Search NASA⌕ Search

SEARCH · Search NASA

Results for “Concrete Curing”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Issue Resolution During the Development of the Performance Assessment for the Savannah River Site Saltstone Disposal Facility - 20125

In 2019, Savannah River Remediation developed a revision to the performance assessment (PA) on behalf of the U.S. Department of Energy (DOE) Savannah River Operations Office (SR) for the near-surface disposal of low-level waste at the Savannah River Site (SRS) Saltstone Disposal Facility (SDF). Soluble waste from SRS Tank Farms undergoes salt processing to remove cesium and other high-activity constituents. The low-activity decontaminated salt solution (DSS) is then immobilized by mixing it into a cementitious waste form known as saltstone. After mixing, the saltstone is poured into leak-tight concrete vaults, known as saltstone disposal units (SDUs), where the waste form cures. By the time of facility closure, the SDF is expected to consist of 15 SDUs with a combined capacity of 1.06 E+09 L (280 Mgal) of cured saltstone. The facility operates under a Disposal Authorization Statement from DOE and a permit from the South Carolina Department of Health and Environmental Control (SCDHEC). Since the start of operations in 1990, the SDF has received almost 6.7 E+07 L (18 Mgal) of DSS, resulting in the safe disposal of 2.7 E+16 Bq (7.3 E+05 Ci) of activity. Due to the radioactive decay of short-lived contaminants, the total remaining activity in the disposed waste is estimated to be approximately 1.4 E+16 Bq (3.9 E+05 Ci), as of September 2018. The Disposal Authorization Statement requires a demonstration that the system of engineered and natural features of the disposal facility will limit releases from the facility and be protective of human health and the environment for at least the next 1,000 years. The long-term performance of the facility was evaluated under the requirements of the DoE's Radioactive Waste Management Manual (US DOE Manual 435.1-1). Simulations were performed to demonstrate that the disposal facility would meet performance objectives specified in the manual. The evaluation was based on numerical models that simulate the releases of contaminants from the saltstone waste form. Contaminants were transported through groundwater and air pathways to points of assessment to evaluate compliance (i.e., 100 m from the SDUs). In addition, the potential consequences of an inadvertent human intrusion (IHI) were also evaluated. A number of issues were overcome during the development of these simulations. These issues were identified as part of internal technical reviews. Simulations are developed by people and people make mistakes, so the internal technical review process is a vital step in PA development. Specific examples of resolved issues include a unit-conversion error, an inappropriate definition for a model boundary condition, a model time-stepping issue, and an error in the calculation for the buildup of contaminants in soil. Actions taken to address these issues resulted in an improved product with a better supported technical basis and more defensible results. The identification and correction of these issues are discussed. By understanding these issues, model developers and technical reviewers working on PAs in the future may avoid repeating these types of mistakes. Transparency with respect to these mistakes builds trust between waste management sites, regulators, and stakeholders. (authors)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Update to the Performance Assessment for the Savannah River Site Saltstone Disposal Facility - 20124

In 2019, Savannah River Remediation developed a revision to the performance assessment (PA) on behalf of the U.S. Department of Energy (DOE) Savannah River Operations Office (SR) for the near-surface disposal of low-level waste at the Savannah River Site (SRS) Saltstone Disposal Facility (SDF). Soluble waste from SRS Tank Farms undergoes salt processing to remove cesium and other high activity constituents. The low-activity decontaminated salt solution (DSS) is then immobilized by mixing it into a cementitious waste form known as saltstone. After mixing, the saltstone is poured into leak-tight concrete vaults, known as saltstone disposal units (SDUs), where the waste form cures. By the time of facility closure, the SDF is expected to consist of 15 SDUs with a combined capacity of 1.06 E+09 L (280 Mgal) of cured saltstone. The facility operates under a Disposal Authorization Statement (DAS) from DOE and a permit from the South Carolina Department of Health and Environmental Control (SCDHEC). Since the start of operations in 1990, the SDF has received almost 6.7 E+07 L (18 Mgal) of DSS, resulting in the safe disposal of 2.7 E+16 Bq (7.3 E+05 Ci) of activity. Due to the radioactive decay of short-lived contaminants, the total remaining activity in the disposed waste is estimated to be approximately 1.4 E+16 Bq (3.9 E+05 Ci), as of September 2018. The Disposal Authorization Statement requires a demonstration that the system of engineered and natural features of the disposal facility will limit releases from the facility and be protective of human health and the environment for at least the next 1,000 years. The long-term performance of the facility was evaluated under the requirements of the DoE's Radioactive Waste Management Manual (US DOE Manual 435.1-1). Simulations were performed to demonstrate that the disposal facility would meet performance objectives specified in the manual. The evaluation was based on numerical models that simulate the releases of contaminants from the saltstone waste form. Contaminants were transported through groundwater and air pathways to points of assessment to evaluate compliance. In addition, the potential consequences of an inadvertent human intrusion (IHI) were also evaluated. In accordance with the guidance and recommendations in US DoE's technical standard for DAS, deterministic and probabilistic analyses were performed to demonstrate the SDF system, which includes the engineered cover system, the SDUs, the waste form, and the natural features of the site, provides a reasonable expectation that saltstone disposal will meet performance objectives. Post-closure doses to future members of the public (MOP) were evaluated; dose estimates from the air pathway were well below the 1.0 E-04 Sv/yr (10 mrem/yr) performance objective within 1,000 years, and the calculated doses to the MOP from all exposure pathways, including the groundwater and air pathways, were well below the 2.5 E-04 Sv/yr (25 mrem/yr) performance objective within 1,000 years. Doses following an assumed intrusion event within the facility boundaries were well below the IHI performance objectives, where the acute IHI dose was below the acute IHI dose performance objective of 5.0 E-03 Sv (500 mrem) and the chronic IHI dose was below the chronic IHI dose performance objective of 1.0 E-03 Sv/yr (100 mrem/yr) within 1,000 years. (author)

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Nondestructive detection and characterization of carbonation in concrete

Exposure of concrete to the environment leads to changes in composition, microstructure, and properties; these effects often start from the surface of a concrete structure. A specific, widespread environmental effect is carbonation, where carbon dioxide penetrates the surface of concrete and reacts with calcium hydroxide that is a product of Portland cement hydration in concrete. Carbonation is of interest not only because it can lead to the initiation of reinforcement corrosion, but also carbon is increasingly used during curing to alter the surface properties of cement-based materials as a method to 'sink' carbon in cement-based materials. Nonlinear Rayleigh surface wave measurements are performed on uncarbonated and carbonated concrete samples to assess any mechanical changes induced by carbonation,. In order to minimize the effects of contact conditions, the generated signals are detected by a noncontact air-coupled transducer (100 kHz) at locations along the propagation axis. The nonlinearity parameter, β is used to quantitatively characterize the degree of carbonation. To more accurately analyze the data, corrections are made for the effects of attenuation and diffraction. A comparison between the carbonated and uncarbonated samples demonstrates that pores and micro-cracks are affected by the carbonation product and these significantly change the measured nonlinearity parameter.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Determining the water-cement ratio, cement content, water content and degree of hydration of hardened cement paste: Method development and validation on paste samples

We propose a new method to estimate the initial cement content, water content and free water/cement ratio (w/c) of hardened cement-based materials made with Portland cements that have unknown mixture proportions and degree of hydration. This method first quantifies the composition of the hardened cement paste, i.e. the volumetric fractions of capillary pores, hydration products and unreacted cement, using high-resolution field emission scanning electron microscopy (FE-SEM) in the backscattered electron (BSE) mode and image analysis. From the obtained data and the volumetric increase of solids during cement hydration, we compute the initial free water content and cement content, hence the free w/c ratio. The same method can also be used to calculate the degree of hydration. The proposed method has the advantage that it is quantitative and does not require comparison with calibration graphs or reference samples made with the same materials and cured to the same degree of hydration as the tested sample. This paper reports the development, assumptions and limitations of the proposed method, and preliminary results from Portland cement pastes with a range of w/c ratios (0.25-0.50) and curing ages (3-90 days). We also discuss the extension of the technique to mortars and concretes, and samples made with blended cements.

36 MATERIALS SCIENCE↗

Development of high-early-strength fiber-reinforced self-compacting concrete

High-early-strength fiber-reinforced self-compacting concrete (FRSCC) is a practical material for the precast concrete industry to double its production capacity. In this study, we developed high-early-strength FRSCC mixtures that achieved a compressive and flexural strength of at least 24 MPa and 3.5 MPa, respectively, at 6 h, using commercially available components, typical mixing procedures, and air curing. A mix design process was developed based on the literature and experimental results. The effect of six different fiber reinforcements on the fresh and mechanical properties of concrete was analyzed. The cost limit was set at 523 USD/m 3 to make the concrete mix cost-effective.

36 MATERIALS SCIENCE↗

HYDRAULIC AND PHYSICAL PROPERTIES OF MCU SALTSTONE

The Saltstone Disposal Facility (SDF), located in the Z-Area of the Savannah River Site (SRS), is used for the disposal of low-level radioactive salt solution. The SDF currently contains two vaults: Vault 1 (6 cells) and Vault 4 (12 cells). Additional disposal cells are currently in the design phase. The individual cells of the saltstone facility are filled with saltstone., Saltstone is produced by mixing the low-level radioactive salt solution, with blast furnace slag, fly ash, and cement or lime to form a dense, micro-porous, monolithic, low-level radioactive waste form. The saltstone is pumped into the disposal cells where it subsequently solidifies. Significant effort has been undertaken to accurately model the movement of water and contaminants through the facility. Key to this effort is an accurate understanding of the hydraulic and physical properties of the solidified saltstone. To date, limited testing has been conducted to characterize the saltstone. The primary focus of this task was to estimate the hydraulic and physical properties of MCU (Modular Caustic Side Solvent Extraction Unit) saltstone relative to two permeating fluids. These fluids included simulated groundwater equilibrated with vault concrete and simulated saltstone pore fluid. Samples of the MCU saltstone were prepared by the Savannah River National Laboratory (SRNL) and allowed to cure for twenty eight days prior to testing. These samples included two three-inch diameter by six inch long mold samples and three one-inch diameter by twelve inch long mold samples.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Assessment and prediction of drying shrinkage cracking in bonded mortar overlays

Restrained drying shrinkage cracking was investigated on composite beams consisting of substrate concrete and bonded mortar overlays, and compared to the performance of the same mortars when subjected to the ring test. Stress development and cracking in the composite specimens were analytically modeled and predicted based on the measurement of relevant time-dependent material properties such as drying shrinkage, elastic modulus, tensile relaxation and tensile strength. Overlay cracking in the composite beams could be very well predicted with the analytical model. The ring test provided a useful qualitative comparison of the cracking performance of the mortars. The duration of curing was found to only have a minor influence on crack development. This was ascribed to the fact that prolonged curing has a beneficial effect on tensile strength at the onset of stress development, but is in the same time not beneficial to the values of tensile relaxation and elastic modulus. -- Highlights: •Parameter study on material characteristics influencing overlay cracking. •Analytical model gives good quantitative indication of overlay cracking. •Ring test presents good qualitative indication of overlay cracking. •Curing duration has little effect on overlay cracking.

36 MATERIALS SCIENCE↗

Making A Precisely Level Floor

Floor-pouring procedure yields large surface level, smooth, and hard. Floor made of self-leveling, slow-curing epoxy with added black pigment. Epoxy poured to thickness no greater than 0.33 in. (0.84 cm) on concrete base. Base floor seasoned, reasonably smooth and level, and at least 4 in. (10cm) thick. Base rests on thermal barrier of gravel or cinders and contains no steel plates, dividers, or bridges to minimize thermal distortion. Metal retaining wall surrounds base.

Simpson, William G.↗

Multi-faceted framework for extrapolating early age flexural strength to facilitate rapid lifting/handling of high-volume fly ash precast members

Maintaining adequate early-age structural performance for precast concrete components has grown in importance as more sustainable mix designs become more widespread. Achieving high-early flexural strength is particularly crucial to facilitate rapid removal of hardened concrete components from formwork, often within 24 h after fresh concrete placement. Limited research has assessed the effectiveness of traditional design methods in correlating flexural strength with compressive strength for next-generation mix designs, or demonstrated extrapolation of such material performance to larger-scale structural tests. This paper presents a multi-faceted framework to reassess early-age flexural strength for concretes made with relatively high proportions of fly ash from both fresh and harvested sources. Here, the framework provides several pathways, from which the user can select based upon available resources and the specific application, to improve accuracy of early-age cracking moment calculations. Furthermore, the scope includes evaluation of strength performance under curing conditions emulative of those in a precast facility, recommending modulus of rupture equations which are more performance-driven than current design provisions, and experimental tests on prefabricated concrete beams to validate the proposed methodologies. Correlations of early-age strength with both concrete age and maturity measurements compare the effectiveness of utilizing in-situ data to further enhance the prediction methods. Ultimately, the proposed framework helped reduce errors when calculating cracking moment capacity at early ages by tailoring calculations to reflect mix-dependent behavior. Furthermore, most estimates of cracking moment were within 25 % of their corresponding experimental test results, thus promoting confidence for using these strategies with high-volume fly ash precast structures.

42 ENGINEERING↗

SALTSTONE AND RADIONUCLIDE INTERACTIONS: RADIONUCLIDE SORPTION AND DESORPTION, AND SALTSTONE REDUCTION CAPACITY

The overall objective of this study was to measure a number of key input parameters quantifying geochemical processes in the subsurface environment of the Savannah River Site's (SRS's) Saltstone Facility. For the first time, sorption (K{sub d}) values of numerous radionuclides were measured with Saltstone and Vault 2 concrete. Particular attention was directed at understanding how Tc adsorbs and desorbs from these cementitious materials with the intent to demonstrate that desorption occurs at a much slower rate than adsorption, thus permitting the use of kinetic terms instead of (or along with) the steady state K{sub d} term. Another very important parameter measured was the reduction capacity of these materials. This parameter is used to estimate the duration that the Saltstone facility remains in a reduced chemical state, a condition that maintains several otherwise mobile radionuclides in an immobile form. Key findings of this study follow. K{sub d} values for Am, Cd, Ce, Co, Cs, Hg, I, Np, Pa, Pu, Se, Sn, Tc, U, and Y for Saltstone and Vault 2 concrete were measured under oxidized and reduced conditions. Precipitation of several of the higher valence state radionuclides was observed. There was little evidence that the Vault 2 and Saltstone K{sub d} values differed from previous SRS K{sub d} values measured with reducing grout (Kaplan and Coates 2007). These values also supported a previous finding that K{sub d} values of slag-containing cementitious materials, tend to be greater for cations and about the same for anions, than regular cementitious materials without slag. Based on these new findings, it was suggested that all previous reducing concrete K{sub d} values be used in future PAs, except Np(V) and Pu(IV) K{sub d} values, which should be increased, and I values, which should be slightly decreased in all three stages of concrete aging. The reduction capacity of Saltstone, consisting of 23 wt-% blast furnace slag, was 821.8 microequivalents per gram ({micro}eq/g). This value was approximately the same value as the one measured for 100% blast furnace slag. The cause for this approximately four-fold greater reduction capacity than anticipated is not known, but may be the result of the higher pH of Saltstone (pH {approx}11) compared to blast furnace slag (pH {approx}8), the presence of reducing minerals in the fly ash used to make the Saltstone, or to the Saltstone possibly having semi-conductor properties. These reduction capacity values will result in a near four-fold increase in the estimated duration that the Saltstone facility will remain in a reduced chemical state. The implication of this result is that oxidation-state-sensitive contaminants, such as Pu, Np, and Tc, will remain for a longer duration in a much less mobile form than previously believed. The reduction capacity of vault concrete, which consisted of 10 wt-% blast furnace slag, was 240 {micro}eq/g. Essentially all Am, Cd, Ce, Co, Cs, Hg, Sr, and Y was (ad)sorbed within four hours, whereas <3% of the adsorbed metals desorbed from these solids after 90 hours of continuous leaching. In particular, desorption of Tc (under oxidizing conditions) was >10{sup 3} fold slower than (ad)sorption (under reducing conditions). An important implication of this finding is that if groundwater by-passes or short-circuits the reduction capacity of the Saltstone by flowing along a crack, the ability of the oxygenated water to promote Tc desorption is appreciably less than that predicted based on the K{sub d} value. Relatively low Tc K{sub d} values, 6 to 91 mL/g, were measured in these studies indicating that little if any of the Tc(VII) introduced into the Saltstone or Vault 2 concrete suspensions was reduced to Tc(IV). Such a reduction results in apparent K{sub d} values on the order of 10{sup 4} mL/g. As such, these Tc sorption/desorption experiments need additional investigation to fully represent Saltstone environmental conditions. It is important to understand the limits of these data. They do not provide insight into how radionuclides cured and immobilized in Saltstone will leach from the Saltstone. However they do provide insight into how radionuclides once released into porewater will interact with Saltstone or vault concrete. The use of these site-specific data would greatly improve the pedigree of the input data for the Saltstone performance assessment. Additionally, these studies provided important guidance and technical justification for the conceptual geochemical model to be used in the Saltstone performance assessment.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗

Modelling the interlayer bond strength of 3D printed concrete with surface moisture

Highlights: • An analytical model for interlayer adhesion of 3DPC is proposed based on the amount of surface moisture on the interlayer. • For this mix, the model accurately (RMSE=2.5%) predicts the reduction in interlayer adhesion from 30% to 50%. • Internal curing with superabsorbent polymers increases the interlayer adhesion by 10% and flexural strength by 19%. • SAPs also improve the initial thixotropy by 49% and buildability by 25% compared to the reference. Providing additional water to the hydrating cementitious particles is essential to achieve the optimal mechanical performance of the low w/b concrete mixes preferred for 3D printing. This study incorporates superabsorbent polymers (SAP) and additional water in 3D printed concrete (3DPC) to promote the hydration process through delayed internal water release. The study shows that a retentive SAP modifies the rheological development by absorbing the pore fluid for a short period after printing. The absorption-induced stiffening increases the thixotropy and buildability by 49% and 25%, respectively. A retentive SAP increases the flexural strength and interlayer adhesion by 19% and 10%, respectively. This is due to the internal water release that promotes hydration. Evaporation of the interlayer moisture during the pass time has the opposite effect— evaporation reduces the interlayer adhesion. Based on this assumption, an analytical model is proposed. The model accounts for the pass time, bleeding, and the environmental evaporation rate to estimate the surface moisture and predict the lack of interlayer adhesion. In this study, the model accurately (RMSE = 2.5%) predicted an interlayer adhesion reduction from 30% to 50%. The interlayer adhesion results of other studies could also be predicted.

36 MATERIALS SCIENCE↗

Effect of temperature on the microstructure of calcium silicate hydrate (C-S-H)

Temperature affects the properties of concrete through its effect on the hydration of cement and its associated microstructural development. This paper focuses on the modifications to C-S-H induced by isothermal curing between 5 and 60 °C. The results show that as the temperature increases (within the range studied) the C/S ratio of C-S-H changes only slightly, with a higher degree of polymerisation of silicate chains, but there is a significant decrease in its bound water content and an increase of apparent density of 25%. This increase seems to come from a different packing of C-S-H at the nanoscale. As a consequence of these changes, the microstructure of the cement paste is much coarser and porous, which explains the lower final strengths obtained by curing at elevated temperatures. -- Highlights: •C-S-H structure studied at the atomic level •Multiple analytical techniques used •Studies conducted at temperatures above and below normal temperatures.

36 MATERIALS SCIENCE↗

Calcium Carbonate Cement: A Carbon Capture, Utilization, and Storage (CCUS) Technique

A novel calcium carbonate cement system that mimics the naturally occurring mineralization process of carbon dioxide to biogenic or geologic calcium carbonate deposits was developed utilizing carbon dioxide-containing flue gas and high-calcium industrial solid waste as raw materials. The calcium carbonate cement reaction is based on the polymorphic transformation from metastable vaterite to aragonite and can achieve >40 MPa compressive strength. Due to its unique properties, the calcium carbonate cement is well suited for building materials applications with controlled factory manufacturing processes that can take advantage of its rapid curing at elevated temperatures and lower density for competitive advantages. Examples of suitable applications are lightweight fiber cement board and aerated concrete. The new cement system described is an environmentally sustainable alternative cement that can be carbon negative, meaning more carbon dioxide is captured during its manufacture than is emitted.

36 MATERIALS SCIENCE↗

Diagnosing delayed ettringite formation in concrete structures

There has been a number of cases involving deteriorated concrete structures in North America where there has been considerable controversy surrounding the respective contributions of alkali-silica reaction (ASR) and delayed ettringite formation (DEF) to the observed damage. The problem arises because the macroscopic symptoms of distress are not unequivocal and microscopical examinations of field samples often reveal evidence of both processes making it difficult to separate the individual contributions. This paper presents the results of an investigation of a number of concrete columns carrying a raised expressway in North America; prior studies had implicated both DEF and ASR as possible causes of deterioration. Although the columns were not deliberately heat-cured, it is estimated that the peak internal temperature would have exceeded 70 deg. C and perhaps even 80 deg. C, in some cases. The forensic investigation included scanning electron microscopy with energy-dispersive X-ray analysis and expansion testing of cores extracted from the structure. Small-diameter cores stored in limewater expanded significantly (0.3 to 1.3%) and on the basis of supplementary tests on laboratory-produced concrete specimens it was concluded that expansion under such conditions is caused by DEF as the conditions of the test will not sustain ASR. In at least one column, DEF was diagnosed as the sole contributory cause of damage with no evidence of any contribution from ASR or any other deterioration process. In other cases, both ASR and DEF were observed to have contributed to the apparent damage. Of the columns examined, only concrete containing fly ash appeared to be undamaged. The results of this study confirm that, under certain conditions, the process of DEF (acting in isolation of other processes) can result in significant deterioration of cast-in-place reinforced concrete structures.

36 MATERIALS SCIENCE↗

Microstructural and micromechanical characteristics of ultra-high performance concrete with superabsorbent polymer (SAP)

In this study, the hydration product, C-S-H density, and pore structure at different layers from the drying surface were measured. Besides, the zone affected by the released internal curing water from SAP was identified by assessing the nanoindentation modulus. The results found that the SAP affected the moisture distribution and changed the evaporation and self-desiccation rates in the inner and outer layers. Such imposed moisture gradients affected the micromechanical properties of UHPC at different layers due to the change in the hydration degree of the binder, the density of C-S-H, and the pore structure of the matrix. The addition of SAP improved the hydration dynamics and transferred the LD C-S-H into HD or UHD C-S-H. As the distance from the drying surface increased, the affected zone of SAP increased from 60 to 120 μm, showing the more effectiveness of SAP at inner layers.

36 MATERIALS SCIENCE↗

Low Weight, High Strength Coal-Based Building Materials for Infrastructure Products (Rev.A)

Semplastics has developed, tested, and proven the viability of a new class of composite infrastructure components that use coal as the primary component. Phase I resulted in the production of brick and block components, called X-BRIX and X-BLOX, with dimensions comparable to commercially available bricks and concrete blocks, but with superior mechanical strength, lower weight, greater hardness, improved toughness, greater abrasion resistance, and greater chemical resistance than concrete. Multiple samples of full-size (16” × 8” × 8”) X-BLOX and full-size (8” × 4” × 2.5”) X-BRIX were made to demonstrate the technology, and to support the development of mortar or joining techniques. Phase I moved the coal-based composite materials technology from a current Technology Readiness Level (TRL) of 3 to TRL 5. Semplastics’ coal-based composite materials exhibit a number of high-performance characteristics, including high strength (five times the flexure strength of the best commercial brick, and more than twice the compressive strength of construction-grade concrete block), lower density (by 37 to 41%), improved mechanical durability and abrasion resistance, and resistance to chemicals, acids, salts, and chemical wastewater. These properties offer significant improvements over conventional bricks, concrete blocks, and pavers. The coal particles are completely encapsulated and bonded using a specially formulated polymer-derived ceramic (PDC) that is cured to form an “aggregate” of coal and PDC resin. This aggregate can be further processed and lightly pressed (at 10 to 50 psi) to produce a brick. After pyrolyzing (similar to the processing used to make standard clay bricks), the finished coal-based brick is significantly harder and more abrasion-resistant than regular bricks. We have produced prototype X-BRIX and X-BLOX that contain at least 55% coal by weight (71% carbon by weight, due to the controlled carbon content of the PDC) and showed their superior mechanical properties through in-house and contracted testing.

01 COAL, LIGNITE, AND PEAT↗

Lunar cement and lunar concrete

Results of a study to investigate methods of producing cements from lunar materials are presented. A chemical process and a differential volatilization process to enrich lime content in selected lunar materials were identified. One new cement made from lime and anorthite developed compressive strengths of 39 Mpa (5500 psi) for 1 inch paste cubes. The second, a hypothetical composition based on differential volatilization of basalt, formed a mineral glass which was activated with an alkaline additive. The 1 inch paste cubes, cured at 100C and 100 percent humidity, developed compressive strengths in excess of 49 Mpa (7100 psi). Also discussed are tests made with Apollo 16 lunar soil and an ongoing investigation of a proposed dry mix/steam injection procedure for casting concrete on the Moon.

Lin, T. D.↗

Removable, Sequestration Coatings for Mitigating Hazardous Contaminants Related to Deactivation and Decommissioning Activities

This project is a collaborative effort between InnoSense LLC (ISL) and Oak Ridge National Laboratory (ORNL) aimed at mitigating the mercury (Hg) contamination problem at the Y-12 National Security Complex (NSC). The report summarizes the research and technology development work of the Phase IIB Project, led by Dr. Uma Sampathkumaran at ISL for the period of July 31, 2017–October 31, 2021. The Y-12 site cleanup includes technologies for safe and cost-effective facility demolition, soil remediation, and on-site treatment and disposal of mercury bearing wastes. One of the technology demonstration goals was a reactive strippable coating for targeted pre-demolition and de-contamination to limit Hg mobilization and the volume of debris requiring treatment for disposal. Toward this, ISL has developed a water-based reactive strippable coating (Trap & See-Hg™) to sequester elemental Hg(0) and mercuric Hg(II) species in the coating. The coating provides multiple benefits including (1) Hg vapor suppression, (2) sealing in the hazardous contaminants, (3) visually locating the contaminant through color changes, and (4) remediating the contaminated surfaces upon coating removal. Through collaboration between ORNL and ISL in Phase II work, the team successfully demonstrated the Trap & See-Hg technology to (1) visually locate the presence of Hg on concrete, soil and drywall surfaces, (2) effectively sequester all mercury species (elemental, soluble and insoluble Hg) from lab-generated and ex-situ soil and brick/rubble samples collected from the Y 12 site with 80 to 95% efficiency to capture/reduce Hg vapor concentration, (3) be applied by manual and robotic spray applicators and cure at room ambient, (4) remain a cohesive and peelable coating upon drying, and (5) sequester Hg0 from walls in the alpha-2 building basement at Y-12 during a small scale in-situ field trial. In Phase IIB, ISL’s effort was focused on refining the coating formulations with additives containing passive and reactive sorbents, colorimetric indicator, and thixotropic agents to achieve the desired performance. The paints were then evaluated at ORNL for applicability to metal and concrete surfaces of different sizes and shapes, and soil rubble, Hg-sorption capacity and achieving sag-free coating on surfaces when applied by a manual spray applicator. Ambient cure of the coating resulted in a dry thickness of 16–20 mil. The coatings were removed from smooth or rough surfaces with low to moderate force. Both lab-generated Hg-contaminated samples and soil and brick/rubble samples containing a range of Hg concentrations (collected from the Y-12 site by UCOR) were used in this project. Optimized formulations were applied to these samples and evaluated for ability to suppress Hg vapors, sequester Hg 0 and Hg(II) species and color mapping of mercury species on the test surface. The ORNL team initially identified three to four potential sites at Y-12 and ORNL for potential demonstration. However, the pandemic closed any possible avenues for on-site demonstration of the robotic spray applicator. The metal and concrete samples with low to high Hg content provided by UCOR from an ongoing demolition were subsequently used for ex-situ sample characterization and analysis at ORNL over a period of 25 days. The coatings suppressed Hg vapors with an efficiency of 95–99% from heavily contaminated metal and 60% from concrete substrate. Analysis of total Hg in the peeled paints indicates sorption capacities ranging from 12 µg Hg/g of paint from concrete to 1.2 mg Hg/g of paint from the metal substrates while peeled paints from soil samples could capture a total Hg from 2.3 mg Hg/g to 66 mg/g paint. Toxicity characteristic leaching procedure (TCLP) tests recovered total mercury leached at 0.15±0.0008 µg/L for concrete to 126.81±0.67 µg/L and 377.25±5.67 µg/L for the two metal substrates, to allow for informed decisions on downstream disposal considerations. Together, this Phase IIB demonstrated the potential value of the Trap & See-Hg for Hg uptake, vapor suppression, and color mapping, and may thus be used to enhance worker safety during site cleanup, facility demolition, and downstream waste disposal at Y-12 NSC.

12 MANAGEMENT OF RADIOACTIVE AND NON-RADIOACTIVE W↗