Search NASA⌕ Search

SEARCH · Search NASA

Results for “INTERMETALLIC COMPOUNDS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 883 records · Page 49

Structure and plasticity in hot deformed FeAl intermetallic phase base alloy

This paper constitutes part of research conducted on the possibility of forming alloys based on intermetallic phases from the Fe-Al system via thermoplastic processing. Insufficient plasticity, which is an inhibitor of further development of these intermetallics as construction materials, makes the range of their applications limited. In the paper, an analysis is conducted of the influence of deformation parameters on the structure of an alloy of Fe-Al with the B2 type structure. Axi-symmetric compression tests were carried out at temperatures ranging from 600 deg. C to 1200 deg. C and at a deformation rate from 0.001 s{sup 1} to 10 s{sup -1}. Structural examination was carried out using light microscopy and transmission electron microscopy. A quantitative evaluation of the structure was made with the use of 'Met-Ilo'. The results obtained will be used for the development of mathematical models determining the influence of deformation parameters on the alloy structure.

36 MATERIALS SCIENCE↗

Microstructural developments in TLP bonds using thin interlayers based on Ni-B coatings

Oxide dispersion strengthened alloy MA 758 was transient liquid phase (TLP) bonded using thin interlayers based on Ni-B electrodeposited coatings and the microstructural developments across the joint region were studied. The bonding surfaces were electrodeposited with a coat thickness of 2-9 {mu}m and microstructural features were characterized by scanning electron microscopy and energy dispersive X-ray spectroscopy. The homogeneity of the joint was assessed performing micro-hardness test. The results showed that the coating thickness as well as the amount of melting point depressants (boron) in the coatings had a significant effect on the microstructural developments within the joint region. TLP bonds made using a 2 {mu}m thick coating interlayer produced a joint with no visible precipitate formation and parent metal dissolution, and the absence of precipitates was attributed to the lower volume concentration of boron in the 2 {mu}m thick coating interlayer.

36 MATERIALS SCIENCE↗

Influence of constitutional liquation on corrosion behaviour of aluminium alloy 2017A

The purpose of this work was to investigate microstructural aspects of constitutional liquation in the aluminium alloy 2017A and to determine its effect on corrosion behaviour of this alloy. Non-equilibrium melting of the alloy in the naturally aged condition was provoked by rapid heating above the eutectic temperature and immediate cooling in air. Corrosion testing was performed by exposure to a marine onshore atmosphere. The microstructure examinations were carried out using light microscopy, scanning electron microscopy, X-ray energy dispersion and X-ray diffraction analysis. It was found that, due to rapid heating rate, coarse {theta} (Al{sub 2}Cu) particles were melted by constitutional liquation and this way introduced strong susceptibility of 2017A alloy to intergranular corrosion.

36 MATERIALS SCIENCE↗

Determination of the composition of Co-Pt thin films with quantitative electron-probe microanalysis

Quantitative electron-probe microanalysis (EPMA) with energy-dispersive (EDS) and wavelength-dispersive (WDS) X-ray spectroscopy was performed to determine the chemical composition of Co-Pt ferromagnetic thin films. The conventional 'bulk' EPMA approach was applied and tested in detail by using several analytical set-ups with different combinations of Co and Pt spectral lines, beam energies and quantitative matrix-correction programs. The analyses with dedicated, thin-film EPMA programs were also made for comparison. The results were critically examined in order to assess their reliability and accuracy. The commonly used EDS analyses showed significant scatter between the set-ups and generally suffered from a poor analytical sensitivity. In contrast, the quantitative WDS analyses were fully consistent and practically independent of the analytical set-up. With the optimized WDS a high analytical precision, an improved sensitivity and an ultimate quantitative accuracy of better than 1% relative were achieved. The results confirmed that by using WDS microanalysis at low beam energies and by measuring the low-energy Co-L{alpha} and Pt-M{alpha} X-rays we were able to obtain the most accurate and reliable, quantitative, compositional analyses of Co-Pt thin films with thicknesses down to {approx} 100 nm.

36 MATERIALS SCIENCE↗

Effect of rapid solidification on the microstructure and mechanical properties of hot-pressed Al-20Si-5Fe alloys

The aim of this work is to study the effect of cooling rate and subsequent hot consolidation on the microstructural features and mechanical strength of Al-20Si-5Fe-2X (X = Cu, Ni and Cr) alloys. Powder and ribbons were produced by gas atomization and melt spinning processes at two different cooling rates of 1 x 10{sup 5} K/s and 5 x 10{sup 7} K/s. The microstructure of the products was examined using optical microscopy, scanning electron microscopy, transmission electron microscopy, and X-ray diffraction. The particles were consolidated by hot pressing at 400 deg. C/250 MPa/1 h under a high purity argon atmosphere and the microstructure, hardness and compressive strength of the compacts were evaluated. Results showed a profound effect of the cooling rate, consolidation stage, and transition metals on the microstructure and mechanical strength of Al-20Si-5Fe alloys. While microstructural refining was obtained at both cooling rates, the microstructure of the atomized powder exhibited the formation of fine primary silicon ({approx} 1 {mu}m), eutectic Al-Si phase with eutectic spacing of {approx} 300 nm, and {delta}-iron intermetallic. Supersaturated Al matrix containing 5-7 at.% silicon and nanometric Si precipitates (20-40 nm) were determined in the microstructure of the melt-spun ribbons. The hot consolidation resulted in coarsening of Si particles in the atomized particles, and precipitation of Si and Fe-containing intermetallics from the supersaturated Al matrix in the ribbons. The consolidated ribbons exhibited higher mechanical strength compared to the atomized powders, particularly at elevated temperatures. The positive influence of the transition metals on the thermal stability of the Al-20Si-5Fe alloy was noticed, particularly in the Ni-containing alloy.

36 MATERIALS SCIENCE↗

Morphological characteristic of the conventional and melt-spun Al-10Ni-5.6Cu (in wt.%) alloy

The Al-10Ni-5.6Cu alloy was prepared by conventional casting and further processed melt-spinning technique. The resulting conventional cast and melt-spun ribbons were characterized using X-ray diffraction, optical microscopy, scanning electron microscopy together with energy dispersive spectroscopy, differential scanning calorimetry and microhardness techniques. The X-ray diffraction analysis indicated that ingot samples were {alpha}-Al, intermetallic Al{sub 3}Ni and Al{sub 2}Cu phases. The optical microscopy and scanning electron microscopy results show that the microstructures of rapidly solidified ribbons are clearly different from their ingot alloy. Al-10Ni-5.6Cu ribbons reveal a very fine cellular structure with intermetallic Al{sub 3}Ni particles. Moreover, at high solidification rates the melt-spun ribbons have a polygonal structure dispersed in a supersaturated aluminum matrix. The differential scanning calorimetry measurements revealed that exothermic reaction was between 290 deg. C and 440 deg. C which are more pronounced in the ternary Al-10Ni-5.6Cu alloy.

36 MATERIALS SCIENCE↗

Solidification structure of C{sub 2.08}Cr{sub 25.43}Si{sub 1.19}Mn{sub 0.43}Fe{sub 70.87} powders fabricated by high pressure gas atomization

Powders of hypoeutectic high chromium white cast iron (C{sub 2.08}Cr{sub 25.43}Si{sub 1.19}Mn{sub 0.43}Fe{sub 70.87}) were produced by high pressure gas atomization. The microstructure of the powders was characterized using light microscopy, scanning electron microscopy and X-ray diffraction. The results showed that the as-atomized powders were mainly composed of austenite and M{sub 7}C{sub 3} (M = Fe, Cr) type carbide, and became ferrite and carbide after annealing. With the decrease of the powder diameter, the number of austenite grains, primary dendrite length and second dendrite arm spacing were decreased. The relationship between cooling rate and microstructure was also determined.

36 MATERIALS SCIENCE↗

3D characterization of intermetallics in a high pressure die cast Mg alloy using focused ion beam tomography

The degree of spatial interconnection of the Mg{sub 17}Al{sub 12} ({beta}-phase) intermetallic in a Mg-9Al-1Zn alloy was assessed through serial sectioning at the centre and near a corner in a casting cross-section. The three dimensional reconstructions showed that the intermetallics were profusely interconnected forming a scaffold-like network over the entire cross-section, but especially near the casting surface. The scale and degree of the interconnection appeared determined by the local concentration of large dendritic grains injected from the shot sleeve. The volume fractions of intermetallics obtained through the 3D reconstruction indicated a higher content of {beta}-phase at the corner regions in comparison with the core. The volume fractions obtained by FIB were consistent with theoretical and experimental values obtained using other techniques.

36 MATERIALS SCIENCE↗

Deformation-induced {alpha}{sub 2} {yields} {gamma} phase transformation in TiAl alloys

Deformation-induced {alpha}{sub 2} {yields} {gamma} phase transformation in high Nb containing TiAl alloys was investigated using high-resolution transmission electron microscopy (HREM) and energy dispersive X-ray spectroscopy (EDS). The dislocations appearing at the tip of deformation-induced {gamma} plate (DI-{gamma}) and the stacking sequence change of the {alpha}{sub 2} matrix were two key evidences for determining the occurrence of the deformation-induced {alpha}{sub 2} {yields} {gamma} phase transformation. Compositional analysis revealed that the product phase of the room-temperature transformation was not standard {gamma} phase; on the contrary, the product phase of the high-temperature transformation was standard {gamma} phase.

36 MATERIALS SCIENCE↗

A study of the composition and microstructure of nanodispersed Cu-Ni alloys obtained by different routes from copper and nickel oxides

Mixtures of CuO and NiO were prepared by two different techniques, and then the oxides were reduced with H{sub 2}. Method A involved the preparation of mechanical mixtures of CuO and NiO using different milling and pelletizing processes. Method B involved the chemical synthesis of the mixture of CuO and NiO. The route used to prepare the copper and nickel oxide mixture was found to have great influence on the characteristics of bimetallic Cu-Ni particles obtained. Observations performed using the X-ray diffraction (XRD) technique showed that although both methods led to the Cu-Ni solid solution, the diffractogram of the alloy obtained with method A revealed the presence of NiO together with the alloy. The temperature-programmed reduction (TPR) experiments indicated that the alloy is formed at lower temperatures when using method B. The scanning electron microscopy (SEM) studies revealed notable differences in the morphology and size distribution of the bimetallic particles synthesized by different routes. The results of the electron probe microanalysis (EPMA) studies evidenced the existence of a small amount of oxygen in both cases and demonstrated that the alloy synthesized using method B presented a homogeneous composition with a Cu-Ni ratio close to 1:1. On the contrary, the alloy obtained using method A was not homogeneous in all the volume of the solid. The homogeneity depended on the mechanical treatment undergone by the mixture of the oxides. - Research Highlights: {yields}Study of the properties of Cu-Ni alloys synthesized by two different routes. {yields}Mixtures of Cu and Ni oxides prepared by two techniques were reduced with H{sub 2}. {yields}Mixtures of oxides were obtained by a mechanical process and the citrate-gel route. {yields}The characterizations were carried out by TPR, XRD, SEM and EPMA. {yields}The route used to prepare oxide mixtures influences on the Cu-Ni alloy obtained.

36 MATERIALS SCIENCE↗

Characterisation of Sm-Co-Sn alloys

Cast SmCo{sub 5-x}Sn{sub x} (x = 0.00, 0.01, 0.06 and 0.12) alloys were prepared by arc melting with subsequent thermal homogenisation. Microstructural and x-ray diffraction studies revealed that the alloys were constituted of three phases i.e. SmCo{sub 5}, Sm{sub 2}Co{sub 7} and Sm{sub 2}Co{sub 17}. The addition of Sn caused grain refinement of the alloys. It was found that the Sn addition promoted nucleation of Sm{sub 2}Co{sub 17}, segregation of solute atoms and increase in unit cell volume; consequently, significant augmentation in remanence to maximum magnetization ratios was achieved. - Research Highlights: 1. Tin up to 0.12% was added in a Samarium cobalt-SmCo5 system; discernable changes in the microstructure and phase distribution were achieved; {yields} the nucleation of Sm2Co17 phase, {yields} segregation of Sn and samarium rich Sm2Co7 phase on the grain boundaries {yields} refinement of the microstructure in term of grain size 2. Moreover, addition of Sn caused twofold increase in magnetic properties (Remanence-Mr) of the Sm-Co alloy as compared to the binary SmCo5 system.

36 MATERIALS SCIENCE↗

Electrodeposition, characterization and morphological investigations of NiFe/Cu multilayers prepared by pulsed galvanostatic, dual bath technique

NiFe/Cu multilayers were grown sequentially by pulsed electrodeposition on copper (Cu) substrates. The layers were prepared in galvanostatic mode using a dual bath technique. The morphology, thickness, roughness and composition of the layers were studied using scanning electron microscopy, scanning transmission electron microscopy with energy dispersive X-ray spectroscopy, X-ray diffraction and atomic force microscopy. Analysis showed that the resulting multilayers were continuous layers with a root mean square roughness of 30 nm and a grain size of 20-60 nm. The Cu substrate and the electrodeposited Cu layer were preferentially (200) oriented while the NiFe layers were polycrystalline but with a preferred (200) texture. The thinnest multilayers produced were 20/40, NiFe/Cu, respectively. - Research Highlights: {yields} Thin MLs of Cu and Py can be ED utilizing a pulsed-galvanostatic, DBT. {yields} The resulting multilayers were continuous layers with an rms of 30 nm. {yields} The smallest average thickness achieved by DBT was 40 nm/20 nm for Cu/NiFe.

36 MATERIALS SCIENCE↗

Electron microscopy studies of lutetium doped erbium silicide (Er{sub 0.9}Lu{sub 0.1}){sub 5}Si{sub 4}

Examination of bulk microstructures of lutetium doped erbium silicide (Er{sub 0.9}Lu{sub 0.1}){sub 5}Si{sub 4} (space group: Pnma) using scanning and transmission electron microscopy (SEM, TEM) reveals the existence of thin plates of a hexagonal phase (space group: P6{sub 3}/mcm) where the stoichiometric ratio in moles between the rare earths and Si is 5 to 3, i. e the 5:3 phase. The orientation relationship between the matrix and the plates was determined as [010]{sub m} {approx} -parallel [-1010]{sub p.} This observation adds credence to the assumption that all linear features noted in alloys of the rare-earth intermetallic family R{sub 5}(Si{sub x}Ge{sub 1-x}){sub 4} are of the stoichiometric ratio 5:3 and possess a common orientation relationship with the parent 5:4 alloys. - Highlights: {yields} The linear features observed in the (Er{sub 0.9}Lu{sub 0.1}){sub 5}Si{sub 4} sample are hexagonal 5:3 plates. {yields} Thickness of 5:3 plates in 5:4 alloys made by tri-arc pulling is greater than made by arc-melting. {yields} The orientation relationship between 5:3 plates and the matrix is [010]{sub m} {approx} ||[-1010]{sub p}.

36 MATERIALS SCIENCE↗

The microstructure of near-equiatomic B2/f.c.c. FeNiMnAl alloys

A microstructural analysis of two FeNiMnAl alloys, Fe{sub 30}Ni{sub 20}Mn{sub 30}Al{sub 20} and Fe{sub 25}Ni{sub 25}Mn{sub 30}Al{sub 20}, was performed by a combination of atom probe tomography and transmission electron microscopy techniques. Although the microstructures of both alloys, which consist of alternating platelets aligned along < 100> of the B2-ordered phase, are similar to B2/b.c.c. two-phase alloys previously observed in the FeNiMnAl system, the two phases present in the current alloys are B2-ordered and f.c.c., with the latter phase being heavily twinned. Very fine ({approx} 5 nm) precipitates, whose chemistry was similar to that of the f.c.c. (Fe, Mn)-rich phase, were found within the B2 (Ni, Al)-rich phase in both alloys. - Highlights: {yields} The microstructures of the novel alloys Fe{sub 30}Ni{sub 20}Mn{sub 30}Al{sub 20} and Fe{sub 25}Ni{sub 25}Mn{sub 30}Al{sub 20} were characterized. {yields} Atom probe tomography and transmission electron microscopy were used in the study. {yields} A < 100>-aligned B2-ordered phase and heavily-twinned f.c.c. phase were present. {yields} Very fine (Fe, Mn)-rich precipitates were found within the B2 (Ni, Al)-rich phase.

36 MATERIALS SCIENCE↗

Morphology and composition of Ni-Co electrodeposited powders

The morphology, phase and chemical composition of Ni-Co alloy powders electrodeposited from an ammonium sulfate-boric acid containing electrolyte with different ratio of Ni/Co ions were investigated. The ratios of Ni/Co ions were 1/1, 1/2 and 1/3. The morphology, chemical composition and phase composition of the electrodeposited alloy powders were investigated using AES, SEM, EDS and XRD analysis. Composition of the electrolyte, i.e. the ratio of Ni/Co concentrations was found to influence both, the alloy phase composition and the morphology of Ni-Co alloy powders. At the highest ratio of Ni/Co = 1/1 concentrations typical 2D fern-like dendritic particles were obtained. With a decrease of Ni/Co ions ratio among 2D fern-like dendrites, 3D dendrites and different agglomerates were obtained. X-ray diffraction studies showed that the alloy powders mainly consisted of the face-centered cubic {alpha}-nickel phase and hexagonal close-packed {epsilon}-cobalt phase and minor proportions of face-centered cubic {alpha}-cobalt phase. The occurrence of the latter phase was observed only in the alloy powder with the higher cobalt concentration in electrolyte. The electrodeposition of Ni-Co powders occurred in an anomalous manner. - Highlights: Black-Right-Pointing-Pointer Ni-Co alloys powders were successfully electrodeposited. Black-Right-Pointing-Pointer Composition of the electrolyte (Ni/Co ions ratio) was found to influence on morphology of powders. Black-Right-Pointing-Pointer The electrodeposition of Ni-Co powders occurred in an anomalous manner.

36 MATERIALS SCIENCE↗

Plasma electrolytic oxidation coating of synthetic Al-Mg binary alloys

The binary Al-Mg synthetic alloys were prepared in a vacuum/atmosphere controlled furnace with the addition of 0.5, 1, 2, 4, 7, and 15 wt.% pure Mg into pure aluminum as substrate material. The surfaces of the Al-Mg alloys and pure aluminum were coated for 120 min by plasma electrolytic oxidation in the same electrolyte of 12 g/L sodium silicate and 2 g/L KOH in distilled water. The coating was characterized by X-ray diffraction, scanning electron microscopy, profilometry and Vickers microhardness measurements. There regions of loose outer layer, dense inner layer with precipitate like particles of {alpha}-Al{sub 2}O{sub 3} and a thin transition layer were identified for the coated samples. The coating thickness increases from 85 to 150 {mu}m with Mg contents in the alloys. The surface morphology becomes more porous and consequently surface roughness tends to increase with plasma electrolytic oxidation treatment and further with Mg content. The increase in magnesium content reduces the formation of {alpha}-Al{sub 2}O{sub 3} and crystalline mullite phases in the coating and decreases microhardness of coating. The Mg concentration is constant throughout the other loose and dense regions of coating though it gradually decreases in the thin inner region. - Research Highlights: Black-Right-Pointing-Pointer The average thickness of PEO coating of Al-Mg alloys increases with Mg content. Black-Right-Pointing-Pointer The addition of Mg reduces and prevents the formation of {alpha}-Al{sub 2}O{sub 3} and mullite. Black-Right-Pointing-Pointer The surface roughness increases with Mg content in the Al-Mg alloys. Black-Right-Pointing-Pointer The hardness values of the coating decreases with the Mg amount in the substrate. Black-Right-Pointing-Pointer The Mg concentration is constant throughout the main regions of coating.

36 MATERIALS SCIENCE↗

Experimental and calculated phases in two as-cast and annealed Mg-Zn-Y alloys

The CALPHAD (Calculation of Phase Diagram) method was used to select ternary alloys from Mg-Zn-Y system, aimed at determining the role of precipitates in the microstructure and texture evolution of Mg during and after deformation. The selected alloys are Mg-6Zn-1.2Y and Mg-5Zn-2Y. The constituent phases in the as-cast Mg-6Zn-1.2Y alloy are {alpha}-Mg solid solution phase and I (Mg{sub 3}YZn{sub 6}) intermetallic phase. The as-cast Mg-5Zn-2Y alloy is composed of {alpha}-Mg, I and W (Mg{sub 3}Y{sub 2}Zn{sub 3}) phases. The intermetallics in the two alloys form by eutectic reaction, which in Mg-5Zn-2Y alloy results in initially W-phase formation and ultimately I-phase formation during solidification. After heat treatment, the Mg-6Zn-1.2Y and Mg-5Zn-2Y alloys contain nearly the same amount of ternary intermetallics (I and W phases, respectively) in equilibrium with {alpha}-Mg solid solution phase. The main solute in {alpha}-Mg phase is Zn with the same amount in the two alloys. The type and quantity of the phases obtained experimentally disagree with the results obtained from the thermodynamic database. One important discrepancy is that, in Mg-6Zn-1.2Y alloy, the I phase is not stable at the temperature of 430 Degree-Sign C, and that the W phase is the stable phase at this temperature. The differences in the experimental and calculated data indicate that the Mg-Zn-Y system requires to be reassessed with more experimental data. - Highlights: Black-Right-Pointing-Pointer Mg-6Zn-1.2Y and Mg-5Zn-2Y alloys were selected by FactSage Trade-Mark-Sign Thermodynamic software. Black-Right-Pointing-Pointer The I and W intermetallics in the two alloys form by eutectic reaction. Black-Right-Pointing-Pointer The alloys contain similar amounts of different intermetallics in equilibrium with {alpha}-Mg. Black-Right-Pointing-Pointer In Mg-6Zn-1.2Y, the I phase is not stable at the temperature of 430 Degree-Sign C. Black-Right-Pointing-Pointer The hardness of W phase is determined to be lower than that of I phase.

36 MATERIALS SCIENCE↗

Precipitation in a lead calcium tin anode

Samples from a hot rolled sheet of a tin and calcium bearing lead alloy were solution heat treated at 300 Degree-Sign C and cooled down to room temperature at different rates; these samples were left at room temperature to study natural precipitation of CaSn{sub 3} particles. The samples were aged for 45 days before analysing their microstructure, which was carried out in a scanning electron microscope using secondary and backscattered electron detectors. Selected X-ray spectra analyses were conducted to verify the nature of the precipitates. Images were taken at different magnifications in both modes of observation to locate the precipitates and record their position within the images and calculate the distance between them. Differential scanning calorimeter analyses were conducted on selected samples. It was found that the mechanical properties of the material correlate with the minimum average distance between precipitates, which is related to the average cooling rate from solution heat treatment. - Highlights: Black-Right-Pointing-Pointer The distance between precipitates in a lead alloy is recorded. Black-Right-Pointing-Pointer The relationship between the distance and the cooling rate is established. Black-Right-Pointing-Pointer It is found that the strengthening of the alloy depends on the distance between precipitates.

36 MATERIALS SCIENCE↗