Search NASA⌕ Search

SEARCH · Search NASA

Results for “MATERIALS EROSION”

Search indexed NASA NTRS and DOE OSTI research on propulsion, heat transfer, battery materials and energy systems. Follow report and document links to the original sources.

Quote a phrase for an exact phrase match. Source license links do not imply unrestricted reuse.

At least 91 records · Page 5

Erosion of iron-chromium alloys by glass particles

The material loss upon erosion was measured for several iron-chromium alloys. Two types of erodent material were used: spherical glass beads and sharp particles of crushed glass. For erosion with glass beads the erosion resistance (defined as the reciprocal of material loss rate) was linearly dependent on hardness. This is in accordance with the erosion behavior of pure metals, but contrary to the erosion behavior of alloys of constant composition that were subjected to different heat treatments. For erosion with crushed glass, however, no correlation existed between hardness and erosion resistance. Instead, the erosion resistance depended on alloy composition rather than on hardness and increased with the chromium content of the alloy. The difference in erosion behavior for the two types of erodent particles suggested that two different material removal mechanisms were involved. This was confirmed by SEM micrographs of the eroded surfaces, which showed that for erosion with glass beads the mechanism of material removal was deformation-induced flaking of surface layers, or peening, whereas for erosion with crushed glass it was cutting or chopping.

Salik, J.↗

100-kW class applied-field MPD thruster component wear

Component erosion and material deposition sites were identified and analyzed during tests of various configurations of 100 kW class, applied-field, water-cooled magnetoplasmadynamic (MPD) thrusters. Severe erosion of the cathode and the boron nitride insulator was observed for the first series of tests, which was significantly decreased by reducing the levels of propellant contamination. Severe erosion of the copper anode resulting from sputtering by the propellant was also observed. This is the first observation of this phenomenon in MPD thrusters. The anode erosion indicates that development of long life MPD thrusters requires the use of light gas propellants such as hydrogen, deuterium, or lithium.

Mantenieks, Maris A.↗

Experimental investigation of jet impingement on surfaces of fine particles in a vacuum environment

The erosion characteristics of a bed of fine particles under vacuum conditions (10 -4 torr) resulting from an impinging jet exhaust were investigated for various particle sizes and jet heights above the dust surface. The investigation included measurements of the craters during erosion, measurements of the visibility reduction, and photographs of the erosion process. The results of this investigation indicate that there exists a finite jet height above which particles will not be eroded. This height, for given nozzle conditions, varies with surface-particle size. In addition, the results indicate that the magnitude of surface erosion also depends on-surface-particle size; erosion is most rapid with the coarsest particles. These and other associated test results are presented and compared with available theory.

Jet exhaust↗

Damage to solids caused by cavitation.

Water and mercury cavitation damage on solids in cavitating venturi tunnels consisting of single event symmetrical craters and irregular fatigue- type failures

MATERIALS EROSION↗

Geology of Chryse Planitia

Chryse Planitia, the site of the first successful landing on Mars by Viking 1, is an asymmetrical basin, centered at 45 deg W and 24 deg N, about 2000 km northeast of Valles Marineris. High-resolution Viking orbiter images show Chryse Planitia to be much more complex than had been suspected from Mariner 9 images. On the basis of a study of the Viking pictures it is concluded that the geological history of Chryse Planitia involves a complex sequence of impact cratering, mantling by extensive deposits of unknown origin, redistribution of mantling and crater materials by erosion and deposition with concurrent eruptions of flood-type basalts, and aeolian activity.

Greeley, R.↗

Erosion and transport of eolian materials on Mars

An abrasion chamber was constructed to produce grain to grain impacts and to eliminate, as far as possible, grain to wall impact. Quartz, basalt, olivine, and volcanic ash were used as abrasives to determine particle longevity on Mars during eolian abrasion. The various abrasion velocities, measured velocity or particles, calculated velocity of collision, time during which abrasion took place, the charge (material) in grams, and the percent remaining after completion are tabulated. The tests show that if coarse sand-sized particles of the composition presumably present on Mars are moved at the wind velocities given, almost complete destruction can occur in geologically insignificant time periods. Grain to rock collisions are not necessary for almost complete destruction; grain to grain collisions are sufficient.

Krinsley, D.↗

Surface-material maps of Viking landing sites on Mars

Researchers mapped the surface materials at the Viking landing sites on Mars to gain a better understanding of the materials and rock populations at the sites and to provide information for future exploration. The maps extent to about 9 m in front of each lander and are about 15 m wide - an area comparable to the area of a pixel in high resolution Viking Orbiter images. The maps are divided into the near and far fields. Data for the near fields are from 1/10 scale maps, umpublished maps, and lander images. Data for the far fields are from 1/20 scale contour maps, contoured lander camera mosaics, and lander images. Rocks are located on these maps using stereometric measurements and the contour maps. Frequency size distribution of rocks and the responses of soil-like materials to erosion by engine exhausts during landings are discussed.

Moore, H. J.↗

Environmental Durability Issues for Solar Power Systems in Low Earth Orbit

Space solar power systems for use in the low Earth orbit (LEO) environment experience a variety of harsh environmental conditions. Materials used for solar power generation in LEO need to be durable to environmental threats such as atomic oxygen, ultraviolet (UV) radiation, thermal cycling, and micrometeoroid and debris impact. Another threat to LEO solar power performance is due to contamination from other spacecraft components. This paper gives an overview of these LEO environmental issues as they relate to space solar power system materials. Issues addressed include atomic oxygen erosion of organic materials, atomic oxygen undercutting of protective coatings, UV darkening of ceramics, UV embrittlement of Teflon, effects of thermal cycling on organic composites, and contamination due to silicone and organic materials. Specific examples of samples from the Long Duration Exposure Facility (LDEF) and materials returned from the first servicing mission of the Hubble Space Telescope (HST) are presented. Issues concerning ground laboratory facilities which simulate the LEO environment are discussed along with ground-to-space correlation issues.

Degroh, Kim K.↗

Diagnostic Techniques Used to Study Chemical-Vapor-Deposited Diamond Films

The advantages and utility of chemical-vapor-deposited (CVD) diamond as an industrial ceramic can only be realized if the price and quality are right. Until recently, this technology was of interest only to the academic and basic research community. However, interest has grown because of advances made by leading CVD diamond suppliers: 1) Reduction of the cost of CVD polycrystalline diamond deposition below $5/carat ($8/sq cm); 2) Installation of production capacity; 3) Epitaxial growth of CVD single-crystal diamond. Thus, CVD diamond applications and business are an industrial reality. At present, CVD diamond is produced in the form of coatings or wafers. CVD diamond film technology offers a broader technological potential than do natural and high-pressure synthetic diamonds because size, geometry, and eventually cost will not be as limiting. Now that they are cost effective, diamond coatings - with their extreme properties - can be used in a variety of applications. Diamond coatings can improve many of the surface properties of engineering substrate materials, including erosion, corrosion, and wear resistance. Examples of actual and potential applications, from microelectromechanical systems to the wear parts of diamond coatings and related superhard coatings are described. For example, diamond coatings can be used as a chemical and mechanical barrier for the space shuttles check valves, particularly on the guide pins and seat assemblies.

Miyoshi, Kazuhisa↗

NASA Benefits Earth

This slide presentation reviews several ways in which NASA research has benefited Earth and made life on Earth better. These innovations include: solar panels, recycled pavement, thermometer pill, invisible braces for straightening teeth, LASIK, aerodynamic helmets and tires for bicycles, cataract detection, technology that was used to remove Anthrax spores from mail handling facilities, study of atomic oxygen erosion of materials has informed the restoration of artwork, macroencapsulation (a potential mechanism to deliver anti cancer drugs to specific sites), and research on a salmonella vaccine. With research on the International Space Station just beginning, there will be opportunities for entrepreneurs and other government agencies to access space for their research and development. As well as NASA continuing its own research on human health and technology development.

Robinson, Julie A.↗