Effects of Undercooling and Cooling Rate on Peritectic Phase Crystallization Within Ni-Zr Alloy Melt

The liquid Ni-16.75 at. pct Zr peritectic alloy was substantially undercooled and containerlessly solidified by an electromagnetic levitator and a drop tube. The dependence of the peritectic solidification mode on undercooling was established based on the results of the solidified microstructures, crystal growth velocity, as well as X-ray diffraction patterns. Below a critical undercooling of 124 K, the primary Ni{sub 7}Zr{sub 2} phase preferentially nucleates and grows from the undercooled liquid, which is followed by a peritectic reaction of Ni{sub 7}Zr{sub 2}+L → Ni{sub 5}Zr. The corresponding microstructure is composed of the Ni{sub 7}Zr{sub 2} dendrites, peritectic Ni{sub 5}Zr phase, and inter-dendritic eutectic. Nevertheless, once the liquid undercooling exceeds the critical undercooling, the peritectic Ni{sub 5}Zr phase directly precipitates from this undercooled liquid. However, a negligible amount of residual Ni{sub 7}Zr{sub 2} phase still appears in the microstructure, indicating that nucleation and growth of the Ni{sub 7}Zr{sub 2} phase are not completely suppressed. The micromechanical property of the peritectic Ni{sub 5}Zr phase in terms of the Vickers microhardness is enhanced, which is ascribed to the transition of the peritectic solidification mode. To suppress the formation of the primary phase completely, this alloy was also containerlessly solidified in free fall experiments. Typical peritectic solidified microstructure forms in large droplets, while only the peritectic Ni{sub 5}Zr phase appears in smaller droplets, which gives an indication that the peritectic Ni{sub 5}Zr phase directly precipitates from the undercooled liquid by completely suppressing the growth of the primary Ni{sub 7}Zr{sub 2} phase and the peritectic reaction due to the combined effects of the large undercooling and high cooling rate.

36 MATERIALS SCIENCE↗

Formation of β-NiAl Phase During Casting of a Ni-Based Superalloy

A high-refractory Ni-based superalloy prototype was melted on a research scale while simulating industry practices. Ingots were vacuum induction melted and subjected to a computationally optimized homogenization heat treatment prior to fabrication which consisted of forging and hot rolling. Failure of one of the ingots at the early stage of the forging process was attributed to the precipitation of the β-NiAl phase during melting which stabilized the eutectic constituent.

36 MATERIALS SCIENCE↗

On the Solidification and Structure Formation during Casting of Large Inserts in Ferritic Nodular Cast Iron

The graphite nodule count and size distributions for boiling water reactor (BWR) and pressurized water reactor (PWR) inserts were investigated by taking samples at heights of 2160 and 1150 mm, respectively. In each cross section, two locations were taken into consideration for both the microstructural and solidification modeling. The numerical solidification modeling was performed in a two-dimensional model by considering the nucleation and growth in eutectic ductile cast iron. The microstructural results reveal that the nodule size and count distribution along the cross sections are different in each location for both inserts. Finer graphite nodules appear in the thinner sections and close to the mold walls. The coarser nodules are distributed mostly in the last solidified location. The simulation result indicates that the finer nodules are related to a higher cooling rate and a lower degree of microsegregation, whereas the coarser nodules are related to a lower cooling rate and a higher degree of microsegregation. The solidification time interval and the last solidifying locations in the BWR and PWR are also different.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Microstructure and Properties of the Al-27Si/Cu/Al-50Si Joint Brazed by the Partial Transient Liquid Phase Bonding

Al-27Si and Al-50Si were brazed by using a thin Cu interlayer. The metallurgical bonding without obvious defects is achieved, and a wide brazing seam consisting of fine eutectic structures and coarse Si particles is formed in the Al-27Si/Cu/Al-50Si joint. The deposition of Si element in the liquid phases during solidification results in the formation of the larger Si particles and ultra-small Si particles in the brazing seam. The shear strength of the joint reaches 63 MPa.

36 MATERIALS SCIENCE↗

Formation Mechanism of Nanoscale Al{sub 3}Fe Phase in Al-Fe Alloy During Semisolid Forming Process

The formation mechanism of nanoscale Al{sub 3}Fe phase in Al-1Fe (wt pct) alloy during rheo-extrusion was investigated, and the mechanical property of the prepared alloy was also measured. The results show that the average length of Al{sub 3}Fe phase in Al-1Fe alloy prepared by rheo-extrusion is 300 nm, which is much more refined than the needlelike Al{sub 3}Fe phase in as-cast Al-1Fe alloy (50 μm). In rheo-extrusion, Al{sub 3}Fe phase formed by eutectic reaction is bonelike, but it could be continuously refined by the shear deformation in the wheel groove, in equal channel angular flow, and in expansion extrusion mold. The total equivalent strain of the shear deformation is higher than 4.82. The tensile strength and elongation of Al-1Fe alloy prepared by rheo-extrusion are 135 MPa and 30 pct, respectively. The tensile strength of Al-1Fe alloy prepared by rheo-extrusion is 58.8 pct higher than that of as-cast Al-1Fe alloy, and the elongation is 19 pct higher than that of as-cast Al-1Fe alloy. Compared with as-cast Al-1Fe alloy, the improvements of tensile strength and elongation caused by shear deformation in rheo-extrusion are higher than the reported improvements induced by rare earth modification.

36 MATERIALS SCIENCE↗

Yttria-Stabilized Zirconia Aided Electrochemical Investigation on Ferric Ions in Mixed Molten Calcium and Sodium Chlorides

Electrolytic reduction of dissolved iron oxide to metal iron in molten salts with an inert anode is an alternative short route for steelmaking without CO{sub 2} emissions. A novel and simple integrated yttria-stabilized zirconia (YSZ) cell was constructed from a YSZ tube with a closed end. The YSZ tube played multiple functions, including the container for the molten salts, the solid electrolyte membrane in the O{sup 2−}|YSZ|Pt|O{sub 2} (air) reference electrode (RE), and the solid electrolyte membrane between the working and counter electrodes (WE and CE). Electrochemical behavior of ferric ions (Fe{sup 3+}) that were formed by dissolution of 0.5 wt pct Fe{sub 2}O{sub 3} in the molten CaCl{sub 2}-NaCl eutectic mixture was investigated on a Pt WE at 1273 K by various electrochemical techniques including cyclic voltammetry, linear scan voltammetry, square wave voltammetry, chronopotentiometry, chronoamperometry, and potentiostatic electrolysis. Analysis of the mechanism of electrode reactions was further assisted by scanning electron microscopy, energy dispersive X-ray spectroscopy, and X-ray diffraction. Some electrochemical parameters were obtained, including the number of exchanged electrons and the diffusion coefficient of ferric ions in the mixed molten salts. The results from various electrochemical techniques are in good agreement with each other, and show that the electrochemical reduction of Fe{sup 3+} to Fe in the molten salt mixture could be a single three-electron transfer step and diffusion-controlled reaction that was also possibly reversible. This work may form the foundation for extraction of iron and alloys from molten salts and also provide a stable O{sup 2−}|YSZ|Pt|O{sub 2} (air) RE with wide applicability for investigation on electrochemical properties of other electroactive metal oxides in molten salts.

36 MATERIALS SCIENCE↗

Studies on Highly Fluxed Iron Ore Pellets Hardened at 1100 °C to 1200 °C

The behaviors of highly fluxed (basicity 2, 4, 6, and 8) iron ore pellets heat hardened in the temperature range 1100 °C to 1200 °C were examined and are reported here. The highly fluxed (basicity 8) pellets exhibited 103 kg/pellet crushing strength and 43.65 pct porosity when heat hardened at 1180 °C. During heat hardening, calcium di-ferrite and calcium ferrite phases were observed; however, when they were heated at 1200 °C, high crushing strength (458.63 kg/pellet) with low porosity (4.57 pct) were noted due to low melting eutectic formation. In this study, it was possible to prepare highly fluxed pellets without sticking at 1180 °C with good strength and porosity.

36 MATERIALS SCIENCE↗

Separation of Refined Silicon from Al-Si Alloys by Air Pressure Filtration

The separation of refined silicon from Al-Si alloys through a solvent refining process was studied. Purified silicon particles were separated by air pressure filtration using stainless steel sieves as the filtration media. After the efficient removal of impurities in the refining process, the effects of the mesh number (N), separation temperature (T), silicon content in the alloy (ω{sub (a)}), and pressure differential (p) on the separation efficiency were evaluated. At N = 80, T = 873 K (600 °C), ω{sub (a)} = 45 wt pct and p = 0.25 MPa, the recovery rate of refined silicon was 98.2 pct, and the residual aluminum in the separated silicon was less than 8 wt pct. The separation process was efficient when N = 60 to 150. It was advisable for the separation temperature to approach the eutectic temperature. Efficient filtration could be achieved when ω{sub (a)} = 35 to 55 wt pct. The filtration efficiency was improved with a higher pressure differential, and the separation was efficient at p ≥ 0.10 MPa. The results show that air pressure filtration is a promising method to separate refined silicon.

36 MATERIALS SCIENCE↗

Formation Mechanisms and Microstructure Characterization of Al/Al{sub 3}Ni In-situ Composite by Compound Casting

The Compound casting method was used to produce an Al/Ni bimetal composite. The mechanisms of formation of the reinforcing intermetallic phases were studied and the produced bimetal composite’s microstructure was then characterized. The results showed that the Al/Ni interface consisted of two intermetallic layers including Al{sub 3}Ni{sub 2} and Al{sub 3}Ni. It is suggested that the Al{sub 3}Ni reinforcing particles of the composite originated from two sources. (1) Some Al{sub 3}Ni particles detached from the Al{sub 3}Ni layer formed at the interface between the Ni core and the Al melt and dispersed in the liquid Al and (2) Al-Al{sub 3}Ni eutectic phase, which formed during the solidification process. The increase in the temperature led to the formation of more reinforcing particles and extended the depth of dispersion of the particles in the Al matrix.

36 MATERIALS SCIENCE↗

Effect of Holding Pressure on Microstructure and Mechanical Properties of A356 Aluminum Alloy

In this study, the effect of holding pressure on microstructure and mechanical properties of low-pressure die cast A356 aluminum alloy was investigated. The results showed that the application of high holding pressure (300 kPa) generated castings with denser structure and superior mechanical properties. By increasing the holding pressure up to 300 kPa, the size of secondary dendrite arm spacing greatly reduced by 22.7% at the cooling rate of 1°C/s and decreased by 12.8% at 10°C/s. The Feret’s diameter and aspect ratio of eutectic silicon particles decreased by 8.4 and 5.1% at the cooling rate of 1°C/s and decreased by 9.3 and 6.4% at 10°C/s, respectively. Meanwhile, the density of A356 aluminum alloy increased to 2.678 g/cm{sup 3} and the area fraction of porosity decreased to 0.035%. Thus, tensile properties of A356 aluminum alloy obtained at high holding pressure were enhanced, especially the ductility. All these could be associated with the better filling capability and faster cooling rate caused by high holding pressure. In the analytical range of experimental conditions, the correlation of mechanical properties with process parameters was established by statistical models to predict the ultimate tensile strength and elongation of low-pressure die cast A356 aluminum alloy.

36 MATERIALS SCIENCE↗

Comparative Analysis of the Microstructural Features of 28 wt.% Cr Cast Iron Fabricated by Pulsed Plasma Deposition and Conventional Casting

The effect of pulsed plasma deposition (by an electrothermal axial plasma accelerator) followed by post-heat treatment on the structure and microhardness of a 28 wt.% Cr white cast iron is analyzed and discussed with respect to the microstructure of the conventionally cast monolithic counterpart. The cast iron (as deposited on a 14 wt.% Cr cast iron substrate) had a microhardness of 630-750 HV{sub 0.05}; it had layered light contrast/dark contrast structure where dark contrast layers contain fine carbide network. Pulsed plasma deposition followed by heat treatment resulted in a substantial refinement of the microstructure: eutectic M{sub 7}C{sub 3} coarse acicular plates in the conventional cast iron were replaced by fine M{sub 7}C{sub 3}, M{sub 3}C{sub 2}, M{sub 3}C particles (Cr depleted in favor of Fe), while the initial carbide particle of 2-3 μm was reduced to 0.6 μm. Secondary dendrite arm spacing decreased from 15 to 1.3 μm, accordingly. The carbide volume fraction in the post-heat-treated coating remarkably increased with respect to the conventional counterpart resulting in a substantial increase in the coating hardness (1300-1750 HV{sub 0.05}). The heat-treated coating displayed higher resistance to three-body abrasion than the as-deposited coating and similar resistance with that of the conventionally cast iron.

36 MATERIALS SCIENCE↗

Ca Addition Effects on the Microstructure, Tensile and Corrosion Properties of Mg Matrix Alloy Containing 8 wt.% Mg{sub 2}Si

The microstructure, tensile properties and corrosion behavior of the Mg-8 wt.% Mg{sub 2}Si-x%Ca alloy have been studied by the use of optical microscopy, scanning electron microscopy equipped with energy-dispersive spectroscopy, x-ray diffraction, standard tensile testing, polarization test and electrochemical impedance spectroscopy (EIS) measurements. Microstructural studies indicated that Ca modifies both primary and eutectic Mg{sub 2}Si phase. It was found that the average size of primary Mg{sub 2}Si particles is about 60 μm, which is dropped by about 82% in the alloy containing 0.05 wt.% Ca. By the addition of different Ca contents, Ca-rich intermetallics (i.e., CaSi{sub 2} and CaMgSi) were formed. The modification mechanism of adding Ca during solidification was found to be due to the strong effect of CaMgSi phase as a heterogonous nucleation site, apart from CaSi{sub 2} which was reported before, for Mg{sub 2}Si intermetallics. Tensile testing results ascertained that Ca addition enhances both ultimate tensile strength (UTS) and elongation values. The optimum amount of Ca was found to be 0.1 wt.%, which improved UTS and elongation values from about 130 MPa and 2% to 165 MPa and 5.5%, whereas more Ca addition (i.e., 3 wt.%) reduced the tensile properties of the alloy to about 105 MPa and 1.8%, which can be due to the formation of CaMgSi intermetallics with deteriorating needle-like morphology. Polarization and EIS tests also showed that the Mg-3%Si-0.5%Ca alloy pronounces as the best anti-corrosion alloy. Nevertheless, further added Ca (up to 3 wt.%) deteriorated the corrosion resistance due to predominance of worse galvanic coupling effect stemmed from the presence of stronger CaMgSi cathode in comparison with Mg{sub 2}Si. With higher Ca additions, an adverse effect was seen on corrosion resistance of the Mg-3%Si alloy, as a result of forming a weak film on the alloy specimen surface.

36 MATERIALS SCIENCE↗

Formation of Al{sub 15}Mn{sub 3}Si{sub 2} Phase During Solidification of a Novel Al-12%Si-4%Cu-1.2%Mn Heat-Resistant Alloy and Its Thermal Stability

The formation of Al{sub 15}Mn{sub 3}Si{sub 2} phase in Al-12Si-4Cu-1.2Mn (wt.%) alloy during solidification was investigated by adopting CALPHAD method and microstructural observation by optical microscopy, SEM–EDS, TEM–EDS/SAD and XRD analysis; SEM fixed-point observation method was applied to evaluate its thermal stability. As-cast microstructural observation consistently demonstrates the solidification sequence of the studied alloy predicted by phase diagram calculation. Based on the phase diagram calculation, SEM–EDS, TEM–EDS/SAD and XRD analysis, as well as evidences on Al-Si-Mn-Fe compounds from the literature, the primary and eutectic Mn-rich phases with different morphologies in the studied alloy are identified to be Al{sub 15}Mn{sub 3}Si{sub 2} that has a body-centered cubic (BCC) structure with a lattice constant of a = 1.352 nm. SEM fixed-point observation and XRD analysis indicate that Al{sub 15}Mn{sub 3}Si{sub 2} phase has more excellent thermal stability at high temperature than that of CuAl{sub 2} phase and can serve as the major strengthening phase in heat-resistant aluminum alloy that has to face a high-temperature working environment. Results of tension test show that addition of Mn can improve the strength of Al-Si-Cu alloy, especially at elevated temperature.

36 MATERIALS SCIENCE↗

Relationships Between Solidification Parameters in A319 Aluminum Alloy

The design of high-performance materials depends on a comprehensive understanding of the alloy-specific relationships between solidification and properties. However, the inconsistent use of a particular solidification parameter for presenting materials characterization in the literature impedes inter-study comparability and the interpretation of findings. Therefore, there is a need for accurate expressions relating the solidification parameters for each alloy. In this study, A319 aluminum alloy castings were produced in a permanent mold with various preheating temperatures in order to control metal cooling. Analysis of the cooling curve for each casting enabled the identification of its liquidus, Al-Si eutectic, and solidus temperatures and times. These values led to the calculation of the primary solidification rate, total solidification rate, primary solidification time, and local solidification time for each casting, which were related to each other as well as to the average casting SDAS and material hardness. Expressions for each of their correlations have been presented with high coefficients of determination, which will aid in microstructural prediction and casting design.

36 MATERIALS SCIENCE↗

The Effects of Grain Refinement and Rare Earth Intermetallics on Mechanical Properties of As-Cast and Wrought Magnesium Alloys

The effects of rare earth intermetallics and grain refinement by alloying and hot extrusion on the mechanical properties of Mg-Gd-Al-Zn alloys have been studied to elucidate some useful ways to enhance the mechanical properties of magnesium alloys. It was revealed that aluminum as an alloying element is a much better grain refining agent compared with gadolinium, but the simultaneous presence of Al and Gd can refine the as-cast grain size more efficiently. The presence of fine and widely dispersed rare earth intermetallics was found to be favorable to achieve finer recrystallized grains during hot deformation by extrusion. The presence of coarse dendritic structure in the GZ61 alloy, grain boundary eutectic containing Mg{sub 17}Al{sub 12} phase in the AZ61 alloy, and rare earth intermetallics with unfavorable morphology in the Mg-4Gd-2Al-1Zn alloy was found to be detrimental to mechanical properties of the alloy in the as-cast condition. As a result, the microstructural refinement induced by hot extrusion process resulted in a significant enhancement in strength and ductility of the alloys. The presence of intermetallic compounds in the extruded Mg-4Gd-2Al-1Zn and Mg-2Gd-4Al-1Zn alloys deteriorated tensile properties, which was related to the fact that such intermetallic compounds act as stress risers and microvoid initiation sites.

36 MATERIALS SCIENCE↗

High Chromium Cast Irons: Destabilized-Subcritical Secondary Carbide Precipitation and Its Effect on Hardness and Wear Properties

This work evaluates the effect of a destabilization treatment combined with a subcritical diffusion (SCD) and a subsequent quenching (Q) steps on precipitation of secondary carbides and their influence on the wear properties of HCCI (16%Cr). The destabilization of the austenite at high temperature leads to a final microstructure composed of eutectic and secondary carbides, with an M{sub 7}C{sub 3} nature, embedded in a martensitic matrix. An improved wear resistance was observed in the SCD + Q samples in comparison with the Q one, which was attributed to the size of secondary carbides.

36 MATERIALS SCIENCE↗

The Effect of Boron and Zirconium on the Structure and Tensile Properties of the Cast Nickel-Based Superalloy ATI 718Plus

The effects of boron and zirconium on cast structure, hardness, and tensile properties of the nickel-based superalloy 718Plus were investigated. For this purpose, five alloys with different contents of boron and zirconium were cast via vacuum induction melting and then purified via vacuum arc remelting. Microstructural analysis by light-optical microscope and scanning electron microscope equipped with energy-dispersive x-ray spectroscopy and phase studies by x-ray diffraction analysis were performed. The results showed that boron and zirconium tend to significantly reduce dendritic arm spacing and increase the amount of Laves, Laves/gamma eutectic, and carbide phases. It was also found that boron led to the formation of B{sub 4}C and (Cr, Fe, Mo, Ni, Ti){sub 3}B{sub 2} phases and zirconium led to the formation of intermetallic phases and ZrC carbide. In the presence of boron and zirconium, the hardness and its difference between dendritic branches and inter-dendritic spaces increased by concentrating such phases as Laves in the inter-dendritic spaces. These elements had a negative effect on tensile properties of the alloy, including ductility and strength, mainly because of the increase in the Laves phase. It should be noted that the largest degradation of the tensile properties occurred in the alloys containing the maximum amount of zirconium.

36 MATERIALS SCIENCE↗

Mechanical Properties and Microstructural Evolution of Yb-Modified Al-20%Si Alloy

In the study, the mechanical properties and microstructural evolution of hypereutectic Al-20%Si-xYb alloys (x = 0, 0.1, 0.3, 0.5 and 0.7 wt.%) were studied. The as-prepared samples were characterized by scanning electron microscopy, optical microscope, x-ray diffraction (XRD) and electron probe microanalysis. The characterization results showed with the addition amount of Yb increasing to 0.5%, the eutectic Si structure was gradually modified from coarse needle-like/platelet-like structure into fine coral-like fibrous structure and the primary Si phases were gradually converted from coarse platelet-like/star-like/polygonal shape into fine blocky shape. In particular, according to the results of WDS and XRD analyses, the Yb-rich intermetallic phase in the Al-20%Si alloy is Al{sub 3}Yb. Tensile test was carried out to study the mechanical properties of Al-20%Si-x%Yb alloys, and results showed that the elongation and ultimate tensile strength increased by 73.6% and 64.5%, respectively.

36 MATERIALS SCIENCE↗