EBSD characterization of the growth mechanism of SiC synthesized via direct microwave heating

Well-crystallized 3C-silicon carbide (SiC) grains/nanowires have been synthesized rapidly and conveniently via direct microwave heating, simply using silicon dioxide powders and artificial graphite as raw materials. The comprehensive characterizations have been employed to investigate the micro-structure of the obtained 3C-SiC products. Results indicated that, different from the classic screw dislocation growth mechanism, the 3C-SiC grains/nanowires synthesized via high-energy vacuum microwave irradiation were achieved through the two-dimension nucleation and laminar growth mechanism. Especially, the electron backscattered diffraction (EBSD) was employed to characterize the crystal planes of the as-grown SiC products. The calculated Euler angles suggested that the fastest-growing crystal planes (211) were overlapped gradually. Through the formation of the (421) transformation plane, (211) finally evolved to (220) which existed as the side face of SiC grains. The most stable crystal planes (111) became the regular hexagonal planes in the end, which could be explained by the Bravais rule. The characterization results of EBSD provided important experimental information for the evolution of crystal planes. - Graphical abstract: The formation of 3C-SiC prepared via direct microwave heating follows the mechanism of two-dimension nucleation and laminar growth. - Highlights: • 3C−SiC grains/nanowires were obtained via direct microwave heating. • 3C−SiC followed the mechanism of two-dimension nucleation and laminar growth. • In-situ EBSD analysis provided the experimental evidences of the growth.

36 MATERIALS SCIENCE↗

Hot rolling of ZK60 magnesium sheet with isotropic tensile properties from tubing made by Shear Assisted Processing and Extrusion (ShAPE)

In order to evaluate the viability of ShAPE processed Mg alloys as a feedstock for fabricating lightweight sheet material, tubes consisting of ShAPE-extruded Mg alloy ZK60 were flattened into plates and hot rolled at 450 °C to reductions of 37%, 68%, and 93%. The mechanical properties and microstructure of the rolled material were characterized through tensile testing and electron backscattered diffraction (EBSD). ZK60 specimens rolled to 68% reduction had tensile properties similar to published properties of rolled ZK60 sheets fabricated using conventional processes, and exhibited negligible tensile anisotropy referenced to the rolling direction. Additional rolling from 68% to 93% reduced the ultimate tensile stress in the rolling direction from 341.74±5.96 MPa to 260.76±22.4MPa. The yield stress and elongation to failure of the material also decreased from 292.16±1.11 MPa to 256.93±18.4 MPa and 6.95±1.94% to 3.38±0.51%, respectively, but negligible little anisotropy was observed with respect to loading direction. EBSD mapping indicated that the as-extruded ZK60 had texture rotated away from the basal direction which developed into a strong basal texture over numerous hot rolling steps. This evolution in texture has been observed after rolling for hot-rolled ZK60 fabricated through conventional extrusion processes. The initial grain structure was found to have experienced noticeable twinning from flattening the tube into plate. After hot rolling, the grain structure became more equiaxed, but the average grain diameter did not change appreciably from 5.15 ± 3.39 µm in the ShAPE extruded material, to 5.27 ± 12.44 µm in the 93% hot rolled sheet. This response to hot rolling is similar to the response of ZK60 fabricated using other methods such as Equal Channel Angular Processing (ECAP). Therefore, this work demonstrates ShAPE has the potential as an alternative method to producing feedstock for Mg alloy sheets. Modifications to the experimental procedure which could lead to improvements in observed properties are briefly discussed.

36 MATERIALS SCIENCE↗

Workability Characteristics and Deformation Mechanisms of Die-Cast AM60 and AZ91 Magnesium Alloys: Correlation with Processing Maps

Thermo-mechanical deformation behavior of the die-cast AM60 and AZ91 alloys was assessed by performing uniaxial compression tests on Gleeble 3800 simulator under different temperatures and strain rate conditions. Low-temperature deformation behavior of both alloys was accessed at 25, 100, and 150 °C, at the strain rates of 0.1 and 1 s{sup −1}. Processing maps at a true strain of 0.5 were generated to study the intrinsic hot workability of AM60 and AZ91 alloys. Optimum processing windows were identified, and the evolution of microstructures and textures was correlated with the imposed deformation conditions. The processing map for the AM60 alloy exhibited three dynamic recrystallization (DRX) domains in the ranges: (1) 320-400 °C and 0.2-1.5 s{sup −1}, (1A) 300-325 °C and 0.1-0.2 s{sup −1}, and (2) 360-400 °C and 3-5 s{sup −1}. In Domain 1, DRX occurred predominantly by pyramidal slip and recovery mechanisms by cross-slip as confirmed by the randomized textures. Deformation in Domain 1A is by the combination of basal and prismatic slip. In Domain 2, dynamic recovery was a softening mechanism controlled by the climb. The processing map for AZ91 alloy exhibited two DRX domains in the ranges: (1) 260-310 °C and 0.1-0.5 s{sup −1} and (2) 325-350 °C and 0.8-3 s{sup −1}. The rate-controlling mechanism was climb by lattice self-diffusion in Domain 1 and by grain boundary self-diffusion in Domain 2. Both alloys exhibited flow instability at 200 and 250 °C, and therefore, they were unsuitable for processing at these temperatures.

36 MATERIALS SCIENCE↗

Synergies between H, He and radiation damage in dual and triple ion irradiation of candidate fusion blanket materials

Three ferritic/martensitic alloys were studied to understand the synergistic effect between single ion beam (Fe 2+ ), dual ion beam (Fe 2+ +He 2+ and Fe 2+ +H + ), and triple ion beam (Fe 2+ +He 2+ +H + ) irradiations on cavity evolution. A commercial alloy, F82H, a castable nanostructured alloy, CNA3, and a high purity model alloy, Fe8Cr2W, were irradiated at 400°C to 600°C to a damage level of 50 dpa at a damage rate of 1 × 10 –3 dpa/s with He and H injection rates of 10 and 40 appm/dpa, respectively. Post-irradiation characterization via bright field transmission electron microscopy and high-angle annular dark-field scanning transmission electron microscopy was performed on all irradiated conditions to characterize the cavity size distribution and determine the effects of H/He injection on cavity microstructure. In all three alloys, hydrogen co-injection with helium resulted in an increased cavity number density and maximum cavity size, producing an increase in swelling over that from helium injection alone. Swelling in F82H appears to peak between 450°C and 500°C. At 600°C, swelling was minimal and cavities of high density and small size were confined to grain boundaries and dislocations while at 400°C, swelling is also low with a nearly homogeneous, high density, distribution of very small cavities throughout. Swelling was least in the commercial alloy F82H due to the high sink strength. The CNA3 alloy underwent dissolution of precipitates that lowered the sink strength and resulted in higher swelling than F82H, but less than the model alloy. Electron energy loss spectroscopy (EELS) elemental mapping revealed hydrogen forming a halo-like structure about the periphery of the cavities and helium residing within the cavities themselves. Finally, this observation suggests that hydrogen reduces the surface energy of helium-filled cavities which results in both increased cavity number density and cavity size in triple beam irradiation over dual beam irradiation.

36 MATERIALS SCIENCE↗

Transmission electron microscopy investigation of phase transformation and fuel constituent redistribution in neutron irradiated U-10wt.%Zr fuel

Uranium-10wt.%zirconium (U-10wt.%Zr) is a primary candidate for fast reactor nuclear fuels. However, there is a lack of data characterizing neutron irradiated crystallographic phases and chemistry. In the current study, the microstructural evolution of a U-10wt.%Zr fuel neutron irradiated to a burnup of 5.7 at.% was investigated by scanning transmission electron microscopy, energy dispersive spectroscopy, and selected area electron diffraction to determine the major phases, alterations in microstructure, and variations in local chemical composition at different localities of a fuel cross-section. The current study revealed that the irradiated U-10wt.%Zr fuel was comprised of various major phases, including a-U, ß-U, and d-UZr2, as well as amorphous and crystalline solid fission product (FP) precipitates within different regions of the fuel cross-section. Regions A and A/B in the center of the fuel were comprised of U-rich, U-intermediate, and U-lean localities with a-U and d-UZr 2 composing the major phases. Regions B and C in the intermediate and peripheral fuel localities, respectively, were comprised of a-U grains, U-rich (ß-U) grains with Zr-rich precipitates, U-intermediate grains (d-UZr2), and solid FP precipitates. The major phases identified were associated with the nanoscopic chemical concentrations, the phase diagram, and the as-characterized specimen temperature, with the exception of the non-equilibrium ß-U phase identified in region B. The U-lean localities in regions A, A/B, B, and C were Zr-enriched pathways along subgrain/grain boundaries. This phenomenon suggests that Zr is susceptible to radiation-induced segregation in U-Zr fuels and indicates a new mechanism for constituent redistribution.

36 MATERIALS SCIENCE↗

Effect of Final Cooling Temperature on Microstructure and Mechanical Properties of a Cr-Ni-Mo-V Bainite Steel

The microstructural evolution and mechanical properties of a low-carbon high-strength bainitic steel under different final cooling temperatures were studied. The microstructures of the experimental steel at different final cooling temperatures were composed of acicular ferrite and granular bainite. A decrease in final cooling temperature resulted in an increase in volume fraction of granular bainite and a decrease in volume fraction of acicular ferrite. The specimen with the lowest final cooling temperature (459 °C) exhibited the highest yield strength, tensile strength, and yield ratio, and a lower total elongation than the specimens with the highest final cooling temperatures (501 and 535 °C) because of the higher volume fraction of granular bainite and finer bainitic ferrite lath. The specimen with the lowest final cooling temperature had a lower absorbed energy than that of the highest final cooling temperature, because the strip-like martensite–austenite (M-A) constituents that existed between the bainitic ferrite or in prior austenite grain boundaries reduced its toughness. At an intermediate final cooling temperature of 501 °C, the experimental steel exhibited excellent mechanical properties with a yield strength, tensile strength, and absorbed energy of 825 MPa, 1232 MPa, and 102 J, respectively.

36 MATERIALS SCIENCE↗

Investigation of the shear response and geometrically necessary dislocation densities in shear localization in high-purity titanium

The influence of microstructural anisotropy on shear response of high-purity titanium was studied using the compact forced-simple-shear specimen (CFSS) loaded under quasi-static loading conditions. Post-mortem characterization reveals significant difference in shear response of different directions in the same material due to material crystallographic texture anisotropy. Shear bands are narrower in specimens in which the shear zone is aligned along the direction with a strong {0001} basal texture. Twinning was identified as an active mechanism to accommodate strains in the shear region in both orientations. This paper confirms the applicability of the CFSS design for the investigation of differences in the shear response of materials as a function of process-induced crystallographic texture. A detailed, systematic approach to quantifying shear band evolution by evaluating geometrically necessary dislocations (GND) associated with crystallographic anisotropy is presented. Finally, the results show that: i) line average GND density profiles, for Ti samples that possess a uniform equiaxed-grain structure, but with strong crystallographic anisotropy, exhibit significant differences in GND density close to the shear band center; ii) GND profiles decrease steadily away from the shear band as the plastic strain diminishes, in agreement with Ashby's theory of work hardening, where the higher GND density in the through-thickness (TT) orientation is a result of restricted < a > type slip in the shear band compared with in-plane (IP) samples; iii) the anisotropy in deformation response is derived from initial crystallographic texture of the materials, where GND density of < a > GNDs are higher adjacent to the shear band in the through-thickness sample oriented away from easy slip, but the density of < c+a > type GNDs are very similar in these two samples; and iv) the increase in grain average GND density was determined to have strong correlation to an increase in the Euler Φ angle of the grain average orientation, indicating an increased misorientation angle evolution.

36 MATERIALS SCIENCE↗

Microstructural Evolution During a Solid State Tube Pinch Weld of Type 304l Stainless Steel

Microstructure development is examined for a specialized spot weld that is used as a solid-state closure process for austenitic stainless steel tubing, referred to as pinch welding. In order to elucidate the microstructural evolution of the weld, a series of test welds were made at nominal conditions using tubing and production like components. These pinch welds normally terminate after twelve cycles of a 60 Hz AC weld process. In this study, production tubes were welded from one to twelve cycles and the microstructure and weld variables after each individual weld cycle number were characterized using radiography and optical metallography. Two electrochemical etchants were used to highlight different microstructural features. The study revealed that: (1) this type pinch weld is largely complete after about six cycles of 60 Hz AC current, half the weld time utilized; (2) the resistance, deformation, and closure length approach “steady-state” conditions after six cycles; and (3) both oxalic and nitric acid electrolytic etchants are useful for highlighting specific microstructural attributes of type 304 L stainless steel. Finally, two distinct microstructural regions can be identified for these welds: the edge of the weld, which is driven by concentrated deformation, recrystallization, and grain growth, and the center region, which is more typical of forge welding and micro-asperity breakdown followed by diffusion and grain-growth.

36 MATERIALS SCIENCE↗

Phase transformations, microstructural refinement and defect evolution mechanisms in Al-Si alloys under non-hydrostatic diamond anvil cell compression

Non-hydrostatic compression of materials using a diamond anvil cell (DAC) can transform equilibrium microstructure of an alloy to novel, potentially metastable states. In this study, in situ synchrotron X-ray diffraction (XRD) during compression up to 24 GPa and subsequent ex situ, high resolution analytical electron microscopy (AEM) after decompression of an Al-Si alloy provided insight into the crystallographic changes during the compression as well as microstructural refinement, and defect structures caused by such a high pressure compression-decompression process. Pressure resolved in-situ synchrotron XRD was used to detail the phase transformation pathway of the eutectic Si phase in Al-Si alloy, from Si-I → Si-XI → Si-V during compression, and a final transformation predominantly to Si-III after decompression. Using scanning and transmission electron microscopy (S/TEM), site specific analysis of the alloy immediately underneath the anvil contact surface demonstrated a highly complex microstructure. A narrow region of thick amorphous Al oxide interspersed with nanocrystalline grains was found at the top surface. Underneath this Al oxide, while the majority the eutectic Si was transformed into highly-deformed, polycrystalline (PC) Si-III, a complex intermediate layer was discovered at the interface between Al and Si, comprised of a small fraction of Al nanocrystals and a majority of nanocrystalline Si-I. This combination of pressure resolved in-situ synchrotron XRD coupled with subsequent high resolution, electron microscopy resolved the phase transformation as well as non-equilibrium microstructures in a metallic alloy induced by a non-hydrostatic high pressure compression followed by decompression.

36 MATERIALS SCIENCE↗

Correlation of the energy product with evolution of the nanostructure in Y,Dy,Nd-(Fe,Co)-B magnetic alloy

The devitrification behavior of nanocrystalline MRE{sub 2}(Fe,Co){sub 14}B+ZrC (MRE = Nd+Y+Dy) was studied using differential scanning calorimetry (DSC), synchrotron high temperature x-ray diffraction, and analytical transmission electron microscopy (TEM) techniques. Alloy ribbons were melt spun at 25 m/s to obtain an amorphous structure. Optimum hard magnetic properties (B{sub r} = 7.2 kG, H{sub c} = 12.7 kOe and (BH){sub max} = 10.8 MG Oe) were obtained in ribbons annealed at 750 C for 15 min. A reduced annealing temperature of 638 C and holding time from 0 to 11 min were chosen based on DSC analysis. Large changes in both microstructure and hard magnetic properties were found in a narrow window of annealing time, 4.5-6 min, resulting in a dramatic increase in energy product, remanence and coercivity: 0.96 MG Oe, 5.2 kG, 2.7 kOe to 5.7 MG Oe, 7.2 kG, 8.5 kOe for (BH){sub max}, B{sub r} and H{sub c}, respectively. Energy dispersive x-ray spectroscopy and energy filtered TEM analyses indicate that Zr- and C-rich particles ({approx} 5 nm) and thin grain boundary layers (1-2 nm thick) are formed surrounding 2-14-1 hard phase grains when the annealing time is over 6 min. Further annealing resulted in a more distinct hard phase surrounded by a nonmagnetic grain boundary phase {approx} 1 nm in thickness. The thin grain boundary layer phase starts to disappear with annealing time over 11 min. The partitioning behavior of various elements at different annealing conditions appears to be associated with significant changes in magnetic properties, leading to an improved optimum microstructure.

36 MATERIALS SCIENCE↗

Simulation Kinetics of Austenitic Phase Transformation in Ti+Nb Stabilized IF and Microalloyed Steels

In the present study, the influence of cooling rates (low to ultrafast) on diffusion controlled and displacive transformation of Ti-Nb IF and microalloyed steels has been thoroughly investigated. Mechanisms of nucleation and formation of non-equiaxed ferrite morphologies (i.e., acicular ferrite and bainitic ferrite) have been analyzed in details. The continuous cooling transformation behavior has been studied in a thermomechanical simulator (Gleeble 3800) using the cooling rates of 1-150 °C/s. On the basis of the dilatometric analysis of each cooling rate, continuous cooling transformation (CCT) diagrams have been constructed for both the steels to correlate the microstructural features at each cooling rate in different critical zones. In the case of the IF steel, massive ferrite grains along with granular bainite structures have been developed at cooling rates > 120 °C/s. On the other hand, a mixture of lath bainitic and lath martensite structures has been formed at a cooling rate of ~ 80 °C/s in the microalloyed steel. A strong dependence of the cooling rates and C content on the microstructures and mechanical properties has been established. The steel samples that were fast cooled to a mixture of bainite ferrite and martensite showed a significant improvement of impact toughness and hardness (157 J, for IF steel and 174 J for microalloyed steel) as compared to that of the as-received specimens (133 J for IF steel and 116 J for microalloyed steel). Thus, it can be concluded that the hardness and impact toughness properties are correlated well with the microstructural constituents as indicated by the CCT diagram. Transformation mechanisms and kinetics of austenitic transformation to different phase morphologies at various cooling rates have been discussed in details to correlate microstructural evolution and mechanical properties.

36 MATERIALS SCIENCE↗

Effect of stored strain energy heterogeneity on microstructure evolution of 90% cold rolled AISI 304L stainless steel during interrupted annealing treatment

Highlights: • Study of usefulness of stored strain energy distribution map of the material for variable temperature range. • Advantage of using stored strain energy distribution map • Variation observed in stored energy between isothermal annealing treatment and interrupted annealing treatment. - Abstract: This research work is an attempt to understand the effect of stored strain energy heterogeneity over macro-scale, induced during interrupted annealing treatment, on the micro structural evolution in a heavily cold rolled AISI 304L austenitic stainless steel. The cold rolled AISI 304L stainless steel (SS) samples were subjected to different annealing treatments. The microstructures obtained after each annealing treatment were characterized using optical and electron microscopy techniques. Further, an attempt was made to estimate the stored strain energy by a novel approach of micro hardness measurement both over small scale (area 3600 μm{sup 2}) and large scale (area ~0.25 mm{sup 2}). The stored strain energy was determined using hardness values. Using these data, spatial stored strain energy distribution contour maps were created. They were, in turn, used to characterize the local softening behavior both at micro and macro-scale levels after each interrupted annealing treatment. The results showed that, interrupted annealing treatment induces increased stored strain energy heterogeneity after each annealing interruptions. Also, it was possible to determine recrystallization kinetics of the material using stored strain energy map, which helps in designing annealing cycles for achieving ultrafine grained microstructure.

36 MATERIALS SCIENCE↗

In Situ X-ray Measurements to Follow the Crystallization of BaTiO 3 Thin Films during RF-Magnetron Sputter Deposition

Here, we report on adding an important dimension to the fundamental understanding of the evolution of the thin film micro structure evolution. Thin films have gained broad attention in their applications for electro-optical devices, solar-cell technology, as well storage devices. Deep insights into fundamental functionalities can be realized via studying crystallization microstructure and formation processes of polycrystalline or epitaxial thin films. Besides the fundamental aspects, it is industrially important to minimize cost which intrinsically requires lower energy consumption at increasing performance which requires new approaches to thin film growth in general. Here, we present a state of the art sputtering technique that allows for time-resolved in situ studies of such thin film growth with a special focus on the crystallization via small angle scattering and X-ray diffraction. Focusing on the crystallization of the example material of BaTiO 3 , we demonstrate how a prototypical thin film forms and how detailed all phases of the structural evolution can be identified. The technique is shaped to enable a versatile approach for understanding and ultimately controlling a broad variety of growth processes, and more over it demonstrate how to in situ investigate the influence of single high temperature sputtering parameters on the film quality. It is shown that the whole evolution from nucleation, diffusion adsorption and grain growth to the crystallization can be observed during all stages of thin film growth as well as quantitatively as qualitatively. This can be used to optimize thin-film quality, efficiency and performance.

36 MATERIALS SCIENCE↗

High-temperature deformation behavior of the extruded Ti-22Al-25Nb alloy fabricated by powder metallurgy

Highlights: • The high-temperature deformation behavior of the extruded Ti-22Al-25Nb alloy was analyzed. • A true strain-compensated Arrhenius-type constitutive model was established. • The processing maps of true strains 0.2, 0.4, and 0.6 were constructed to optimize the processing parameters. • Microstructural evolution and deformation mechanism in different conditions were explained. - Abstract: The hot-deformation behavior of the extruded Ti-22Al-25Nb alloy was investigated by compression testing in the 1213–1333 K temperature range, under a 0.001–1.0 s{sup −1} strain-rate range. The activation energy, Q, at a deformation strain of 0.3, was calculated to be 574.80 kJ mol{sup −1}. A strain-compensated Arrhenius-type constitutive model was established for this alloy, with an average absolute relative error (AARE) and correlation coefficient (R) of 7.64% and 0.994, respectively. Based on the dynamic materials model (DMM), processing maps were developed by combining the power dissipation and instability maps. An instability region was identified in the 1213–1278 K temperature range and 0.022–1.0 s{sup −1} strain-rate range. The microstructure of specimens deformed under different conditions were analyzed to characterize the corresponding deformation mechanisms. The main softening mechanisms in the stability regions were dynamic recrystallization (DRX) and dynamic globularization. The grain size of the specimen deformed at 1313 K/0.001 s{sup −1} was approximately 15.2 μm.

36 MATERIALS SCIENCE↗

Effect of powder layer thickness on the microstructural development of additively manufactured SS316

By Increasing the powder layer thickness we could increase material deposition rates and reduce build times during laser powder bed fusion (LPBF). However, increasing the powder layer thickness could also negatively affect the local melting and subsequent microstructure of the printed material. This study systematically investigated, for the first time, the defect evolution and microstructural changes of LPBF stainless steel 316 (SS316) processed by using various powder layer thicknesses of 40, 80, and 120 μm while also varying the laser dwell time for the pulsed laser. Through image analysis, the pore density was found to increase with increasing powder layer thickness, particularly when the dwell time was too high or too low. The maximum achievable density (>99%) was found over a wide processing window when using the smallest powder layer thickness of 40 μm between dwell times of 60 and 100 μs. Increasing the powder layer thicknesses to 80 and 120 μm resulted in maximum densities of 98.7 and 96.8%, respectively, but the window for acceptable laser dwell times that could achieve these densities narrowed considerably. A microstructural analysis of the melt pools was performed to measure the melt pool depths and widths, both of which increased with increasing dwell time. However, increasing the powder layer thickness did not affect the melt pool depth and only minorly affected the width. A sub-grain cellular structure distinguished the melt pool boundaries. The cell size increased with increasing dwell time and decreasing powder layer thickness. Moreover, the cell size was used to calculate a cooling rate that had a magnitude of 10 7 K/s and increased with increasing powder layer thickness.

36 MATERIALS SCIENCE↗

Microstructural evolution and mechanical properties of maraging steel produced by wire + arc additive manufacture process

Highlights: • Wire + arc additive manufacture (WAAM) was applied to produce maraging steel structures. • Microstructure evolution of WAAM alloy was characterized and correlated with the layer-by-layer building manner. • Mechanical properties of WAAM alloy were tested and correlated with the aging response of WAAM microstructure. • Retained austenite content was measured and correlated with the tensile strength loss. - Abstract: Wire + arc additive manufacture is developed for producing large-scale metallic components. In this paper, maraging steel parts were produced, and the microstructure and mechanical properties were investigated. The microhardness and tensile strength of the as deposited alloy reduced from the bottom to the top due to the transient thermal cycling, which resulted in partial aging and non-uniform formation of intermetallic compounds along the building direction. Solutionizing, followed by 3 h aging, significantly reduced the microstructural heterogeneity and increased the mechanical properties by 24.7% through the formation of large amounts of finely distributed precipitates. The as deposited alloy possessed superior strength to the wrought alloy in solutionized condition but inferior to the later in aged condition, which was attributed to the less pronounced aging response of the low-angle columnar grains characterized microstructure and the presence of retained and reverted austenite.

36 MATERIALS SCIENCE↗

Controlling Cu–Sn mixing so as to enable higher critical current densities in RRP ® Nb 3 Sn wires

Dipole magnets for the proposed Future Circular Collider (FCC) demand specifications significantly beyond the limits of all existing Nb 3 Sn wires, in particular a critical current density (J c ) of more than 1500 A mm -2 at 16 T and 4.2 K with an effective filament diameter (D eff ) of less than 20 μm. The restacked-rod-process (RRP ® ) is the technology closest to meeting these demands, with a J c (16 T) of up to 1400 A mm -2 , residual resistivity ratio > 100, for a sub-element size D s of 58 μm (which in RRP ® wires is essentially the same as D eff ). An important present limitation of RRP ® is that reducing the sub-element size degrades J c to as low as 900 A mm -2 at 16 T for D s = 35 μm. To gain an understanding of the sources of this J c degradation, we have made a detailed study of the phase evolution during the Cu–Sn 'mixing' stages of the wire heat treatment that occur prior to Nb 3 Sn formation. Using extensive microstructural quantification, we have identified in this paper the critical role that the Sn–Nb–Cu ternary phase (Nausite) can play. The Nausite forms as a well-defined ring between the Sn source and the Cu/Nb filament pack, and acts as an osmotic membrane in the 300 °C–400 °C range—greatly inhibiting Sn diffusion into the Cu/Nb filament pack while supporting a strong Cu counter-diffusion from the filament pack into the Sn core. This converts the Sn core into a mixture of the low melting point (408 °C) η phase (Cu 6 Sn 5 ) and the more desirable ε phase (Cu 3 Sn), which decomposes at 676 °C. After the mixing stages, when heated above 408 °C towards the Nb 3 Sn reaction, any residual η liquefies to form additional irregular Nausite on the inside of the membrane. All Nausite decomposes into NbSn 2 on further heating, and ultimately transforms into coarse-grain (and often disconnected) Nb 3 Sn which has little contribution to current transport. Understanding this critical Nausite reaction pathway has allowed us to simplify the mixing heat treatment to only one stage at 350 °C for 400 h which minimizes Nausite formation while encouraging the formation of the higher melting point ε phase through better Cu–Sn mixing. Finally, at a D s of 41 μm, the Nausite control heat treatment increases the J c at 16 T by 36%, reaching 1300 A mm -2 (i.e. 2980 A mm -2 at 12 T), and moving RRP ® closer to the FCC targets.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Spatially resolved texture and microstructure evolution of additively manufactured and gas gun deformed 304L stainless steel investigated by neutron diffraction and electron backscatter diffraction

In this study, we report the characterization of a 304L stainless steel cylindrical projectile produced by additive manufacturing. The projectile was compressively deformed using a Taylor Anvil Gas Gun, leading to a huge strain gradient along the axis of the deformed cylinder. Spatially resolved neutron diffraction measurements on the HIgh Pressure Preferred Orientation time-of-flight diffractometer (HIPPO) and Spectrometer for Materials Research at Temperature and Stress diffractometer (SMARTS) beamlines at the Los Alamos Neutron Science CEnter (LANSCE) with Rietveld and single-peak analysis were used to quantitatively evaluate the volume fractions of the α, γ, and ε phases as well as residual strain and texture. The texture of the γ phase is consistent with uniaxial compression, while the α texture can be explained by the Kurdjumov–Sachs relationship from the γ texture after deformation. This indicates that the material first deformed in the γ phase and subsequently transformed at larger strains. The ε phase was only found in volumes close to the undeformed material with a texture connected to the γ texture by the Shoji–Nishiyama orientation relationship. This allows us to conclude that the ε phase occurs as an intermediate phase at lower strain, and is superseded by the α phase when strain increases further. Furthe, we found a proportionality between the root-mean-squared microstrain of the γ phase, dominated by the dislocation density, with the α volume fraction, consistent with strain-induced martensite α formation. In conclusion, knowledge of the sample volume with the ε phase from the neutron diffraction analysis allowed us to identify the ε phase by electron back scatter diffraction analysis, complementing the neutron diffraction analysis with characterization on the grain level.

304L stainless steel↗