Search NASASearch

SEARCH · Search NASA

Results for “ELASTIC MODULUS”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Ni-Ti Alloys for Aerospace Bearing Applications

Nickel-rich Ni-Ti alloys are emerging candidate materials for aerospace bearing applications. These alloys exhibit a unique combination of physical, chemical, and tribological properties that are highly relevant to challenging aerospace bearings and other mechanical components. Despite being made solely from metals, Ni-Ti alloys are classified as intermetallics with properties akin to both metals and ceramics. For instance, like metals, they are electrically conductive but they tend to be brittle like ceramics. When properly processed, they have high hardness, low elastic modulus and an extensive elastic deformation range that imparts extraordinarily high resilience and resistance to denting. New alloy compositions enable simpler thermal processing and machining and intensive microstructural analyses have helped elucidate the materials science mechanisms governing hardness. In this paper, the application of state-of-art in NiTi alloys for aerospace bearings and mechanical components is explored. In addition to reviewing future trends and remaining challenges, the unique approaches and methods of tailoring bearing design to accommodate NiTis unique properties is discussed.

intermetallics

Minimum film thickness in elliptical contacts for different regimes of fluid-film lubrication

The film-parameter equations are provided for four fluid-film lubrication regimes found in elliptical contacts. These regimes are isoviscous-rigid; viscous-rigid; elastohydrodynamic of low-elastic-modulus materials, or isoviscous-elastic; and elastohydrodynamic, or viscous-elastic. The influence or lack of influence of elastic and viscous effects is the factor that distinguishes these regimes. The film-parameter equations for the respective regimes come from earlier theoretical studies by the authors on elastohydrodynamic and hydrodynamic lubrication of elliptical conjunctions. These equations are restated and the results are presented as a map of the lubrication regimes, with film-thickness contours on a log-log grid of the viscosity and elasticity parameters for five values of the ellipticity parameter. The results present a complete theoretical film-parameter solution for elliptical contacts in the four lubrication regimes.

Hamrock, B. J.

Mechanical properties of brittle materials

Brittle materials are difficult to tensile test because of gripping problems. They either crack in conventional grips or they are crushed. Furthermore, they may be difficult to make into tensile specimens having, for example, threated ends or donut shapes. To overcome the problem, simple rectangular shapes can be used in bending (i.e., a simple beam) in order to obtain the modulus of rupture and the elastic modulus. The equipment necessary consists of a fixture for supporting the specimens horizontally at two points, these points contact points being rollers which are free to rotate. The force necessary to bend the specimen is produced by a tup attached to the crosshead of an Instron machine. Here, the experimental procedure is explained.

Cornwell, L. R.

Nanotubular Toughening Inclusions

Conventional toughening agents are typically rubbery materials or small molecular weight molecules, which mostly sacrifice the intrinsic properties of a matrix such as modulus, strength, and thermal stability as side effects. On the other hand, high modulus inclusions tend to reinforce elastic modulus very efficiently, but not the strength very well. For example, mechanical reinforcement with inorganic inclusions often degrades the composite toughness, encountering a frequent catastrophic brittle failure triggered by minute chips and cracks. Thus, toughening generally conflicts with mechanical reinforcement. Carbon nanotubes have been used as efficient reinforcing agents in various applications due to their combination of extraordinary mechanical, electrical, and thermal properties. Moreover, nanotubes can elongate more than 20% without yielding or breaking, and absorb significant amounts of energy during deformation, which enables them to also be an efficient toughening agent, as well as excellent reinforcing inclusion. Accordingly, an improved toughening method is provided by incorporating nanotubular inclusions into a host matrix, such as thermoset and thermoplastic polymers or ceramics without detrimental effects on the matrix's intrinsic physical properties.

Park, Cheol

Nanotubular Toughening Inclusions

Conventional toughening agents are typically rubbery materials or small molecular weight molecules, which mostly sacrifice the intrinsic properties of a matrix such as modulus, strength, and thermal stability as side effects. On the other hand, high modulus inclusions tend to reinforce elastic modulus very efficiently, but not the strength very well. For example, mechanical reinforcement with inorganic inclusions often degrades the composite toughness, encountering a frequent catastrophic brittle failure triggered by minute chips and cracks. Thus, toughening generally conflicts with mechanical reinforcement. Carbon nanotubes have been used as efficient reinforcing agents in various applications due to their combination of extraordinary mechanical, electrical, and thermal properties. Moreover, nanotubes can elongate more than 20% without yielding or breaking, and absorb significant amounts of energy during deformation, which enables them to also be an efficient toughening agent, as well as excellent reinforcing inclusion. Accordingly, an improved toughening method is provided by incorporating nanotubular inclusions into a host matrix, such as thermoset and thermoplastic polymers or ceramics without detrimental effects on the intrinsic physical properties of the matrix.

Park, Cheol

Through-Thickness Tensile Properties of Triaxial Braided Composites

The through-thickness strength of triaxial braided composites was measured using thin specimens bonded to metallic tabs. Despite providing reasonable engineering estimates of the bulk properties, some test specimen limitations were noted: For strong epoxies, significant shear and tensile stresses occur and induce failure between the first layer and bond-line; the strains over much of the exterior are ~10% lower than interior strains, which are representative of the nominal state; and failure often occurred near or along the adhesive bond line. These interference were partially overcome by adding a large radius to the gage section. Based on the finite element analysis and experimental measurements, the nominal elastic modulus and Poisson's ratio are E(sub 33) = 10.7 GPa and v(sub 31) = 0.08 for the three triaxial braided composites tested. Strengths vary from 14 to 40 MPa depending on the resin. Relative to the in-plane properties, the through thickness modulus, fracture strength, failure strain, and Poisson's ratio are 1/5th, 1/30th, 1/6th, and 1/4th. Interlaminar failure occurred with varying degrees of fiber tear out along with little damage to axial tows, resulting is a smooth undulating fracture surface. Post cure temperature excursions to 177 deg C (350 deg F) had little effect on elastic constants but reduced the strength E862 based composites severely. The strength of PR520 and 5208 based composites increased.

composite

Composite wall concept for high temperature turbine shrouds: Survey of low modulus strain isolator materials

Plasma sprayed yttria stabilized zirconium oxide turbine seal specimens, incorporating various low modulus porous metal strain isolator pads between the zirconium oxide and a dense metal substrate, were subjected to cyclic thermal shock testing. Specimens that had a low modulus pad composed of sintered FeNiCrAlY fibermetal survived 1000 thermal shock cycles without spalling of the ceramic. A figure of merit for the low modulus pad materials taking into consideration the elastic modulus, thermal conductivity, strength, and oxidation resistance of the pad was proposed, and showed reasonable agreement with the thermal shock results. A potential surface distress problem on the zirconium oxide, associated with nonuniform temperature distribution and rapid stress relaxation was identified. One approach to solving the surface distress problem through application of laser surface fusion of the zirconium oxide layer showed some promise, but improvements in the laser surface fusion process are necessary to prevent process associated damage to the ceramic.

Bill, R. C.

The Effect of Pre-Stressing on the Static Indentation Load Capacity of the Superelastic 60NiTi

Superelastic nickel-titanium alloys, such as 60NiTi (60Ni-40Ti by wt.%), are under development for use in mechanical components like rolling element bearings and gears. Compared to traditional bearing steels, these intermetallic alloys, when properly heat-treated, are hard but exhibit much lower elastic modulus (approx.100 GPa) and a much broader elastic deformation range (approx.3 percent or more). These material characteristics lead to high indentation static load capacity, which is important for certain applications especially space mechanisms. To ensure the maximum degree of elastic behavior, superelastic materials must be pre-stressed, a process referred to as "training" in shape memory effect (SME) terminology, at loads and stresses beyond expected use conditions. In this paper, static indentation load capacity tests are employed to assess the effects of pre-stressing on elastic response behavior of 60NiTi. The static load capacity is measured by pressing 12.7 mm diameter ceramic Si3N4 balls into highly polished, hardened 60NiTi flat plates that have previously been exposed to varying levels of pre-stress (up to 2.7 GPa) to determine the load that results in shallow but measurable (0.6 m, 25 in. deep) permanent dents. Hertz stress calculations are used to estimate contact stress. Without exposure to pre-stress, the 60NiTi surface can withstand an approximately 3400 kN load before significant denting (>0.4 m deep) occurs. When pre-stressed to 2.7 GPa, a static load of 4900 kN is required to achieve a comparable dent, a 30 percent increase. These results suggest that stressing contact surfaces prior to use enhances the static indentation load capacity of the superelastic 60NiTi. This approach may be adaptable to the engineering and manufacture of highly resilient mechanical components such as rolling element bearings.

DellaCorte, Christopher

Characterization of Polyamide Thin Films by Atomic Force Microscopy

This study directly compares the mechanical behavior of novel molecular layer deposition (MLD) and analogous interfacial polymerization (IP) polyamide thin films in environments relevant to reverse osmosis (RO) membrane operation. The elastic modulus of the films was determined using atomic force microscopy (AFM) in dry, hydrated, and chlorinated states. Surface roughness characteristics were also obtained given their potential influence on AFM modulus measurements. The much smoother MLD films demonstrated a statistically higher modulus in all states as compared to their IP counterparts. The MLD films maintained a modulus ~3X and ~5X greater than that of IP films after hydration and chlorination, respectively. Such differences in behavior may be due to the higher density and correspondingly lower void content of the MLD films. Results from this study provide a rationale for future development of MLD for fabrication of polyamide films for incorporation in RO membranes.

atomic force microscopy

On the length scale and rate-dependent mechanical behavior of monolithic (oxy)sulfidic glassy solid-state electrolytes

In the controlled atmosphere of a dedicated glove box, nanoindentation performed with a diamond Berkovich indenter tip has been used to examine the mechanical behavior of three (oxy)sulfide solid-state electrolytes (SSEs), 70Li 2 S·(30–x)P 2 S 5 ·xP 2 O 5 (x = 0, 2, and 5). At a drive frequency of 120 Hz, the elastic modulus is found to be predominantly depth independent over the range of 100 nm to 1 μm and generally insensitive to the varying mol fraction of oxygen (0, 2, and 5%) as well as the imposed strain rates of 0.025, 0.05, and 0.1 1/s. All three SSEs exhibit significant room-temperature creep. Strain burst activity observed during loading (potentially representative of pore collapse or cracking) is attenuated with the addition of oxygen. The hardness is found to be insensitive to the imposed strain rates but varying with depth and oxygen content. Furthermore, the highest oxygen concentration yields the lowest hardness and strongest depth dependence.

36 MATERIALS SCIENCE

Experimental and computational studies on high-entropy carbide MoNbTaVWC 5 under high pressures

High-entropy carbide, MoNbTaVWC 5 , was synthesized from oxide precursors of the constituent metals, mixed with graphite powder in a microwave-generated hydrogen plasma at 26.66 kPa and 2100 °C. Ambient x-ray diffraction analysis confirms the full conversion of oxide precursors into a single-phase, face-centered cubic structure with a lattice parameter a = 4.3309 Å. Nanoindentation measured a hardness of 24.5 ± 1.3 GPa and an elastic modulus of 386 ± 22 GPa. The synthesized sample, mixed with a copper pressure marker, was studied by the radial x-ray diffraction technique with beryllium gasketing in a diamond anvil cell up to 70 GPa. The experimentally measured pressure–volume curve and shear strength were compared with theoretical predictions using the special quasi-random structure technique and density functional theory. MoNbTaVWC 5 achieved a 12% volume compression at 70 GPa and exhibited a high shear strength of 6.6 GPa. The present study demonstrates that the high-entropy carbide MoNbTaVWC 5 exhibits exceptional incompressibility and high strength under extreme conditions.

36 MATERIALS SCIENCE

Structure-Property Relationships of Bismaleimides

The purpose of this research was to control and systematically vary the network topology of bismaleimides through cure temperature and chemistry (addition of various coreactants) and subsequently attempt to determine structure-mechanical property relationships. Characterization of the bismaleimide structures by dielectric, rheological, and thermal analyses, and density measurements was subsequently correlated with mechanical properties such as modulus, yield strength, fracture energy, and stress relaxation. The model material used in this investigation was 4,4'-BismaleiMidodIphenyl methane (BMI). BMI was coreacted with either 4,4'-Methylene Dianiline (MDA), o,o'-diallyl bisphenol A (DABA) from Ciba Geigy, or Diamino Diphenyl Sulfone (DDS). Three cure paths were employed: a low- temperature cure of 140 C where chain extension should predominate, a high-temperature cure of 220 C where both chain extension and crosslinking should occur simultaneously, and a low-temperature (140 C) cure followed immediately by a high-temperature (220 C) cure where the chain extension reaction or amine addition precedes BMI homopolymerization or crosslinking. Samples of cured and postcured PMR-15 were also tested to determine the effects of postcuring on the mechanical properties. The low-temperature cure condition of BMI/MDA exhibited the highest modulus values for a given mole fraction of BMI with the modulus decreasing with decreasing concentration of BMI. The higher elastic modulus is the result of steric hindrance by unreacted BMI molecules in the glassy state. The moduli values for the high- and low/high-temperature cure conditions of BMI/MDA decreased as the amount of diamine increased. All the moduli values mimic the yield strength and density trends. For the high-temperature cure condition, the room- temperature modulus remained constant with decreasing mole fraction of BMT for the BMI/DABA and BMI/DDS systems. Postcuring PMR-15 increases the modulus over that of the cured material even though density values of cured and postcured PMR were essentially the same. Preliminary results of a continuous and intermittent stress relaxation experiment for BMI:MDA in a 2:1 molar ratio indicate that crosslinking is occurring when the sample is in the undeformed state. Computer simulation of properties such as density, glass transition temperature, and modulus for the low- temperature cure conditions of BMI/MDA and BMI/DABA were completed. The computer modeling was used to help further understand and confirm the structure characterization results. The simulations correctly predicted the trends of these properties versus mole fraction BMI and were extended to other BMI/diamine systems.

Tenteris-Noebe, Anita D.

Quasistatic vs. Dynamic Modulus Measurements Of Plasma-Sprayed Thermal Barrier Coatings

Plasma-sprayed 8wt% yttria-stabilized zirconia (8YSZ) thermal barrier coatings (TBCs) have been demonstrated to exhibit nonlinear hysteretic elastic behavior by quasistatic cyclic compression and cylindrical punch indentation measurements. In particular, the instantaneous (tangential) elastic modulus increases with applied stress and exhibits significant hysteresis during cycling. Sound velocity (dynamic) measurements also show an increase in TBC modulus with applied compressive stress, but in contrast show no significant hysteresis for the modulus during cycling. The nonlinear elastic behavior of the TBCs evidenced by these tests is attributed to coating compaction and internal sliding. The differences between the quasistatic and dynamic measurements are explained by the relative absence of the effect of internal sliding in the dynamic modulus measurements. By incorporating short load reversals into the larger loading cycle and measuring the instantaneous modulus at the start of each load reversal, the effects of internal sliding can be substantially reduced in the quasistatic measurements, and the resulting modulus values show good agreement with the modulus values determined by dynamic sound velocity measurements.

Eldridge, J. I.

Inelastic column behavior

The significant findings of a theoretical study of column behavior in the plastic stress range are presented. When the behavior of a straight column is regarded as the limiting behavior of an imperfect column as the initial imperfection (lack of straightness) approaches zero, the departure from the straight configuration occurs at the tangent-modulus load. Without such a concept of the behavior of a straight column, one is led to the unrealistic conclusion that lateral deflection of the column can begin at any load between the tangent-modulus value and the Euler load, based on the original elastic modulus. A family of curves showing load against lateral deflection is presented for idealized h-section columns of various lengths and of various materials that have a systematic variation of their stress-strain curves.

Duberg, John E

Modeling stiffness loss in boron/aluminum below the fatigue limit

Boron/aluminum can develop significant internal matrix cracking when fatigued. These matrix cracks can result in a 40 percent secant modulus loss in some laminates, even when fatigued below the fatigue limit. It is shown that the same amount of fatigue damage will develop during stress or strain-controlled tests. Stacking sequence has little influence on secant modulus loss. The secant modulus loss in unidirectional composites is small, whereas the losses are substantial in laminates containing off-axis plies. A simple analysis is presented that predicts unnotched laminate secant modulus loss due to fatigue. The analysis is based upon the elastic modulus and Poisson's ratio of the fiber and matrix, fiber volume fraction, fiber orientations, and the cyclic-hardened yield stress of the matrix material. Excellent agreement was achieved between model predictions and experimental results. With this model, designers can project the material stiffness loss for design load or strain levels and assess the feasibility of its use in stiffness-critical parts.

Johnson, W. S.

Modeling stiffness loss in boron/aluminum laminates below the fatigue limit

Boron/aluminum can develop significant internal matrix cracking when fatigued. These matrix cracks can result in a 40 percent secant modulus loss in some laminates, even when fatigued below the fatigue limit. It is shown that the same amount of fatigue damage will develop during stress or strain-controlled tests. Stacking sequence has little influence on secant modulus loss. The secant modulus loss in unidirectional composites is small, whereas the losses are substantial in laminates containing off-axis plies. A simple analysis is presented that predicts unnotched laminate secant modulus loss due to fatigue. The analysis is based upon the elastic modulus and Poisson's ratio of the fiber and matrix, fiber volume fraction, fiber orientations, and the cyclic-hardened yield stress of the matrix material. Excellent agreement was achieved between model predictions and experimental results. With this model, designers can project the material stiffness loss for design load or strain levels and assess the feasibility of its use in stiffness-critical parts. Previously announced in STAR as N82-24298

Johnson, W. S.

Prediction of Material Properties of Nanostructured Polymer Composites Using Atomistic Simulations

Atomistic models of epoxy polymers were built in order to assess the effect of structure at the nanometer scale on the resulting bulk properties such as elastic modulus and thermal conductivity. Atomistic models of both bulk polymer and carbon nanotube polymer composites were built. For the bulk models, the effect of moisture content and temperature on the resulting elastic constants was calculated. A relatively consistent decrease in modulus was seen with increasing temperature. The dependence of modulus on moisture content was less consistent. This behavior was seen for two different epoxy systems, one containing a difunctional epoxy molecule and the other a tetrafunctional epoxy molecule. Both epoxy structures were crosslinked with diamine curing agents. Multifunctional properties were calculated with the nanocomposite models. Molecular dynamics simulation was used to estimate the interfacial thermal (Kapitza) resistance between the carbon nanotube and the surrounding epoxy matrix. These estimated values were used in a multiscale model in order to predict the thermal conductivity of a nanocomposite as a function of the nanometer scaled molecular structure.

Hinkley, J.A.