heat and mass transfer rates during the thermal treatment processes. In this research, thermal behaviour of ground pine chip particles and ground pine pellet particles in the range of 0.25–5 mm was investigated. A single particle from ground pellets was almost 3 to 4 times denser than a single particle from ground chips at a similar size and volume of particle. Temperature was ramped up from room temperature (~25 °C) to 600 °C with heating rates of 10, 20, 30, and 50 °C/min. Pellet particles took 25–88 % longer time to dry than the chip particles. Microscopic examination of 3 mm and larger chip particles showed cracks during drying. No cracks were observed for pellet particles. The mass loss due to treatment at temperatures higher than 200 °C was about 80% both for chip and pellet particles. It took 4 min for chip and pellet particles to lose roughly 63% of their dry mass at a heating rate of 50 °C/min. The SEM structural analysis showed enlarged pores and cracks in cell walls of the pyrolyzed wood chips. As a result, these pores were not observed in pyrolyzed pellet particles.

09 BIOMASS FUELS↗