Search NASA⌕ Search

SEARCH · Search NASA

Results for “interphase”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 829 records · Page 46

In-situ synthesis of porous metal fluoride@carbon composite via simultaneous etching/fluorination enabled superior Li storage performance

Transition metal fluorides as Li-free conversion-type cathode materials have high theoretical specific capacities, however, their preparation strategy, sluggish electrochemical kinetic and poor cyclability have impeded their wide adoption in lithium-ion batteries. Herein, a facile in-situ synthesis of porous metal-fluoride-carbon composites is accomplished via simultaneous polytetrafluorethylene-based hard template etching and metal fluorination. This not only facilitates fast electron transfer and lithium-ion diffusion kinetics, but also buffers severe volume fluctuation during lithiation/delithation and enables the formation of a uniform and thin Li 2 CO 3 /LiF-rich cathode-electrolyte interphase. Here, as a proof of concept, the as-prepared porous FeF 3 @C (p-FeF 3 @C) indeed exhibits a high specific capacity of 230 mAh g -1 at 0.1 C together with an excellent capacity retention of 92.5% at 1 C for 200-cycles. Moreover, the practicality of the strategy is demonstrated by the superb electrochemical performance of the full-cells coupled with pre-lithiated graphite anodes. Therefore, the proposed novel synthetic strategy will enlighten the future design of high-performance metal-fluoride-carbon composites with porous structure for energy storage applications.

25 ENERGY STORAGE↗

A novel polymeric lithicone coating for superior lithium metal anodes

Lithium metal (Li) is commonly regarded as the “holy grail” of rechargeable batteries and can serve as anodes for constituting various high-energy lithium metal batteries (LMBs). However, it suffers from two notorious issues: (1) continuous formation of inhomogeneous solid electrolyte interphase and (2) Li dendritic growth. Here, in this study, we developed a novel polymeric lithicone via a new molecular layer deposition (MLD) process, using lithium tert-butoxide (LTB) and hydroquinone (HQ) as precursors. We revealed that such an MLD process enabled the resultant LiHQ to grow linearly in a highly controllable and cyclic mode at a growth rate of 4 Å cycle −1 . Furthermore, its low process deposition temperature of 150 °C made it possible to practice high-quality coatings over Li anodes directly. We demonstrated that, very compellingly, this LiHQ coating could protect Li anodes from corrosion and dendritic growth. As a consequence, this LiHQ coating has enabled Li||Li symmetric cells an extremely long cyclability up to 8000 Li-plating/stripping cycles without failure. More excitingly, we demonstrated that, coupled with LiNi 0.8 Mn 0.1 Co 0.1 O 2 (NMC811) cathodes, the LiHQ-modified Li anodes could help the resultant Li||NMC811 realize a much better capacity retention and much longer cyclability. Thus, this study represents a strategic route for developing commercializeable LMBs.

25 ENERGY STORAGE↗

Multi-phase characterization of pitch-carbon coated nano-silicon anodes for lithium-ion batteries

Silicon (Si) is a leading next-generation Li-ion battery anode candidate that meets rigorous performance demands for portable power including enhanced power and energy density with robust cycling performance. However, a series of complex and interrelated reactions lead to reduced calendar life in Si-containing systems and therefore challenge practical adoption. In the present work, we probe the mechanisms underlying observed performance improvements by adding a pitch-carbon coating onto nano-Si material. We pair solid-phase (X-ray photoemission spectroscopy, Fourier-transform infrared), semi-volatile phase (solid-phase microextraction-gas chromatography-mass spectrometry), and gas-phase (gas chromatography-flame-ionization detector) characterization signals to comprehensively evaluate the impact of pitch-carbon coating on the evolution of the Si solid-electrolyte interphase (SEI) and the associated impacts on electrode/electrolyte reactivity. The pitch-carbon is found to serve as a physicochemical barrier, reducing the electro-active surface area for Si/electrolyte reactivity and preventing Si oxidation. Further, the pitch-carbon coating promotes the evolution of a more-favorable SEI by subsuming substantial functionality typically associated with the fluoroethylene carbonate (FEC) electrolyte additive - such as alkoxide scavenging and suppression of transesterification pathways - and by shifting the competitive electrolyte degradation pathways' favorability. The multi-phase characterization approach enables holistic end-products evaluation from complex (electro)chemical interfacial reactions, which informs a robust interpretation of the carbon coating's role in electrochemical performance improvements. The present mechanistic evaluation aids the rational design for improved nano-Si materials.

25 ENERGY STORAGE↗

Quantifying lithium loss in amorphous silicon thin-film anodes via titration-gas chromatography

Silicon with a high theoretical capacity (3,579 mAh/g) is a promising anode candidate for lithium-ion batteries. However, commercialization is still impeded by low Coulombic efficiency, caused by solid electrolyte interphase (SEI) formation and trapped lithium (Li)-silicon (Si) alloy during repeated volume change. Quantifying capacity losses from each factor is crucial to formulate rational design strategies for further improvement. In this work, titration-gas chromatography and cryogenic transmission electron microscopy are applied to characterize the evolution of trapped Li-Si alloy and SEI growth in a silicon thin-film anode. It is found that continuous growth of the SEI is the dominant factor for lithium inventory loss during cycling, with only a marginal increase in trapped Li-Si alloy. This study offers a quantitative approach to differentiate Li in the SEI from trapped Li in Li-Si alloy through a silicon thin-film anode, providing unique insights into identifying critical bottlenecks for developing Si anodes.

25 ENERGY STORAGE↗

Understanding the reversible electrodeposition of aluminum in low-cost room-temperature molten salts

Aluminum is the most earth-abundant metal, trivalent, and inert in ambient air; it also has a density approximately five times that of lithium at room temperature, making it attractive for cost-effective, long-duration storage in batteries. Here, we investigate structural requirements and physicochemical and transport properties of ionic liquid (IL) electrolytes thought to enable high reversibility of Al battery anodes. We find that intentionally designed, low-cost IL analogs, including ammonium-based molten salts, offer comparable Al anode reversibility to state-of-the-art imidazolium-based IL melts. A critical ratio of solvated Al-ion species is required to balance the effects of Lewis acidity needed to continuously etch native Al 2 O 3 and form a stable solid electrolyte interphase on Al. Our findings open new opportunities for developing simple, cost-effective, room-temperature Al batteries that enable long-duration electrical energy storage.

25 ENERGY STORAGE↗

What Makes Fluoroethylene Carbonate Different?

Rechargeable lithium-ion batteries containing silicon-based negative electrodes have the potential to revolutionize electrical energy storage, but carbonate solvents (such as ethylene carbonate) that are commonly used in graphite Li-ion batteries, yield unsatisfactory performance when used with such Li alloying electrodes. It has been found by trial-and-error that additions of the closely related carbonate additive, fluoroethylene carbonate (FEC) to conventional electrolytes, yields a robust solid electrolyte interphase (SEI) on the LixSiy alloy surface. Several mechanisms for this protective action have been considered in the literature and modeled theoretically; however, at present these mechanisms remain speculative. In this study, we use radiolysis, laser photoionization, electron paramagnetic resonance, and transient absorption spectroscopy to establish the redox chemistry of FEC. While the oxidation chemistry is similar to that of other carbonates, the reduction chemistry is strikingly different. Specifically, one-electron reduction of FEC causes the fission of two (instead of one) C-O bonds, resulting in concerted defluorination and decarboxylation. This reaction yields the vinoxyl radical that can abstract an H atom from FEC, initiating both the chain reaction causing FEC decomposition and radical polymerization involving the reaction products. The resulting polymer can further defluorinate yielding the interior radicals that migrate and recombine to produce a highly cross-linked network. We suggest that the outer SEI resulting from FEC addition has elastomeric properties, which account for its cohesion during expansion and contraction of silicon particles in the course of Li alloying/dealloying cycling.

electron paramagnetic resonance↗

Electrolyte Vapor Induced Passivation and Transition Metal Redox on Electrode Active Materials

The gaseous environment that battery electrodes are exposed to is critical to their electrochemical performance, and yet, the impact of vapor-phase components in the glovebox is relatively unexplored. In this study, we examine how the surface of Li 4 Ti 5 O 12 and LiFePO 4 composite electrodes evolve upon exposure to 1 M LiPF 6 in ethylene carbonate:dimethyl carbonate electrolyte vapors in an argon-filled glovebox. Spatially resolved X-ray photoemission electron microscopy and X-ray photoelectron spectroscopy reveal that even brief (15 minutes) contact with electrolyte vapor initiates the formation of a LiF film and changes the oxidation state of transition metals at the particle surface. Notably, these modifications occur selectively on active material particles and not on binder or conductive carbon, underscoring the specificity of vapor-induced reactions. Prolonged exposure to electrolyte vapor over the course of 1 week yields thicker, more chemically complex interphases containing both LiF and lithium oxyfluorophosphate species (Li x PO y F z ). Subsequent electrochemical testing shows that vapor-induced passivation layers influence first cycle capacities, lithium (de)insertion overpotentials, and charge-transfer resistance values. In conclusion, these results indicate that vapor–electrode interactions may be a source of variability in electrochemical behavior over time and suggest that other, more reactive electrode materials may also be susceptible to interactions with electrolyte vapor.

36 MATERIALS SCIENCE↗

Chemical stability of Lithium 2-trifluoromethyl-4,5-dicyanoimidazolide, an electrolyte salt for Li-ion cells

Lithium hexafluorophosphate (LiPF 6 ) is ubiquitous in commercial lithium-ion batteries, but it is hydrolytically unstable and corrosive on electrode surfaces. Using a more stable salt would confer multiple benefits for high-voltage operation, but many such electrolyte systems facilitate anodic dissolution and pitting corrosion of aluminum current collectors that negate their advantages. Lithium 2-trifluoromethyl-4,5-dicyanoimidazolide (LiTDI) is a new salt that was designed specifically for high-voltage cells. In this study we demonstrate that in carbonate electrolytes, LiTDI prevents anodic dissolution of Al current collectors, which places it into a select group of corrosion inhibitors. However, we also demonstrate that LiTDI becomes reduced on lithiated graphite, undergoing sequential defluorination and yielding a thick and resistive solid-electrolyte interphase (SEI), which increases impedance and lowers electrode capacity. The mechanistic causes for this behavior are examined using computational chemistry methods in the light of recent spectroscopic studies. Here, we demonstrate that LiTDI reduction can be prevented by certain electrolyte additives, which include fluoroethylene carbonate, vinylene carbonate and lithium bis(oxalato)borate. This beneficial action is due to preferential reduction of these additives over LiTDI at a higher potential vs. Li/Li + , so the resulting SEI can prevent the direct reduction of LiTDI at lower potentials on the graphite electrode.

25 ENERGY STORAGE↗

Chemistry of Electrolyte Reduction on Lithium Silicide

Silicon anodes are promising for next-generation lithium-ion batteries due to high theoretical capacity. However, their performance and lifetime are currently limited by continuous electrolyte reduction and solid-electrolyte interphase (SEI) formation. Thus, SEI studies are important but often complicated due to the rough morphology of samples, buried interfaces, and the presence of binders. Here, we demonstrate the chemical origin of SEI formation by electrolyte reduction on lithium silicide thin films, synthesized by diffusion of pure evaporated lithium into smooth sputtered silicon. These model samples allowed for accurate estimation of irreversible capacity loss due to electrolyte reduction and for precise characterization of the resulting SEI by vibrational and photoelectron spectroscopies. Spectroscopic characterizations showed clear evidence that lithium silicide reduced electrolyte directly upon contact. Negligible first-cycle irreversible capacity loss was observed for the lithium silicide compared to silicon, indicating that the decomposition product of electrolyte on lithium silicide is able to stop further electrolyte reduction to a large extent. Fluoro-ethylene carbonate was shown to significantly affect the chemistry of electrolyte reduction on lithium silicide and subsequent cycling performance. The results of this basic study reveal the chemistry occurring at the interface of the lithium silicide and electrolyte and help in understanding the limited calendar lifetime of Li-ion batteries with Si anodes.

25 ENERGY STORAGE↗

Reduction of Electrolyte Components on a Coated Si Anode of Lithium-Ion Batteries

Surface modification of Si anodes in Li-ion batteries by deposition of a thin alucone coating has demonstrated an effective way to help maintain a stable anode/electrolyte interface and good battery performance. In this paper, we investigate the interactions and reactivity of the film with electrolyte components using ab initio molecular dynamics simulations. Adsorption of solvent molecules (ethylene carbonate, EC) and salt (LiPF 6 ), and reduction by two mechanisms depending on the Li content of the film (yielding open EC adsorbed on the film or C 2 H 4 + CO 3 2- ) take place near the film/electrolyte and film/anode interfaces. Finally, reactions products incorporate to the structure of the film and create a new kind of solid-electrolyte interphase layer.

25 ENERGY STORAGE↗

In Situ Study of Silicon Electrode Lithiation with X-ray Reflectivity

Surface sensitive X-ray reflectivity (XRR) measurements were performed to investigate the electrochemical lithiation of a native oxide terminated single crystalline silicon (100) electrode in real time during the first galvanostatic discharge cycle. This allows us to gain nanoscale, mechanistic insight into the lithiation of Si and the formation of the solid electrolyte interphase (SEI). We describe an electrochemistry cell specifically designed for in situ XRR studies and have determined the evolution of the electron density profile of the lithiated Si layer (Li x Si) and the SEI layer with subnanometer resolution. We propose a three-stage lithiation mechanism with a reaction limited, layer-by-layer lithiation of the Si at the Li x Si/Si interface.

36 MATERIALS SCIENCE↗

Enhanced Interfacial Stability of Si Anodes for Li-Ion Batteries via Surface SiO2 Coating

Silicon is a promising alloying anode for lithium-ion batteries owing to its high capacity and low cost. However, its use has been hampered by mechanical failure arising from the large volume change upon cycling and by an insufficiently stable solid-electrolyte interphase (SEI). SEI formation depends on the Si surface, which is often an oxide (SiO x ). In this study we compare three different Si surfaces using Si wafers: 1.3 nm native SiO x , 1.4 nm thermally grown SiO2, and a SiOx-free surface. The oxide-free surface showed the worst electrochemical performance, never exceeding 94% Coulombic efficiency (CE). Furthermore, it also exhibited the thickest SEI and the highest overpotential for lithiation, which correlated with uninhibited electrolyte reduction and the incorporation of P-F species into the SEI. The oxide-coated surfaces performed significantly better, demonstrating a CE above 99% beyond the second cycle, low overpotential for lithiation, and a thinner and more stable SEI. The oxides lower the onset potential for electrolyte reduction, and yield an SEI with fewer P-F species. However, it was found that the CE with the native oxide surface decays from the fifth cycle onwards and correlates with a resurgence of electrolyte reduction. A 1-2 nm thermal SiO 2 coating is optimum for achieving a stable SEI that minimizes side reactions and sustains efficient cycling.

25 ENERGY STORAGE↗

Influence of Electrolyte Additives on Interfacial Stability of Manganese-Rich Lithium-Ion Battery Cathodes

Affordable, long-lasting energy storage has become critical to support increased electricity demand in recent years. Cobalt-free, lithium- and manganese-rich lithium nickel manganese oxide (LMR-NM) cathodes stand to reduce cost and supply-chain concerns associated with traditional cobalt-containing cathodes for lithium-ion batteries by leveraging more earth-abundant materials; however, they have shown issues with long-term cycling stability. Here, we investigate lithium difluoro(oxalate)borate (LiDFOB), tris(trimethylsilyl) phosphite (TMSPi), and vinylene carbonate (VC) electrolyte additives for their ability to improve cycling performance of LMR-NM (0.3 Li 2 MnO 3 + 0.7 LiMn 0.5 Ni 0.5 0 2 ) cells. Cryogenic scanning transmission electron microscopy (cryo-STEM) with electron energy loss spectroscopy enables the construction of a structure–function relationship between cathode electrolyte interphase (CEI) characteristics and the electrochemical performance of cells aged with these additives. We find the combination of 2 wt % TMSPi + 1 wt % LiDFOB performs better than any single additive, achieving a 28% improvement in specific capacity over the baseline electrolyte after long-term cycling. We attribute this to LiDFOB mitigating Mn ion dissolution, with cryo-STEM showing Mn stabilized up to the CEI surface, coupled with improved CEI structure and chemistry enabled by TMSPi, evidenced by a moderately thick (∼7–15 nm) CEI that appears to protect against further electrolyte reactions with the particle. These results, achieved through site-specific nanoscale characterization, directly reveal mechanisms through which electrolyte engineering can improve the performance of earth-abundant cathodes, enabling informed development of more affordable and reliable batteries to meet future energy storage needs.

25 ENERGY STORAGE↗

XPS on Li-Battery-Related Compounds: Analysis of Inorganic SEI Phases and a Methodology for Charge Correction

Accurate identification of chemical phases associated with the electrode and solid-electrolyte interphase (SEI) is critical for understanding and controlling interfacial degradation mechanisms in lithium-containing battery systems. To study these critical battery materials and interfaces X-ray photoelectron spectroscopy (XPS) is a widely used technique that provides quantitative chemical insights. However, due to the fact that a majority of chemical phases relevant to battery interfaces are poor electronic conductors, phase identification that relies primarily on absolute XPS core-level binding-energies (BEs) can be problematic. Charging during XPS measurements leads to BE shifts that can be difficult to correct. These difficulties are often exacerbated by the coexistence of multiple Li-containing phases in the SEI with overlapping XPS core levels. To facilitate accurate phase identification of battery-relevant phases (and electronically insulating phases in general), we propose a straightforward approach for removing charging effects from XPS data sets. We apply this approach to XPS data sets acquired from six battery-relevant inorganic phases including lithium metal (Li0), lithium oxide (Li 2 O), lithium peroxide (Li 2 O 2 ), lithium hydroxide (LiOH), lithium carbonate (Li 2 CO 3 ), and lithium nitride (Li 3 N). Specifically, we demonstrate that BE separations between core levels present in a particular phase (e.g., BE separation between the O 1s and Li 1s core levels in Li 2 O) provide an additional constraint that can significantly improve reliability of phase identification. For phases like Li 2 O 2 and LiOH where the Li-to-O ratios and BE separations are nearly identical, X-ray excited valence-band spectra can provide additional clues that facilitate accurate phase identification. To accurately identity the phases in this study, we show that in situ growth of Li 2 O on Li 0 provides a means for determining absolute core-level positions, where all charging effects can be accurately removed. Finally, as an exemplary case we apply the charge-correction methodology to XPS data acquired from a symmetric cell based on a Li 2 S-P 2 S 5 solid electrolyte. This analysis demonstrates that accurately accounting for XPS BE shifts as a function of current-bias conditions can provide a direct probe of ionic conductivities associated with battery materials.

25 ENERGY STORAGE↗

Surface SiO 2 Thickness Controls Uniform-to-Localized Transition in Lithiation of Silicon Anodes for Lithium-Ion Batteries

Silicon is a promising anode material for lithium-ion batteries because of its high capacity, but its widespread adoption has been hampered by a low cycle life arising from mechanical failure and the absence of a stable solid–electrolyte interphase (SEI). Understanding SEI formation and its impact on cycle life is made more complex by the oxidation of silicon materials in air or during synthesis, which leads to SiO x coatings of varying thicknesses that form the true surface of the electrode. Here, the lithiation of SiO 2 -coated Si is studied in a controlled manner using SiO 2 coatings of different thicknesses grown on Si wafers via thermal oxidation. SiO 2 thickness has a profound effect on lithiation: below 2 nm, SEI formation followed by uniform lithiation occurs at positive voltages versus Li/Li + . Si lithiation is reversible, and SiO 2 lithiation is largely irreversible. Above 2 nm SiO 2 , voltammetric currents decrease exponentially with SiO 2 thickness. For 2–3 nm SiO 2 , SEI formation above 0.1 V is suppressed, but a hold at low or negative voltages can initiate charge transfer whereupon SEI formation and uniform lithiation occur. Cycling of Si anodes with an SiO 2 coating thinner than 3 nm occurs at high Coulombic efficiency (CE). If an SiO 2 coating is thicker than 3–4 nm, the behavior is totally different: lithiation at positive voltages is strongly inhibited, and lithiation occurs at poor CE and is highly localized at pinholes which grow over time. As they grow, lithiation becomes more facile and the CE increases. Pinhole growth is proposed to occur via rapid transport of Li along the SiO 2 /Si interface radially outward from an existing pinhole, followed by the lithiation of SiO 2 from the interface outward.

25 ENERGY STORAGE↗

Nonpassivated Silicon Anode Surface

A stable solid electrolyte interphase (SEI) has been proven to be a key enabler to most advanced battery chemistries, where the reactivity between the electrolyte and the anode operating beyond the electrolyte stability limits must be kinetically suppressed by such SEIs. The graphite anode used in state-of-the-art Li-ion batteries presents the most representative SEI example. Because of similar operation potentials between graphite and silicon (Si), a similar passivation mechanism has been thought to apply on the Si anode when using the same carbonate-based electrolytes. Herein, we found that the chemical formation process of a proto-SEI on Si is closely entangled with incessant SEI decomposition, detachment, and reparation, which lead to continuous lithium consumption. Using a special galvanostatic protocol designed to observe the SEI formation prior to Si lithiation, we were able to deconvolute the electrochemical formation of such dynamic SEI from the morphology and mechanical complexities of Si and showed that a pristine Si anode could not be fully passivated in carbonate-based electrolytes.

25 ENERGY STORAGE↗

Electrochemical Reactivity and Passivation of Silicon Thin-Film Electrodes in Organic Carbonate Electrolytes

This work focuses on the mechanisms of interfacial processes at the surface of amorphous silicon thin-film electrodes in organic carbonate electrolytes to unveil the origins of the inherent nonpassivating behavior of silicon anodes in Li-ion batteries. Attenuated total reflection Fourier-transform infrared spectroscopy, X-ray absorption spectroscopy, and infrared near-field scanning optical microscopy were used to investigate the formation, evolution, and chemical composition of the surface layer formed on Si upon cycling. Herein, we found that the chemical composition and thickness of the solid/electrolyte interphase (SEI) layer continuously change during the charging/discharging cycles. This SEI layer “breathing” effect is directly related to the formation of lithium ethylene dicarbonate (LiEDC) and LiPF6 salt decomposition products during silicon lithiation and their subsequent disappearance upon delithiation. Furthermore, the detected appearance and disappearance of LiEDC and LiPF6 decomposition compounds in the SEI layer are directly linked with the observed interfacial instability and poor passivating behavior of the silicon anode.

25 ENERGY STORAGE↗

Enabling Ether-Based Electrolytes for Long Cycle Life of Lithium-Ion Batteries at High Charge Voltage

Lithium-ion batteries (LIBs) with high-nickel (Ni) content LiNi x Mn y Co z O 2 ( x + y + z = 1) (NMC with Ni ≥ 0.6) cathodes operated at high charge voltages have been considered as one of the most promising candidates for addressing the challenge of increasing energy density demand. Conventional LiPF 6 –organocarbonate electrolytes exhibit incompatibility with such cell chemistries under certain testing conditions because of the instability of electrode/electrolyte interphases. In response to this challenge, ether-based electrolytes with finely tuned structure and composition of solvation sheaths were developed and evaluated in graphite (Gr)∥NMC811 cell chemistry in 2.5–4.4 V, despite ethers being conventionally considered to be unfavorable electrolyte solvents for LIBs because of their anodic instability above 4.0 V and cointercalation into Gr electrodes. Furthermore, the functional ether-based electrolytes in this work enable both excellent cycle life and high rate capability of Gr∥NMC811 cells. Mechanistic studies reveal that the unique structure and composition of the solvation sheath of the functional ether electrolytes are the main reasons behind their excellent anodic stability and effective protection of the Gr electrode and, consequently, the extraordinary cell performances when operated at high charge cutoff voltages. This work also provides a feasible approach in developing highly stable functional electrolytes for high-energy density LIBs.

25 ENERGY STORAGE↗