Search NASA⌕ Search

SEARCH · Search NASA

Results for “STRESS RELAXATION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

868 records · Page 49

Anomalous lattice expansion in yttria stabilized zirconia under simultaneous applied electric and thermal fields: A time-resolved in situ energy dispersive x-ray diffractometry study with an ultrahigh energy synchrotron probe

Nonisothermal densification in 8% yttria doped zirconia (8YSZ) particulate matter of 250 nm median particle size was studied under 215 V/cm dc electric field and 9 Degree-Sign C/min heating rate, using time-resolved in-situ high temperature energy dispersive x-ray diffractometry with a polychromatic 200 keV synchrotron probe. Densification occurred in the 876-905 Degree-Sign C range, which resulted in 97% of the theoretical density. No local melting at particle-particle contacts was observed in scanning electron micrographs, implying densification was due to solid state mass transport processes. The maximum current draw at 905 Degree-Sign C was 3 A, corresponding to instantaneous absorbed power density of 570 W/cm{sup 3}. Densification of 8YSZ was accompanied by anomalous elastic volume expansions of the unit cell by 0.45% and 2.80% at 847 Degree-Sign C and 905 Degree-Sign C, respectively. The anomalous expansion at 905 Degree-Sign C at which maximum densification was observed is characterized by three stages: (I) linear stage, (II) anomalous stage, and (III) anelastic recovery stage. The densification in stage I (184 s) and II (15 s) was completed in 199 s, while anelastic relaxation in stage III lasted 130 s. The residual strains ({epsilon}) at room temperature, as computed from tetragonal (112) and (211) reflections, are {epsilon}{sub (112)} = 0.05% and {epsilon}{sub (211)} = 0.13%, respectively. Time dependence of (211) and (112) peak widths ({beta}) show a decrease with both exhibiting a singularity at 905 Degree-Sign C. An anisotropy in (112) and (211) peak widths of {l_brace} {beta}{sub (112)}/{beta}{sub (211)}{r_brace} = (3:1) magnitude was observed. No phase transformation occurred at 905 Degree-Sign C as verified from diffraction spectra on both sides of the singularity, i.e., the unit cell symmetry remains tetragonal. We attribute the reduction in densification temperature and time to ultrafast ambipolar diffusion of species arising from the superposition of mass fluxes due to Fickian diffusion, thermodiffusion (Soret effect), and electromigration, which in turn are a consequence of a superposition of chemical, temperature, and electrical potential gradients. On the other hand, we propose defect pile-up at particle-particle contacts and subsequent tunneling as a mechanism creating the 'burst-mode' discontinuous densification at the singularities observed at 847 and 905 Degree-Sign C.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Crack formation in strained β-(AlxGa 1−x ) 2 O 3 films grown on (010) β-Ga 2 O 3 substrates

The cracking and local strain relaxation in (010) (Al x Ga 1−x ) 2 O 3 films grown on Ga 2 O 3 substrates are assessed in terms of film composition and thickness. We utilize x-ray diffraction and electron microscopy techniques combined with simulation and modeling to investigate that film cracking on curvature (flatness) has a directly proportional relationship with film thickness and/or aluminum content. Cross section transmission electron microscopy reveals that cracks along both the (001) and (100) cleavage planes penetrate into the substrate. The diffuse scattered intensity observed in reciprocal space maps (RSMs) is directly correlated with the tilt that is introduced due to the change in the deformation conditions near the cracks. While asymmetric RSMs show that the layers are fully strained, the diffuse scattering distribution in reciprocal space can be interpreted to show that the cracking relaxes and locally tilts the lattice ∼350 nm from the crack edges, which is consistent with the larger radius of curvature associated with the films with higher crack densities. For example, a 200 nm (Al 0.13 Ga 0.87 ) 2 O 3 thick film has an average inter-crack spacing of 3.3 µm, so most of the epitaxial layer is fully strained except near the cracks where it deforms elastically and is consistent with the gallium oxide Poisson ratio. A reciprocal space model was developed, which imports the strain and tilt distributions (based on finite element modeling) to match the features observed in the experimental maps. We also note that previous studies involving (Al x Ga 1−x ) 2 O 3 films may show evidence of cracking as observed in their symmetric and asymmetric RSMs.

36 MATERIALS SCIENCE↗

Mechanism-Informed Breakdown: Understanding Degradation by Controlling Voltage-Hold Patterns in Proton Exchange Membrane Water Electrolyzers

Low catalyst loadings pose challenges to performance stability in proton exchange membrane (PEM) water electrolysis over extended operation. To study the impact of degradation mechanisms and voltage loss rates, different stress tests are applied to membrane electrode assemblies. Potential cycling conditions were observed to induce higher degrees of iridium (Ir) oxide crystallization, ionomer degradation, and catalyst layer (CL) thinning, which likely contributed to higher kinetic loss rates. On the other hand, while Ir migrating into the PEM (Ir band) generally impairs performance, the interconnected and more uniform Ir band formed under a constant 2 V hold may allow for Ir at the catalyst/membrane interface to remain electronically connected and kinetically accessible, as well as indicate greater Ir site access during the applied stressor. The 2 V hold also demonstrates improved kinetic durability through a lower Tafel slope, faster polarization kinetics, and reduced charge transfer resistance. In contrast, potential cycling caused the migration of disconnected Ir agglomerates into the membrane bulk and created a steady increase in charge transfer resistance, a more dramatic decrease in capacitance (46.7% loss), and significant damage to the surrounding ionomer, indicating a decline in both the quality and quantity of active sites in the anode CL. This work underscores the distinct degradation pathways associated with load holds versus cycling, highlighting the role of catalyst-ionomer interactions in kinetic performance and long-term stability. These insights can inform operational strategies for PEM electrolyzers powered by intermittent energy sources, aiming to minimize efficiency losses over extended operation.

36 MATERIALS SCIENCE↗