Aging Hanford Nuclear Waste Using Carbon Dioxide to Evaluate Corrosion at Lower pH Limits - 18467
Samples of Hanford Nuclear Reservation (HNR) tank waste and simulated Hanford tank waste were exposed to carbon dioxide gas (CO{sub 2}) in the laboratory in order to decrease the pH of the solution. Sodium hydroxide is required to be added to some tanks according to waste handling specifications to keep tanks protected from pitting corrosion, but the maximum-allowed volume in some tanks is currently approaching capacity. Decreasing the pH of tank solutions using CO{sub 2} gas mimics the environmental exposure chemistry, does not add sodium, and allows for testing on solutions currently categorized as out-of-specification according to technical waste handling documents. Legacy alloy A537 Class 1 carbon steel was used to construct the AN tanks on the HNR and was utilized for this testing. The planned testing of three solutions included a simulant for feasibility and a waste solution from Tank 241-AN-102 (AN-102), taken in 2013, which was run in duplicate. The solutions were evaluated for corrosion potential using cyclic potentiodynamic polarization (CPP) scans to determine the propensity for stress corrosion cracking and pitting corrosion. Results in all solutions showed that pitting potential was low when the pH was above 11 and temperatures were below 40 deg. C. As solution pHs dipped into the 10- 10.5 range, there were mixed results. CPP scans were initially run at the higher temperature of 50 deg. C, accelerating corrosion rates. Solution pHs that did not indicate corrosion were further exposed to CO{sub 2}. Solutions with mixed or positive pitting results were rerun at 40 deg. C. The first failed run on the tank solution was seen when testing the duplicate sample at 50 deg. C and a pH of 13.01. When this solution was retested at 40 deg. C, the CPP scan did not show corrosion. A mixed corrosion result was obtained from a scan run at the final pH of 10 when tested at 50 deg. C. Upon completion of testing a visual inspection of the coupon did not show corrosion products on its surface. These results provide assurance that tanks containing slightly reduced pHs are still protected from pitting corrosion. Tank integrity assurance at a lower pH limit in Tank AN-102 could slow sodium addition and the rising volume of hazardous waste. Other benefits of reducing the pH specification would be reduced costs associated with retrieving and storing smaller volumes of hazardous waste, a reduced number of radiation exposure events (required for pH modification of tank waste), and a potential for a decreased volume required to be immobilized for long-term storage in a vitrified (glass) phase. (authors)