Multiscale-Informed Modeling of High Temperature Component Response with Uncertainty Quantification

This report summarizes a joint effort between Argonne National Laboratory, Idaho National Laboratory, and Los Alamos National Laboratory to develop and deploy constitutive models targeted at predicting the life of Grade 91 alloy components subjected to high temperature environments typical of those that structural components in advanced nuclear reactors would experience. Two distinct, but complementary constitutive modeling approaches have been taken here. The first employs a phenomenological viscoplastic model for which parameters have been calibrated based on experimental data for a wide range of Grade 91 alloy that has undergone a variety of processing. A Bayesian approach was used to derive distributions of uncertain parameters for this model based on this data set. The second approach is a reduced order model suitable for engineering-scale analysis that is based on the results of a large set of mesoscale simulations. Mesoscale models allow for the microstructure and composition of a particular alloy to be directly taken into account in the computation of the viscoplastic response, but are computationally expensive, which makes it impractical to directly call those models for the material constitutive response in an engineering-scale simulation. The reduced-order representation of the response of the underlying model used here allows for an engineering-scale model to take into account the characteristics of the underlying microstructure, while only incurring a reasonable computational expense. Both of these approaches have different strengths, and are applicable for different parts of the design/analysis process. The phenomenological models can be readily parameterized based on a set of experimental data for a given class of materials and used for scoping calculations. Once a specific material is chosen and adequately characterized, the reduced order models can accurately predict the response of that specific alloy, and because the models are based on predictive models of the underlying microstructure, they can be used to more confidently predict the response under conditions in regions where there is limited experimental data. Both of these models have been integrated in the Grizzly code, which is used here to perform proof-of-concept uncertainty quantification analyses of a simple component under prototypical conditions. The built- in stochastic analysis capabilities in the MOOSE framework that Grizzly is built on are used here to run large sets of simulations for this uncertainty quantification analysis. As would be expected, because the reduced order models are developed for a much more tightly defined alloy, they predict tighter distributions of the time to failure than the phenomenological models, which are calibrated to a broader set of data. Also important is that these simulations demonstrate that a reduced order modeling approach can be successfully deployed to propagate uncertainties from the material scale to practical engineering-scale component simulations.

42 ENGINEERING↗

Portable Vibro-acoustic Testing System for In Situ Microstructure Characterization and Metrology

Portable Vibro-acoustic Testing System for In situ Microstructure Characterization and Metrology James A. Smith, Corrie I. Nichol Idaho National Laboratory, Idaho Falls ID Mostafa Fatemi, Mayo Clinic, Rochester MN There is a need in research reactors like the INL to inspect irradiated materials and structures. The goal of this work is to develop a portable scanning infrastructure for a material characterization technique called vibro-acoustography (VA) that has been developed by INL [1] for nuclear applications to characterize fuel, cladding materials, and structures. The proposed VA technology is based on ultrasound and acoustic waves; however, it provides information beyond what is available from the traditional ultrasound techniques and can expand the knowledge on nuclear material characterization and microstructure evolution. VA is a three-dimensional (3D) imaging modality based on ultrasound-stimulated acoustic emission. VA uses the force caused by the beating of two frequencies to generate an acoustic emission signal. Due to absorption or reflection, the energy density in the object at an acoustic focal point changes to produce a “radiation force.” This force locally vibrates the object, which results in an acoustic field that depends on the characteristics of the object at that point. This acoustic field is detected for every point in the object; the resulting data is used to make an image of the object’s mechanical properties. This technology is fundamentally different from traditional ultrasound imaging. More specifically, VA is: (a) based on the “radiation force,” a nonlinear phenomenon in sound propagation, and (b) sensitive to both high and low frequency dynamic responses of the object. The combination of these two response types provides information about characteristics of the object beyond what is possible by traditional ultrasound imaging. High spatial resolution is achieved, since the radiation force is localized to the focal point of the ultrasound beam. Low-frequency information, which is a representative of structural characteristics, is gained through the radiation force mechanism at a low (beat) frequency. This paper will report on the development of a portable scanning that can be set up to characterize materials and component in open water reactors and canals in situ. We will show some initial laboratory results of images generated by vibro-acoustics of surrogate fuel plates and graphite structures and discus the design of the portable system. 1. Smith, J. A., and Kunerth, D. C., “Vibro-acoustic Sensors for Materials Characterization and Related Methods and Systems,” Patent Application 13226280, 09/06/2011.

36 MATERIALS SCIENCE↗

Exploratory evaluation of ceramics for automobile thermal reactors

An exploratory evaluation of ceramics for automobile thermal reactors was conducted. Potential ceramic materials were evaluated in several reactor designs using both engine dynamometer and vehicle road tests. Silicon carbide contained in a corrugated metal support structure exhibited the best performance lasting over 800 hours in engine dynamometer tests and over 15,000 miles (24,200 km) of vehicle road tests. Reactors containing glass-ceramic components did not perform as well as silicon carbide. But the glass-ceramics still offer good potential for reactor use. The results of this study are considered to be a reasonable demonstration of the potential use of ceramics in thermal reactors.

Stone, P. L.↗

Semi-Annual Report for Horizontal Compact High Temperature Gas Reactor (HC-HTGR) Development during Performance Period October 2022-March 2023

Horizontal Compact High Temperature Gas Reactor (HC-HTGR) is being designed by a multi-disciplinary team of nuclear, mechanical, and structural engineers under the support of a DOE-NE Advanced Reactor Demonstration Program’s Advanced Reactor Concepts-20 (ARC-20) award. The objective of this ARC-20 project is to deliver a conceptual design for the proposed HC-HTGR in 3 years and support its commercialization as a safe, low-cost HTGR. Argonne National Laboratory (Argonne) is responsible for the design and analysis of the reactor cavity cooling system (RCCS) as a safety system for passive decay heat removal of the reactor concept. Additionally, Argonne is providing analysis of the primary heat transport system to ensure temperatures in the reactor systems, structures and components with significant safety margins during normal operation and design basis accident scenarios. This third semi-annual report summarized the progress made at Argonne on the two tasks during the first half of FY23. As a part of the RCCS design task, a design process for the water panel and the system configuration was performed to improve the thermal performance of the RCCS. The updated water panel design had achieved enhanced thermal performance with 0.96 MWth capability with major design updates made in structural interfaces with the RPV and initial configuration of the water tanks. The loop configuration of the RCCS has been proposed to have two independently working loops for system redundancy. A water panel material study was performed focusing on the use of carbon steel in water systems. Additional modeling strategies of primary system thermal fluids analyses were developed to meet modeling needs that are not well suited for the 1D-3D assembly level approach. The first of these is a reduced order assembly model, in which fuel centered unit cells are used to represent a fuel assembly. The 2D approach used in this model is much more computationally efficient, making this model useful for full core transient scenarios where fuel to coolant heat transfer is still the dominant flow path. The next model is the 3D core conduction model to be used to analyze decay heat removal in loss of primary system flow scenarios. Because these scenarios require a large domain to be modeled, a homogenized core model is being pursued to reduce the required computational costs. To accurately model decay heat scenarios it is necessary to couple a RCCS model to the 3D core conduction model. A simplified case is presented to demonstrate how the coupling methodology will be applied to the full core 3D conduction model.

21 SPECIFIC NUCLEAR REACTORS AND ASSOCIATED PLANTS↗

Effect of Welding Processes on the Microstructure, Mechanical Properties and Residual Stresses of Plain 9Cr-1Mo Steel Weld Joints

9Cr-1Mo steel designated as P9 is widely used in the construction of power plants and high-temperature applications. It is chosen for fabricating hexcan fuel subassembly wrapper components of fast breeder reactors. Arc welding processes are generally used for fabricating 9Cr-1Mo steel weld joints. A-TIG welding process is increasingly being adopted by the industries. In the present study, shielded metal arc (SMA), tungsten inert gas (TIG) and A-TIG welding processes are used for fabricating the 9Cr-1Mo steel weld joints of 10 mm thickness. Effect of the above welding processes on the microstructure evolution, mechanical properties and residual stresses of the weld joints has been studied in detail. All the three weld joints exhibited comparable strength and ductility values. 9Cr-1Mo steel weld joint fabricated by SMAW process exhibited lower impact toughness values caused by coarser grain size and inclusions. 9Cr-1Mo steel weld joint fabricated by TIG welding exhibited higher toughness due to finer grain size, while the weld joint fabricated by A-TIG welding process exhibited adequate toughness values. SMA steel weld joint exhibited compressive residual stresses in the weld metal and HAZ, while TIG and A-TIG weld joint exhibited tensile residual stresses in the weld metal and HAZ.

36 MATERIALS SCIENCE↗

Effectiveness of Bronze as a Zinc Getter After Being Subjected to Simulated Exposures

We report that gamma-emitting zinc-65 was detected in piping contained in a tritium glovebox after a vacuum thermal process. This contaminate was created during irradiation of components in a nuclear reactor and was borne of natural zinc. The Tritium Extraction Facility prefers to capture the zinc in a high radiation area to minimize potential dose to the worker and to reduce the likelihood of spreading contamination to other areas of the facility. Previous efforts have shown that bronze is an excellent candidate material to act as a zinc getter in the as-fabricated condition. In reality, the extraction process may contain moisture and hydrogen which could cause oxidation or reduction of the surfaces of the zinc getters. A series of experiments was conducted to determine the efficacy of the zinc getters after oxidation and reduction exposures. Lastly, it was determined that the bronze coupons were moderately effective in most of the oxidized conditions and in all the oxidized and reduced conditions.

36 MATERIALS SCIENCE↗

Neutronic Performance of a Compact 10 MWe Nuclear Reactor with Low Enrichment (ThxU1−x)N Fuel

Abstract Recent interest in compact nuclear reactors for applications in space or in remote locations drives innovation in nuclear fuel design, especially non-oxide ceramic nuclear fuels. This work details neutronic modeling designed to support the development of a new nuclear fuel concept based on a mixture of thorium and uranium nitride. A Monte Carlo N-Particle Version 6.2 (MCNP-6) model of a compact 10 MWe reactor design which incorporates (Th x U 1− x )N fuel is presented. In this context, a “compact” reactor is a completely assembled reactor which may be emptied of coolant and transported by specialized commercial vehicle, deployed by a C130J aircraft, or launched into space. Core geometry, reflector barrels, and the heat exchange zones are designed to support reduction of overall reactor volume of core components while maintaining criticality with a fixed total fuel mass of 4500 kg. Dense mixed nitrides of thorium nitride (ThN) additions in uranium nitride (UN) in 5 wt.% increments between $$0.05 \le x \le 0.5$$ 0.05 ≤ x ≤ 0.5 have been considered for calculation of $$k_{\infty }$$ k ∞ and $$k_{{{\text{effective}}}}$$ k effective . ThN additions in UN results in a slight increase in the magnitude of the temperature coefficient of reactivity, which is negative by design. The isotopic distribution of the principal actinide inventory as a function of burnup, time, and initial fuel composition is presented and discussed within the context of the proliferation risk of this core design.

Parker, S. S. (ORCID:000000018597440X)↗

Thermal diffusivity recovery and defect annealing kinetics of self-ion implanted tungsten probed by insitu transient grating spectroscopy

Tungsten is a promising candidate material for plasma-facing armour components in future fusion reactors. A key concern is irradiation-induced degradation of its normally excellent thermal transport properties. In this comprehensive study, thermal diffusivity degradation in ion-implanted tungsten and its evolution from room temperature (RT) to 1073 K is considered. Five samples were exposed to 20 MeV self-ions at RT to achieve damage levels ranging from 3.2 x 10 -4 to 3.2 displacements per atom (dpa). Transient grating spectroscopy with in-situ heating was then used to study thermal diffusivity evolution as a function of temperature. Using a kinetic theory model, an equivalent point defect density is estimated from the measured thermal diffusivity. The results showed a prominent recovery of thermal diffusivity between 450 K and 650 K, which coincides with the onset of mono-vacancy mobility. After 1073 K annealing samples with initial damage of 3.2 x 10 -3 dpa or less recover close to the pristine value of thermal diffusivity. For doses of 3.2 x 10 -2 dpa or higher, on the other hand, a residual reduction in thermal diffusivity remains even after 1073 K annealing. Transmission electron microscopy reveals that this is associated with extended, irradiation-induced dislocation structures that are retained after annealing. A sensitivity analysis shows that thermal diffusivity provides an efficient tool for the assessing total defect content in tungsten up to 1000 K.

36 MATERIALS SCIENCE↗

Transition in helium bubble strengthening of copper from quasi-static to dynamic deformation

Damage from low-temperature irradiation and the subsequent degradation of materials performance pose significant challenges for the storage of radioactive materials and for peripheral components in some nuclear reactor designs. Fully understanding the mechanical behavior of such materials requires test data for strain rates in both the quasi-static (< 10/s) and dynamic (>> 10/s) regimes. While dynamic testing has generally been avoided in the past for neutron irradiated (contamination concerns) and ion irradiated (insufficient volume) materials, surface-sensitive Richtmyer-Meshkov instability (RMI) tests were used in the present work to overcome these limitations. Here, nanopillar compression, nanoindentation, and RMI testing data from a helium implanted surface layer (~10 µm thick) were compiled to explore the effects of helium bubbles on the materials strength of high-purity copper at strain rates of 0.001/s – 10 8 /s. While nano-mechanical testing revealed increases in yield strength and hardness with increasing helium dose from 1000 to 4000 appm He, RMI indicated no significant changes in strength as compared to unimplanted copper. Here, this discrepancy in behavior was rationalized through a combination of recent literature and follow-on molecular dynamics (MD) simulations, leading to the conclusion that the nanoscale helium bubbles acting as dispersed barriers to dislocation motion at quasi-static strain rates collapse under shock loading and cease to be effective barriers at high strain rates.

36 MATERIALS SCIENCE↗

A neutron tomography study to visualize fluoride salt (FLiNaK) intrusion in nuclear-grade graphite

Manufactured graphite is a preferred material for in-core components of molten salt reactors and fluoride salt-cooled high-temperature reactors, which are in permanent contact with liquid salts. However, owing to the porous nature of nuclear graphite, under certain conditions, molten salts may intrude graphite's pores and affect graphite's properties and functionality. Therefore, a better understanding of molten salt intrusion (distribution across sample cross section and penetration depth) is needed to assess its effects. Here, in this work, we have demonstrated the use of neutron imaging (computed tomography) in the evaluation of salt penetration and distribution of a wide range of graphite grades with diverse microstructures that have been subjected to FLiNaK (LiF–NaF–KF) intrusion at 750 °C and 5 bar pressure for 12 h. Because of the great neutron attenuation contrast from scattering and adsorption between Li (from FLiNaK) and the graphite matrix, we have obtained direct visualization of FLiNaK salt distribution in the salt-impregnated graphites for the first time. Three-dimensional reconstructed images and cross-sectional concentration profiles demonstrate that salt penetration and density distribution are greatly dependent on the microstructural properties of the graphite grade.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

MHD thermohydraulics analysis and supporting R&D for DCLL blanket in the FNSF

A Fusion Nuclear Science Facility (FNSF) has been recognized in the fusion community as a necessary facility to resolve the critical technology issues of in-vessel components prior to the construction of a DEMO reactor (Abdou et al., 1996) [1]. Among these components, development of a reliable, low-cost and safe blanket system that provides self-sufficient tritium breeding and efficient conversion of the extracted fusion energy to electricity, while meeting all material, design and configuration limitations is among the most important but still challenging goals. In the recent FNSF study in the US (Kesel et al., 2015) [2], a Dual-Coolant Lead-Lithium (DCLL) blanket has been selected as the main breeding blanket concept. This paper summarizes the most important details of the proposed DCLL blanket design, presents the MHD thermohydraulic analysis for the PbLi flows in the blanket conduits and introduces supporting R&D studies, which are presently ongoing at UCLA. We also discuss the required pre-FNSF R&D in the area of MHD Thermofluids to support the further work on the DCLL blanket design & analysis and its integration into the fusion facility.

70 PLASMA PHYSICS AND FUSION TECHNOLOGY↗

A review of irradiation effects on LWR core internal materials - neutron embrittlement.

Austenitic stainless steels (SSs) are used extensively as structural alloys in the internal components of light water reactor (LWR) pressure vessels because of their relatively high strength, ductility, and fracture toughness. However, exposure to neutron irradiation for extended periods not only changes the microstructure and microchemistry of these steels, but also degrades their fracture properties. The existing data on irradiated austenitic SSs are reviewed to determine the effects of key parameters such as material type and condition and irradiation temperature, dose, and dose rate on neutron embrittlement. Differences in the radiation-induced degradation of fracture properties between LWR and fast-reactor irradiations are also discussed. The results are used to (a) define a threshold fluence above which irradiation effects on fracture toughness of the material are significant, (b) evaluate the potential of neutron embrittlement under LWR operating conditions, and (c) assess the potential effects of voids on fracture toughness.

36 MATERIALS SCIENCE↗

In-situ TEM study of the ion irradiation behavior of U 3 Si 2 and U 3 Si 5

We report that U 3 Si 2 and U 3 Si 5 are two important uranium silicide phases currently under extensive investigation as potential fuel forms or components for light water reactors (LWRs) to enhance accident tolerance. In this paper, their irradiation behaviors are studied by ion beam irradiations with various ion mass and energies, and their microstructure evolution is investigated by in-situ transmission electron microscopy (TEM). U 3 Si 2 can easily be amorphized by ion beam irradiations (by 1MeV Ar 2+ or Kr 2+ ) at room temperature with the critical amorphization dose less than 1 dpa. The critical amorphization temperatures of U 3 Si 2 irradiated by 1MeV Kr 2+ and 1MeV Ar 2+ ion are determined as 580±10K and 540±5K, respectively. In contrast, U 3 Si 5 remains crystalline up to 8 dpa at room temperature and is stable against ion irradiation-induced amorphization up to ~50 dpa by either 1MeV Kr 2+ or 150KeV Kr + at 623K. In conclusion, these results provide valuable experimental data to guide future irradiation experiments, support the relevant post irradiation examination, and serve as the experimental basis for the validation of advanced fuel performance models

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

The effect of helium on cavity swelling in dual-ion irradiated Fe and Fe-10Cr ferritic alloys

We report Ferritic-martensitic (FM) steels for in-vessel components in proposed fusion reactors are expected to suffer from high levels of displacement damage and helium (He) generation by neutron transmutation. However, a thorough understanding of the He synergistic effects on the cavity swelling in FM steels is still not well established. To gain fundamental insights into the He effect on cavity swelling, high purity Fe and Fe-10 wt.% Cr ferritic model alloys were irradiated with 8 MeV Ni ions and co-implanted He ions at 400 to 550 °C up to 30 displacements per atom (dpa) with He implantation rates of 0.1, 10 and 50 appm He/dpa. The current study focuses on the 50 appm He/dpa, 500 °C behavior vs. 0.1 and 10 appm He/dpa. Irradiation-induced defects, including cavities, dislocation loops, and dislocation networks were characterized using transmission electron microscopy (TEM). In the grain interior, a bimodal cavity size distribution was observed in the 10 and 50 appm He/dpa samples, but not for 0.1 appm He/dpa. Cavity swelling was maximized at intermediate He implantation rates of ~10 appm He/dpa for both ion-irradiated Fe and Fe-10Cr alloys. The cavity swelling behavior as a function of He implantation rate appears to be controlled by the He/dpa-dependent variation of cavity sink strengths. Treating small bubbles as biased sinks for interstitial absorption can significantly increase the ratio of biased to unbiased sink strengths (Q) and results in maximized cavity swelling for a Q ratio close to one.

36 MATERIALS SCIENCE↗

Hydrogen trapping energetics at BCC iron-helium interfaces

Density functional theory (DFT) calculations have been performed to assess the trapping and segregation strength of hydrogen (H) to helium (He) interfaces in BCC (Fe) as a function of He density and surface orientation. The He density ranges from 0 to 2 He/V which corresponds to equilibrium bubbles that are expected to form in the structural components in a fusion reactor environment. The DFT calculations consist of a slab of BCC metal and an initial lattice of FCC He. Here, the report on the binding energy of H to these interfaces as well as the migration barriers into and away from the surface, which together provide information on the de-trapping energy for H at He bubbles. It was found that the binding energy of H to He-Fe interfaces decreases with increasing He density. Migration barriers are also modified due to the He density, which are sensitive to the surface orientation as well as the diffusion pathway. These results provide valuable first-principles energetics that are necessary for higher-order, mesoscale models, and provide insight into the extent to which He bubbles may trap tritium in fusion structural materials.

42 ENGINEERING↗

The interaction of edge dislocations with hydrogen-helium bubbles in tungsten

In fusion reactors, plasmas-facing components undergo degradation due to displacement damage and injection of gas impurities. Significant amounts of hydrogen (H) and helium (He) impurities can be introduced into materials through plasma exposure and nuclear transmutation, and their synergistic effects lead to the formation of mixed He/H bubbles under irradiation, changing their hardening mechanisms. In this study, molecular dynamics (MD) models were developed to study the interaction between ½<111> edge dislocations with mixed He/H-bubbles in W. The critical resolved shear stress (CRSS) that is required for dislocation breakaway increases with He/H-to-vacancy ratio at 600 K, indicating strong pinning effects of mixed He/H bubbles. However, as the temperature increases up to 1400 K, the mixed He/H bubbles become unstable as the H atoms are increasingly emitted from the mixed He/H bubbles and migrate into W matrix, which lowers bubble pressure and CRSS. Overall, these results highlight the synergistic effects of He and H on dislocation behavior in irradiated W during deformation.

36 - MATERIALS SCIENCE↗

Formation of gradient microstructure and mechanical properties of hot-pressed W-20 wt% Cu composites after sliding friction severe deformation

Highlights: • W particles of composites were refined during sliding friction treatment (SFD). • Dislocation, dislocation tangles and boundary clearly exist in deformed W particle. • YS and UTS of SFDed sample are 308.74 MPa and 553.60 MPa owing to the refinement. • Electrical conductivity of SFDed sample decreased from 33 IACS% to 28.5 IACS%. • Fracture mode changing from inter-granular mode to trans-granular. - Abstract: W-based alloys are currently considered promising candidates for high heat flux components in future fusion reactors. In this paper, hot pressed W-20 wt%Cu composites were treated at room temperature using a sliding friction severe deformation (SFD) process, with a moving speed of 0.2 m/s and an applied load of 500 N. Microstructural evolution of composites after the SFD treatment was evaluated and compared with that of the untreated composites. Results showed that there was a gradient structure generated and an obvious refinement in tungsten particles size in the surface layer after the SFD process. The average particle size of tungsten in the SFD treated composites was 2.60 μm, whereas it was 4.5 μm for tungsten in the untreated composites. Fracture surfaces of the composites indicated that the SFD treatment destroyed the W skeleton and changed fracture mode from predominant inter-granular one to trans-granular one due to the decrease in contact area of W-W inter-particles. Yield strength and ultimate tensile strength of composites after the SFD treatment were 308 MPa and 553 MPa, respectively. The treated composites exhibited micro-hardness values with an average reading of about 308 HV. Analysis of the facture microstructures clearly suggested that the tungsten particles in the treated composites are consisted of dislocations and boundaries as well as dislocation tangles. The electrical conductivity of the composites was decreased from 33 IACS% to 28.5 IACS% after the SFD treatment, mainly due to loss or squeezing of copper into the inner surface.