Search NASA⌕ Search

SEARCH · Search NASA

Results for “Fracturing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 847 records · Page 47

The effects of shot-peening residual stresses on the fracture and crack growth properties of D6AC steel

The fracture strength and cyclic crack-growth properties of surface-flawed, shot-peened D6AC steel plate were investigated. For short crack lengths (up to 1.5mm) simple linear elastic fracture mechanics - based only on applied loading - did not predict the fracture strengths. Also, Paris' Law for cyclic crack growth did not correlate the crack-growth behavior. To investigate the effect of shot-peening, additional fracture and crack-growth tests were performed on material which was precompressed to remove the residual stresses left by the shot-peening. Both tests and analysis show that the shot-peening residual stresses influence the fracture and crack-growth properties of the material. The analytical method of compensating for residual stresses and the fracture and cyclic crack-growth test results and predictions are presented.

Elber, W.↗

An investigation of the plastic fracture of AISI 4340 and 18 nickel - 200 grade maraging steels

The mechanisms of plastic fracture (dimpled rupture) in high-purity and commercial 18 Ni, 200 grade maraging steels and quenched and tempered AISI 4340 steels have been studied. Plastic fracture takes place in the maraging alloys through void initiation by fracture of titanium carbo-nitride inclusions and the growth of these voids until impingement results in coalescence and final fracture. The fracture of AISI 4340 steel at a yield strength of 200 ksi occurs by nucleation and subsequent growth of voids formed by fracture of the interface between manganese sulfide inclusions and the matrix. The growth of these inclusion-nucleated voids is interrupted long before coalescence by impingement, by the formation of void sheets which connect neighboring sulfide-nucleated voids.

Cox, T. B.↗

Effects of shot-peening residual stresses on the fracture and crack-growth properties of D6AC steel

The fracture strength and cyclic crack-growth properties of surface-flawed, shot-peened D6AC steel plate were investigated. For short crack lengths (up to 1.5 mm) simple linear elastic fracture mechanics - based only on applied loading - did not predict the fracture strengths. Also, Paris' Law for cyclic crack growth did not correlate the crack-growth behavior. To investigate the effect of shot-peening, additional fracture and crack-growth tests were performed on material which was precompressed to remove the residual stresses left by the shot-peening. Both tests and analysis show that shot-peening residual stresses influence the fracture and crack-growth properties of the material. This report presents the analytical method of compensating for residual stresses and the fracture and cyclic crack-growth test results and predictions.

Elber, W.↗

Fracture analysis of surface and through cracks in cylindrical pressure vessels

A previously developed fracture criterion was applied to fracture data for surface- and through-cracked cylindrical pressure vessels to see how well the criterion can correlate fracture data. Fracture data from the literature on surface cracks in aluminum alloy, steel, and epoxy vessels, and on through cracks in aluminum alloy, titanium alloy steel, and brass vessels were analyzed by using the fracture criterion. The criterion correlated the failure stresses to within + or - 10 percent for either surface or through cracks over a wide range of crack size and vessel diameter. The fracture criterion was also found to correlate failure stresses to within + or - 10 percent for flat plates (center-crack or double-edge-crack tension specimens) and cylindrical pressure vessels containing through cracks.

Newman, J. C., Jr.↗

Developments in fracture mechanics test methods standardization; Proceedings of the Symposium, St. Louis, Mo., May 4, 1976

Experience in plane-strain fracture toughness testing per ASTM Method E 399 is considered along with fracture toughness testing using the C-shaped specimen, an analysis of radially cracked ring segments subject to forces and couples, compliance calibration of specimens used in the R-curve practice, heavy-section fracture toughness screening specimen, and sharply notched cylindrical tension specimens for screening plane-strain fracture toughness. Attention is also given to an investigation of some problems in developing standards for precracked Charpy specimen strength ratios, fracture testing with surface crack specimens, and the estimation of plane strain fracture toughness values from slow bend precracked Charpy specimen strength ratios.

Brown, W. F., Jr.↗

Fracture modes of high modulus graphite/epoxy angleplied laminates subjected to off-axis tensile loads

Angelplied laminates of high modulus graphite fiber/epoxy were studied in several ply configurations at various tensile loading angles to the zero ply direction in order to determine the effects of ply orientations on tensile properties, fracture modes, and fracture surface characteristics of the various plies. It was found that fracture modes in the plies of angleplied laminates can be characterized by scanning electron microscope observation. The characteristics for a given fracture mode are similar to those for the same fracture mode in unidirectional specimens. However, no simple load angle range can be associated with a given fracture mode.

Sinclair, J. H.↗

Fracture behavior of hybrid composite laminates

The tensile fracture behavior of 15 center-notched hybrid laminates was studied. Three basic laminate groups were tested: (1) a baseline group with graphite/epoxy plies, (2) a group with the same stacking sequence but where the zero-deg plies were one or two plies of S-glass or Kevlar, and (3) a group with graphite plies but where the zero-deg plies were sandwiched between layers of perforated Mylar. Specimens were loaded linearly with time; load, far field strain, and crack opening displacement (COD) were monitored. The loading was stopped periodically and the notched region was radiographed to reveal the extent and type of damage (failure progression). Results of the tests showed that the hybrid laminates had higher fracture toughnesses than comparable all-graphite laminates. The higher fracture toughness was due primarily to the larger damage region at the ends of the slit; delamination and splitting lowered the stress concentration in the primary load-carrying plies. A linear elastic fracture analysis, which ignored delamination and splitting, underestimated the fracture toughness. For almost all of the laminates, the tests showed that the fracture toughness increased with crack length. The size of the damage region at the ends of the slit and COD measurements also increased with crack length.

Kennedy, J. M.↗

Metallurgical characterization of the fracture of several high strength aluminum alloys

The fracture behavior for structural aluminum alloys (2024, 6061, 7075, and 7178) was examined in selected heat treatments. The investigation included tensile, shear, and precracked notch-bend specimens fractured at ambient temperature under monotonic loading. Specimens were obtained from thin sheets and thick plates and were tested in longitudinal and transverse orientations at different strain rates. Microstructures of alloys were examined using the optical microscope and the scanning electron microscope with associated energy dispersive X ray chemical analysis. Several different types of second phase particles, some not reported by other investigators, were identified in the alloys. Fracture morphology was related to microstructural variables, test variables, and type of commercial product. Specimen orientation examined in the present investigation had little effect on fracture morphology. Test strain rate changes resulted in some change in shear fracture morphology, but not in fracture morphology of tensile specimens.

Bhandarkar, M. D.↗

Fracture behavior of thick, laminated graphite/epoxy composites

The effect of laminate thickness on the fracture behavior of laminated graphite epoxy (T300/5208) composites was studied. The predominantly experimental research program included the study of the 0/+ or - 45/90 sub ns and 0/90 sub ns laminates with thickness of 8, 32, 64, 96 and 120 plies and the 0/+ or - 45 sub ns laminate with thickness of 6, 30, 60, 90 and 120 plies. The research concentrated on the measurement of fracture toughness utilizing the center-cracked tension, compact tension and three point bend specimen configurations. The development of subcritical damage at the crack tip was studied nondestructively using enhanced X-ray radiography and destructively using the laminate deply technique. The test results showed fracture toughness to be a function of laminate thickness. The fracture toughness of the 0 + or - 45/90 sub ns and 0/90 sub ns laminates decreased with increasing thickness and asymptotically approached lower bound values of 30 ksi square root of in. (1043 MPa square root of mm and 25 ksi square root of in (869 MPa square root of mm respectively. In contrast to the other two laminates, the fracture toughness of the 0/+ or - 45 sub ns laminate increased sharply with increasing thickness but reached an upper plateau value of 40 ksi square root of in (1390 MPa square root of mm) at 30 plies. Fracture toughness was independent of crack size for both thin and thick laminates for all three laminate types except for the 0/90 sub 2s laminate which spilt extensively. The center cracked tension, three point bend and compact tension specimens gave comparable results.

Harris, C. E.↗

Computational simulation of progressive fracture in fiber composites

Computational methods for simulating and predicting progressive fracture in fiber composite structures are presented. These methods are integrated into a computer code of modular form. The modules include composite mechanics, finite element analysis, and fracture criteria. The code is used to computationally simulate progressive fracture in composite laminates with and without defects. The simulation tracks the fracture progression in terms of modes initiating fracture, damage growth, and imminent global (catastrophic) laminate fracture.

Chamis, C. C.↗

References and conference proceedings towards the understanding of fracture mechanics

A list of books, reports, periodicals, and conference proceedings, as well as individual papers, centered on specific aspects of fracture phenomenon has been compiled by the ASTM Committee E-24 on Fracture Testing. A list of basic references includes the articles on the development of fracture toughness, evaluation of stress intensity factors, fatigue crack growth, fracture testing, fracture of brittle materials, and fractography. Special attention is given to the references on application of fracture mechanics to new designs and on reevaluation of failed designs, many of them concerned with naval and aircraft structures.

Toor, P. M.↗

Fracture of thick graphite/epoxy laminates with part-through surface flaws

Fracture behavior of tensile specimens containing through-the-thickness flaws and part-through semi-elliptic surface flaws was investigated. The material was T300/5208 graphite/epoxy, with a stacking sequence 0/+ or - 45/90 sub ns. Laminate thicknesses ranged from 8 to 120 plies. Fracture toughness for specimens with through-the-thickness flaws was a function of laminate thickness. Fracture toughness was also independent of crack size. Fracture toughness for the thick laminates was also independent of specimen geometry (center-cracked tension specimen, compact tension specimen, and three-point bend specimen). Using the asymptotic value of fracture toughness and linear elastic isotropic fracture mechanics, the notched strength of tensile specimens with semi-elliptic surface flaws was predicted. The strength ratio is a function of the flaw depth (a/t) and flaw aspect (a/c) ratios. Comparisons between predicted and experimental strengths are good for large values of a/t. The notched strength of filament wound graphite/epoxy tensile specimens with part-through surface flaws was also predicted.

Harris, C. E.↗

A comparison of the fracture behavior of thick laminated composites utilizing compact tension, three-point bend, and center-cracked tension specimens

An experimental study of the effects of specimen configuration and laminate thickness on the fracture behavior of notched laminated composites is presented. The behavior of (0/+, 45/90)ns, (0/90)ns and (0/+, - 45)ns graphite/epoxy T300/5208 laminates was studied. When fracture toughness was computed at the failing load of the center-cracked tension specimen, laminate thickness significantly influenced fracture toughness. If fracture toughness was computed at the interception of the 5 percent secant line with the load-COD record, fracture toughness was found to be independent of both laminate thickness and specimen configuration. Defined in this manner, fracture toughness can be physically interpreted as an indicator of the onset of significant notch-tip damage.

Harris, C. E.↗

The effect of diffusive hydrogen segregation on fracture of polycrystalline nickel

Hydrogen embrittlement of polycrystalline nickel was studied under conditions which allowed the diffusion and segregation of hydrogen to grain boundaries to be controlled. It was shown that even at high solute concentrations of hydrogen, the fracture mode was ductile shear rupture, if transport of hydrogen to the grain boundaries was not allowed. As the amount of hydrogen segregation to the grain boundaries was increased, the fracture mode became increasingly intergranular. Analysis of the temperature dependence of this transition from ductile rupture to transgranular fracture yields a hydrogen segregation enthalpy of 11.6 kJ/mol. The transition in the fracture mode was also observed at a constant aging temperature by increasing the solute hydrogen concentration. The kinetics of this fracture transition suggest that the hydrogen segregation layer extends about 35 nm from the grain boundary. It is suggested that the fracture mechanism is a softening of the material in this segregation region due to the high hydrogen concentration.

Lassila, D. H.↗

A parametric study of fracture toughness of fibrous composite materials

Impacts to fibrous composite laminates by objects with low velocities can break fibers giving crack-like damage. The damage may not extend completely through a thick laminate. The tension strength of these damage laminates is reduced much like that of cracked metals. The fracture toughness depends on fiber and matrix properties, fiber orientations, and stacking sequence. Accordingly, a parametric study was made to determine how fiber and matrix properties and fiber orientations affect fracture toughness and notch sensitivity. The values of fracture toughness were predicted from the elastic constants of the laminate and the failing strain of the fibers using a general fracture toughness parameter developed previously. For a variety of laminates, values of fracture toughness from tests of center-cracked specimens and values of residual strength from tests of thick laminates with surface cracks were compared to the predictions to give credibility to the study. In contrast to the usual behavior of metals, it is shown that both ultimate tensile strength and fracture toughness of composites can be increased without increasing notch sensitivity.

Poe, C. C., Jr.↗

Case histories involving fatigue and fracture mechanics; Proceedings of the Symposium, Charleston, SC, Mar. 21, 22, 1985

Papers are presented on cracking at nozzle corners in the nuclear pressure vessel industry, applied fracture mechanics for assessing defect significance in a crude oil pipeline, failure analysis of a large wind-tunnel compressor blade, analysis of a compressor-wheel failure, and preventing fracture by inspection and analysis. Consideration is also given to the fatigue crack growth predictions of welded aircraft structures containing flaws in the residual stress field, the fatigue and fracture mechanics analysis of a compression loaded aircraft structure, fracture of an aircraft horizontal stabilizer, fatigue life analysis of fuel tank skins under combined loads, and aircraft structural maintenance recommendations based on fracture mechanics analysis. Additional papers discuss an analysis of two metal-forming die failures, an analysis of a failed saw arbor, and the role of fracture mechanics in assessing the effect on fatigue life of design changes in welded fabrications.

Hudson, C. Michael↗

A parametric study of fracture toughness of fibrous composite materials

Impacts to fibrous composite laminates by objects with low velocities can break fibers giving crack-like damage. The damage may not extend completely through a thick laminate. The tension strength of these damage laminates is reduced much like that of cracked metals. The fracture toughness depends on fiber and matrix properties, fiber orientations, and stacking sequence. Accordingly, a parametric study was made to determine how fiber and matrix properties and fiber orientations affect fracture toughness and notch sensitivity. The values of fracture toughness were predicted from the elastic constants of the laminate and the failing strain of the fibers using a general fracture toughness parameter developed previously. For a variety of laminates, values of fracture toughness from tests of center-cracked specimens and values of residual strength from tests of thick laminates with surface cracks were compared to the predictions to give credibility to the study. In contrast to the usual behavior of metals, it is shown that both ultimate tensile strength and fracture toughness of composites can be increased without increasing notch sensitivity.

Poe, C. C., Jr.↗

Fracture toughness of polycrystalline ceramics in combined mode I and mode II loading

The present investigation of the fracture of alumina and zirconia polycrystalline ceramic specimens of precracked-disk type, in diametral compression, evaluated fracture toughness in pure mode I, combined mode I/mode II, and pure mode II, depending on the alignment of the center crack relative to the loading diameter. The mixed-mode fracture-toughness envelope thus obtained exhibits significant deviation to higher fracture toughness in mode II, relative to the predictions of linear elastic fracture mechanics theory. Crack-surface resistance due to grain-interlocking and abrasion are identified as the primary sources of increased fracture resistance in mode II loading of the polycrystalline ceramics.

Singh, Dileep↗