Atomic Layer Deposition of Rhenium–Aluminum Oxide Thin Films and ReO x Incorporation in a Metal–Organic Framework
Explore the source record for details and available documents.
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Explore the source record for details and available documents.
Abstract not provided.
Aluminum-doped zinc oxide thin films have been grown by atomic layer deposition at a temperature of 200°C. Using X-ray diffraction, it has been established that the ZnO:Al thin films exhibits the reflections from the (100), (002), (110), and (201) ZnO hexagonal phase planes. The (101) and (102) planes have also been detected by electron diffraction. The ZnO:Al thin films grow smooth with a root-mean-square roughness of R{sub q} = 0.33 nm and characteristic nanocrystallite sizes of ~70 and ~15 nm without additional aluminum or aluminum oxide phases. The transmission at a wavelength of 550 nm with regard to the substrate has been found to be 96%. The refractive indices and absorption coefficients of the ZnO:Al thin films in the wavelength range of 250–900 nm have been determined. The maximum refractive indices and absorption coefficients have been found to be 2.09 at a wavelength of 335 nm and 0.39 at a wavelength of 295 nm, respectively. The optical band gap is 3.56 eV. The resistivity, Seebeck coefficient, and power factor of the ZnO:Al thin films are ∼1.02 × 10{sup –3} Ω cm, –60 μV/K, and 340 μW m{sup –1} K{sup –2} at room temperature, respectively. The maximum power factor attains 620 μW m{sup –1} K{sup –2} at a temperature of 200°C.
Reflective surfaces are one of the key elements of solar plants to concentrate energy in the receivers of solar thermal electricity plants. Polymeric substrates are being considered as an alternative to the widely used glass mirrors due to their intrinsic and processing advantages, but optimizing both the reflectance and the physical stability of polymeric mirrors still poses technological difficulties. In this work, polymeric surfaces have been functionalized with ceramic thin-films by atomic layer deposition. The characterization and optimization of the parameters involved in the process resulted in surfaces with a reflection index of 97%, turning polymers into a real alternative to glass substrates. The solution we present here can be easily applied in further technological areas where seemingly incompatible combinations of polymeric substrates and ceramic coatings occur.
Co1-xPtx clusters of 2.9-nm size with a range of atomically precise Pt/Co atomic ratios (x = 0, 0.25, 0.5, 0.75, 1) were synthesized using the mass-selected low-energy cluster beam deposition (LECBD) technique and soft-landed onto an amorphous alumina thin film prepared by atomic layer deposition (ALD). Utilizing ex situ X-ray photoemission spectroscopy (XPS), the oxidation state of the as-made clusters supported on Al2O3 was determined after both a 1-h-long exposure to air and aging for several weeks while exposed to air. Next, the aged duster samples were characterized by grazing-incidence X-ray absorption spectroscopy (GIXAS) and then pretreated with diluted hydrogen and further exposed to the mixture of diluted CO and H-2 up to 225 degrees C at atmospheric pressure, and the temperature-dependent evolutions of the particle size/shape and the oxidation states of the individual metal components within the dusters were monitored using in situ grazing-incidence small-angle X-ray scattering and X-ray absorption spectroscopy (GISAXS/GIXAS). The changes in the oxidation states of Co and Pt exhibited a nonlinear dependence on the Pt/Co atomic ratio of the dusters. For example, a low Pt/Co ratio (x <= 0.5) facilitates the formation of Co(OH)(2), whereas a high Pt/Co ratio (x = 0.75) stabilizes the Co3O4 composition instead through the formation of a Co-Pt core-shell structure where the platinum shell inhibits the reduction of cobalt in the core of the Co1-xPtx alloy dusters. The obtained results indicate methods for optimizing the composition and structure of binary alloy clusters for catalysis.
Local environment surrounding Zr atoms in the thin films of nanocrystalline zirconia (ZrO{sub 2}) has been investigated by using the extended x-ray absorption fine structure (EXAFS) technique. These films prepared by the ion beam assisted deposition exhibit long-range structural order of cubic phase and high hardness at room temperature without chemical stabilizers. The local structure around Zr probed by EXAFS indicates a cubic Zr sublattice with O atoms located on the nearest tetragonal sites with respect to the Zr central atoms, as well as highly disordered locations. Similar Zr local structure was also found in a ZrO{sub 2} nanocrystal sample prepared by a sol-gel method. Variations in local structures due to thermal annealing were observed and analyzed. Most importantly, our x-ray results provide direct experimental evidence for the existence of oxygen vacancies arising from local disorder and distortion of the oxygen sublattice in nanocrystalline ZrO{sub 2}. These oxygen vacancies are regarded as the essential stabilizing factor for the nanostructurally stabilized cubic zirconia.
We report an atomic layer deposition based zinc oxide channel material integrated thin film transistor using wavy channel architecture allowing expansion of the transistor width in the vertical direction using the fin type features. The experimental devices show area efficiency, higher normalized output current, and relatively lower power consumption compared to the planar architecture. This performance gain is attributed to the increased device width and an enhanced applied electric field due to the architecture when compared to a back gated planar device with the same process conditions.
HfO{sub 2} thin films have been deposited by an atomic layer deposition (ALD) process using alternating pulses of tetrakis(dimethyl)amino hafnium and H{sub 2}O precursors at a substrate temperature of 200-325 deg. C. The initial stage of film growth on OH- and H-terminated Si(100) surfaces is investigated using Rutherford backscattering spectrometry (RBS), x-ray photoelectron spectroscopy (XPS), and spectroscopic ellipsometry (SE). The authors observe an initial growth barrier on the Si-H surface for the first approximately four process cycles, where film growth is more efficient on the OH-terminated surface. Both starting surfaces require about 15 cycles to reach a steady growth rate per cycle, with the OH-terminated surface displaying a slightly higher growth rate of 2.7x10{sup 14} Hf/cm{sup 2} compared to 2.4x10{sup 14} Hf/cm{sup 2} for Si-H. Combining the RBS and SE data we conclude that the films deposited on the OH-terminated surface are denser than those deposited on the Si-H surface. Angle-resolved XPS measurements reveal the formation of an {approx}8 A interfacial layer after four ALD cycles on the H-terminated surface for a deposition temperature of 250 deg. C, and transmission electron microscopy verifies that the thickness of the interfacial layer does not change substantially between the 4th and the 25th process cycles. The interfacial layer appears to depend weakly on the deposition temperature from 200 to 325 deg. C, ranging from 6.9 to 8.4 A.
The functional design of nanoscale transition metal oxide heterostructures depends critically on the growth of atomically flat epitaxial thin films. Much of the time, improved functionality is expected for heterostructures and surfaces with orientations that do not have the lowest surface free energy. For example, crystal faces with a high surface free energy, such as rutile (001) planes, frequently exhibit higher catalytic activities but are correspondingly harder to synthesize due to energy-lowering faceting transitions. We propose a broadly applicable rapid-anneal solid phase epitaxial synthesis approach for the creation of atomically flat, high surface free energy oxide heterostructures. We also demonstrate its efficacy via the synthesis of atomically flat, epitaxial RuO 2 (001) films with a superior oxygen evolution activity, quantified by their lower onset potential and higher current density, relative to that of more common RuO 2 (110) films.
In order to combine niobium (Nb) with lanthanum (La) and cerium (Ce), Nb ions were deposited within a thin film of these two elements. According to the Hume-Rothery rules, these elements cannot be combined into a traditional crystalline metallic solid. The creation of an amorphous metallic glass consisting of Nb, La, and Ce is then investigated. Amorphous metallic glasses are traditionally made using fast cooling of a solution of molten metals. In this paper, we show the results of an experiment carried out to form a metallic glass by implanting 9 MeV Nb 3+ atoms into a thin film of La and Ce. Prior to implantation, the ion volume distribution is calculated by Monte Carlo simulation using the SRIM tool suite. As a result, using multiple methods of electron microscopy and material characterization, small quantities of amorphous metallic glass are indeed identified.
As a powerful and versatile thin film deposition technique, atomic layer deposition (ALD) has been increasingly involved in the manufacturing of many energy harvesting and storage devices. Next to the applications of ALD in lithium ion batteries and supercapacitors, ALD in photoelectrochemical (PEC) electrode and triboelectric nanogenerators (TENGs) development is relatively new. Most current progress in these two promising directions is not quite comprehensively covered. This article intends to summarize the most recent and representative research regarding the application of ALD in the fabrication of PEC electrodes and TENG active materials. We first discuss ALD of nanostructured electrochemically active materials and surface coating for PEC photoelectrodes, and the corresponding influence on solar energy conversion efficiency and electrode stability are discussed and compared. A unique high-temperature ALD-based approach, called surface-reaction-limited pulsed chemical vapor deposition (SPCVD) is then introduced as a new approach to the synthesis of 3D branched NW architecture, which offers tremendous advantages in photoelectrode design. At last, a new exploration of ALD in the field of mechanical energy harvesting is presented as an effective strategy to modify the dielectric property of polymer thin films for TENG development.
Copper sulfide is a simple binary material with promising attributes for low-cost thin film photovoltaics. However, stable Cu 2 S-based device efficiencies approaching 10% free from cadmium have yet to be realized. In this paper, transient absorption spectroscopy is used to investigate the dynamics of the photoexcited state of isolated Cu 2 S thin films prepared by atomic layer deposition or vapor-based cation exchange of ZnS. While a number of variables including film thickness, carrier concentration, surface oxidation, and grain boundary passivation were examined, grain structure alone was found to correlate with longer lifetimes. A map of excited state dynamics is deduced from the spectral evolution from 300 fs to 300 μs. Finally, revealing the effects of grain morphology on the photophysical properties of Cu 2 S is a crucial step toward reaching high efficiencies in operationally stable Cu 2 S thin film photovoltaics.
We report on the thermal conductivity of atomic layer deposition-grown amorphous alumina thin films as a function of atomic density. Using time domain thermoreflectance, we measure the thermal conductivity of the thin alumina films at room temperature. The thermal conductivities vary ∼35% for a nearly 15% change in atomic density and are substrate independent. No density dependence of the longitudinal sound speeds is observed with picosecond acoustics. The density dependence of the thermal conductivity agrees well with a minimum limit to thermal conductivity model that is modified with a differential effective-medium approximation.
The effects of homogenous electron beam (EB) irradiation on the crystal growth and thermoelectric properties of n-type Bi-Se-Te and p-type Bi-Sb-Te thin films were investigated. Both types of thin films were prepared by flash evaporation, after which homogeneous EB irradiation was performed at an acceleration voltage of 0.17 MeV. For the n-type thin films, nanodots with a diameter of less than 10 nm were observed on the surface of rice-like nanostructures, and crystallization and crystal orientation were improved by EB irradiation. The resulting enhancement of mobility led to increased electrical conductivity and thermoelectric power factor for the n-type thin films. In contrast, the crystallization and crystal orientation of the p-type thin films were not influenced by EB irradiation. The carrier concentration increased and mobility decreased with increased EB irradiation dose, possibly because of the generation of defects. As a result, the thermoelectric power factor of p-type thin films was not improved by EB irradiation. The different crystallization behavior of the n-type and p-type thin films is attributed to atomic rearrangement during EB irradiation. Selenium in the n-type thin films is more likely to undergo atomic rearrangement than the other atoms present, so only the crystallinity of the n-type Bi-Se-Te thin films was enhanced.
A model is presented and the interaction of accelerated electrons with atoms in a thin film “shooting through” Be target is theoretically described. The algorithm is based on the Monte Carlo simulation of the electron motion in the target accompanied by energy losses in elastic and inelastic interactions. The conversion of the electron energy to the radiation energy in the 11.4-nm K{sub α} line of Be and the emission spectrum are calculated. The maximum conversion efficiency to the solid angle 4π CE = 3.0 × 10{sup –4} is achieved for the electron energy E{sub e} = 2.0 keV and a 40-nm-thick freely suspended beryllium film. 200-nm and 400-nm-thick films were experimentally investigated. The maximum conversion efficiency to the solid angle 4π for a 200‑nm-thick film and the electron energy E{sub e} = 2.75 keV was CE{sub exp} = 9.2 × 10{sup –5}, whereas the calculated value was CE{sub calc} = 2.5 × 10{sup –4}. The observed discrepancy between the theory and experiment is explained in the paper.
The enclosed document provides a final report to document the research performed at the University of Delaware under Grant DE-SC0005403: Improved Electrochemical Performance of Strained Lattice Electrolytes via Modulated Doping. The ultimate goal of this project was to learn how to systematically strain the inter-atomic distance in thin ceramic films and how to use this newfound control to improve the ease by which oxygen ions can conduct through the films. Increasing the ionic conductivity of ceramics holds the promise of drastic improvements in the performance of solid oxide fuel cells, chemical sensors, gas permeation membranes, and related devices. Before this work, the experimental evidence advocating for strain-based techniques was often controversial and poorly characterized. Enabling much of this work was a new method to quickly create a very wide range of ceramic nanostructures that was established during the first phase of the project. Following this initial phase, we created a variety of promising nanostructured epitaxial films and multilayers with systematic variations in lattice mismatch and dopant content. Over the course of the work, a positive effect of tensile atomic strain on the oxygen conductivity was conclusively found using a few different forms of samples and experimental techniques. The samples were built by sputtering, an industrially scalable technique, and thus the technological implementation of these results may be economically feasible. Still, two other results consistently achieved over multiple efforts in this work give pause. The first of these results was that very specific, pristine surfaces upon which to build the nanostructures were strictly required in order to achieve measurable results. The second of these results was that compressively strained films with concomitant reductions in oxygen conductivity are much easier to obtain relative to tensile-strained films with increased conductivity.
In this work, we present a method for producing tunnel junctions from cuprate thin films grown by atomic layer-by-layer molecular beam epitaxy (ALL-MBE). Our approach utilizes microfabrication processing and relies on the atomically precise interfaces provided by the ALL-MBE synthesis technique. The method is suitable for a wide range of junction dimensions and materials and allows for more complex designs such as superconducting quantum interference devices and junction arrays. Fully superconducting electrodes ensure that the contact resistances in the devices created by this method remain very low.
The authors have examined ultrathin (≤10 Å) tantalum nitride (TaN{sub x}) thin films deposited by atomic layer deposition (ALD) on three surfaces relevant to interconnect layers in microelectronic devices: thermally grown SiO{sub 2}; a Cu thin film grown by physical vapor deposition, and a carbon-doped SiO{sub 2} porous low-κ thin film. The authors have employed ex situ angle-resolved x-ray photoelectron spectroscopy (ARXPS), low-energy ion scattering spectroscopy (LEISS), and atomic force microscopy (AFM) to determine the continuity of these thin films, and by implication, the abruptness of the thin film/substrate interface. On SiO{sub 2} and low-κ, the authors find similar results: both ARXPS and AFM indicate that smooth, uniform thin films are deposited, consistent with nearly layer-by-layer growth of TaN{sub x} on these surfaces. Examination of these films using LEISS reveals that while the 10 Å TaN{sub x} thin films are continuous, the 5 Å TaN{sub x} thin films are not continuous and may possess on the order of ∼10% exposed substrate in the form of small subnanometer inclusions. On Cu, the situation is quite different. The TaN{sub x} thin films on these surfaces are not continuous, and our results point to a mixed layer of TaN{sub x} and Cu forming during ALD. In all cases, if one were to rely solely on results from ARXPS, the picture would be incomplete as the results from LEISS are ultimately decisive concerning thin film continuity.