At least 91 records · Page 5

Corrosion Behavior of AZ31 Magnesium Alloy Produced by Continuous Variable Cross Section Direct Extrusion

In order to study the corrosion behavior of magnesium alloys of high performance in the simulated seawater by continuous variable cross section direct extrusion (CVCDE), an electrochemical method and weight loss method were used to study the difference between AZ31 magnesium alloys produced by CVCDE with different numbers of interim dies to examine the electrochemical corrosion behavior and corrosion rate at 3.5 wt.% NaCl solution in this paper. Scanning electron microscopy and x-ray diffraction were used to analyze the morphology of corrosion surfaces and the composition of the corrosion products of samples soaked for different times. The results show that after CVCDE with different numbers of interim dies, the size of the microstructure is refined gradually, and the grain orientation is also different; with the increase in the number of interim dies, the thermodynamic corrosion tendencies are different, and the corrosion resistance of samples extruded by conventional extrusion is relatively good; the charge transfer and material transfer process are the two main factors affecting the corrosion rate, which determines the direction of the electrochemical reaction; the corrosion form of the sample extruded by CVCDE is the local corrosion which is the filiform corrosion and pitting corrosion, and the corrosion product is mainly water-insoluble Mg(OH){sub 2}.

36 MATERIALS SCIENCE↗

Technical Note: Characterization of Corrosion Films Formed on Austenitic Stainless Steel in Supercritical CO 2 Containing H 2 O and O 2

Future technologies require structural alloys resistant to corrosion in supercritical CO 2 (sCO 2 ) fluids containing impurities such as H 2 O and O 2 . Traditional pipeline steels are potentially unsuitable for these environments and more corrosion resistant alloys such as stainless steels might be required. Little is known about the corrosion products formed on, and hence the processes which control corrosion of, stainless steels in impure sCO 2 environments. In this study, austenitic stainless steel 347H (UNS S34709) was exposed to sCO 2 containing H 2 O and O 2 at 8 MPa and 50°C or 250°C, and separately to the aqueous phase in equilibrium with the sCO 2 at 50°C, to simulate conditions expected in sCO 2 -based power cycles and carbon capture and storage pipelines. Only thin (< 20 nm) surface films formed after 500 h resulting in small mass changes and corrosion rates < 10 –4 mm/y, suggesting the material resists significant degradation in these environments. X-ray photoelectron spectroscopy and transmission electron microscopy were used to characterize the corrosion films in detail. Here, the exposure to the aqueous phase resulted in a thin (< 5 nm) Cr-oxide and/or -hydroxide passive film, while exposure to sCO 2 phases resulted in a multilayer Fe-rich oxide structure characteristic of a gas-phase oxidation process.

36 MATERIALS SCIENCE↗

Effect of Natural Organic Matter on Radionuclide Partitioning in Nuclear Fuel Storage Ponds - 17136

One of the nuclear fuel storage ponds at Sellafield is open to the air, and has contained a significant inventory of corroded Magnox fuel and sludge for several decades, with some fission products having been released into solution. The sludge is predominantly composed of brucite (Mg(OH){sub 2}), a corrosion product from the magnesium-based fuel cladding, amongst other corrosion products resulting from the uranium metal fuel. Sr-90 is known to constitute a small mass of the radionuclides present in the pond, but due to its solubility and activity, it is a radionuclide that is at risk of challenging effluent discharge limits. Organic molecules are known to be present also due to the ponds being open to the air, with occasional algal blooms restricting visibility. Understanding the chemical interactions of these components is important to inform ongoing sludge retrievals and effluent management. Batch sorption-desorption experiments have been performed with brucite, Sr-90 and natural organic matter (NOM) (namely humic acid (HA) and Pseudanabaena catenata cyano-bacterial growth supernatant) in both binary and ternary systems at high pH. Ionic strength, pH and order of addition of components were varied. Sr-90 was shown not to interact strongly with the bulk brucite surface in binary or ternary systems under pH conditions relevant to the pond. Humic acid in both binary and ternary systems demonstrated a strong affinity for the brucite surface. In ternary systems HA appeared to enhance sorption of Sr-90, and vice versa, regardless of the order of addition of components. There was no distinct effect of varying ionic strength or pH. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion of MA754 and MA956 in a Commercial Aluminum Melter

The University of North Dakota Energy & Environmental Research Center is working with Oak Ridge National Laboratory to test two oxide dispersion-strengthened alloys that could be used to construct very high-temperature heat recuperators for the aluminum-melting industry. For the initial tests, uncooled rings of MA754 and MA956 piping were exposed for 5 months to gases leaving an aluminum melter furnace at 1200 1290 C. The MA956 suffered spotty areas of severe corrosion and lost 25% of its weight. Scanning electron microscopy showed that there were small spots of alkali-rich corrosion products on the alloy surfaces, indicating the impact of droplets of fluxing agents. The corrosion products in these areas were mixed Fe, Cr, and Al oxides, which were depleted in Cr near the gas surface. However, Al concentrations in the remaining metal were typically between 3.5% and 4.0%, so there was a sufficient reservoir of Al remaining in the alloy to prevent simple breakaway corrosion which could have occurred if the Al were significantly depleted. The MA754 lost approximately 15% of its weight and showed void formation within 2 mm of the gas metal surfaces. Within the porous area, the Cr had largely segregated into oxide precipitates up to 50 9m in diameter, leaving the remaining metal Ni-rich. Below the porous layer, the alloy composition was relatively unchanged. Remains of Na- and Al-rich particles that had impacted the surface sporadically were visible but had not obviously affected the surface scale as they had with the MA956.

36 MATERIALS SCIENCE↗

Chemical Characterization and Reactivity Testing of Fuel-Oxidizer Reaction Product (Test Report)

The product of incomplete reaction of monomethylhydrazine (MMH) and nitrogen tetroxide (NTO) propellants, or fuel-oxidizer reaction product (FORP), has been hypothesized as a contributory cause of an anomaly which occurred in the chamber pressure (PC) transducer tube on the Reaction Control Subsystem (RCS) aft thruster 467 on flight STS-51. A small hole was found in the titanium-alloy PC tube at the first bend below the pressure transducer. It was surmised that the hole may have been caused by heat and pressure resulting from ignition of FORP. The NASA Johnson Space Center (JSC) White Sands Test Facility (WSTF) was requested to define the chemical characteristics of FORP, characterize its reactivity, and simulate the events in a controlled environment which may have lead to the Pc-tube failure. Samples of FORP were obtained from the gas-phase reaction of MMH with NTO under laboratory conditions, the pulsed firings of RCS thrusters with modified PC tubes using varied oxidizer or fuel lead times, and the nominal RCS thruster firings at WSTF and Kaiser-Marquardt. Fourier transform infrared spectroscopy (FTIR), differential scanning calorimetry (DSC), accelerating rate calorimetry (ARC), ion chromatography (IC), inductively coupled plasma (ICP) spectrometry, thermogravimetric analysis (TGA) coupled to FTIR (TGA/FTIR), and mechanical impact testing were used to qualitatively and quantitatively characterize the chemical, thermal, and ignition properties of FORP. These studies showed that the composition of FORP is variable but falls within a limited range of compositions that depends on the fuel loxidizer ratio at the time of formation, composition of the post-formation atmosphere (reducing or oxidizing), and reaction or postreaction temperature. A typical composition contains methylhydrazinium nitrate (MMHN), ammonium nitrate (AN), methylammonium nitrate (MAN), and trace amounts of hydrazinium nitrate and 1,1-dimethylhydrazinium nitrate. The thermal decomposition reactions of FORP compositions used in this study were unremarkable, Neither the various compositions of FORP, the pure major components of FORP, nor mixtures of FORP with propellant-system corrosion products showed any unusual thermal activity when decomposed under laboratory conditions. Off-limit thruster operations were simulated by rapid mixing of liquid MMH and liquid NTO in a confined space. The test hardware was constructed with pressure- and temperature-measurement devices to determine if the expected fuel oxidizer reaction would result in increased energy release when FORP, FORP constituents, or propellant-system corrosion products were present. These tests demonstrated that FORP, MMHN, AN, or Inconel corrosion products can induce a mixture of MMH and NTO to produce component-damaging energies. The simulation-test program was not extensive enough to provide statistical probabilities for these events but did show that such events can occur. Damaging events required FORP or metal salts to be present at the initial mixing of MMH and NTO. Based on the results of these studies, it is suggested that removal or mitigation of a buildup of these materials may decrease the incidence of these high-energy, potentially damaging events.

Source record↗

Best Practices for Shielding Analyses of Activated Metals and Spent Resins from Reactor Operation

This report investigated best practices for performing shielding evaluations of Type B waste packages, as defined in 10 CFR Part 71 regulations on packaging and transportation of radioactive material, or packages for which the contents are not defined before loading and may include a broad range of nuclides, geometries, and non-fuel materials. The following non-fuel waste streams were analyzed: Activated metals from decommissioned commercial power reactors, including Type 304 stainless steel, reactor vessel steel, and Inconel, Control blades from boiling water reactors, Neutron-activated corrosion products on surfaces of activated metals, and Spent resins from power plant operations. Measured elemental compositions, including major constituents and impurities, for steel and Inconel samples from commercial power reactors were used in activation calculations to determine radionuclide inventories in activated metals. For a simplified cask model, 60 Co contribution to the total external package dose rate at 30 days after shutdown varied from approximately 60% to 95%, depending on the activated metal, initial cobalt impurity concentration in the metal, and the thickness of the overpack gamma shield. Its maximum contribution to the total external package dose rate of approximately 100% was reached within the time interval of 2 to 5 years after shutdown and was maintained for up to 45 to 60 years after shutdown, depending on material, initial cobalt impurity concentration, and shield thickness. Thereafter, the 60 Co contribution to external package dose rate decreased with increasing decay time. Cobalt-60 is primarily produced by neutron reactions with the cobalt impurity in steel and Inconel. Other important radionuclides in activated metals contributing to package external dose rate are radionuclides with relatively short decay times, including 51 Cr, 59 Fe, 58 Co, and 54 Mn. These radionuclides may be represented as an equivalent 60 Co activity/source because 60 Co gamma ray emissions are bounding in terms of source strength and energy to other important radionuclides identified in the analyzed activated metals. Approaches for modeling the neutron-activated corrosion products that may be attached to activated reactor components were analyzed in this report. It was demonstrated that a surface source is more conservative than a uniform volumetric source for the treatment of neutron-activated corrosion products with respect to external package dose rates. An analysis of the maximum radionuclide loadings reported on spent resins identified the radionuclides 137 Cs, 60 Co, 134 Cs, 65 Zn, and 58 Co as the primary contributors to external package dose rate. For a resin cooled for 3.08 years, the external package dose rate was entirely produced by the reported 137 Cs and 60 Co inventory. The neutron sources from actinides found on spent resins or activated metals produced negligible dose rates and may be ignored in dose rate analyses. Effects of idealized waste material, source geometry, and spatial material/source distributions on external package dose rates were determined based on dose rate results for a simplified cask model under normal conditions of transport. Type 304 stainless steel, zirconium, and aluminum with adjusted mass densities based on a maximum content weight were analyzed for material modeling effects on external package dose rate. These materials produced identical external package dose rates within the statistical uncertainties of the dose rate estimates. Among four different source geometry configurations with homogeneous material of different mass densities, uniform volumetric source distribution, and the same source strength, the geometry configuration with lowest mass density (i.e., minimum self-shielding effect among the four cases) was most conservative. Spatial source distributions that better represent localized peak 60 Co activity values were more conservative than a uniform volumetric source distribution, assuming the same weight and total source strength per package. The increase in external dose rate caused by localized source peaks can be as much as the ratio between source peak activity density to average activity density, depending on the location of the activated metal with peak activity density. Therefore, the shielding analysis may be simplified if localized peak activities and the average activity per package can be measured/determined and documented at the time of cask loading. For simplicity, external package dose rates may be determined based on average source activity and a uniform volumetric source distribution. The dose rate results from that calculation model multiplied by the ratio of peak activity density to average activity density will produce maximum dose rate values for conservative estimates.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Corrosion Behavior of Q235 Steel Exposed in Deepwater of South China Sea

For the first time, the corrosion behavior of Q235 steel in 1200, 2000 and 3000 m deepwater of South China Sea for 0.5 year was reported in this study. The corrosion morphology and corrosion products properties were investigated using different techniques, such as 3D optical microscope, scanning electron microscope, x-ray diffraction analyzer and electrochemical impedance spectroscopy. The main environmental factors influencing the corrosion rate of Q235 in deep sea were discussed by applying gray relational analysis. The results indicated that uniform thinning occurred after exposure. A large number of tiny pits were distributed under the corrosion products with a two-layer structure. The corrosion rate and average pitting depth of samples exposed at 2000 m were lower than those exposed at 1200 and 3000 m, and the main environmental factors determining the variation of corrosion rate at different depths were temperature and dissolved oxygen concentration. Hydrostatic pressure had slight effect on the corrosion rate of Q235 steel, but promoted the formation of a more uniform corrosion morphology.

36 MATERIALS SCIENCE↗

Corrosion Resistance of Cu-Ni-Si Alloy Under High-Temperature, High-Pressure H{sub 2}S and Cl{sup −} Environments

In this study, Cu-Ni-Si alloy was subjected to corrosion resistance tests under simulated high-temperature, high-pressure H{sub 2}S and Cl{sup −} environments. The corrosion rates, electrochemical performance, surface morphologies, and chemical compositions of the Cu-Ni-Si alloy after corrosion were analyzed by the mass loss method, electrochemical impedance spectroscopy, scanning electron microscopy, energy-dispersive x-ray spectrometry, and x-ray diffraction. The results showed that, at the initial stage of corrosion, because of the loose corrosion product layer initially formed on the surface, a high corrosion rate was observed for the Cu-Ni-Si alloy under high-temperature, high-pressure environments. With the progress of corrosion, the corrosion rate gradually decreased and reached a steady state. Because at the later stage, a passive film was formed on the alloy surface, further inhibiting the corrosion of the alloy and improved its corrosion resistance. The Cu-Ni-Si alloy exhibited good corrosion resistance under high-temperature, high-pressure H{sub 2}S and Cl{sup −} environments.

36 MATERIALS SCIENCE↗

Liquid Interfacial Electron Microscopy Identifies Nanogalvanic Corrosion in Pearlitic Steel

The nanoscale mechanisms of localized corrosion in low carbon steels have remained elusive due to the complexity of studying the degradative material behavior at nanoscale solid-liquid interfaces. We identified various steps in the nanogalvanic corrosion processes using in-situ liquid-cell scanning transmission electron microscopy (STEM) using a microfluidic holder by Hummingbird Scientific. Initial work, performed at low magnification, identified the initiation point on a 1018 low-carbon steel surface. This initiation point was determined to be a triple junction of two ferrite grains bridging a cementite grain in contact with a baseline electrolyte of 6 uM CO2 dissolved in a buffered (2.78 uM Na2SO4) aqueous solution, pH 6.1. The pre-etched low-carbon steel surface was prepared using focused ion beam lift-out procedures to extract a cross-section of the low-carbon steel surface, which then was thinned to about 150 nm and transferred to a SiN membrane microfluidic window. The transfer was made using a lift-out needle to attach the low-carbon steel lamella to the corner of the SiN window, and then Pt/C deposition held the lamella in contact with the window while it was released from the lift out needle. To identify the triple point on the low carbon steel lamella, prior to attachment on the SiN window, the sample was characterized for compositional variations with energy dispersive x-ray spectroscopy mapping, grain orientation and phase mapping with precession electron diffraction, and thickness mapping with energy filtered transmission electron microscopy. This pre-characterization prior to the in-situ experiment provided a map of the multiphase and multigrain structure, where the in-situ liquid cell imaging provided a clear understanding of the initiation point on the sample. These data were cross-correlated to paint a holistic picture of the triple junction site, enabling low electron-fluence in-situ snapshot imaging to avoid dominating the native corrosion reactions with effects from the incident electron beam. This initial result identified that localized, nanogalvanic corrosion at the phase interface was the dominant corrosion process in the low-carbon steel, so we next targeted the observation of an array of these nanogalvanic features phase boundaries in a pearlite grain. Near-surface ferrite/cementite phase interfaces that typify pearlitic low-carbon steel were extracted, pre-characterized, and imaged for the in-situ corrosion processes. The sample was a cross-section from a pearlite grain, with alternating ferrite and cementite grains that extended microns down from the pre-etched low-carbon steel pipe surface. After contact with a buffered aqueous solution, the phase boundaries between the ferrite and cementite began to dissolve, with observable material loss and thickness changes in the dark-field and bright-field STEM images. Within minutes, the corrosion front proceeded deeper into the material, claiming a thin layer of ferrite around all exposed phase boundaries before progressing laterally into the ferrite matrix, converting the ferrite to corrosion product normal to each buried cementite grain. Formation of the corrosion product causes a volumetric expansion, creating a lateral wedging force that mechanically ejects the cementite grains from their grooves and leaves behind percolation channels into the steel substructure. Rapid and deleterious, this nanogalvanic corrosion pathway represents an important target for understanding and preventing run-away degradation in this common building material. Observation of this corrosion mechanism was enabled by the combination of pre-characterization using standard structural, grain, and compositional analysis in the TEM, which provides maps for understanding the reaction propagation captured in low-dose, in-situ, liquid-cell STEM.

corrosion↗

Corrosion Mechanism and Applicability Assessment of N80 and 9Cr Steels in CO{sub 2} Auxiliary Steam Drive

Corrosion tests were conducted in a high-temperature high-pressure (HTHP) autoclave to simulate the conditions of CO{sub 2} auxiliary steam drive in gas injection wells. Weight loss tests were performed with the sheets of N80 and 9Cr steels under the testing conditions. The morphology and composition of corrosion products were explored by SEM, EDS, XRD and XPS. The corrosion resistance of 9Cr steel was better than that of N80 steel under the testing conditions. The corrosion rates of N80 and 9Cr met the application requirements in CO{sub 2} auxiliary steam drive. The results broke the constraint in ISO-15156 standards. The corrosion process of N80 steel was mainly affected by the flow velocity. However, the corrosion process of 9Cr steel was mainly affected by temperature. The corrosion resistance of 9Cr steel depended on the FeCO{sub 3} content of Cr-rich layer, which was closely related to temperature. The low flow velocity influenced the diffusion process of N80 steel corrosive ions, whereas the high flow velocity influenced the integrity of corrosion scales. Considering the influence of flow velocity on the corrosion of tubing and casing, in the gas injection well, 9Cr steel and N80 steel were, respectively, selected as the materials of tubing and casing.

36 MATERIALS SCIENCE↗

Hydrochlorination of Uranium Dioxide in a Molten Salt Mixture- Phase 2: Sparged Benchtop Reaction Vessel Experiment

In 2023, Metatomic® Inc., a South Carolina based company, was awarded a Gateway for Advanced Innovation in Nuclear (GAIN) research voucher for a proposed series of experiments aimed at demonstrating the viability of a spent nuclear fuel (SNF) recycling process patented by Metatomic Inc. For the GAIN voucher, Metatomic Inc. selected Savannah River National Laboratory (SRNL) as a partner in executing the proposed proof-of-concept experiments. This report outlines the proof-of-concept experiments performed by SRNL for Metatomic Inc. during Phase 2 (of 2) experimentation. Though Phase 1 provided evidence of successful hydrochlorination, Phase 2 highlighted the nuances and challenges associated with scaling the reaction. The target UCl 4 species generated by the hydrochlorination of UO 2 generates water, which consumes UCl 4 . Compared to the single datapoint obtained at the end of the Phase 1 experiments, data collected at multiple timepoints during Phase 2 experiments indicated a presumed maximum percent conversion of 23% for this system that is likely influenced by water generation. Engineering improvements might be able to increase the percent conversion, but not likely to the degree needed for successful implementation of the technology. Moisture also presents an issue for the Hastelloy C276 reaction vessel. Eventually, corrosion will compromise the integrity of the reaction vessel, and the corrosion products could potentially affect the hydrochlorination chemistry. The presence of corrosion products, which were not produced in the Phase 1 alumina crucible, can and have created challenges when analyzing samples.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Comparison of Crevice Corrosion of Fe-Based Amorphous Metal and Crystalline Ni-Cr-Mo Alloy

The crevice corrosion behaviors of an Fe-based bulk metallic glass alloy (SAM1651) and a Ni-Cr-Mo crystalline alloy (C-22) were studied in 4M NaCl at 100 C with cyclic potentiodynamic polarization and constant potential tests. The corrosion damage morphologies, corrosion products and the compositions of corroded surfaces of these two alloys were studied with optical 3D reconstruction, Scanning Electron Microscopy (SEM), Energy Dispersive Spectroscopy (EDS) and Auger Electron Spectroscopy (AES). It was found that the Fe-based bulk metallic glass (amorphous alloy) SAM1651 had a more positive breakdown potential and repassivation potential than crystalline alloy C-22 in cyclic potentiodynamic polarization tests and required a more positive oxidizing potential to initiate crevice corrosion in constant potential test. Once crevice corrosion initiated, the corrosion propagation of C-22 was more localized near the crevice border compared to SAM1651, and SAM1651 repassivated more readily than C-22. The EDS results indicated that the corrosion products of both alloys contained high amount of O and were enriched in Mo and Cr. The AES results indicated that a Cr-rich oxide passive film was formed on the surfaces of both alloys, and both alloys were corroded congruently.

36 MATERIALS SCIENCE↗

Laser diagnostics for NTP fuel corrosion studies

Viewgraphs and explanations on laser diagnostics for nuclear thermal propulsion (NTP) fuel corrosion studies are presented. Topics covered include: NTP fuels; U-Zr-C system corrosion products; planar laser-induced fluorescence (PLIF); utilization of PLIF for corrosion product characterization of nuclear thermal rocket fuel elements under test; ZrC emission spectrum; and PLIF imaging of ZrC plume.

Wantuck, Paul J.↗

Electrochemical Study on the Kinetic Properties of Fe 2+ /Fe, Ni 2+ /Ni, Cr 2+ /Cr and Cr 3+ /Cr 2+ in Molten MgCl 2 -KCl-NaCl Salts

Here, the fundamental kinetic parameters of corrosion product ions (Fe, Ni and Cr ions) are of significant importance to understand the corrosion mechanisms of the structural materials in the molten salts. In the present study, the fundamental data of Fe 2+ , Ni 2+ , Cr 2+ and Cr 3+ (diffusion coefficient D, exchange current density i 0 , charge transfer coefficient α, limiting current density i L and standard rate constant k0) were measured at different concentrations (1.53 × 10 –6 –7.48 × 10 –4 mol cm –3 ) and temperatures (600 °C–800 °C). The values of D are independent of concentrations and follow Arrhenius law with temperature, which descend in the order of D Cr 2+ > D Fe 2+ > D Cr 3+ > D Ni 2+ with values ranging from 0.94 × 10 –5 to 3.31 × 10 –5 cm 2 s –1 . Both i 0 and k 0 depend on the temperatures, which also follow Arrhenius law.

14 SOLAR ENERGY↗

Atmospheric Corrosion Behavior and Mechanism of a Ni-Advanced Weathering Steel in Simulated Tropical Marine Environment

Corrosion behavior of Ni-advanced weathering steel, as well as carbon steel and conventional weathering steel, in a simulated tropical marine atmosphere was studied by field exposure and indoor simulation tests. Meanwhile, morphology and composition of corrosion products formed on the exposed steels were surveyed through scanning electron microscopy, energy-dispersive x-ray spectroscopy and x-ray diffraction. Results indicated that the additive Ni in weathering steel played an important role during the corrosion process, which took part in the formation of corrosion products, enriched in the inner rust layer and promoted the transformation from loose γ-FeOOH to dense α-FeOOH. As a result, the main aggressive ion, i.e., Cl{sup −}, was effectively separated in the outer rust layer which leads to the lowest corrosion rate among these tested steels. Thus, the resistance of Ni-advanced weathering steel to atmospheric corrosion was significantly improved in a simulated tropical marine environment.

36 MATERIALS SCIENCE↗

Engineering Glass Passivation Layers -Model Results

The immobilization of radioactive waste into glass waste forms is a baseline process of nuclear waste management not only in the United States, but worldwide. The rate of radionuclide release from these glasses is a critical measure of the quality of the waste form. Over long-term tests and using extrapolations of ancient analogues, it has been shown that well designed glasses exhibit a dissolution rate that quickly decreases to a slow residual rate for the lifetime of the glass. The mechanistic cause of this decreased corrosion rate is a subject of debate, with one of the major theories suggesting that the decrease is caused by the formation of corrosion products in such a manner as to present a diffusion barrier on the surface of the glass. Although there is much evidence of this type of mechanism, there has been no attempt to engineer the effect to maximize the passivating qualities of the corrosion products. This study represents the first attempt to engineer the creation of passivating phases on the surface of glasses. Our approach utilizes interactions between the dissolving glass and elements from the disposal environment to create impermeable capping layers. By drawing from other corrosion studies in areas where passivation layers have been successfully engineered to protect the bulk material, we present here a report on mineral phases that are likely have a morphological tendency to encrust the surface of the glass. Our modeling has focused on using the AFCI glass system in a carbonate, sulfate, and phosphate rich environment. We evaluate the minerals predicted to form to determine the likelihood of the formation of a protective layer on the surface of the glass. We have also modeled individual ions in solutions vs. pH and the addition of aluminum and silicon. These results allow us to understand the pH and ion concentration dependence of mineral formation. We have determined that iron minerals are likely to form a complete incrustation layer and we plan to look more closely at Vivianite [Fe3(PO4)2-8(H2O)] and Siderite [FeCO3] in the next stage of the project.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Ce post-treatment for increased corrosion resistance of AA2024-T3 anodized in tartaric-sulfuric acid

Here, the effect of a post-treatment for short time in 50 mM Ce(NO 3 ) 3 solution, with or without H 2 O 2 , on the corrosion of AA2024-T3 anodized in tartaric-sulfuric acid was investigated. Electrochemical (EIS, polarization curves) and corrosion (immersion) tests showed improved performance for samples post-treated at 50 °C in the H 2 O 2 containing solution. Microstructural characterization (SEM, STEM, GDOES) evidenced the presence of Ce oxyhydroxides both at the surface and within the pores of the anodized layer, and their preferential interaction with defective sites both at micro and nanoscale. Important amounts of Ce-species were found near corrosion products, indicating active corrosion protection by Ce ions.

36 MATERIALS SCIENCE↗

Criticality effect of long-term changes in material compositions and geometry in disposal canisters

For the Swedish final repository the basic requirement concerning margin to criticality is that k{sub eff} should be less than 0.95. This criterion is always fulfilled if the disposal canister is dry. If it is assumed that a canister is filled with water it is shown that the criticality criterion is fulfilled using burnup-credit for PWR fuel and credit for burnable poison for BWR fuel. If water is assumed to leak in, long term chemical processes will change the material compositions and geometries in the canister during the one million year analysis period. The main process expected to affect significantly the chemical composition of the materials in the canister is the corrosion of cast iron and carbon steel of the insert, the corrosion of the stainless steel, Inconel or Zircaloy in the fuel element structural material, the corrosion of Zircaloy cladding and finally the corrosion of spent fuel itself. During metal corrosion, various anoxic corrosion products are formed, usually with lower density than the metal itself, causing thus a volume increase in the canister, accompanied by geometrical changes. In this paper the reactivity effects of these changes are analysed and results presented. It is shown that the largest reactivity increase is due to the decrease of the water gap between the fuel and the fuel channel, due to the formation of Magnetite. Other process that possibly will increase the reactivity is if Siderite is produced besides from Magnetite, the production of Hydrogen, corrosion of the fuel and radial movements of fuel rods. (authors)