Synthesis of nanometer-sized fayalite and magnesium-iron(II) mixture olivines
Not Available
SEARCH · Search NASA
Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.
Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.
Not Available
A set of column experiments was conducted to investigate the chemical and physical heterogeneity effect on colloid facilitated transport under slow pore velocity conditions. Pore velocities were kept below 100 cm d-1 for all experiments. Glass beads were packed into columns establishing four different conditions: 1) homogeneous, 2) mixed physical heterogeneity, 3) sequentially layered physical heterogeneity, and 4) chemical heterogeneity. The homogeneous column was packed with glass beads (diameter 500-600 µm), and physical heterogeneities were created by sequential layering or mixing two sizes of glass bead (500-600 µm and 300-400 µm). A chemical heterogeneity was created using 25% of the glass beads coated with hydrophobic molecules (1H-1H-2H-2H-perfluorooctyltrichlorosilane) mixed with 75% pristine glass beads (all 500-600 µm). Input solution with 0.5 mM CsI and 50 mg L-1 colloids (1-µm diameter SiO2) was pulsed into columns under saturated conditions. The physical heterogeneity in the packed glass beads retarded the transport of colloids compared to homogeneous (R = 25.0), but showed only slight differences between sequentially layered (R = 60.7) and mixed heterogeneity(R = 62.4). The column with the chemical, hydrophobic/hydrophilic, heterogeneity removed most of the colloids from the input solution. All column conditions stripped Cs from colloids onto the column matrix of packed glass beads.
The effect of composition on the viscosity of multicomponent glasses was expressed as a function of temperature and composition for three composition regions containing various subsets of Al2O3, B2O3, Bi2O3, CaO, Cr2O3, F, Fe2O3, K2O, Li2O, MgO, MnO, Na2O, NiO, P2O5, SiO2, UO2, and ZrO2. Limits of applicability of the composition models are discussed.
As part of ongoing studies to evaluate the relationships between structural variations in silicate glasses and rates of glass dissolution in aqueous media, molecular structures present in sodium borosilicate glasses of composition Na2O.xB2O3.(3-x)SiO2, with x 1 (Na2O/B2O3 ratio 1), were analyzed using deep-UV Raman spectroscopy. The results were quantified in terms of the fraction of SiO4 tetrahedra with one non-bridging oxygen (Q3) and then correlated with Na2O and B2O3 content. Increasing Na2O was found to raise the fraction of Q3 units in the glasses systematically, in agreement with studies on related glasses, and, as long as the value of x was not too high, contribute to higher rates of dissolution in single pass flow-through testing. The finding was obtained across more than one series of silica-rich glasses prepared for independent dissolution studies. In contrast, dissolution rates were less strongly determined by the Q3 fraction when the value of x was near unity and appeared to grow larger upon further reduction of the Q3 fraction. The results were interpreted to indicate the increasingly important role of network hydrolysis in the glass dissolution mechanism as the BO4 tetrahedron replaces the Q3 unit as the charge-compensating structure for Na+ ions. Finally, the use of deep-UV Raman spectroscopy was found to be advantageous in studying finely powdered glasses in cases where visible Raman spectroscopy suffered from weak Raman scattering and fluorescence interference.
Sodium and aluminum rich high level nuclear waste glasses are prone to nepheline (NaAlSiO4) crystallization. Since nepheline removes three moles of glass forming oxides (Al2O3 and SiO2) per each mole of Na2O, its formation can result in sever deterioration of the chemical durability. The present study aims at investigating the relationships between the molecular-level structure of sodium alumino-borosilicate based simulated high-level nuclear waste glasses and their crystallization behavior by infrared spectroscopy (FTIR) and x-ray diffraction, respectively. The molecular structure of most of the investigated glasses comprises of a mixture of Q2 and Q3 (Si) units while aluminum and boron are predominantly present in tetrahedral and trigonal coordination, respectively. The increasing boron content has been shown to suppress the nepheline formation in the glasses. The structural influence of various glass components on nepheline crystallization has been discussed.
Aluminum is one of the most common components included in nuclear waste glasses. Therefore, Monte Carlo (MC) simulations were carried out to investigate the influence of aluminum on the rate and mechanism of dissolution of sodium borosilicate glasses in static conditions. The glasses studied were in the compositional range (70-2x)% SiO2 x% Al2O3 15% B2O3 (15+x)% Na2O, where 0 ≤ x ≤ 15%. The simulation results show that increasing amounts of aluminum in the pristine glasses slow down the initial rate of dissolution as determined from the rate of boron release. However, the extent of corrosion - as measured by the total amount of boron release - initially increases with addition of Al2O3, up to 5 Al2O3 mol%, but subsequently decreases with further Al2O3 addition. The MC simulations reveal that this behavior is due to the interplay between two opposing mechanisms: (1) aluminum slows down the kinetics of hydrolysis/condensation reactions that drive the reorganization of the glass surface and eventual formation of a blocking layer; and (2) aluminum strengthens the glass thereby increasing the lifetime of the upper part of its surface and allowing for more rapid formation of a blocking layer. Additional MC simulations were performed whereby a process representing the formation of a secondary aluminosilicate phase was included. Secondary phase formation draws dissolved glass components out of the aqueous solution, thereby diminishing the rate of condensation and delaying the formation of a blocking layer. As a result, the extent of corrosion is found to increase continuously with increasing Al2O3 content, as observed experimentally. For Al2O3 < 10 mol%, the MC simulations also indicate that, because the secondary phase solubility eventually controls the aluminum content in the part of the altered layer in contact with the bulk aqueous solution, the dissolved aluminum and silicon concentrations at steady state are not dependent on the Al2O3 content of the pristine aluminoborosilicate glass.
Borosilicate nuclear waste glasses develop complex altered layers as a result of coupled processes such as hydrolysis of network species, condensation of Si species, and diffusion. However, diffusion has often been overlooked in Monte Carlo models of the aqueous corrosion of borosilicate glasses. Therefore, three different models for dissolved Si diffusion in the altered layer were implemented in a Monte Carlo model and evaluated for glasses in the compositional range (75-x) mol% SiO2 (12.5+x/2) mol% B2O3 and (12.5+x/2) mol% Na2O, where 0 ≤ x ≤ 20%, and corroded in static conditions at a surface-to-volume ratio of 1000 m-1. The three models considered instantaneous homogenization (M1), linear concentration gradients (M2), and concentration profiles determined by solving Fick’s 2nd law using a finite difference method (M3). Model M3 revealed that concentration profiles in the altered layer are not linear and show changes in shape and magnitude as corrosion progresses, unlike those assumed in model M2. Furthermore, model M3 showed that, for borosilicate glasses with a high forward dissolution rate compared to the diffusion rate, the gradual polymerization and densification of the altered layer is significantly delayed compared to models M1 and M2. Models M1 and M2 were found to be appropriate models only for glasses with high release rates such as simple borosilicate glasses with low ZrO2 content.
Liquidus temperature (TL) was measured for simulated high-level waste borosilicate glasses covering a Hanford composition region, using an optical method and a crystal-fraction extrapolation method with X-ray diffraction data from isothermal heat treatments. The 38 glasses encompassed a one-component-at-a-time variation of a 16-component matrix. The TL values ranged from 1006°C to 1603°C. First-order polynomial models were fitted to data to obtain coefficients in terms of the effect of 1 mass% component addition on the TL: TL-increasing oxides Cr2O3 (264°C), “Others” (minor components, 163°C), oxides of noble metals (137°C), NiO (91°C), Al2O3 and Fe2O3 (~19–21°C); TL-decreasing oxides K2O (-26°C), Na2O (-41°C), and Li2O (-68°C); oxides of little effect MnO, P2O5, ZrO2, F, Bi2O3, SiO2, B2O3, and CaO (9 to -12°C). Also presented are temperatures (T1%) at which glasses contain 1 vol% of spinel as these values are considered relevant to the Hanford Tank Waste Treatment and Immobilization Plant. The measured and estimated values are compared and contrasted and the effect of TL and T1% on glass formulation is discussed.
Silicon carbide (SiC) is suggested as an oxygen getter in UO2 kernels used for TRISO particle fuels to lower oxygen potential and prevent kernel migration during irradiation. Scanning electron microscopy and X-ray diffractometry analyses performed on sintered kernels verified that internal gelation process can be used to incorporate SiC in urania fuel kernels. Sintering in either Ar or Ar-4%H2 at 1500 C lowered the SiC content in the UO2 kernels to some extent. Formation of UC was observed as the major chemical phase in the process, while other minor phases such as U3Si2C2, USi2, U3Si2, and UC2 were also identified. UC formation was presumed to be occurred by two reactions. The first was the SiC reaction with its protective SiO2 oxide layer on SiC grains to produce volatile SiO and free carbon that subsequently reacted with UO2 to form UC. The second process was direct UO2 reaction with SiC grains to form SiO, CO, and UC, especially in Ar-4%H2. A slightly higher density and UC content was observed in the sample sintered in Ar-4%H2, but the use of both atmospheres produced kernels with ~95% of theoretical density. It is suggested that incorporating CO in the sintering gas would prevent UC formation and preserve the initial SiC content.
Not Available
This paper discusses work to develop Na2O-B2O3-SiO2 glass binders for immobilizing LiCl-KCl eutectic salt waste in a glass-bonded sodalite waste form following electrochemical reprocessing of used metallic nuclear fuel. Here, five new glasses with high Na2O contents were designed to generate waste forms having higher sodalite contents and fewer stress fractures. The structural, mechanical, and thermal properties of the new glasses were measured using variety of analytical techniques. The glasses were then used to produce ceramic waste forms with surrogate salt waste. The materials made using the glasses developed during this study were formulated to generate more sodalite than materials made with previous baseline glasses used. The coefficients of thermal expansion for the glass phase in the glass-bonded sodalite waste forms made with the new binder glasses were closer to the sodalite phase in the critical temperature region near and below the glass transition temperature. These improvements should result in lower probability of cracking in the full-scale monolithic ceramic waste form, leading to better long-term chemical durability. Additionally, a model generated during this study for predicting softening temperature of silicate binder glasses is presented.
Not Available
Glass-bonded sodalite composite waste forms have been developed for the immobilization of liquid radioactive wastes resulting from off-gas treatment during aqueous reprocessing of used nuclear fuel, with a particular focus on 129I. The proposed composite waste form is comprised of aluminosilicate ceramic phases containing volatile radionuclides bonded with a glassy matrix. In this work, a suite of ten candidate low-temperature glass binders (ZnO-Bi2O3-based glasses and a Na2O-B2O3-SiO2 glass) were examined. Six glasses were mixed with caustic scrubber waste simulant previously converted into a sodalite-rich material (to provide glass fractions of 10 and 20 wt.%), uniaxially pressed into pellets, and sintered at 350 °C or 550 °C for 8 h in air. Iodine retention after heat treatment was assessed by neutron activation analysis, showing retention of 67-100 % of expected iodine. The aqueous durabilities of the resulting materials were then determined, following the ASTM C1308 standard test, showing iodine releases of 1 to 23 g m-2 after 4 d. The cumulative iodine release for the best performing system (a zinc-bismuth-borate glass binder) was <1 g m-2, and its iodine retention from processing was 67 %. The iodine releases compared favorably with other waste forms. In parallel, this best-performing composition was also consolidated via hot isostatic pressing (HIP) in a stainless-steel canister at 550 °C for 2 h under 100 MPa pressure. The HIPed sample was produced at the ~20 g scale and showed improved densification and minimal reaction with the canister.
A series of barium aluminosilicate glasses modified with CaO and B2O3, were prepared and evaluated with respect to their suitability in sealing planar solid oxide fuel cells (SOFCs). At a target operating temperature of 750ºC, the long-term CTE of one particular composition (35 mol% BaO, 15 mol% CaO, 10 mol% B2O3, 5 mol% Al2O3, bal. SiO2) was found to be particularly stable, due to devitrification to a mixture of glass and ceramic phases. This sealant composition exhibits minimal chemical interaction with the yttria-stabilized zirconia electrolyte, yet forms a strong bond with this material. Interactions with metal components were found to be more extensive and depended on the composition of the metal oxide scale that formed during sealing. Generally alumina-scale formers exhibited a more compact reaction zone with the glass than chromia-scale forming alloys. Mechanical measurements conducted on the bulk glass-ceramic and on seals formed using these materials indicate that the sealant is anticipated to display adequate long-term strength for most conventional stationary SOFC applications.
Graphical abstract: We have demonstrated a novel yet simple method for fabricating graphene-based vertical hybrid structures by performing the CVD growth of graphene at an h-BN/Cu interface. Our systematic Raman measurements combined with plasma etching process indicate that a graphene film is grown under exfoliated h-BN rather than on its top surface, and that an h-BN/graphene vertical hybrid structure has been fabricated. Electrical transport measurements of this h-BN/graphene, transferred on SiO2, show the carrier mobility up to approximately 2250 cm{sup 2} V{sup −1} s{sup −1}. The developed method would enable the exploration of the possibility of novel hybrid structure integration with two-dimensional material systems. - Abstract: We have demonstrated a novel yet simple method for fabricating graphene-based vertical hybrid structures by performing the CVD growth of graphene at an h-BN/Cu interface. Our systematic Raman measurements combined with plasma etching process indicate that a graphene film is grown under exfoliated h-BN rather than on its top surface, and that an h-BN/graphene vertical hybrid structure has been fabricated. Electrical transport measurements of this h-BN/graphene, transferred on SiO{sub 2}, show the carrier mobility up to approximately 2250 cm{sup 2} V{sup −1} s{sup −1}. The developed method would enable the exploration of the possibility of novel hybrid structure integration with two-dimensional material systems.
Brillouin scattering measurements on single-crystal stishovite, a high-pressure polymorph of SiO2, were carried out to 22 GPa. Acoustic velocities in three 30-em thick crystal platelets of synthetic stishovite were measured in a forward symmetric scattering geometry, and the full set of elastic constants were retrieved to 12 GPa. The measured velocity data were fit to Christoffel's equation, yielding ambient-pressure elastic constants of C11 = 455(1) GPa, C33 = 762(2) GPa, C12 = 199(2) GPa, C13 = 192(2) GPa, C44 = 258(1) GPa, and C66 = 321(1) GPa. The elastic modulus (C11 - C12)/2 was observed to decrease with pressure, indicating acoustic mode softening, consistent with theoretical predications for the behavior of stishovite as it approaches the transition to the CaCl2-type phase. The bounds on the aggregate adiabatic bulk and shear moduli are KS0 = 315(1) GPa, G0 = 240(1) GPa for the Voigt bound, KS0 = 301(1) GPa, G0 = 216(1) GPa for the Reuss bound. Pressure derivatives of aggregate bulk and shear moduli were constrained to be (?KS/?P)T0 = 4.34(16) and (?G/?P)0 = 0.7(1) for the Reuss bound, and (?KS/?P)T0 = 4.0(1) and (?G/?P)0 = 1.1(1) for the Voigt-Reuss-Hill (VRH) average, respectively, by fitting the data to Eulerian finite strain equations. The volume compression curve obtained from our Brillouin measurement is in very good agreement with previous compression studies up to 50 GPa.
The volumetric properties of silicate glasses and supercooled liquid are examined at high pressures and temperatures using X-ray computed tomography (CT) and absorption. The high pressure X-ray microtomography (HPXMT) system at the Advanced Photon Source, Argonne National Laboratory (GeoSoilEnvironCARS 13-BM-D beamline) consists of two opposing anvils compressed within an X-ray-transparent containment ring supported by thrust bearings and loaded using a 250-ton hydraulic press. This system permits the pressure cell to rotate under the load, while collecting radiographs through at least 180{sup o} of rotation. The 13-BM-D beamline permits convenient switching between monochromatic radiation required for radiography and polychromatic radiation for pressure determination by energy dispersive diffraction. We report initial results on several refractory magnesium silicate glasses synthesized by levitation laser heating. Volume changes during room temperature compression of Mg-silicate glasses with 33 mol% and 38 mol% SiO2 up to 11.5 GPa give an isothermal bulk moduli of 93--100 GPa for a K' of 1. These values are consistent with ultrasonic measurements of more silica-rich glasses. The volumetric properties of amorphous MgSiO{sub 3} at 2 GPa were examined during annealing up to 1000 C. We consider the consequences of heating through the glass transition and the implications for thermal expansivity of supercooled liquids at high pressure. Our results illustrate the capabilities of HPXMT for studies of refractory glasses and liquids at high pressure and offer strategies for future studies of liquid densities within the melting interval for magmas in planet interiors.