Phosphorus-containing imide resins - Modification by elastomers

The syntheses and general features of addition-type maleimide resins based on bis(m-aminophenyl)phosphine oxide and tris(m-aminophenyl)phosphine oxide have been reported previously. These resins have been used to fabricate graphite cloth laminates having excellent flame resistance. These composites did not burn even in pure oxygen. However, these resins were somewhat brittle. This paper reports the modification of these phosphorus-containing resins by an amine-terminated butadiene-acrylonitrile copolymer (ATBN) and a perfluoroalkylene diaromatic amine elastomer (3F). An approximately two-fold increase in short beam shear strength and flexural strength was observed at 7 percent ATBN concentration. The tensile, flexural, and shear strengths were reduced when 18 percent ATBN was used. Anaerobic char yields of the resins at 800 C and the limiting oxygen indexes of the laminates decreased with increasing ATBN concentration. The perfluorodiamine (3F) was used with both imide resins at 6.4 percent concentration. The shear strength was doubled in the case of the bisimide with no loss of flammability characteristics. The modified trisimide laminate also had improved properties over the unmodified one. The dynamic mechanical analysis of a four-ply laminate indicated a glass transition temperature above 300 C. Scanning electron micrographs of the ATBN modified imide resins were also recorded.

Varma, I. K.↗

One-Piece Force-Transducer Body

Rugged unit designed to operate in severe environment. Forcetransducer body designed for measurement of loads on specimens tested in hydrogen gas at temperatures up to 2,000 degree F (1,090 degree C). Body has symmetrical radial-shear-beam configuration and machined in one piece from bar stock.

Meyer, R. A.↗

Ground exposure of composite materials for helicopters

Residual strength results are presented on four composite material systems that were exposed for three years at locations on the North American Continent. The exposure locations are near the areas where Bell Model 206L Helicopters, that are in a NSA/U.S. Army sponsored flight service program, are flying in daily commercial service. The composite systems are: (1) Kevlar-49 fabric/F-185 epoxy; (2) Kevlar-49 fabric/LRF-277 epoxy; (3) Kevlar-49 fabric/CE-306 epoxy; and (4) T-300 Graphite/E-788 epoxy. All material systems exhibited good strength retention in compression and short beam shear. The Kevlar-49/LRF-277 epoxy retained 88 to 93 percent of the baseline strength while the other material systems exceeded 95 percent of baseline strength. Residual tensile strength of all materials did not show a significant reduction. The available moisture absorption data is also presented.

Baker, D. J.↗

Graphite/PMR polyimide composites with improved toughness

The toughness of composites made with modified PMR (Polymerization of monomer reactants) polyimides and Celion 6000 graphite fibers was studied. Various types/levels of monomer reactants containing flexible links were incorporated into PMR resin compositions used to prepare composites. The composites were evaluated for toughness using instrumented drop weight and 10 deg off axis tensile tests at room temperature, and for strength using flexure and short beam shear tests at room temperature and at elevated temperature. The effect of resin composition on composite processability, thermo-oxidative stability, toughness and mechanical properties are discussed.

Vannucci, R. D.↗

Design of test specimens and procedures for generating material properties of Douglas fir/epoxy laminated wood composite material: With the generation of baseline data at two environmental conditions

In support of the design of wind turbine generator airfoils/blades utilizing Douglas Fir/West System Epoxy laminated composite material, a program was undertaken to define pertinent material properties utilizing small scale test specimens. Task 1 was the development of suitable monotonic tension, compression, short beam shear and full reversed cyclic specimen designs and the companion grips and testing procedures. Task 2 was the generation of the material properties at two environmental conditions utilizing the specimens and procedures developed in Task 1. The monotonic specimens and procedures generated results which compare favorably with other investigators while the cyclic results appear somewhat conservative. Adding moisture and heat or scarf joints degraded the monotonic performance but had a more nebulus effect with cyclic loading.

Johnson, Paul E.↗

Thermoplastic matrix composites - LARC-TPI, polyimidesulfone and their blends

Composites were fabricated from unidirectional unsized AS-4 carbon fiber and two baseline polyimides: benzophenone dianhydride-3,3'-diaminodiphenylsulfone (PISO2) and benzophenone dianhydride-3,3'-diaminobenzophenone (LARC-TPI). In addition, each polymer solution prior to prepregging was doped with various amounts of crystalline LARC-TPI powder to enhance melt flow during press molding. The 2:1, 1:1, and 1:2 ratios of crystalline to amorphous resin, respectively, were studied in the LARC-TPI system and the 1:2 ratio in the PISO2 system. Matrix characterization, prepreg fabrication/characterization and composite fabrication and physical/mechanical properties are described. The latter include three point short beam shear and flexure, dry and wet, as well as fracture toughness properties in selected compositions.

Johnston, Norman J.↗

Effect of long-term thermal aging on coated Celion/LARC-160 composites

Coated and uncoated unidirectional laminates of Celion (Trademark)/LARC-160 graphite/polyimide were thermally aged in air at temperatures of 204, 260, and 316 C for various times up to 15,000 hours. Selected panels were coated with a high temperature coating resin (polyphenyl quinoxaline--PPQ): 1) edges only; 2) top and bottom only; 3)completely; or 4) not at all. Periodically during aging, panels were removed from the ovens, weighed, and short beam shear (SBS) specimens cut from selected locations in the panels. The protective coating did not influence the retention of SBS strength during thermal aging but did not lessen the amount of weight-loss incurred. The integrity of the PPQ coating was completely destroyed during aging at 316 C.

Nelson, James B.↗

A thermally modified polymer matrix composite material with structural integrity to 371 C

The potential for utilizing surface coatings to inhibit the thermal oxidation of polymer matrix composites was studied. Isothermal, inert gas exposures of graphite/PMR-15 composites indicated that after an initial loss of weight, no significant amounts of thermal degradation products are given off during high temperature exposures in the absence of oxygen. As long as a coating remains effective, the composite material should remain stable. It was also found that the glass transition temperature T sub g of the matrix resin could be increased to values in excess of 400 C. This resulted in measured short beam shear strengths of 75.9 MPa (11 Ksi), flexural strengths of 1172 MPa (170 Ksi) and flexural moduli of 141 GPa (20.5 Msi) for the material at a test temperature of 371 C. The treatment that was used caused a decrease in the PMR-15 resin density from 1.31 to 1.29 gm/cc. It was concluded that state-of-the-art composites, protected by oxygen-impervious coatings, can be used as materials of construction with structural integrity to at least 371 C and possibly above.

Bowles, Kenneth J.↗

Polyimide Matrix composites: Polyimidesulfone/LARC-TPI (1:1) blend

Polyimide matrix composites were fabricated from unidirectional unsized AS-4 carbon fiber and a doped 1:1 blend of two polyimides: benzophenone dianhydride-3,3'-diamino diphenylsulfone (PISO2) and benzophenone dianhydride-3,3'-diamino benzophenone (LARC-TPI). To enhance melt flow properties, the molecular weight of the PISO2 was controlled by end-capping with phthalic anhydride and addition of 5 percent by weight p-phenylene diamine-phthalic anhydride bisamic acid dopant. Prepreg was drum-wound using a diglyme slurry comprised of the soluble polyamideacid of PISO2, the soluble bisamideacid of the dopant, and the insoluble imidized LARC-TPI powder. Melt flow studies with a rotary rheometer and parallel plate plastometer on neat resin and prepreg helped develop an optimum cure cycle. Composite mechanical properties at room and elevated temperatures, dry and moisture-saturated, were evaluated, including short beam shear strength and flexure, tensile, shear, and compression properties. Two 18 in. x 24 in. skin-stringer panels were fabricated, one of which was tested in compression to failure.

Johnston, Norman J.↗

A thermally modified polymer matrix composite material with structural integrity to 371 C

The potential for utilizing surface coatings to inhibit the thermal oxidation of polymer matrix composites was studied. Isothermal, inert gas exposures of graphite/PMR-15 composites indicated that after an initial loss of weight, no significant amounts of thermal degradation products are given off during high temperature exposures in the absence of oxygen. As long as a coating remains effective, the composite material should remain stable. It was also found that the glass transition temperature T sub g of the matrix resin could be increased to values in excess of 400 C. This resulted in measured short beam shear strengths of 75.9 MPa (11 Ksi), flexural strengths of 1172 MPa (170 Ksi) and flexural moduli of 141 GPa (20.5 Msi) for the material at a test temperature of 371 C. The treatment that was used caused a decrease in the PMR-15 resin density from 1.31 to 1.29 gm/cc. It was concluded that state-of-the-art composites, protected by oxygen-impervious coatings, can be used as materials of construction with structural integrity to at least 371 C and possibly above.

Bowles, Kenneth J.↗

Aging behavior and life prediction of graphite composites

This paper presents experimental data from two independent tests, designed to determine the long-term reliability of composite materials. The technique of accelerated aging at elevated temperatures is employed. In the first set, graphite fiber, epoxy composites in five ply layups are manufactured and tested in the standard short-beam shear mode. In the second set, Nomex honeycomb, graphite fiber/epoxy composite face and rear sheet sandwich coupons are tested. After satisfying simple consistency checks, data interpretation is attempted within the framework of an Arrhenius degradation model. The elevated temperature is assumed to influence the degradation according to this temperature-dependent rate law. From these tests on five-ply composites and honeycomb sandwiches, it is concluded that aging is not a serious problem.

Ramohalli, Kumar↗

Polyimide matrix composites - Polyimidesulfone/LARC-TPI (1:1) blend

Polyimide matrix composites were fabricated from unidirectional unsized AS-4 carbon fiber and a doped 1:1 blend of two polyimides: PISO2 and LARC-TPI. To enhance melt flow properties, the molecular weight of the PISO2 was controlled by end-capping with phthalic anhydride and addition of 5 percent by weight p-phenylenediamine-phthalic anhydride bisamic acid dopant. Prepreg was drum-wound using a diglyme slurry comprised of the soluble polyamideacid of PISO2, the soluble bisamideacid of the dopant, and the insoluble imidized LARC-TPI powder. Melt flow studies with a rotary rheometer and parallel plate plastometer on neat resin and prepreg helped develop an optimum cure cycle. Composite mechanical properties at room and elevated temperatures, dry and moisture-saturated, were evaluated, including short beam shear strength and flexure, tensile, shear, and compression properties. Two 18 x 24-inch skin-stringer panels were fabricated, one of which was tested in compression to failure.

Johnston, Norman J.↗

Thermoplastic coating of carbon fibers

Using a continuous powder coating process, more than 1500 meters of T 300/LaRC-TPI prepreg were produced. Two different types of heating sections in the coating line, namely electrical resistance and convection heating, were utilized. These prepregs were used to fabricate unidirectional composites. During composite fabrication the cure time of the consolidation was varied, and composites samples were produced with and without vacuum. Under these specimens, the effects of the different heating sections and of the variation of the consolidation parameters on mechanical properties and void content were investigated. The void fractions of the various composites were determined from density measurements, and the mechanical properties were measured by tensile testing, short beam shear testing and dynamic mechanical analysis.

Edie, D. D.↗

LDEF-space environmental effects on materials: Composites and silicone coatings

The objective of the Lockheed experiment is to evaluate the effects of long term low Earth orbit environments on thermal control coatings and organic matrix/fiber reinforced composites. Two diverse categories are reported: silicone coatings and composites. For composites physical and structural properties were analyzed; results are reported on mass/dimensional loss, microcracking, short beam shear, CTE, and flexural properties. The changes in thermal control properties, mass, and surface chemistry and morphology are reported and analyzed for the silicon coatings.

Petrie, Brian C.↗

Toughening of PMR composites by semi-interpenetrating networks

Polymerization of monomer reactants (PMR-15) type polyimide and RP46 prepregs were drum wound using IM-7 fibers. Prepregging and processing conditions were optimized to yield good quality laminates with fiber volume fractions of 60 percent (+/- 2 percent). Samples were fabricated and tested to determine comprehensive engineering properties of both systems. These included 0 deg flexure, short beam shear, transverse flexure and tension, 0 deg tension and compression, intralaminar shear, short block compression, mode 1 and 2 fracture toughness, and compression after impact properties. Semi-2-IPN (interpenetrating polymer networks) toughened PMR-15 and RP46 laminates were also fabricated and tested for the same properties.

Tiwari, S. N.↗

LDEF-space environmental effects on materials: Composites and silicone coatings

The effects of long term low Earth orbit environments on thermal control coatings and organic matrix/fiber reinforced composites are discussed. Two diverse categories are reported here: silicone coatings and composites. For composites physical and structural properties were analyzed; results are reported on mass/dimensional loss, microcracking, short beam shear, coefficient of thermal expansion (CTE), and flexural properties. The changes in thermal control properties, mass, and surface chemistry and morphology are reported and analyzed for the silicone coatings.

Petrie, Brian C.↗

Polymer matrix composites on LDEF experiments M0003-9 and M0003-10

Over 250 polymer matrix composites were exposed to the natural space environment on Long Duration Exposure Facility (LDEF) experiments M0003-9 and 10. The experiments included a wide variety of epoxy, thermoplastic, polyimide, and bismalimide matrix composites reinforced with graphite, glass, or organic fibers. A review of the significant observations and test results obtained to date is presented. Estimated recession depths from atomic oxygen exposure are reported and the resulting surface morphologies are discussed. The effects of the LDEF exposure on the flexural strength and modulus, short beam shear strength, and coefficient of thermal expansion of several classes of bare and coated composites are reviewed. Lap shear data are presented for composite-to-composite and composite-to-aluminum alloy samples that were prepared using different bonding techniques and subsequently flown on LDEF.

Steckel, Gary L.↗

Toughening of PMR composites by gradient semi-interpenetrating networks

The toughening of the PMR-15 and LARC RP-46 high temperature thermosetting polyimides is presently attempted through the construction of a semiinterpenetrating network at ply interfaces through the use of the Matrimid 5218 thermoplastic polyimide powder, whose 315-320 glass transition temperature is compatible with the PMR matrices. The 60 vol pct fiber composites thus prepared for the two resins, with and without toughening, were comprehensively characterized in flexure, tension, intralaminar and short beam shear, compression and quasi-isotropic short-block compression, as well as modes I and II interlaminar fracture toughness and compression after impact.

Johnston, N. J.↗