Search NASA⌕ Search

SEARCH · Search NASA

Results for “CORROSIVE”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 865 records · Page 48

Effect of Grain Boundary and Crystallographic Orientation on the Stress Corrosion Behavior of an Al-Zn-Mg Alloy

The effect of grain boundary and crystallographic orientation on the stress corrosion behavior of an Al-4.5Zn-1.4Mg alloy was investigated by comparing the performance of constant load stress corrosion test (CLSCT) and tensile test of specimens parallel to the longitudinal and transverse directions of the extruded plate. The results revealed that the strength of the longitudinal and transverse specimens decreased by 9.68 and 18.13%, respectively, after 10-day CLSCT. The transverse specimens show poor resistance to stress corrosion cracking (SCC). The grain boundaries (GB) of the longitudinal section are less dense, and more of them are distributed along the extrusion direction compared with the cross section with selected areas of the same size. The SCC of all specimens starts from the side faces of the specimen, and it is dominated by intergranular cracking. But the corrosion of the transverse specimens was more serious. The cracks of all specimens tend to propagate along the GBs with misorientation of about 50°-60°, and the difference of Schmidt factor (SF) values of grains on both sides of the crack is significantly large. The crack of longitudinal specimens propagates relatively parallel to the tensile direction, while propagation of the crack in transverse specimens is more zigzag.

36 MATERIALS SCIENCE↗

Aqueous Corrosion Behavior of Cast CoCrFeMnNi Alloy

CoCrFeMnNi high-entropy alloy demonstrates good mechanical properties and can be further strengthened by thermomechanical processes. A sample alloy prepared by vacuum casting in a graphite mold was further investigated for its corrosion resistance. One-millimeter thin strips of cast alloy were used to investigate its corrosion behavior at room temperature. Linear potentiodynamic tests of the alloy in sodium chloride solution confirmed uniform corrosion property comparable to stainless steel AISI 304. However, a positive cyclic hysteresis loop indicated susceptibility to pitting corrosion. In sodium hydroxide solution, metastable pit formation was observed, while sulfuric acid solution passivated the alloy. In both cases, the alloy did not show any spontaneous pitting tendency.

36 MATERIALS SCIENCE↗

The study of stress application and corrosion cracking on Ni-16 Cr-9 Fe (Alloy 600) C-ring samples by polychromatic X-ray microdiffraction

Microscopic strains associated with stress corrosion cracks have been investigated in stressed C-rings of Ni-16 Cr-9 Fe (Alloy 600) boiler tubing. Polychromatic X-ray microdiffraction was used to measure deviatoric strain tensors and the distribution of dislocations near cracks that had been propagated in electrochemically accelerated corrosion tests. An associated investigation of the C-ring-induced strains prior to corrosion showed significant tensile strain in the stress axis direction by the torsional closure of the alloy tube section in the C-ring test. Significant grain lattice rotation and pronounced plastic strain at some grain boundaries were noted. Stress-corrosion-cracking-generated intergranular cracks were produced in two Alloy 600 specimens after 6 h and 18 h tests. The diffraction patterns and resultant strain tensors were mapped around the cracked area to a 1 μm spatial resolution. The strain tensor transverse to the crack growth direction showed tensile strain at the intergranular region just ahead of the crack tip for both specimens. Both cracks were found to follow grain boundary pathways that had the lowest angle of misorientation. Dislocation distributions within each grain were qualitatively obtained from the shapes of the diffraction spots and the effect of 'hard' and 'soft' grains on the crack pathway was explored for both 6 h and 18 h specimens. The Schmid factor of one of the grains adjacent to the crack at the 6 h and 18 h initiation sites was found to be the lowest, compared to Schmid factors calculated for surface grains away from the initiation site, and also along the crack path into the bulk.

36 MATERIALS SCIENCE↗

Solution chemistry of Mo(III) and Mo(IV): Thermodynamic foundation for modeling localized corrosion.

To investigate the behavior of molybdenum dissolution products in systems that approximate localized corrosion environments, solubility of Mo(III) in equilibrium with solid MoO{sub 2} has been determined at 80 C as a function of solution acidity, chloride concentration and partial pressure of hydrogen. The measurements indicate a strong increase in solubility with acidity and chloride concentration and a weak effect of hydrogen partial pressure. The obtained results have been combined with literature data for systems containing Mo(III), Mo(IV), and Mo(VI) in solutions to develop a comprehensive thermodynamic model of aqueous molybdenum chemistry. The model is based on a previously developed framework for simulating the properties of electrolyte systems ranging from infinite dilution to solid saturation or fused salt limit. To reproduce the measurements, the model assumes the presence of a chloride complex of Mo(III) (i.e., MoCl{sup 2+}) and hydrolyzed species (MoOH{sup 2+}, Mo(OH){sup 2+}, and Mo(OH){sub 3}{sup 0}) in addition to the Mo{sup 3+} ion. The model generally reproduces the experimental data within experimental scattering and provides a tool for predicting the phase behavior and speciation in complex, concentrated aqueous solutions. Thus, it provides a foundation for simulating the behavior of molybdenum species in localized corrosion environments.

08 HYDROGEN↗

Understanding a novel form of intergranular corrosion of stainless steel 316L exposed to molten LiCl-Li 2 O-Li

We report stainless steel 316 L exposed to LiCl-Li2O molten salt containing Li metal for 500 and 1000 h experiences deep intergranular attack and bulk void formation. This degradation is due to a synergistic corrosion mechanism, different than other forms of molten salt corrosion, where Cr and Mn oxides and carbides form along grain boundaries and are dissolved by Li metal. Synchrotron transmission X-ray microscopy 3D imaging is used to show corrosion morphology and Cr enrichment and depletion in a novel format that has not previously been used for bulk corrosion samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Electrochemical stability and corrosion behavior of Ni-Cr alloy in molten LiCl-KCl salt

This study investigated the electrochemical properties and potential-dependent stability of Cr(II) and Ni(II) in a eutectic LiCl-KCl molten salt at 500 °C under an argon atmosphere using a three-electrode cell configuration with a glassy carbon working electrode, Ag/Ag + reference electrode, and graphite counter electrode. Cyclic voltammetry was employed to characterize the Cr(0)/Cr(II)/Cr(III) and Ni(0)/Ni(II) redox transitions, yielding diffusion coefficients of 0.50 (±0.01) × 10 −5 cm 2 s −1 for Cr(II) and 0.91 (±0.16) × 10 −5 cm 2 s −1 for Ni(II) at 500 °C. The redox stability domains of these species provided insight into the corrosion mechanisms of a Ni-Cr alloy (80–20 wt %) in LiCl-KCl salt. The measured open circuit potential of the alloy corresponded to the range of potentials where the Ni(0) and Cr(II) species are stable, indicating a preferential dissolution of Cr. Immersion testing of the alloy for 336 h confirmed significant Cr depletion (or Ni-enrichment) at the surface layer, corroborating Cr dealloying as the dominant corrosion reaction under open circuit conditions. Additionally, the application of a small anodic overpotential (0.11 V) resulted in selective Cr dissolution while a large anodic overpotential (0.25 V) resulted in co-dissolution of both Cr and Ni. Furthermore, these results demonstrate that the corrosion mechanisms of a Ni-Cr alloy in LiCl-KCl depend upon the applied potential, and thus the redox conditions of the molten salt should be carefully controlled in the design of a redox buffer to mitigate corrosion in molten salt environments.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Corrosion of 316 SS in direct contact with Zircaloy-4 in repository relevant conditions

The effects of interfacial contact between 316 stainless steel (316 SS) waste canister and spent fuel cladding material (Zircaloy-4) in case of water intrusion into a deep geological repository are investigated. Hydrothermal corrosion experiments of 316 SS and Zircaloy-4 in direct contact were performed at elevated temperatures in MilliQ water and simulated Mont Terri groundwater. Hematite, magnetite, chromite, and baddeleyite form as secondary phases. pH of the Mont Terri solution increases with corrosion duration and magnetite forms preferentially instead of hematite. Thermodynamic modeling shows that iron oxidation in 316 SS controls the pH and redox potential of the aqueous environment and is in good agreement with experimental Mont Terri results, showing that experimental Mont Terri results trend to equilibrium. All oxides except hematite are predicted to exist at thermodynamic equilibrium based on calculations, implying that experimentally formed hematite will be reduced or transformed to magnetite at equilibrium. The thermodynamically predicted chromite was observed to form only at the interface where 316 SS was in contact with Zircaloy-4 at 250°C, showing that contact with Zircaloy-4 seems to accelerate the 316 SS corrosion to thermodynamic equilibrium. Finally, Mont Terri groundwater readily trends towards thermodynamic equilibrium, leading to a pH and redox buffered system that is dominated by iron in solution coming from the accelerated corrosion of 316 SS caused by Zircaloy-4 contact.

316 stainless steel↗

The corrosion behavior of Ce-implanted magnesium alloys

The aim of this study was to investigate the effect of cerium ion implantation on the corrosion behavior of AZ31 magnesium alloys. Samples were implanted with doses of 5 x 10{sup 16}, 1 x 10{sup 17} and 5 x 10{sup 17} ion/cm{sup 2}, respectively, using a metal vapor vacuum arc (MEVVA) source at an extraction voltage of 45 kV. Auger electron spectrometry (AES) and X-ray photoelectron spectroscopy (XPS) were used to analyze the depth distribution and the valence states of elements in the implanted layer, respectively. The potentiodynamic polarization technique was applied to evaluate the corrosion resistance of the implanted samples in a 3.5 wt.% NaCl solution saturated with Mg(OH){sub 2}. The results showed that under an optimal dose the corrosion resistance of the implanted sample was improved compared with that of the bare sample. Finally, the corrosion mechanism of the Ce-implanted samples was discussed.

36 MATERIALS SCIENCE↗

Friction stir welded AM50 and AZ31 Mg alloys: Microstructural evolution and improved corrosion resistance

One of the major drawbacks of Mg alloys is poor weldability, caused by porosity formation during conventional fusion welding processes. Friction Stir Welding (FSW) is promising technique in this context since it is a solid state technique. Contradicting results were published in the literature regarding the FSWed Mg alloys joint's properties. Current research was performed in order to investigate the microstructure and corrosion properties of FSWed Mg alloys, studying representatives of two commercial families: wrought AZ31-H24 and die cast AM50. It was found that in both alloys recrystallization occurred during the FSW. In AM50 the mechanism of the recrystallization was continuous, manifested by dislocation rearrangement into sub grain boundaries. In AZ31 discontinuous recrystallization had occurred through grain boundaries migration - twins rotated with respect to the matrix, turning into low angle grain boundaries. Corrosion resistance has improved during the FSW in both alloys to different extents. In the AM50 alloy, the nugget exhibited significantly higher surface potential than the base metal mainly due to the higher Al concentration in the matrix of the nugget, resulting from the dissolution of Al-enrichment and β-Mg{sub 17}Al{sub 12} phase. In the AZ31 alloy, no change in Al concentration had occurred, and the surface potential measured in the nugget was only slightly higher than in the base metal. These results underline the appropriateness of the FSW for Mg alloys since during the conventional welding deterioration of the corrosion resistance occurs. - Highlights: • Following FSW, AZ31-H24 experienced discontinuous recrystallization. • In AZ31 grain boundaries migration occurred, thus twins rotated. • In die cast AM50 continuous recrystallization occurred during the FSW. • In AM50 - dislocations rearranged into sub grain boundaries. • Corrosion resistance has improved during the FSW in both alloys to different extent.

36 MATERIALS SCIENCE↗

Effect of cerium on structure modifications of a hybrid sol–gel coating, its mechanical properties and anti-corrosion behavior

Highlights: ► New sol–gel routes to replace chromates for corrosion protection of aluminum. ► Effect of cerium concentration on the microstructure of xerogel. ► Electrochemical and mechanical performances of hybrid coating with different cerium contents. ► Good correlation between the different results with an optimal cerium content of 0.01 M. -- Abstract: An organic–inorganic hybrid coating was developed to improve the corrosion resistance of the aluminum alloy AA 2024-T3. Organic and inorganic coatings derived from glycidoxypropyl-trimethoxysilane (GPTMS) and aluminum tri-sec-butoxide Al(O{sup s}Bu){sub 3}, with different cerium contents, were deposited onto aluminum by dip-coating process. Corrosion resistance and mechanical properties were investigated by electrochemical impedance measurements and nano-indentation respectively. An optimal cerium concentration of 0.01 M was evidenced. To correlate and explain the hybrid coating performances in relation to the cerium content, NMR experiments were performed. It has been shown that when the cerium concentration in the hybrid is higher than 0.01 M there are important modifications in the hybrid structure that account for the mechanical properties and anti-corrosion behavior of the sol–gel coating.

36 MATERIALS SCIENCE↗

Development in corrosion resistance by microstructural refinement in Zr-16 SS 304 alloy using suction casting technique

Highlights: • Grain refinement was made in Zr–16 wt.% SS alloy while prepared by suction casting process. • Distribution of Laves phase, e.g., Zr{sub 2}(Fe, Cr) was raised in suction cast (SC) Zr–16 wt.% SS. • Corrosion resistance was improved in SC alloy compared to that of arc-melt-cast alloy. • Grain refinement in SC alloy assisted for an increase in its corrosion resistance. - Abstract: Zirconium (Zr)-stainless steel (SS) hybrid alloys are being considered as baseline alloys for developing metallic-waste-form (MWF) with the motivation of disposing of Zr and SS base nuclear metallic wastes. Zr–16 wt.% SS, a MWF alloy optimized from previous studies, exhibit significant grain refinement and changes in phase assemblages (soft phase: Zr{sub 2}(Fe, Cr)/α-Zr vs. hard phase: Zr{sub 3}(Fe, Ni)) when prepared by suction casting (SC) technique in comparison to arc-cast-melt (AMC) route. Variation in Cr-distribution among different phases are found to be low in suction cast alloy, which along with grain refinement restricted Cr-depletion at the Zr{sub 2}(Fe, Cr)/Zr interfaces, prone to localized attack. Hence, SC alloy, compared to AMC alloy, showed lower current density, higher potential at the breakdown of passivity and higher corrosion potential during polarization experiments (carried out under possible geological repository environments, viz., pH 8, 5 and 1) indicating its superior corrosion resistance.

36 MATERIALS SCIENCE↗

Considerations for realistic atmospheric environments: An application to corrosion testing

Measured salt compositions in dust collected over roughly the last decade from surfaces of in-service stainless-steel alloys at four locations around the United States are presented, along with the predicted brine compositions that would result from deliquescence of these salts. The salt compositions vary greatly from ASTM seawater and from laboratory salts (i.e., NaCl or MgCl 2 ) commonly used on corrosion testing. The salts contained relatively high amounts of sulfates and nitrates, evolved to basic pH values, and exhibited deliquescence relative humidity values (RH) higher than seawater. Additionally, inert dust in components were quantified and considerations for laboratory testing are presented. The observed dust compositions are discussed in terms of the potential corrosion behavior and are compared to commonly used accelerated testing protocols. Finally, ambient weather conditions and their influence on diurnal fluctuations in temperature (T) and RH on heated metal surfaces are evaluated and a relevant diurnal cycle for laboratory testing a heated surface has been developed. Suggestions for future accelerated tests are proposed that include exploration of the effects of inert dust particles on atmospheric corrosion, chemistry considerations, and realistic diurnal fluctuations in T and RH. Understanding mechanisms in both realistic and accelerated environments will allow development of a corrosion factor (i.e., scaling factor) for the extrapolation of laboratory-scale test results to real world applications.

54 ENVIRONMENTAL SCIENCES↗

Synthesis and Structures of Pb[subscript 3]O[subscript 2](CH[subscript 3]COO)[subscript 2]·0.5H[subscript 2]O and Pb[subscript 2]O(HCOO)[subscript 2]: Two Corrosion Products Revisited

Reactions of carboxylic acids with lead play an important role in the atmospheric corrosion of lead and lead-tin alloys. This is of particular concern for the preservation of lead-based cultural objects, including historic lead-tin alloy organ pipes. Two initial corrosion products, Pb{sub 3}O{sub 2}(CH{sub 3}COO){sub 2} {center_dot} 0.5H{sub 2}O (1) and Pb{sub 2}O(HCOO){sub 2} (2), had been identified through powder diffraction fingerprints in the Powder Diffraction File, but their structures had never been determined. We have crystallized both compounds using hydrothermal solution conditions, and structures were determined using laboratory and synchrotron single-crystal X-ray diffraction data. Compound 1 crystallizes in P{sub t}, and 2 in Cccm. These compounds may be viewed as inorganic-organic networks containing single and double chains of edge-sharing Pb{sub 4}O tetrahedra and have structural similarities to inorganic basic lead compounds. Bond valence sum analysis has been applied to the hemidirected lead coordination environments in each compound. Atmospheric exposure experiments contribute to understanding of the potential for conversion of these short-term corrosion products to hydrocerussite, Pb{sub 3}(CO{sub 3}){sub 2}(OH){sub 2}, previously identified as a long-term corrosion product on lead-rich objects. Each compound was also characterized by elemental analysis, thermogravimetric analysis and differential scanning calorimetry (TGA-DSC), and Raman spectroscopy.

43 PARTICLE ACCELERATORS↗

Study of benzotriazole as corrosion inhibitors of carbon steel in chloride solution containing hydrogen sulfide using electrochemical impedance spectroscopy (EIS)

Corrosion and inhibition studies on API 5LX65 carbon steel in chloride solution containing various concentrations of benzotriazole has been conducted at temperature of 70°C using Electrochemical Impedance Spectroscopy (EIS). Corroded carbon steel surface with and without inhibitor have been observed using X-ray Diffraction (XRD), Scanning Electron Microscope (SEM), and Energy Dispersive Spectroscopy (EDS). The objectives of this research are to study the performance of benzotriazole as corrosion inhibitors. The experimental results of carbon steel corrosion in 3.5% NaCl solution containing 500 mg/l H{sub 2}S at different BTAH concentrations showed that corrosion rate of carbon steel decreases with increasing of BTAH concentrations from 0 to 10 mmol/l. The inhibition efficiency of BTAH was found to be affected by its concentration. The optimum efficiency obtained of BTAH is 93% at concentration of 5 mmol/l. The result of XRD and EDS analysis reveal the iron sulfide (FeS) formation on corroded carbon steel surface without inhibitor. The EDS spectrum show the Nitrogen (N) bond on carbon steel surface inhibited by BTAH.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

Tannin bark Melalauca cajuputi powell (gelam) as green corrosion inhibitor of mild steel

Tannin was extracted from gelam bark and used to produce corrosion inhibitor for mild steel. Tannin was extracted from gelam bark using 70% aqueous acetone for 6 hour. Tannin powder was characterization using fourier transform infrared spectroscopy to analyse chemical component in tannin and Scanning electron microscope (SEM) for tannin physical structure. The tannin effect on the corrosion inhibition of mild steel has been investigated in 1Mol HCl solution for 6 hour followed ASTM. The weight loss method were applied to study the mild steel corrosion behavior in the present and absend of different concentration of tannin (250, 300, 350)ppm. Tannin act good inhibitor as corrosion inhibitor for mild steel in acid medium. Surface morphology of carbon steel with and without inhibitor was investigated by scanning electron microscopy.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The effect of pH on the corrosion behavior of intermetallic compounds Ni{sub 3}(Si,Ti) and Ni{sub 3}(Si,Ti) + 2Mo in sodium chloride solutions

The corrosion behavior of the intermetallic compounds, Ni{sub 3}(Si,Ti) (L1{sub 2}: single phase) and Ni{sub 3}(Si,Ti) + 2Mo (L1{sub 2} and (L12 + Ni{sub ss}) mixture region), has been investigated using an immersion test, electrochemical method and surface analytical method (SEM; scanning electron microscope and EDAX: Energy Dispersive X-ray) in 0.5 kmol/m{sup 3} NaCl solutions at various pH. The corrosion behavior of nickel alloy C-276 was studied under the same experimental conditions as a reference. It was found that the uniform attack was observed on Ni{sub 3}(Si,Ti) for the immersion test at lower pH, while the pitting attack was observed on this compound for this test at neutral solution. Furthermore, Ni{sub 3}(Si,Ti)+2Mo had the preferential dissolution of L1{sub 2} compared to (L1{sub 2} + Ni{sub ss}) mixture region at lower pH, while pitting attack occurred in (L1{sub 2} + Ni{sub ss}) mixture region at neutral solution. For both intermetallic compounds, the magnitude of pitting and uniform attack decrease with increasing pH of solutions. From the immersion test and polarization curves, the corrosion resistance of Ni{sub 3}(Si,Ti)+2Mo is lower than that of Ni{sub 3}(Si,Ti), while the nickel alloy C-276 is the highest one at various pH of solutions. On the other hand, in the lower pH of solutions, the corrosion resistance of tested materials decreased significantly compared to those in neutral and higher pH of solutions.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Sputtered carbon as a corrosion barrier for x-ray detector windows

Sputtered amorphous carbon thin films were explored as corrosion resistant coatings on aluminum thin films to be incorporated into x-ray detector windows. The requirements for this application include high corrosion resistance, low intrinsic stress, high strains at failure, and high x-ray transmission. Low temperature sputtering was used because of its compatibility with the rest of the window fabrication process. Corrosion resistance was tested by exposure of carbon coated and uncoated Al thin films to humidity. Substrate curvature and bulge testing measurements were used to determine intrinsic stress and ultimate strain at failure. The composition and bonding of the carbon films were further characterized by electron energy loss spectroscopy, Raman spectroscopy, and carbon, hydrogen, and nitrogen elemental analyses. Samples had low compressive stress (down to.08 GPa), a high strain at failure (3%), and a low fraction of sp{sup 3} carbon–carbon bonds (less than 5%). The high breaking strain and excellent x-ray transmission of these sputtered carbon films indicate that they will work well as corrosion barriers in this application.

36 MATERIALS SCIENCE↗

Estimating Effects of Various Factors on Corrosion of Pipeline Grade Carbon Steel Under Disbonded Coating (Status Update)

This report provides description of the activities, associated data and results for a work focused on understanding corrosion of pipeline grade carbon steel under coating disbondment. Specifically, the work reported here was for a pipeline that was installed in 1968 with the following characteristics. The line was coated with polyethylene tape coat (brand Polyken), and the line joints were electric-flash welded. The line joints are 34-inch outer diameter, and made of API 5L X52 grade carbon steel. The line was initially operated at 55 °F, but subsequently the line temperature increased to 105 °F due to higher fluid flow rate inside the pipe. Due to age and type of the pipeline coating, coating disbondment has occurred at several locations. The increase in operating temperature, coupled with age of the coating, is likely to have resulted in migration in corrosive species from the soil underneath the coating. As a result, the pipeline is experiencing enhanced corrosion. The objective of this study was to evaluate whether the change in operating temperature has affected the corrosion rate of the pipeline external surfaces under areas of disbonded coating.

36 MATERIALS SCIENCE↗