Detailed characterization of a PWR fuel rod at high burnup in support of LOCA testing

Experimental investigations of the fuel microstructure and volatile fission products along the pellet of a high burnup specimen (local burnup 76 GWd/tHM) have been conducted to support future transient testing. Detailed microscopy examinations have been carried out at different length scales. Transmission electron microscopy has highlighted a significant amount of damage across the entire radius with the formation of networks of dislocations. The optical and scanning electron microscopy determined the formation of three zones in the pellet with different characteristics. An intermediate region with no grain subdivision, lower porosity than the central zone porosity and high retained fission gas in nanometric bubbles and in the matrix was present between r/r0 ˜ 0.55 and 0.8. The high retention of gas in this region might suggest that the region will be prone to fine fragmentation, in addition to the HBS. An abrupt transition in the structure was observed at mid radius, with a third region developing from the mid radius to the pellet center. In this part of the pellet, metallic and grey phases with size between hundreds of nanometers and a few micrometers have formed at grain boundaries. The majority of fission gas has been released from the grain matrix and the original grains have polygonised, forming sub-grain domains separated by low-angle grain boundaries. No final explanation can be given for the polygonization occurring in the center, but on the basis of the irradiation history and the analysis of all the post irradiation examination (PIE) data, it is postulated that the polygonization within the original grains is an effect of dynamic recovery occurring at high temperature in the fuel center.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Identifying High Burnup LOCA Test Conditions to Support LOCA Testing

Presentation summarizing work done by INL and ORNL investigating loss-of-coolant accidents involving high burnup fuel. This includes developing LOCA test conditions for TREAT and SATS experiments and highlighting potential differences between nuclear and electrical heating LOCA experiments.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

A Critical Review of High Burnup Fuel Fragmentation, Relocation, and Dispersal under Loss-Of-Coolant Accident Conditions

High burnup fuel in excess of ~6268 GWd/MTU has been observed to severely fragment when subjected to temperature transient conditions as in a loss-of-coolant accident. In the event of cladding failure, the severely fragmented fuel can relocate into the balloon region and potentially disperse through the burst opening into the reactor’s primary system. This observation has led to implementation of several independent test programs designed to focus on various aspects of fuel fragmentation, relocation, and dispersal. The purpose of this review is to perform a critical, holistic assessment of fuel fragmentation, relocation, and dispersal under loss-of-coolant conditions to identify data gaps in the experimental data base. Phenomena have been identified and well defined through the various testing programs, and general agreement regarding the governing parameters (temperature, burnup, heating rate, cladding deformation, etc.) has been established. However, there is a significant data gap connecting research to commercial application. Furthermore, previous research attempted to evaluate the problem holistically, but has yet to provide a comprehensive understanding of the problem. Major identified data gaps consist of (1) a comprehensive understanding of pretransient fuel rod conditions (fuel temperature, fuel stress, rod internal pressures, microstructure, etc.), (2) definition of prototypic loss-of-coolant accident conditions (heating rate, fuel temperatures, fuel stress), (3) identification of the differences between nuclear and electrical integral loss-of-coolant accident tests, and connection of fuel rod performance (cladding ballooning, burst opening, potential relocation, fragmentation susceptibility, etc.) to fuel fragmentation, relocation, and dispersal severity. Finally, the content of this manuscript provides a clear path for connecting testing and data acquisition to commercial application by providing concrete means for filling data gaps and prioritized testing regimes.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Engineering Assessment of UO 2 and Cladding Behavior under High Burnup LOCA Conditions

To maximize the data extracted from a limited number of high-burnup fuel rod samples, several modeling efforts were performed to elucidate the fuel and the cladding responses of these fuels under transient conditions. These objectives were (1) to determine the role of the fuel stress state in fuel pulverization, (2) to ascertain the differences between conditions of cladding burst during experiments and those expected during a commercial reactor transient, and (3) to develop a method to conservatively calculate the geometry of the cladding rupture’s opening to inform fuel dispersal susceptibility.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

High-burnup Experiments in Reactivity Initiated Accidents (HERA)

HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.

(HERA)↗

High-burnup Experiments in Reactivity Initiated Accidents (HERA)

HERA is a joint experimental program (JEEP) operating within the Nuclear Energy Agency’s (NEA’s) framework for irradiation experiments (FIDES). HERA is dedicated to the understanding of light water reactor (LWR) fuel performance at high burnup under reactivity-initiated accidents (RIA). During RIAs the fuel cladding can be breached by one of two mechanisms; pellet-cladding mechanical interaction or high temperature balloon and rupture. Pellet-cladding mechanical interaction (PCMI) failure occurs in the early phase of an RIA transient where the fuel pellet expands rapidly into the cladding prior to any meaningful heat transfer from the pellet to the cladding. This results in high stresses in the cladding resulting in crack propagation through the base Zircaloy metal and axially along the cladding tube. Failure by PCMI is a brittle failure mode and occurs at low cladding strains, approximately 2% hoop strain. If the cladding survives the PCMI phase of the transient, it may still fail due to ballooning and rupture induced by extended exposure to high temperature. Thermal transport from the fuel pin to the coolant is significantly reduced if a transition to film boiling on the cladding surface occurs. This result in both a rapid increase in fuel temperature, which drives fission gas release, and a spike in cladding temperature, which results in loss of mechanical strength. If the internal pressure of the fuel rod is greater than the system pressure the cladding can inelastically deform and eventually rupture. Failure by swelling and rupture occurs at larger strains, generally greater than 5% hoop strain. While PCMI failures are generally seen as more limiting, the dominance of one failure mode over the other can be affected by both the cladding material conditions, and the transient evolution.

(HERA)↗

(S)TEM/EDS study of native precipitates and irradiation induced Nb-rich platelets in high-burnup M5®

We have investigated microstructure and microchemistry of precipitates and dislocation loops in high-burnup M5® using (scanning) transmission electron microscopy ((S)TEM) equipped with energy dispersive X-ray spectroscopy (EDS). Two (S)TEM lamellae were made by cryo-FIB from the same cladding sample. The Nb-rich native precipitates were found in the metal, in the suboxide and in the oxide. Upon diffraction analysis, most of the Nb-rich native precipitates in the metal matrix remain as β-Nb phase, while no β-Nb native precipitates were found in the oxide. Nearby the oxide and metal (O/M) interface, the native precipitates in the oxide were already oxidized into t-NbO2 phase. At further distance away from the O/M interface, the Nb-rich native precipitates were gradually oxidized and became amorphous. Besides the native precipitates, Nb-rich irradiation induced precipitates (IIPs) were found in the metal matrix. Using g = <0002> vector for imaging, the length of the IIPs was aligned with dislocation loops. However, no Nb segregation to the dislocation loops themselves was observed. For the first time, we report that IIPs indeed exist in the oxide but only within about 1.5 µm away from O/M interface. However, the oxidation state of the IIPs in the oxide is still unclear. The presence of both native precipitates and IIPs in the oxide may indicate the Nb concentration in the oxide solid solution remain low nearby the O/M interface, which may explain the reduced corrosion kinetics of in-pile M5®. On the other hand, no IIPs were observed in the oxide at further distance and this may indicate that they have eventually dissolved back into the oxide. A few mechanisms related to IIPs stability in the oxide are presented.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Combined TREAT-LOC and SATS LOCA Experiment Plan: Integral LOCA Experiments on High-Burnup Fuels

The Transient Reactor Test Facility (TREAT) loss-of-coolant (LOC) and high-burnup (HBu) experiment series, along with the Severe Accident Test Station (SATS) HBu experiment series, are integral LOC accident (LOCA) experiments planned under the DOE AFC program, which aim to support burnup extension needs by addressing identified R&D priorities in order to achieve an improved understanding of fuel fragmentation, relocation, and dispersal (FFRD) of HBu fuel during LOCA events. The data produced under this plan will be used to further validate and confirm existing models and inform future R&D and model development. The experimental program has been specifically designed to address knowledge gaps and opportunities identified through a detailed review of existing public knowledge on LOCA FFRD. The test program employs a unique combination of in- and out-of-pile experimental approaches and state-of-the-art facilities to provide a clear connection to the existing integral and semi-integral LOCA experiment database. The primary goal of the program is to investigate the impact of prototypic HBu fuel/cladding thermomechanical behaviors under postulated LWR LOCA conditions that have not yet been fully studied. These conditions correspond with prototypic decay-energy heatup (DEH) and stored-energy heatup (SEH) conditions. Importantly, TREAT’s unique capability will enable the first evaluation of the impact of SEH conditions on HBu fuels. The test program will emphasize the development of an improved mechanistic understanding of key experimental phenomena through independent experimental systems, development of a database to support fuel performance modeling tools and employing world-leading advanced materials characterization and in-situ diagnostics to evaluate FFRD. The results of the program will provide novel data to support modeling development and validation and will represent a significant advancement in evaluating prototypic conditions, as well as to inform the technical basis for LOCA-induced FFRD.

22 GENERAL STUDIES OF NUCLEAR REACTORS↗

Multiscale modeling for high burnup structure formation and associated pulverization

This report summarizes the lower length scale modeling work performed in the fiscal year 2023 under the Nuclear Energy Advanced Modeling and Simulation (NEAMS) program to capture the microstrutural evolution and associated pulverization criteria in the high burnup regions. This year, the resolution mechanisms within the cluster dynamics code has been updated and it influence on the bubble growth in HBS regions at the mesoscale is studied. To improve the accuracy of phase-field models of fission gas bubble growth, a new Helmholtz free energy for high-density Xe gas is derived from a virial equation of state. Two previously used strategies for representing net vacancy production in phase-field models of fission gas bubble growth are compared with each other and with analytical models of bubble growth. The vacancy source only model is found to be more convenient to parameterize realistically compared with the vacancy source+sink model. Furthermore, the phase-field-fracture simulation have been performed using MD- informed failure stress values and realistic HBS structure obtained from the phase-field simulations. We also present the uncertainty bands on prediction of the critical stress to account for the effect of the lower length scale variabilities on the failure criteria at the mesoscale. It is observed that pulverization may occur in partially restructured regions with restructuring fraction as low as 17%. In light of this, an update to the BISON’s pulverization criteria is recommended.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of Fuel and Cladding In and Near the Pellet-Pellet Gap of a High-Burnup Pressurized Water Reactor Fuel Rod

At TopFuel 2021, we reported on metallographic examinations of a high burnup ZIRLO-clad spent fuel rod operated at the North Anna Power Station having a 3-mm gap between pellets at an elevation of ~1,403 mm. The rod was sectioned axially at that elevation to reveal the pellet-pellet interfaces and the pellet-pellet gap. Sections were mounted and polished to reveal the distribution of cladding inner and outer oxide layer thicknesses above, below, and within the gap. Since then, total cladding hydrogen measurements have been performed to quantify the cladding hydrogen content through the gap and above and below the pellet-pellet gap region. This paper provides the cladding hydrogen concentrations and discusses the overall findings regarding cladding waterside oxidation and cladding hydrogen diffusion to a pellet-pellet gap.

Montgomery, Rose↗

Multiphysics analysis of fuel Fragmentation, Relocation, and dispersal Susceptibility–Part 2: High-Burnup Steady-State operating and fuel performance conditions

The US nuclear industry is pursuing increased cycle lengths and increasing the peak rod-averaged burnup in an effort to increase the economic viability of the US nuclear fleet. Increasing burnup will afford economic viability by enabling utilities to optimize core designs to reduce the number of fresh fuel assemblies per cycle and allow nuclear power plants to operate for a longer period of time. Longer operating periods will also decrease the number of outages experienced by a nuclear power plants and, therefore, offer utilities significant operational savings. However, extending the peak rod-averaged burnup beyond 62 GWd/tU results in operating fuel rods to higher burnup under higher power conditions. This operating regime is expected to result in higher fuel temperatures, fission gas release (FGR), and rod internal pressures (RIPs) that may challenge historical safety basis and affect high-burnup (HBU) experimental testing. In particular, these conditions directly affect fuel fragmentation, relocation, and dispersal (FFRD) susceptibility, so understanding the pretransient operating conditions is critical for developing test plans that evaluate the FFRD and develop strategies to mitigate it. This paper evaluates the operating conditions and fuel performance of HBU (greater than62 GWd/tU rod average) fuel. Additionally, it investigates fuel performance sensitivities and discusses the effect on fuel performance. Here, this work used two codes. Virtual Environment for Reactor Applications (VERA) was used to calculate steady-state power histories, identify HBU operating conditions using 10 different realistic HBU core designs, and down-select rods to a representative subset of fuel rods for subsequent BISON evaluation. The BISON fuel performance code was used to investigate steady-state HBU operating conditions and assess uncertainties associated with FGR and its effect on fuel temperatures and RIPs. The VERA and BISON results will provide direct input for HBU experimental testing and support subsequent TRACE and BISON transient fuel performance analyses.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Short Communication: Observation of Initial Burst Release of Fission Gas from High-Burnup UO 2 Nuclear Fuel During Thermal Transient

A system was developed and tested to provide a deeper understanding of the fission gas release kinetics from nuclear fuel during thermal transients. Pressure, temperature, spectral data, and optical images were simultaneously collected during resistive sample heating, and all released gases were collected in liquid nitrogen-cooled charcoal traps. Standup testing was performed with a high-burnup nuclear fuel segment from rod section with an average local burnup of 77 GWd/tU. During heating, the segment released approximately 6 ± 2% of generated fission gas inventory after ramp heating to 460°C. Here, heating ceased when the sample ejected from the holder, as observed by constant imaging.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Phase-field simulations of fission gas bubbles in high burnup UO2 to inform engineering-scale fuel performance modeling

To improve the economics of commercial nuclear energy generation, U.S. utilities are currently seeking licensing approval to operate UO2 fuel to higher burnups. One significant safety issue that must be addressed to obtain approval is the potential for fine fragmentation/pulverization of the fuel during a loss-of-coolant accident (LOCA). The cause of pulverization has been hypothesized to be the rapid increase of pressure in fission gas bubbles in the high burnup region of the fuel during a LOCA. To better understand this phenomenon, a novel phase-field model of the fission gas bubble microstructure in UO2 has been developed and implemented in Idaho National Laboratory (INL)'s Marmot application for phase-field simulation of nuclear materials. Simulations of the bubble response to steady-state and transient conditions were conducted. Simulation results were used to inform a mechanistic model of pulverization in BISON, INL’s fuel performance simulation code.

11 - NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Multi-scale simulation of high burnup UO2 nuclear fuel during loss-of-coolant accident conditions

To improve the economics of commercial nuclear energy generation, U.S. utilities are currently seeking licensing approval to operate UO2 fuel to higher burnups. One significant safety issue that must be addressed to obtain approval is the potential for fine fragmentation/pulverization of the fuel during a loss-of-coolant accident (LOCA). It has been hypothesized that pulverization is caused by the rapid increase of pressure in fission gas bubbles in the high burnup region of the fuel during a LOCA. To better understand this phenomenon, a novel phase-field model of the fission gas bubble microstructure in UO2 has been developed and implemented in Idaho National Laboratory (INL)'s Marmot application for phase-field simulation of nuclear materials. Simulations of the bubble response to steady-state and transient conditions were conducted, and the results were used to inform a mechanistic model of pulverization in BISON, INL’s fuel performance simulation code.

11 NUCLEAR FUEL CYCLE AND FUEL MATERIALS↗

Characterization of Fuel and Cladding In and Near the Pellet-Pellet Gap of a High-Burnup Pressurized Water Reactor Fuel Rod

Oak Ridge National Laboratory (ORNL) is performing extensive destructive examinations of 15 high-burnup (HBU) spent nuclear fuel (SNF) rods from the North Anna Power Station (NAPS), which is operated by Dominion Energy Virginia [1]. The examinations are being conducted to obtain a baseline condition of the HBU rods before dry storage and are focused on understanding overall SNF rod strength and durability [2,3]. The HBU rods, referred to as sister rods or sibling rods, are similar to rods placed into dry storage at NAPS that are planned to be examined after one decade. The sister rods include several ZIRLO®-clad rods manufactured by Westinghouse Electric Company. One of the ZIRLO®-clad rods examined includes a pellet-pellet gap of 1 mm that was identified during the nondestructive examinations (NDEs) [4]. The rod was sectioned axially at that elevation to reveal the pellet-pellet interfaces and the pellet-pellet gap. The section was mounted and polished to reveal the distribution of hydride precipitates in the cladding above, below, and within the gap [5]. Total cladding hydrogen measurements will be performed to quantify the total cladding hydrogen through the gap and any additional in-solution or precipitated hydrogen in the pellet-pellet gap region

Montgomery, Rose↗