Search NASA⌕ Search

SEARCH · Search NASA

Results for “Bisphenol A”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Thermal expansion of an epoxy-glass microsphere composite

The thermal expansion of a composite of epoxy (diglycidyl ether of bisphenol A) and solid glass microspheres was investigated. The microspheres had surfaces which were either untreated or treated with a silicone release agent, an epoxy coupling agent, or a general purpose silane coupling agent. Both room temperature (about 300 K) and elevated temperature (about 475 K) cures were used for the epoxy. Two microsphere size ranges were used, about 50 microns, which is applicable in filled moldings, and about 125 microns, which is applicable as bond line spacers. The thermal expansion of the composites was measured from 300 to 350 K or from 300 to 500 K, depending on the epoxy cure temperature. Measurements were made on composites containing up to .6 volume fraction microspheres. Two predictive models, which required only the values of thermal expansion of the polymer and glass and their specific gravities, were tested against the experimental data. A finite element analysis was made of the thermal strain of a composite cell containing a single microsphere surrounded by a finite-thickness interface.

Price, H. L.↗

Variation in animal response to different toxicants

The variation in response of different lots of male Swiss albino mice to pyrolysis effluents from surgical cotton and from bisphenol A polycarbonate, and to pure carbon monoxide, is discussed. The variation appeared to be less with the pyrolysis gases from polycarbonate than with pure carbon monoxide.

Hilado, C. J.↗

New adhesive withstands temperature extremes

Adhesive, developed for high-temperature components aboard satellites, is useful at both high and low temperatures and exhibits low-vacuum volatility and low shrinkage. System uses polyfunctional epoxy with high aromatic content, low equivalent weight, and more compact polymer than conventional bisphenol A tape.

Park, J. J.↗

Intumescent coatings containing 4,4'-dinitrosulfanilide

A coating which is stable to the environment and to exposure to water, and which intumesces at a favorable temperature was developed. The composition comprises a mixture of 4, 4 prime dinitrousulfanilide as the intumescent agent in a polymer binder mixture of a chlorinated polyolefin, a bisphenol A epoxy resin, and a rubber-like amine hardener.

Sawko, P. M.↗

The relative fire resistance of select thermoplastic materials

The relative thermal stability, flammability, and related thermochemical properties of some thermoplastic materials currently used in aircraft interiors as well as of some candidate thermoplastics were investigated. Currently used materials that were evaluated include acrylonitrile butadiene styrene, bisphenol A polycarbonate, polyphenylene oxide, and polyvinyl fluoride. Candidate thermoplastic materials evaluated include: 9,9-bis(4-hydroxyphenyl)fluorene polycarbonate-poly(dimethylsiloxane) block polymer, chlorinated polyvinylchloride homopolymer, phenolphthalein polycarbonate, polyethersulfone, polyphenylene sulfide, polyarylsulfone, and polyvinylidene fluoride.

Kourtides, D. A.↗

Synthesis and characteristics of polyarylene ether sulfones

A method utilizing potassium carbonate/dimethyl acetamide, as base and solvent respectively, was used for the synthesis of several homopolymers and copolymers derived from various bisphenols. It is demonstrated that this method deviates from simple second order kinetics; this deviation being due to the heterogeneous nature of the reaction. Also, it is shown that a liquid induced crystallization process can improve the solvent resistance of these polymers. Finally, a Monte Carlo simulation of the triad distribution of monomers in nonequilibrium copolycondensation is discussed.

Viswanathan, R.↗

Reproducibility of polycarbonate reference material in toxicity evaluation

A specific lot of bisphenol A polycarbonate has been used for almost four years as the reference material for the NASA-USF-PSC toxicity screening test method. The reproducibility of the test results over this period of time indicate that certain plastics may be more suitable reference materials than the more traditional cellulosic materials.

Hilado, C. J.↗

The stability of new transparent polymeric materials: The epoxy trimethoxyboroxine system. Part 1: The preparation, characterization and curing of epoxy resins and their copolymers

The effects of resin composition, curing conditions fillers, and flame retardant additives on the flammability of diglycidyl ether of bisphenol-A (DGEBA) as measured by the oxygen index is examined. The oxygen index of DGEBA cured with various curing agents was between 0.198 to 0.238. Fillers and flame retardant additives can increase the oxygen index dependent on the material and the amount used. Changes in the basic cured resin properties can be anticipated with the addition of noncompatible additives. High flame resistant epoxy resins with good stability and mechanical properties are investigated.

Pearce, E.↗

Development of tough, moisture resistant laminating resins

Tough, moisture resistant laminating resins for employment with graphite fibers were developed. The new laminating resins exhibited cost, handleability and processing characteristics equivalent to 394K (250 F) curing epoxies. The laminating resins were based on bisphenol A dicyanate and monofunctional cyanates with hydrophobic substituents. These resins sorb only small quantities of moisture at equilibrium (0.5% or less) with minimal glass transition temperature depression and represent an improvement over epoxies which sorb around 2% moisture at equilibrium. Toughening was accomplished by the precipitation of small diameter particles of butadiene nitrile rubber throughout the resin matrix. The rubber domains act as microcrack termini and energy dissipation sites, allowing increased stress accommodation prior to catastrophic failure. A unique blend of amine terminated butadiene nitrile elastomer (MW 2,000) and a high nitrile content butadiene nitrile rubber yielded the desired resin morphology.

Brand, R. A.↗

Physical aging of linear and network epoxy resins

Network and linear epoxy resins principally based on the diglycidyl ether of bisphenol-A and its oligomers are prepared and studied using diamine and anhydride crosslinking agents. Rubber modified epoxies and a carbon fiber reinforced composite are also investigated. All materials display time-dependent changes when stored at temperatures below the glass transition temperature after quenching (sub-T/g/ annealing). Solvent sorption experiments initiated after different sub-T(g) annealing times demonstrate that the rate of solvent uptake can be indirectly related to the free volume of the epoxy resins. Residual thermal stresses and water are found to have little effect on the physical aging process, which affects the sub-T(g) properties of uniaxial carbon fiber reinforced epoxy material. Finally, the importance of the recovery phenomenon which affects the durability of epoxy glasses is considered.

Kong, E. S.-W.↗

Synthesis of perfluoroalkylene dianilines

The objective of this contrast was to optimize and scale-up the synthesis of 2,2-bis(4-aminophenyl)-hexafluoropropane and 1,3-bis(4-aminophenyl)hexafluoropropane, as well as to explore avenues to other perfluoroalkyl-bridged dianilines. Routes other than Friedel-Crafts reaction leading to 2,2-bis(4-aminophenyl)hexafluoropropane were investigated. The processes utilizing bisphenol-AF were all unsuccessful; reactions aimed at the production of 4-(hexafluoro-2-halo-isopropyl)aniline from the hydroxyl intermediate failed to yield the desired products. Tailoring the conditions of the Friedel-Crafts reaction of 4-(hexafluoro-2-hydroxyisopropyl)aniline, aniline, and aluminum chloride by using hydrochloride salts and selecting optimum reagent ratios, reaction times, and temperature resulted in approx. 20% yield of pure crystallized 2,2-bis(4-aminophenyl)hexafluoropropane in 0.2 mole reaction batches. Yields up to approx. 40% were realized in small, approx. 0.01 mole, batches. The synthesis of 1,3-bis(4-aminophenyl)hexafluoropropane starting with perfluoroglutarimidine was reinvestigated. The yield of the 4-step reaction sequence giving 1,3-bis(4-acetamidophenyl)hexafluoropropane was raised to 44%. The yield of the subsequent hydrolysis process was improved by a factor of approx. 2. Approaches to prepare other perfluoroalkyl-bridged dianilines were unsuccessful. Reactions reported to proceed readily with trifluoromethyl substituents failed when longer chain perfluoroalkyl groups were employed.

Paciorek, K. L.↗

Effect of resin on impact damage tolerance of graphite/epoxy laminates

Twenty-four different epoxy resin systems were evaluated by a variety of test techniques to identify materials that exhibited improved impact damage tolerance in graphite/epoxy composite laminates. Forty-eight-ply composite panels of five of the material systems were able to sustain 100 m/s impact by a 1.27-cm-diameter aluminum projectile while statically loaded to strains of 0.005. Of the five materials with the highest tolerance to impact, two had elastomeric additives, two had thermoplastic additives, and one had a vinyl modifier; all the five systems used bisphenol A as the base resin. An evaluation of test results shows that the laminate damage tolerance is largely determined by the resin tensile properties, and that improvements in laminate damage tolerance are not necessarily made at the expense of room-temperature mechanical properties. The results also suggest that a resin volume fraction of 40 percent or greater may be required to permit the plastic flow between fibers necessary for improved damage tolerance.

Williams, J. G.↗

Polyarylene Ethers with Improved Properties

This invention relates to novel polyarylene ethers which possess the combination of high strength, toughness, and high use temperature with ease of extrusion and formation into complex objects. These polyarylene ethers are suitable for use in adhesives, coatings, films, membranes, and composite matrices. The polyarylene ethers of this invention are the polycondensation products from the reaction of either 1,3-bis (4-chloro or fluorobenzoyl) benzene with any one of the following bisphenolic compounds: bis (3-hydroxyphenyl) methane; bis (4-hydroxyphenyl) methane; 1,1-dimethyl-bis (4-hydroxyphenyl)methane, or 9,9-bis (4-hydroxyphenyl) fluorene. Random and block copolymers are also comprehended.

Hergenrother, P. M.↗

Ultrasonic characterization of changes in viscoelastic properties of epoxy during cure

A technique for using the longitudinal velocity (LV) of an ultrasonic wave to monitor the extent of cross linking (CL) during the cure of thermosetting resins is described. The method was developed by monitoring the rate of change in LV during the cure of a bisphenol-A epoxy resin with an amine adduct. The experiment included variations in the temperature and stoichiometry in order to express the rate of change in terms of the reaction kinetics. The pulse-echo method was used with a single transducer operating at 20 MHz. Numerical models were defined to account for the acoustic response of a single layer, the attenuation and the reflection coefficient. A linear relationship was observed between the inverse of the temperature and the log of the rate of change in the velocity, supporting the theory that the velocity could be used to monitor the extent of the cross-linking reaction. An activation energy of 11.9 kcal/mole was calculated for the mixture being investigated.

Winfree, W. P.↗

Measurement of the degree of cure in epoxies with ultrasonic velocity

The use of ultrasonic longitudinal velocity values to measure the degree of cure (defined for an epoxide system as the concentration of epoxide/amine bonds divided by the initial epoxide concentration) in epoxy resins is investigated. The experimental setup used to measure the changes in longitudinal velocity with time is described, together with the technique used to calculate the degree of cure from the acoustic data, using the principle of additive module. Measurements were done with diglycidyl ether of bisphenol A epoxy resin cured with an amine adduct agent. Good qualitative agreement was shown between the time dependence of the acoustically measured degree of cure and the predicted rate of reaction.

Winfree, W. P.↗

Simulated space environment effects on the optical properties of poly(arylene ethers)

Results are reported from a study of the stability of poly(arylene ethers) formed in a reaction of 1,3 -bis(4-chlorobenzoyl)benzene and various bisphenols after experiencing long-term exposure to space conditions. Transparent poly(arylene ethers) films were subjected to separate electron and UV bombardments, as were polysulfone and Kapton films for comparisons. The order of exposure to the two types of radiation was reversed for two sample populations. The optical properties and glass transition temperatures of the samples were determined after irradiation. The poly(arylene ethers) films exhibited good resistance to the electron radiation but suffered severe degradation in the UV environment. The loss of optical transmissivity was proportional to the UV radiation dose.

Sykes, George F.↗

New polyarylene ethers

A series of new polyarylene ethers (PAEs) were prepared from the reaction of activated dihalo compounds with various bisphenols. Measured number average molecular weights for the PAEs ranged from 13,500 to 39,400 g/mole, and glass transition temperatures varied from 152 to 280 C. Ethynyl-terminated polyarylene ethers (ETPAEs) were also prepared by endcapping hydroxy-terminated polyarylene ethers with 4-ethynylbenzoyl chloride. Structure/property relationships for the PAEs, and the advantages offered by the ETPAEs, are discussed.

Hergenrother, P. M.↗