Search NASA⌕ Search

SEARCH · Search NASA

Results for “Degree of polymerization”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Collective Summary of sCO2 Materials Development (Supercritical Transformational Electric Power Generation (STEP) Level 2 Milestone Report) (Parts I - II)

Polymers such as PTFE (polytetrafluorethylene or Teflon), EPDM (ethylene propylene diene monomer) rubber, FKM fluoroelastomer (Viton), Nylon 11, Nitrile butadiene (NBR) rubber, hydrogenated nitrile rubber (HNBR) and perfluoroelastomers (FF_202) are commonly employed in super critical CO 2 (sCO2) energy conversion systems. O-rings and gaskets made from these polymers face stringent performance conditions such as elevated temperatures, high pressures, pollutants, and corrosive humid environments. In FY 2019, we conducted experiments at high temperatures (100°C and 120°C) under isobaric conditions (20 MPa). Findings showed that elevated temperatures accelerated degradation of polymers in sCO2, and that certain polymer microstructures are more susceptible to degradation over others. In FY 2020, the focus was to understand the effect of sCO2 on polymers at low (10 MPa) and high pressures (40 MPa) under isothermal conditions (100°C). It was clear that the same selectivity was observed in these experiments wherein certain polymeric functionalities showed more propensity to failure over others. Fast diffusion, supported by higher pressures and long exposure times (1000 hours) at the test temperature, caused increased damage in sCO2 environments to even the most robust polymers. We also looked at polymers under compression in sCO2 at 100°C and 20 MPa pressure to imitate actual sealing performance required of these materials in sCO2 systems. Compression worsened the physical damage that resulted from chemical attack of the polymers under these test conditions. In FY 2021, the effect of cycling temperature (from 50°C to 150°C to 50°C) for polymers under a steady sCO2 pressure of 20 MPa was studied. The aim was to understand the influence of cycling temperatures of sCO2 for typical polymers under isobaric (20 MPa) conditions. Thermoplastic polymers (Nylon, and PTFE) and elastomers (EPDM, Viton, Buna N, Neoprene, FF202, and HNBR) were subjected to 20 MPa sCO2 pressure for 50 cycles and 100 cycles in separate experiments. Samples were extracted for ex-situ characterization at 50 cycles and upon the completion of 100 cycles. Each cycle constituted of 175 minutes of cycling from 50°C to 150°C. The polymer samples were examined for physical and chemical changes by Dynamic Mechanical and Thermal Analysis (DMTA), Fourier Transform Infrared (FTIR) spectroscopy, and compression set. Density and mass changes immediately after removal from test were measured for degree of swell comparisons. Optical microscopy techniques and micro computer tomography (micro CT) images were collected on select specimens. Evaluations conducted showed that exposures to super-critical CO2 environments resulted in combinations of physical and/or chemical changes. For each polymer, the dominance of cycling temperatures under sCO2 pressures, were evaluated. Attempts were made to qualitatively link the permanent sCO2 effects to polymer micro- structure, free volume, backbone substitutions, presence of polar groups, and degree of crystallinity differences. This study has established that soft polymeric materials are conducive to failure in sCO2 through mechanisms of failure that are dependent on polymer microstructure and chemistry. Polar pendant groups, large atom substitutions on the backbone are some of the factors that are influential structural factors.

36 MATERIALS SCIENCE↗

Hyperbranched PDMAEMA-functionalized SiO 2 microparticles: ATRP polymerization and grafting in a continuous flow reactor

Flow chemistry offers high reaction yield, kinetic control, improved safety, reliability, scalability, and greater degree of process control. Herein, hyperbranched polymer-grafted silica microparticles (HP-SMPs) are synthesized in a commercially available flow reactor through atom transfer radical polymerization. Initiator-anchored silica microparticles are obtained by in situ silanization in the flow reactor. Hyperbranched poly[2-(dimethylamino)ethylmethacrylate] chains are grafted onto the initiator-anchored SMPs through inimer–monomer ratio control. To demonstrate the efficiency and universality of this approach in grafting polymers onto SMPs, multiple hyperbranched polymeric structures are obtained by varying the inimer concentration. Dye absorption test is conducted to demonstrate the potential applications of HP-SMPs.

36 MATERIALS SCIENCE↗

Nanoscale Amorphization of Poly(Triarylamine) for Efficient and Stable Inverted Perovskite Photovoltaics

Perovskite solar modules require hole-selective layers that combine efficient charge extraction, interfacial uniformity and scalable processing. Poly(triarylamine) (PTAA) is widely used in high-performance inverted perovskite photovoltaics, but its nanoscale crystallization and aggregation on indium tin oxide can disrupt film continuity, increase interfacial recombination and limit module stability. Here we show that 4-fluorobenzylphosphonic acid (4FBPA) modifies the surface of indium tin oxide to induce nanoscale amorphization of PTAA, forming a uniform sub-10-nm hole-selective layer. The molecule binds to indium tin oxide through a dehydration reaction, tunes the work function and surface free energy of the photoanode, and improves energy-level alignment with PTAA. The resulting amorphous PTAA film shows enhanced conductivity and hole extraction, suppresses non-radiative recombination at the buried interface and promotes more uniform perovskite growth. Inverted perovskite solar cells reach a power conversion efficiency of 26.63%, while blade-coated modules achieve a certified quasi-steady-state efficiency of 23.01%. The modules retain 95.9% of their initial efficiency after 2,600 hours of maximum-power-point operation under 1-sun illumination at 65 +- 5 degrees C in nitrogen. These results identify nanoscale amorphization of polymeric hole-selective layers as a route to efficient and stable inverted perovskite photovoltaics.

14 SOLAR ENERGY↗

Mechanical, Morphological, and Charge Transport Properties of NDI Polymers with Variable Built‐in Π‐Conjugation Lengths Probed by Simulation and Experiment

Abstract Mechanically deformable polymeric semiconductors are a key material for fabricating flexible organic thin‐film transistors (FOTFTs)—the building block of electronic circuits and wearable electronic devices. However, for many π‐conjugated polymers achieving mechanical deformability and efficient charge transport remains challenging. Here the effects of polymer backbone bending stiffness and film microstructure on mechanical flexibility and charge transport are investigated via experimental and computational methods for a series of electron‐transporting naphthalene diimide (NDI) polymers having differing extents of π‐conjugation. The results show that replacing increasing amounts of the π‐conjugated comonomer dithienylvinylene (TVT) with the π‐nonconjugated comonomer dithienylethane (TET) in the backbone of the fully π‐conjugated polymeric semiconductor, PNDI‐TVT 100 (yielding polymeric series PNDI‐TVT x , 100 ≥x≥ 0), lowers backbone rigidity, degree of texturing, and π–π stacking interactions between NDI moieties. Importantly, this comonomer substitution increases the mechanical robustness of PNDI‐TVT x while retaining efficient charge transport. Thus, reducing the TVT content of PNDI‐TVT x suppresses film crack formation and dramatically stabilizes the field‐effect electron mobility upon bending (e.g., 2 mm over 2000 bending cycles). This work provides a route to tune π–π stacking in π‐conjugated polymers while simultaneously promoting mechanical flexibility and retaining good carrier mobility in FOTFTs.

Chemistry↗

Strengthening poly(lactic acid) composites with poly(methyl methacrylate) functionalized flax nanofibrils

Biobased reinforcements for poly(lactic acid) (PLA) are needed for more additive manufacturing applications requiring higher strength and sustainability. Flax nanofibrils (FNFs) produced through mechanical refining were explored as a lower energy alternative to cellulose nanofibril (CNF) reinforcements. To compatibilize the FNFs for the PLA matrix, a grafting-through surfactant free emulsion polymerization (SFEP) was performed to functionalize the FNF surface with poly(methyl methacrylate) (PMMA). FNFs produced using different refining energy were functionalized under varying solid contents in suspension. Polymerizations performed at 0.7 wt% FNFs in water yielded the highest degree of PMMA functionality. These optimal conditions were scaled up and the PMMA modified FNFs melt compounded into PLA yielding a 12% increase in tensile strength and 92% increase in the modulus of elasticity as compared to the original PLA. Interestingly, the FNFs with the lowest refining energy yielded the strongest composites using these methods, surpassing the higher refining energy CNF reinforcements. This increase was attributed to improved dispersion of the FNF reinforcements in the PLA matrix that was enabled by the PMMA coating on the FNF surface preventing interfibrillar adhesion and aggregation within the PLA matrix.

Mulligan, Abigail [University of Maine]↗

Anhydrous vs Hydrated f-Element Acetate Polymers Dictated by the Stoichiometry of Protic Acidic/Basic Azole Mixtures

Continuing our investigations of ionic liquid (IL) based routes to a library of f-element/soft donor complexes which could be studied crystallographically, we have explored the dissolution of f-element salts in protic imidazole-based ILs containing only soft donors at high temperatures to drive off volatiles, including water and carboxylic or mineral acids. Here we present our results, reacting acidic and basic azoles in 1:3 or 1:1 stoichiometric compositions at elevated temperature, followed by saturation with Nd(OAc) 3 ·xH 2 O or Ce(OAc) 3 ·xH 2 O, which led to 13 new metal–acetate polymeric complexes identified by single-crystal X-ray diffraction. We found that the diversity in coordination modes of the simple acetate ligand that interfere with substitution of the softer N donors led to several readily crystallizable complexes forming two distinct groups with respect to f-element interaction with the ionic liquid precursors. When the acidic/basic azole ratio was 1:3, acetate and a neutral basic azole were found to be coordinated to the metal centers but no water, although in one case (2) water was observed in the secondary coordination sphere: [Ce(μ 2 -OAc) 3 (C 1 im)] n (1, C 1 im = 1-methylimidazole), [Nd(μ 2 -(OAc) 3 (C 1 im)] n ·nH 2 O (2), [Ce(μ 2 -OAc) 3 (C 2 im)] n (3, C 2 im = 1-ethylimidazole), [Ln(μ 2 -OAc) 3 DMF] n (Ln = Nd (4), Ce (5); dimethylformamide (DMF) was substituted for the azole mixture), and [Nd(μ 2 -OAc) 3 (C 4 im)] n (6, C 4 im = 1-butylimidazole). However, when the stoichiometric ratio was 1:1, water was always observed coordinated to the metal ions with the acidic azole included in the structure as a solvate or cocrystal, despite a higher reaction temperature: [Nd(μ 2 -OAc) 3 (OH 2 )] n ·n(1,2,3-Taz) (7, 1,2,3-Taz = 1,2,3-triazole), [Ln(μ 2 -OAc) 3 (OH 2 )] n ·n(4,5-DCim) (Ln = Nd (8), Ce (9), 4,5-DCim = 4,5-dicyanoimidazole), [Ln(μ 2 -OAc) 3 (OH 2 )] n ·n(3,5-diNH 2 -1,2,4-Taz) (Ln = Nd (10), Ce (11), 3,5-diNH 2 -1,2,4-Taz = 3,5-diamino-1,2,4-triazole), [Ce(μ 2 -OAc) 3 (OH 2 )] n ·n(3-NH 2 -1,2,4-Taz) (12, 3-NH 2 -1,2,4-Taz = 3-amino-1,2,4-triazole), and [Nd(μ 2 -OAc) 3 (OH 2 )] n ·n(5-NH 2 -Tz) (13, 5-NH2-Tz = 5-aminotetrazole). All of the compounds retain the Ln:OAc– ratio of 1:3 and form 1D polymeric chains; however, they exhibit a variety of coordination modes affecting the degree of chain condensation. The isolation of both hydrated and anhydrous products revealed different abilities of the investigated soft N-donors to compete with O-donors finding their place in the coordination sphere of the lanthanide or in the crystal lattice.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

The role of interfacial donor–acceptor percolation in efficient and stable all-polymer solar cells

Polymerization of Y6-type acceptor molecules leads to bulk-heterojunction organic solar cells with both high power-conversion efficiency and device stability, but the underlying mechanism remains unclear. Here we show that the exciton recombination dynamics of polymerized Y6-type acceptors (Y6-PAs) strongly depends on the degree of aggregation. While the fast exciton recombination rate in aggregated Y6-PA competes with electron-hole separation at the donor–acceptor (D–A) interface, the much-suppressed exciton recombination rate in dispersed Y6-PA is sufficient to allow efficient free charge generation. Indeed, our experimental results and theoretical simulations reveal that Y6-PAs have larger miscibility with the donor polymer than Y6-type small molecular acceptors, leading to D–A percolation that effectively prevents the formation of Y6-PA aggregates at the interface. Besides enabling high charge generation efficiency, the interfacial D–A percolation also improves the thermodynamic stability of the blend morphology, as evident by the reduced device “burn-in” loss upon solar illumination.

14 SOLAR ENERGY↗

Mechanical Consequences of Oxygen Inhibition in Vat Polymerization

Vat polymerization is a type of additive manufacturing that is used extensively to produce micro-architected structures for mechanical applications, which brings the mechanical properties of photopolymerized resins into sharp focus. However, it is known that photopolymerization is sensitive to a number of factors, perhaps the most notorious of which is oxygen inhibition. Herein, the degree to which oxygen inhibition influences the macroscopic and microscopic properties of structures made using vat polymerization is explored. This work is motivated by an observation of lattices being >4 times softer in the experiment than predicted by simulation, which is hypothesized to be due to the material at the surface being incompletely cured. Furthermore, this hypothesis is supported by four-point bending tests in which flexural modulus is found to increase with beam thickness. Nanoindentation and bulk compression studies show that this surface softening is present for three distinct resins. Importantly, it is observed that structures post-print cured in nitrogen are stiffer than those post-print cured in air, however, regardless of the post-print curing environment, printing samples in the presence of oxygen makes them softer than samples photocured in nitrogen. Collectively, these results show the outsized influence of oxygen inhibition on micro-architected structures realized using vat polymerization.

36 MATERIALS SCIENCE↗

Iron-Catalyzed Cross-[2 + 2] Cycloaddition of Butadiene and α,ω-Dienes for Ductile and Chemically Recyclable Poly(oligocyclobutanes)

Poly(divinyloligocyclobutanes) (pDVOCBs) are a distinct class of butadiene-derived, chemically recyclable polyolefins prepared from iron-catalyzed [2 + 2] cycloaddition followed by ruthenium-catalyzed ADMET polymerization. These polymers are highly crystalline, with high melting temperatures and unique rotator phases. The high degree of crystallinity in these materials not only leads to high stiffness over a broad temperature range but also results in brittle failure for polymers of modest molecular weights. Iron-catalyzed cross-[2 + 2] cycloaddition of butadiene and α,ω-dienes was accomplished, where the number of methylene units between the four-membered rings was systematically varied. Subsequent ADMET polymerization of the resulting telechelic oligomers provided a new class of chemically recyclable polyolefins that exhibit distinct thermomechanical properties. Specifically, methylene units induce changes in crystallinity that, in combination with the increased molecular weight, favored the formation of stable necks upon tensile deformation, with ∼10× enhanced ductility and improved toughness compared to pDVOCB. Through combined experimental and computational studies, the effects of methylene spacers on the crystal-to-rotator transition of the cyclobutane polymers were established. Ultimately, these methylene-modified cyclobutane polymers expand the range of properties and potential applications of this class of recyclable polyolefins.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

High-Fidelity and High-Performance Computational Simulations for Rapid Design Optimization of Sulfur Thermal Energy Storage

Industrial process heating (IPH) accounts for approximately 70% of US manufacturing energy use and is primarily produced by fossil fuel combustion. Approximately 1500 TWht (approximately 60%) of IPH demand is in the temperature range of 100-300. Industrial applications in this temperature range include drying, hydrothermal processing, thermal enhanced oil recovery, food and beverage, bioethanol production, etc. Cost-effective thermal energy storage (TES) that increases the utilization of waste and renewable heat (solar, geothermal, etc.) could provide significant energy savings and reliable heat sources, decrease emissions, and increase US manufacturing competitiveness through reductions in fuel consumption. TES development has historically been dominated by technologies suitable for deployment with concentrating solar power (CSP). State-of-the-art thermal storage deployed commercially with power tower CSP plants uses a 60%/40% NaNO3/KNO3 molten salt and operates between temperatures of approximately 280 degrees Celsius and 570 degrees Celsius using a two-tank configuration. However, these nitrate salts are unsuitable for operation outside of this temperature range due to a high freezing point of approximately 220 degrees Celsius, and limits on high-temperature salt stability and corrosion resistance of containment alloys. Other materials being investigated for TES include those based on: (1) sensible energy storage (various molten salt compositions, inert solid particles, rocks or pebble beds, sulfur, water, concrete, graphite, etc.), (2) latent energy storage in materials that undergo solid-liquid phase change at relevant temperatures (organic materials for low-temperature applications, inorganic salts and/or metals for high-temperature applications), or (3) thermochemical energy storage (hydrides, hydroxides, carbonates, metal oxides, etc.). The application temperature and challenges pertaining to storage material and/or containment cost, energy density, long-term thermal and cyclic stability, and charge/discharge heat transfer effectiveness drive material selection for a given IPH or electricity generation application. Sulfur is a cheap commodity at $80/ton compared to $1100 - 1300/ton for conventional salts. When using a metric of storage cost per kWh, sulfur costs around 2-3 $/kWh. Previous sulfur TES development focused on high temperature (>600 degrees) concentrated solar power applications with sulfur encapsulated in pipes and flow of gaseous HTF (air) in the shell side. However, for lower-temperature IPH applications in the range of approximately 100-300 degrees Celsius Element 16 adopted a compact and scalable TES design with molten sulfur in the shell and HTF pipes submerged in the molten sulfur bath. The low-cost molten sulfur TES for dispatchable IPH has deployment potential for broad applications. The spatial and temporal evolution of the HTF and sulfur temperature is critical to the TES system performance, and thus detailed modeling can improve understanding of the performance and facilitate design improvements. Using high performance computing and computational fluid dynamics (CFD) a low-cost molten sulfur thermal energy storage (TES) system for industrial process heating (IPH) applications was developed. The unique challenges in CFD modeling of sulfur TES are the sharp property changes of sulfur relevant to the working temperatures. Above 159, liquid sulfur undergoes polymerization, and the viscosity of sulfur rapidly increases by several orders of magnitude between 159 degrees Celsius and 188 degrees Celsius, followed by a decrease in viscosity beyond 188 degrees Celsius due to thermal bound dissociation. In addition, various concentrations of H2S impurities can also modify sulfur viscosity. This numerical challenge is especially relevant to transient simulation of the sulfur TES charging and discharging processes as the extreme property variations limit the applicability of traditional heat transfer correlations. Transient CFD simulations including the temperature-dependent sulfur properties and geometric complexity of the TES design were used to predict the effect of natural convection during charging and discharging on the heat transfer process, sulfur temperature uniformity, charge/discharge rates, and performance of the storage devices. The CFD model was validated with experimental results for a full charge and discharge cycle. The work will show 3D and 2D simulation comparisons aimed to facilitate rapid design iterations and a machine learning based design optimization approach.

CFD↗

Solid composites containing polymeric matrix with carbon fibers embedded therein

A functionalized carbon fiber having covalently bound on its surface a partially cured epoxy or amine-containing sizing agent, wherein at least a portion of epoxide or amine groups in the sizing agent are available as uncrosslinked epoxide or amine groups, which corresponds to a curing degree of epoxide or amine groups of no more than about 0.6. Composites comprised of these functionalized carbon fibers embedded in a polymeric matrix are also described. Methods for producing the functionalized carbon fibers and composites thereof are also described.

36 MATERIALS SCIENCE↗

Power Electronics Materials and Bonded Interfaces - Reliability and Lifetime

Advanced packaging technologies are currently being designed and developed by the power electronics industry however, the maximum operating temperature is still limited to 175 degrees Celsius for the silicon carbide devices. Bonded materials such as sintered copper and polymeric materials are potential candidates for high temperature operation, but it is critical to characterize and evaluate its reliability under harsh operating conditions. In this project, we discuss the results of the accelerated experiments conducted on sintered copper and polymeric materials. Additionally, a novel framework to develop the lifetime prediction model of bonded interfaces through employing statistical and machine learning models are described. In this task, scanning acoustic microscope images of bonded interfaces obtained under thermal cycling experiments are used as the data.

ENGINEERING↗

Stretchable and wearable polymeric heaters and strain sensors fabricated using liquid metals

Wearable electronic devices (WEDs) are receiving significant attention because of the increasing interest in soft robotics, electronic skin, and wearable sensors. Liquid metals (LMs) are compelling for WEDs owing to their metallic conductivity, fluidic nature, and low toxicity. For this study, we fabricated stretchable and soft WEDs using LM (eutectic gallium-indium alloy) wires (LMWs) patterned via force wetting through custom-made stencils on an elastic substrate. LMWs can generate thermal energy via Joule heating upon current application and deliver it to the substrate, resulting in wearable polymeric heaters. The LM mixed with carbonyl iron particles (CIPs) can also be patterned while preserving fluidic behavior. The degree of thermal energy generated through the LMWs can be manipulated as a function of the CIP concentration in the LM and geometrical factors of the electrode patterns, i.e., width and length. An elastic film patterned with LMWs attached to the human body exhibits changes in the effective electrical resistance depending on applied strain, demonstrating potential as a wearable strain sensor. This LM utilized WED that can generate thermal energy upon current application through the LMWs and detect the bodily motion has significant potential for application in wearable thermotherapy, electronic skin, and soft sensors.

47 OTHER INSTRUMENTATION↗

Command of active and responsive elastomers by topological defects and patterns

The project resulted in the development of stimuli-responsive elastomer coatings formed by photopolymerized liquid crystal molecules. The molecular orientation of the liquid crystal elastomers is coupled to rubber-like elasticity. The project developed an approach to produce complex patterns of molecular orientation in elastomers by employing photopatterning technique based on plasmonic metamasks that convert unpolarized incoming light into a transmitted light beam with spatially-varying linear polarization. The polarization-modulated light beam aligns the film of azodye molecules, which serves as the substrate for liquid crystal elastomer coating. The alignment of the azodye molecules follows the polarization pattern with a phase shift of the alignment direction by 90 degrees. The azodye substrate imposes orientation of molecules in the adjacent liquid crystal layer which is preserved after the monomers are polymerized into a liquid crystal elastomer. By using differently aligned substrates one could produce various patterns of molecular orientation in the elastomer, which dictate the mechanical properties of the elastomers and their response to external stimuli such as temperature, humidity, and ultraviolet irradiation. In particular, the predesigned molecular orientation produces deterministically defined topography response of the liquid crystal coatings, in which their free surface changes from flat to either locally elevated or locally compressed, depending on whether the pre-inscribed molecular orientation is predesigned with a splay or bend deformation. The research established that the mechanism of this deterministic relation between the dynamic topography and pre-inscribed molecular orientation is rooted in the change of the tensorial order parameter that characterizes the degree of orientational order, and in the contraction/expansion of polymer molecules in response to the order parameter changes. In particular, lowering the order causes contraction of polymer globules. The work demonstrated that the dynamic topography of elastomer coatings with three-dimensional pattern of orientational order includes up and down motion of the material (along the normal to the coating) and also shifts in lateral directions. We demonstrate that the deterministic relationship between the orientational patterns and variations of coatings’ profile is caused by forces that are mathematically equivalent to active forces in the system of “pullers” or “pushers” in active matter, demonstrating universality of the out-of-equilibrium behavior. The project resulted in theoretical models that predictively describe the dynamic response of coatings. The topography of liquid crystal elastomers is sensitive to stimuli such as temperature, ultraviolet irradiation, and humidity. The applicability of the patterned approach to produce dynamic coatings was expanded from nematic elastomers to their smectic counterparts. The project combined a battery of imaging techniques to unveil the dynamic properties of the coatings, ranging from the state-of-the-art dynamic holographic microscopy to fluorescent confocal polarizing microscopy and polscope microscopy. The research uncovered potential applications of dynamic elastomer coatings, such as control placement of colloidal particles, engineering of living tissues with alignment patterns of cells that follow the orientational order of elastomer coatings. The approach developed in the project can be used to design programmable dynamic coatings with functionalities that mimic biological tissues such as skin.

36 MATERIALS SCIENCE↗

Testing and Characterization to Develop a Mechanistic Explanation for Unsaturated Drift of Fiber Optic Sensors during High-Dose Irradiation

The primary limitation for any optical fiber-based sensor for nuclear reactor applications is radiation-induced attenuation (RIA) of the transmitted and/or reflected signals. Based on several recent studies, RIA is tolerable for some fused silica optical fibers with the proper choice of sensing wavelength and fiber dopants. For extreme temperature applications (> 1000°C), sapphire optical fibers have been proposed; however, recent optical transmission measurements performed on bulk sapphire samples showed prohibitively large RIA. For some sensors, radiation-induced dimensional changes in the fiber materials can also cause significant drift. Moreover, the drift that was observed in numerous experiments performed in the High Flux Isotope Reactor (HFIR), the Advanced Test Reactor, the Massachusetts Institute of Technology Reactor, and other international facilities far exceeded what would be expected based on compaction of fused silica glass. Clearly, additional work is needed to better understand the origins of both RIA and radiation-induced drift in both silica and sapphire optical fiber-based sensors before these sensors can be reliably deployed for nuclear applications. This work evaluated the underlying mechanisms that may be responsible for RIA and drift in silica and sapphire materials. First, detailed characterization was performed on bulk fused silica glass samples that were previously irradiated to different neutron fluences at different temperatures to better understand the structural changes that drive radiation-induced drift in the absence of coating effects that are discussed later. Results show that the non-monotonic compaction that occurs with increasing neutron fluence continues up to fast neutron fluences approaching 10 22 n/cm 2 , which has important implications for physics-based models that may be used to compensate for the sensor drift. Initial Raman spectroscopy and synchrotron x-ray diffraction provide insights into the nature of the structural changes. Next, detailed characterizations were performed on silica fibers with various coatings that were subjected to several different thermal treatments. The hypothesis is that the coatings convert to carbon-rich materials that compact under irradiation, putting a large compressive strain on the fiber. Out-of-pile testing confirms that both polyimide and acrylate fiber coatings convert to glassy carbon (GC) materials when heated under inert conditions, and the degree of order (i.e., graphitization) increases with increasing temperature. The results provide increasingly strong evidence that the combination of polymeric coatings and inert (or vacuum) conditions render fiber optic sensors susceptible to significant radiation-induced drift that would not otherwise exist in uncoated fibers. Finally, transmission electron microscopy was performed on bulk sapphire samples that were irradiated to two neutron fluences at different temperatures to gain insights into the potential mechanisms driving the prohibitive RIA at higher neutron fluences and temperatures. Contrary to previous hypotheses, results show that scattering from radiation-induced voids cannot explain the observed RIA. Similarly, models for scattering losses from dislocation loops also do not agree with the experimental results. Instead, fitting to the experimental data shows that increased absorption from aluminum vacancy centers is the most likely explanation for the the prohibitively large RIA that was observed at high irradiation temperature and dose. In addition, the voids that formed in these single-crystal samples were found to align along the basal plane (a-axis) as opposed to that seen in previous observations of c-axis alignment in polycrystalline samples, which could have important implications for anisotropic swelling and other phenomena that could affect sensor performance at high neutron fluence.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Testing and Characterization to Develop a Mechanistic Explanation for Unsaturated Drift of Fiber Optic Sensors during High-Dose Irradiation

The primary limitation for any optical fiber-based sensor for nuclear reactor applications is radiation-induced attenuation (RIA) of the transmitted and/or reflected signals. Based on several recent studies, RIA is tolerable for some fused silica optical fibers with the proper choice of sensing wavelength and fiber dopants. For extreme temperature applications (> 1000°C), sapphire optical fibers have been proposed; however, recent optical transmission measurements performed on bulk sapphire samples showed prohibitively large RIA. For some sensors, radiation-induced dimensional changes in the fiber materials can also cause significant drift. Moreover, the drift that was observed in numerous experiments performed in the High Flux Isotope Reactor (HFIR), the Advanced Test Reactor, the Massachusetts Institute of Technology Reactor, and other international facilities far exceeded what would be expected based on compaction of fused silica glass. Clearly, additional work is needed to better understand the origins of both RIA and radiation-induced drift in both silica and sapphire optical fiber-based sensors before these sensors can be reliably deployed for nuclear applications. This work evaluated the underlying mechanisms that may be responsible for RIA and drift in silica and sapphire materials. First, detailed characterization was performed on bulk fused silica glass samples that were previously irradiated to different neutron fluences at different temperatures to better understand the structural changes that drive radiation-induced drift in the absence of coating effects that are discussed later. Results show that the non-monotonic compaction that occurs with increasing neutron fluence continues up to fast neutron fluences approaching 10 22 n/cm 2 , which has important implications for physics-based models that may be used to compensate for the sensor drift. Initial Raman spectroscopy and synchrotron x-ray diffraction provide insights into the nature of the structural changes. Next, detailed characterizations were performed on silica fibers with various coatings that were subjected to several different thermal treatments. The hypothesis is that the coatings convert to carbon-rich materials that compact under irradiation, putting a large compressive strain on the fiber. Out-of-pile testing confirms that both polyimide and acrylate fiber coatings convert to glassy carbon (GC) materials when heated under inert conditions, and the degree of order (i.e., graphitization) increases with increasing temperature. The results provide increasingly strong evidence that the combination of polymeric coatings and inert (or vacuum) conditions render fiber optic sensors susceptible to significant radiation-induced drift that would not otherwise exist in uncoated fibers. Finally, transmission electron microscopy was performed on bulk sapphire samples that were irradiated to two neutron fluences at different temperatures to gain insights into the potential mechanisms driving the prohibitive RIA at higher neutron fluences and temperatures. Contrary to previous hypotheses, results show that scattering from radiation-induced voids cannot explain the observed RIA. Similarly, models for scattering losses from dislocation loops also do not agree with the experimental results. Instead, fitting to the experimental data shows that increased absorption from aluminum vacancy centers is the most likely explanation for the the prohibitively large RIA that was observed at high irradiation temperature and dose. In addition, the voids that formed in these single-crystal samples were found to align along the basal plane (a-axis) as opposed to that seen in previous observations of c-axis alignment in polycrystalline samples, which could have important implications for anisotropic swelling and other phenomena that could affect sensor performance at high neutron fluence.

46 INSTRUMENTATION RELATED TO NUCLEAR SCIENCE AND ↗

Calcium Sulfate and Calcium Carbonate Scaling of Thin-Film Composite Polyamide Reverse Osmosis Membranes with Surface-Tethered Polyacrylic Acid Chains

The gypsum and calcite scaling propensities of the thin-film composite polyamide (PA-TFC) reverse osmosis (RO) membrane, modified with a tethered surface layer of polyacrylic acid (PAA) chains, was evaluated and compared to the scaling of selected commercial RO membranes. The tethered PAA layer was synthesized onto a commercial polyamide membrane (i.e., base-PA) via atmospheric pressure plasma-induced graft polymerization (APPIGP). The PAA nano-structured (SNS) base-PA membrane (SNS-PAA-PA) was scaled to a lesser degree, as quantified by a lower permeate flux decline and surface imaging, relative to the tested commercial membranes (Dow SW30, Toray SWRO, and BWRO). The cleaning of gypsum-scaled membranes with D.I. water flushing achieved 100% water permeability recovery for both the SNS-PAA-PA and Dow SW30 membranes, relative to 92–98% permeability restoration for the Toray membranes. The calcium carbonate scaling of SNS-PAA-PA membranes was also lower relative to the commercial membranes, but permeability recovery after D.I. water cleaning was somewhat lower (94%) but consistent with the level of surface scale coverage. In contrast, the calcite and gypsum-scaled membrane areas of the commercial membranes post-cleaning were significantly higher than for the SNS-PAA-PA membrane but with 100% permeability recovery, suggesting the potential for membrane damage when mineral scaling is severe.

37 INORGANIC, ORGANIC, PHYSICAL, AND ANALYTICAL CH↗

FROMP-from-Monomer

This repository provides the 1D reaction-diffusion simulation engine for the multi-scale framework. It takes monomer-level kinetic and thermodynamic descriptors as inputs, approximated from quantum chemical calculations, to simulate and predict the macroscopic propagation behavior of Frontal Ring-Opening Metathesis Polymerization (FROMP). By solving a coupled 1D reaction-diffusion PDE system, this tool predicts front propagation speed, front temperature, and degree of conversion. The solver explicitly captures the three fundamental ROMP steps, initiator activation/inhibition, chain initiation, and propagation, while accounting for high-temperature cycloreversion as a competing pathway. The numerical implementation uses FEniCS to handle the coupled heat diffusion and reaction kinetics.

Chua, Lauren [Massachusetts Inst. of Technology (M↗