Search NASA⌕ Search

SEARCH · Search NASA

Results for “InAs”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Metallic behavior and negative differential resistance properties of (InAs){sub n} (n = 2 − 4) molecule cluster junctions via a combined non–equilibrium Green's function and density functional theory study

In this present work, the geometric structures and electronic transport properties of (InAs){sub n} (n = 2, 3, 4) molecule cluster junctions are comparatively investigated using NEGF combined with DFT. Results indicate that all (InAs){sub n} molecule cluster junctions present metallic behavior at the low applied biases ([−2V, 2V]), while NDR appears at a certain high bias range. Our calculation shows that the current of (InAs){sub 4} molecule cluster–based junction is almost the largest at any bias. The mechanisms of the current–voltage characteristics of all the three molecule cluster junctions are proposed.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Experimental study on vertical scaling of InAs-on-insulator metal-oxide-semiconductor field-effect transistors

We have investigated effects of the vertical scaling on electrical properties in extremely thin-body InAs-on-insulator (-OI) metal-oxide-semiconductor field-effect transistors (MOSFETs). It is found that the body thickness (T{sub body}) scaling provides better short channel effect (SCE) control, whereas the T{sub body} scaling also causes the reduction of the mobility limited by channel thickness fluctuation (δT{sub body}) scattering (μ{sub fluctuation}). Also, in order to achieve better SCEs control, the thickness of InAs channel layer (T{sub channel}) scaling is more favorable than the thickness of MOS interface buffer layer (T{sub buffer}) scaling from a viewpoint of a balance between SCEs control and μ{sub fluctuation} reduction. These results indicate necessity of quantum well channel structure in InAs-OI MOSFETs and these should be considered in future transistor design.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Volmer–Weber InAs quantum dot formation on InP (113)B substrates under the surfactant effect of Sb

We report on Sb surfactant growth of InAs nanostructures on GaAs{sub 0.51}Sb{sub 0.49} layers deposited on InP (001) and on (113)B oriented substrates. On the (001) orientation, the presence of Sb significantly favors the two-dimensional growth regime. Even after the deposition of 5 mono-layers of InAs, the epitaxial film remains flat and InAs/GaAs{sub 0.51}Sb{sub 0.49} type-II quantum wells are achieved. On (113)B substrates, same growth runs resulted in formation of high density InAs islands. Microscopic studies show that wetting layer is missing on (113)B substrates, and thus, a Volmer-Weber growth mode is concluded. These different behaviors are attributed to the surface energy changes induced by Sb atoms on surface.

77 NANOSCIENCE AND NANOTECHNOLOGY↗

Oxide-free InAs(111)A interface in metal-oxide-semiconductor structure with very low density of states prepared by anodic oxidation

In this letter, we present structural, compositional, and electrical characteristics of anodic oxide layer-based metal-oxide-semiconductor (MOS) capacitors on n-type InAs(111)A, along with the effect of a thin fluorinated interfacial passivation layer. Electrochemical oxidation in acid electrolyte with addition of fluorine (NH{sub 4}F) led to the formation of oxygen free well-ordered wide gap fluorinated interfacial layer at InAs(111)A with the fixed charge (Q{sub fix}) and density of interface states (D{sub it}) in the range of (4–6) × 10{sup 10 }cm{sup −2} and (2–12) × 10{sup 10 }eV{sup −1 }cm{sup −2}, respectively. We found that MOS capacitors showed excellent capacitance-voltage characteristics with very small frequency dispersion (<1% and <15 mV). Fluorinated interfacial layer consists of crystalline isostructural compound with the InAs substrate, which remains intact with the atomic smoothness and sharpness that explain unpinned behavior of the Fermi level.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Calculation of the electron spin relaxation times in InSb and InAs by the projection-reduction method

The electron spin relaxation times in a system of electrons interacting with piezoelectric phonons mediated through spin-orbit interactions were calculated using the formula derived from the projection-reduction method. The results showed that the temperature and magnetic field dependence of the relaxation times in InSb and InAs were similar. The piezoelectric material constants obtained by a comparison with the reported experimental result were P{sub pe}=4.0×10{sup 22} eV/m for InSb and P{sub pe}=1.2×10{sup 23} eV/m for InAs. The result also showed that the relaxation of the electron spin by the Elliot-Yafet process is more relevant for InSb than InAs at a low density.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Studies of scattering mechanisms in gate tunable InAs/(Al,Ga)Sb two dimensional electron gases

A study of scattering mechanisms in gate tunable two dimensional electron gases confined to InAs/(Al,Ga)Sb heterostructures with varying interface roughness and dislocation density is presented. By integrating an insulated gate structure the evolution of the low temperature electron mobility and single-particle lifetime was determined for a previously unexplored density regime, 10{sup 11}–10{sup 12 }cm{sup −2}, in this system. Existing theoretical models were used to analyze the density dependence of the electron mobility and single particle lifetime in InAs quantum wells. Scattering was found to be dominated by charged dislocations and interface roughness. It was demonstrated that the growth of InAs quantum wells on nearly lattice matched GaSb substrate results in fewer dislocations, lower interface roughness, and improved low temperature transport properties compared to growth on lattice mismatched GaAs substrates.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Mid-infrared electroluminescence from InAs type-I quantum wells grown on InAsP/InP metamorphic buffers

We report room-temperature (RT) electroluminescence (EL) from InAs/InAs{sub x}P{sub 1−x} quantum well (QW) light-emitting diodes (LEDs) over a wide wavelength range of 2.50–2.94 μm. We demonstrate the ability to accurately design strained InAs QW emission wavelengths while maintaining low threading dislocation density, coherent QW interfaces, and high EL intensity. Investigation of the optical properties of the LEDs grown on different InAs{sub x}P{sub 1−x} metamorphic buffers showed higher EL intensity and lower thermal quenching for QWs with higher barriers and stronger carrier confinement. Strong RT EL intensity from LEDs with narrow full-width at half-maximum shows future potential for InAs QW mid-infrared laser diodes on InAsP/InP.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Optical absorption and intrinsic recombination in relaxed and strained InAs{sub 1–x}Sb{sub x} alloys for mid-wavelength infrared application

The intrinsic carrier recombination lifetime in relaxed and strained InAs{sub 1−x}Sb{sub x} alloys is investigated using the full-band Green's function theory. By computing the phonon-perturbed electron self-energy of the system, both direct and phonon-assisted indirect Auger and radiative processes are studied as functions of antimony molar fractions, lattice temperatures and applied in-plane biaxial strains. To improve the overall accuracy of the calculation, an empirical pseudopotential band structure for the alloy is also fitted to the measured band extrema and effective masses under different biaxial strains. A set of effective screened potentials valid for all the needed antimony fractions x and biaxial strains ϵ, therefore, is obtained and applied to the calculation. The results showed reduced total Auger recombination rates and enhanced radiative recombination rates in InAsSb alloys at room temperature when a compressive strain is applied. Furthermore, the study on the widely employed mid-wavelength infrared detector material, InAs{sub 0.91}Sb{sub 0.09}, strained by an InAs substrate, demonstrated that much longer minority carrier lifetime can be achieved compared to that in the lattice-matched situation when the lattice temperature is above 200 K.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

High performance InAs quantum dot lasers on silicon substrates by low temperature Pd-GaAs wafer bonding

InAs quantum dot (QD) laser heterostructures have been grown by molecular beam epitaxy system on GaAs substrates, and then transferred to silicon substrates by a low temperature (250 °C) Pd-mediated wafer bonding process. A low interfacial resistivity of only 0.2 Ω cm{sup 2} formed during the bonding process is characterized by the current-voltage measurements. The InAs QD lasers on Si exhibit comparable characteristics to state-of-the-art QD lasers on silicon substrates, where the threshold current density J{sub th} and differential quantum efficiency η{sub d} of 240 A/cm{sup 2} and 23.9%, respectively, at room temperature are obtained with laser bars of cavity length and waveguide ridge of 1.5 mm and 5 μm, respectively. The InAs QD lasers also show operation up to 100 °C with a threshold current density J{sub th} and differential quantum efficiency η{sub d} of 950 A/cm{sup 2} and 9.3%, respectively. The temperature coefficient T{sub 0} of 69 K from 60 to 100 °C is characterized from the temperature dependent J{sub th} measurements.

71 CLASSICAL AND QUANTUM MECHANICS, GENERAL PHYSIC↗

Influence of surface nano-patterning on the placement of InAs quantum dots

We have examined the influence of spontaneous nano-patterning on the placement of InAs quantum dots (QDs) on (Al)GaAs surfaces using an experimental-computational approach. Both atomically flat and mounded surfaces, generated via a surface instability induced by the Ehrlich- Schwoebel barrier, are employed as templates for the subsequent deposition of InAs QDs. Using height profiles from atomic-force micrographs, we simulate QD deposition with a 2D phase field model, which describes the time evolution of the InAs layer driven by a chemical potential gradient. For flat surfaces, phase-field simulations result in QD densities comparable to experimental observations. For mounded surfaces, the simulations reveal QDs preferentially positioned in regions of positive curvature (substrate valleys), e.g., at the edge of surface mounds, consistent with the anisotropic QD placement observed experimentally. We discuss the role of curvaturedriven diffusion in the spontaneous ordering of QDs, demonstrating the applicability of this mechanism to AlGaAs mounds.

36 MATERIALS SCIENCE↗

Pressure-induced structural change of liquid InAs and the systematics of liquid III-V compounds

To understand the pressure-induced structural changes of liquid III-V compounds systematically, the pressure dependence of l-InAs was investigated using the synchrotron x-ray diffraction and an ab initio molecular-dynamics simulation (AIMD). The x-ray diffraction experiments revealed that the liquid changes its compression behavior from a nearly uniform type to a nonuniform one around 9 GPa. Corresponding to this change, the coordination number (China), which is maintained up to 9 GPa, markedly increases from 6.0 to 7.5. The AIMD simulation revealed that this change is related to the change in the pressure dependence of all three pair correlations. In particular, a marked change is observed in the As-As correlation; in the low-pressure region, the position of the first peak in g{sub AsAs}(r), r{sub AsAs}, increases while maintaining the CN{sub AsAs}, but in the high-pressure region, the r{sub AsAs} stops increasing and the CN{sub AsAs} begins to increase. The AIMD simulation also revealed that each partial structure of l-InAs is similar to that for the pure-element liquid with the same valence electron number. Upon compression, each partial structure approaches the respective one for a heavier element in the same group. These findings suggest that the structures of liquid compounds are locally controlled by the number of the valence electrons in each ion pair and that the change in each partial structure obeys the empirical rule that the high-pressure state resembles the ambient state of a heavier element in the same group. Comparing the pressure-induced structural change of l-InAs to those of other liquid III-V compounds (GaSb and InSb) has revealed that, although the high-pressure behaviors of these three liquids are apparently different, their structural changes are systematically understood by a common structural sequence. This systematics originates from the same effect on each partial structure between increasing the atomic number and the pressurization.

75 CONDENSED MATTER PHYSICS, SUPERCONDUCTIVITY AND↗

Anomalous spin splitting of electrons in type-II InSb quantum dots in InAs

Magnetooptical studies of heterostructures with type-II InSb quantum dots in the InAs matrix grown by molecular beam epitaxy are carried out. Unusual behavior of magnetophotoluminescence from quantum dots measured in the Faraday geometry in the samples with multiple planes of quantum dots is found. Specifically, the peak with {sigma}{sup -} polarization, which corresponds to transitions of electrons with s = +1/2, has a higher energy than the {sigma}{sup +} peak corresponding to s = -1/2, which contradicts the negative value of the electron g factor both in the InAs matrix and in the InSb quantum dot. The effect can be interpreted as the result of competition of two channels of radiative recombination, which differ by the initial states of electrons belonging either to the InSb quantum dots or to shallow-level donors in the InAs matrix.

36 MATERIALS SCIENCE↗

Change in the electronic properties of an InAs (111)A surface at oxygen and fluorine adsorption

Based on ab initio calculations, the adsorption of oxygen and fluorine on reconstructed (2 Multiplication-Sign 2) and unreconstructed (1 Multiplication-Sign 1) InAs (111)A surfaces is studied. The most stable adsorption positions are determined. It is shown that adsorption of oxygen on both surfaces gives rise to electronic states in the band gap. The preferential positions for oxygen adsorption on an InAs (111)A (2 Multiplication-Sign 2) surface are those where oxygen is bonded both to indium atoms and to arsenic atoms in the surface layer and also the vacant site between three indium atoms (the 'In-hollow position). Adsorption of fluorine brings about a pushing of the surface states out of the band gap; the position above indium atoms (the 'In-top position) is preferential for adsorbed fluorine. Adsorption of fluorine on an InAs (111)A (1 Multiplication-Sign 1) surface leads to the elimination of the surface state formed by indium p orbitals and to an unpinning of the Fermi level.

36 MATERIALS SCIENCE↗

Effect of Bi isovalent dopants on the formation of homogeneous coherently strained InAs quantum dots in GaAs matrices

The distribution of hydrostatic strains in Bi{sup 3+}-doped InAs quantum dots embedded in a GaAs matrix are calculated in the context of the deformation-potential model. The dependences of strains in the material of spherical InAs quantum dots with substitutional (Bi {yields} As) and interstitial (Bi) impurities on the quantum-dot size are derived. The qualitative correlation of the model with the experiment is discussed. The data on the effect of doping on the morphology of self-assembled InAs:Bi quantum dots in a GaAs matrix are obtained.

36 MATERIALS SCIENCE↗

Maximum drift velocity of electrons in selectively doped InAlAs/InGaAs/InAlAs heterostructures with InAs inserts

The dependence of the electron mobility and drift velocity on the growth conditions, thickness, and doping of an InAs insert placed at the center of the quantum well in a selectively doped InAlAs/InGaAs/InAlAs heterostructure has been investigated. Record enhancement of the maximum drift velocity to (2-4) Multiplication-Sign 10{sup 7} cm/s in an electric field of 5 Multiplication-Sign 10{sup 3} V/cm has been obtained in a 17-nm-wide quantum well with an undoped 4-nm-thick InAs insert. In the structures with additional doping of the InAs insert, which facilitates an increase in the density of electrons in the quantum well to 4.0 Multiplication-Sign 10{sup 12} cm{sup -2}, the maximum drift velocity is as high as 2 Multiplication-Sign 10{sup 7} cm/s in an electric field of 7 Multiplication-Sign 10{sup 3} V/cm.

36 MATERIALS SCIENCE↗

Study of the morphology and optical properties of anodic oxide layers on InAs (111)III

The effect of the electrolyte composition on the surface morphology and the dispersion dependences of the refractive index and extinction coefficient of {approx}20-nm-thick anodic layers on InAs (111)III substrates is studied by atomic force microscopy and spectral ellipsometry. It is shown that oxidation in electrolytes with different acidities does not modify the surface morphology of the initial InAs substrates. The films formed upon oxidation exhibit close dispersion dependences, despite the difference in the chemical composition between the films. This makes possible the high-precision monitoring of the thickness of anodic layers on InAs substrates by means of ellipsometry with the optical model of a single-layer isotropic film on an absorbing substrate.

36 MATERIALS SCIENCE↗

Effect of a low-temperature-grown GaAs layer on InAs quantum-dot photoluminescence

The photoluminescence of InAs semiconductor quantum dots overgrown by GaAs in the low-temperature mode (LT-GaAs) using various spacer layers or without them is studied. Spacer layers are thin GaAs or AlAs layers grown at temperatures normal for molecular-beam epitaxy (MBE). Direct overgrowth leads to photoluminescence disappearance. When using a thin GaAs spacer layer, the photoluminescence from InAs quantum dots is partially recovered; however, its intensity appears lower by two orders of magnitude than in the reference sample in which the quantum-dot array is overgrown at normal temperature. The use of wider-gap AlAs as a spacer-layer material leads to the enhancement of photoluminescence from InAs quantum dots, but it is still more than ten times lower than that of reference-sample emission. A model taking into account carrier generation by light, diffusion and tunneling from quantum dots to the LT-GaAs layer is constructed.

36 MATERIALS SCIENCE↗

Enhanced radiative and thermal properties from surface encapsulation of InAs nanowires

In this work, photoluminescence (PL), quantum efficiency and carrier dynamics are investigated in indium arsenide (InAs) nanowires (NWs) with various surface treatments, including a molecular beam epitaxy (MBE)-grown semiconductor shell passivation, sulfur-passivation, alumina (Al 2 O 3 ) coating by atomic layer deposition (ALD) and polydimethylsiloxane (PDMS) spin-coating. The ALD-dielectric layer-coated InAs core-shell NWs show a maximum 13-fold increase in PL intensity. In contrast to the previous reports, this enhancement is found to be due to increased radiative rate from an enhanced Purcell factor, better thermal conductance and higher carrier injection within the NWs instead of improved surface quality. Numeric simulations confirm the experimentally observed increased radiative rate. Further improvements are suggested with even thicker capped InAs NWs. Carrier lifetime in surface-treated NWs is extended and shows long-term stability, critical for practical devices.

36 MATERIALS SCIENCE↗